Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Separate graphite by flotation
What ifWhat if froth flotation produced the graphite-rich feed for purification?
Claim language“leaching black mass”
An aerated flotation cell carries hydrophobic graphite particles into an overflow froth while most metal oxide particles remain in the pulp. A sedimentation thickener concentrates the collapsed froth into a wet graphite-rich feed.
1.2Prepare a dilute acid suspension
What ifWhat if water made up 70% of the total mixture by mass?
Claim language“20-30% water”
A baffled tank with an impeller disperses the residue in dilute sulfuric acid. The high liquid fraction keeps the solids suspended during heating and provides a liquid phase for dissolved impurity salts.
1.3Apply a thermal purification stage
What ifWhat if a dry furnace stage produced heat-treated graphite powder in place of a pugged residue?
Claim language“to obtain a pugged residue”
A dryer removes the liquid, and a mill breaks up the dried solids before they enter an inert-atmosphere graphite resistance furnace. Heating above 2,500 °C drives off volatile inorganic impurities, and a cooled exhaust trap collects condensable vapors.
1.4Cool to a warm setpoint
What ifWhat if the residue cooled to 60 °C before transfer to the reagent stage?
Claim language“at room temperature”
A jacketed screw cooler removes heat from the pugged solids as the screw conveys them toward the discharge. An outlet temperature sensor regulates coolant flow and holds the discharged solids at 60 °C.
1.5Percolate reagent through stationary solids
What ifWhat if reagent flowed through a stationary bed of cooled residue and the treated graphite was dispersed afterward?
Claim language“agitating the cooled residue”
A perforated support holds a shallow bed of granulated residue while a distributor applies dilute acid from above. The acid dissolves soluble impurities as it drains through the bed. Water entrains the treated solids during discharge and forms a slurry for recovery.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Graphite recovery from refractory machining fines
Screen machining fines from resin-bonded graphite refractories to remove coarse fragments, then leach the fines with hydrochloric acid to dissolve accessible magnesium and iron compounds. Mix the dewatered residue with sulfuric acid and water in a jacketed kneader and hold the paste at an elevated temperature. Cool the paste to room temperature and agitate it with water to dissolve soluble sulfates. Filter the slurry, wash the cake with water, and dry it to obtain a graphite-rich fraction.
Component substitution
Pressure filtration with membrane cake washing
Install a recessed-chamber membrane filter press in place of the slurry filter and connect its feed manifold to the agitated extraction tank. Pump slurry into the press and inflate the membranes to express liquid from the cake. Pass water through the cake using the wash manifold and collect the wash liquor separately from the initial filtrate. Squeeze the washed cake again, discharge it, and transfer it to a dryer.
Parameter or scale variation
Ten kilogram batch with dilute extraction
Charge 10 kg of residue on a dry-solids basis to a jacketed kneader and adjust the total water content to 25 mass percent of the paste, accounting for moisture in the incoming cake and acid. Hold the sulfuric acid paste at 90 °C for 60 minutes, then cool it to 20–25 °C. Meter the cooled paste into an agitated tank containing 100 L of water and mix for 45 minutes. Filter the slurry, wash the cake with water, and dry it at 105 °C to constant mass.
Combination with existing systems
Integration with hydroxide precipitation and clarification
Pipe the extraction filtrate and the first cake wash to an equalization tank upstream of a two-stage hydroxide precipitation system. Dose lime slurry in the first stage to precipitate iron and aluminum hydroxides, then remove the solids in a clarifier. Raise the pH of the clarified liquor in the second stage to precipitate dissolved nickel and cobalt, and dewater the resulting sludge in a separate filter press. Route the graphite cake from the extraction filter to a separate wash and drying line.
Automated or data-driven variant
Moisture feedback for paste preparation
Mount a microwave moisture sensor above the residue feed conveyor and use belt load cells to measure the wet feed rate. A programmable controller combines these readings with the acid feed rate and acid concentration to calculate the dry-solids flow and the water already entering the kneader. The controller meters supplemental water to reach a 25 mass percent water setpoint and adjusts the acid pump to maintain the specified acid dose per kilogram of dry residue. A temperature sensor starts the hold timer once the paste reaches the operating setpoint.
Conductivity control for cake washing
Install a temperature-compensated conductivity sensor in the common wash outlet of the filter press and a second sensor in the wash-water supply. A controller passes water through the cake in measured increments and records the difference between outlet and inlet conductivity after each increment. It ends the wash when the difference stays below a threshold calibrated against residual sulfate measurements for two successive increments. The controller then initiates cake dewatering and discharge to the dryer.
Specific version of a part
Leach with acid and peroxide
A stirred tank contacts black mass with aqueous sulfuric acid and metered hydrogen peroxide at 60 °C. The acid and peroxide promote dissolution of cathode metals, and solid-liquid separation recovers the graphite-rich residue.
Blend an acid and water paste
A jacketed twin-shaft mixer blends the leach residue with sulfuric acid and water. The batch mass balance includes moisture already present in the residue and sets total water at 25% of the mixture by mass.
Agitate with dilute hydrochloric acid
A baffled tank mixes the cooled residue with 0.5 mol/L hydrochloric acid at a ratio of 1 kg of dry solids to 10 L of solution. A pitched-blade impeller suspends the solids for 60 minutes while the acid dissolves acid-soluble impurities.
Wash cake in a filter press
A recessed-plate filter press captures graphite on polymer filter cloths. Deionized water flows through the cake until the wash effluent reaches a specified conductivity, and a vacuum tray dryer dries the discharged cake at 105 °C to constant mass.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(a) leaching black mass of spent lithium-ion batteries to obtain a leach residue;
The cast component is then exposed to a leaching solution and high pressure water wash to remove an internal core material and a portion of the VPC shell remainder from the cast component.
A · US 8,828,214 B2 · abstract
Tank and vat leaching both involve placing the ore, after size reduction and classification, into the tanks or vats at ambient operating conditions containing a leaching solution and allowing the valuable material to leach from the ore into solution.
B · US 2019/0060797 A1 · ¶ 5
1.2(b) mixing the leach residue of the spent lithium ion batteries obtained in step (a) with a suitable solvent and 20-30% water to obtain a mixture;
In tank leaching the ground, classified solids are already mixed with water to form the slurry, and this is pumped into the tanks.
B · US 2019/0060797 A1 · ¶ 5
1.3(c) keeping the mixture obtained in step (b) at a predetermined temperature for a pre-defined time to obtain a pugged residue;
1.4(d) cooling the pugged residue obtained in step (c) at room temperature;
1.5(e) agitating the cooled residue obtained in step (d) with a suitable reagent at a predetermined solid-liquid ratio for a pre-defined time to obtain a slurry; and
The submersion vessel is further adapted, in one embodiment, to contain the cast component and a second high agitation leaching solution for a period of approximately three days.
A · US 8,828,214 B2 · ¶ 37
1.6(f) filtering the slurry obtained in step (e) to obtain a residue followed by washing with water and drying the residue to get pure graphite.
According to a further aspect the present invention further provides a method of separating a liquid from particulate solids, comprising the steps of: i) providing an apparatus as described above for dewatering particulate solids, comprising: ii) introducing the particulate solids and liquid into the tank; iii) agitating the particulate solids and liquid to form a slurry; iv) ceasing the agitation to allow the slurry to settle, thereby forming a graded filter bed to drain liq
B · US 2019/0060797 A1 · ¶ 12
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.5. Only Document B has a passage for 1.21.6. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The tanks in the tank leaching method are typically equipped with agitators to keep the solids in suspension in the tanks and improve the solid to liquid to gas contact.
B · US 2019/0060797 A1 · ¶ 4
Related claim parts: 1.5
In a tank leach the slurry is agitated, while in a vat leach the solids remain stationary in the vat, and solution is moved, so typically the retention time required for vat leaching is more than that for tank leaching to achieve the same percentage of recovery of the valuable material being leached.
B · US 2019/0060797 A1 · ¶ 4
Related claim parts: 1.5
One significant complication in modern casting processes is the removal of the casting shell and core from the cast component.
A · US 8,828,214 B2 · ¶ 2
However, commercial component manufacturing requires that core and shell materials be removed as quickly and inexpensively as possible.
A · US 8,828,214 B2 · ¶ 2
The invention relates to methods and apparatus for liquid/solid separation for use in applications such as dewatering particulate solids, and recovery of valuable metals from ore in a leaching process.
B · US 2019/0060797 A1 · ¶ 2
Typical leaching methods have a number of drawbacks, in particular the need to either grind the ore finely for continuous agitation leaching or utilize batch leaching methods on coarser material.
B · US 2019/0060797 A1 · ¶ 3
Cite aspatent.fyi, US 2026/0365520 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365520/, SHA-256 563952308a4117b48d73c9a9c4375c5f39eb4808b7730cf9cd4150b0a6ff7e6c