Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Phosphate coated fine particles
What ifWhat if the first group uses fluorine-free lithium cobalt oxide particles with a lithium phosphate surface coating?
Claim language“lithium, cobalt, nickel, aluminum, magnesium, oxygen, and fluorine”
The fine particles contain nickel, aluminum, and magnesium in the oxide and have a D50 of 3 μm. A wet coating step deposits a lithium phosphate precursor on the particles, and a heat treatment forms a lithium phosphate surface layer.
1.1Electrical sensing of particle size
What ifWhat if the first group is sized by electrical sensing through an aperture?
Claim language“a laser diffraction and scattering method”
A dilute suspension passes through an aperture in a conductive liquid, and each particle displaces liquid and produces a resistance pulse proportional to its volume. The instrument converts the pulses to sphere diameters and reports the diameter at 50% of cumulative particle volume.
1.2Lower coarse particle median
What ifWhat if the second group has a D50 of 7 μm?
Claim language“9 μm and shorter than or equal to 25 μm”
An air classifier collects a fraction centered at 7 μm, and laser diffraction verifies its D50. A first group centered at 3 μm supplies smaller particles that occupy some of the interparticle spaces in the blend.
1.3Sequential coating of particle layers
What ifWhat if each particle group is deposited as a separate layer on the same current collector?
Claim language“mixing the first group of particles and the second group of particles”
Separate slurries contain the coarse or fine particles with conductive carbon and binder. The coarse slurry is coated and dried on aluminum foil, and the fine slurry is deposited on top and dried before the electrode is compacted.
1.4Higher fine particle loading
What ifWhat if the first group makes up 40 weight % of the combined particles?
Claim language“5 weight % and less than or equal to 30 weight %”
Gravimetric feeders meter 40 parts fine powder and 60 parts coarse powder into a mixer. The resulting blend is dispersed with conductive carbon and binder, then coated and compacted on aluminum foil.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Bimodal cathodes for hearing aid cells
A rechargeable hearing aid button cell uses a lithium cobalt oxide positive electrode with nickel, aluminum, magnesium, and fluorine in both particle fractions. The fine fraction has a D50 of 3 μm and accounts for 15 weight percent of the active powder, while the coarse fraction has a D50 of 12 μm. The blended powder is mixed with conductive carbon and binder, coated on aluminum foil, dried, and punched into discs for assembly with a graphite negative electrode and a porous separator.
Component substitution
Electrical sensing for particle size measurement
An electrical sensing zone instrument measures the particle size distribution of the fine and coarse fractions before blending. Each powder sample is dispersed in a compatible conductive electrolyte and measured through an aperture selected for its size range. The instrument converts pulse amplitudes to displaced volumes and computes the volume median diameter for each fraction. A mixer combines measured lots with median diameters of 2–4 μm and 9–25 μm at a fine fraction of 15 weight percent.
Fine powder from spray pyrolysis
An ultrasonic atomizer feeds an aqueous solution of lithium, cobalt, nickel, aluminum, and magnesium salts into a heated air reactor. The droplets dry and decompose into oxide precursor particles, which a filter collects for a subsequent firing step that forms crystalline lithium cobalt oxide. The fired powder receives an ammonium fluoride treatment followed by heating, and laser diffraction verifies a D50 of 2–4 μm after classification. A dry mixer combines 15 weight percent of this powder with a separately formed 9–25 μm D50 fraction containing the same elements.
Parameter or scale variation
Blend with one micrometer fines
Two separately formed lithium cobalt oxide powders each contain nickel, aluminum, magnesium, and fluorine. An air classifier trims the fine powder to a D50 of 0.8–1.2 μm, and a separate classifier trims the coarse powder to a D50 of 14–18 μm, as measured by laser diffraction. A tumble mixer combines 0.8 kg of fine powder with 9.2 kg of coarse powder to produce a 10 kg batch.
Combination with existing systems
Inline blending for continuous electrode coating
Two loss-in-weight feeders meter the fine and coarse active powders into a continuous paddle mixer at 3 and 17 kg/h, respectively. The mixer discharges into a continuous twin-screw slurry mixer, which receives conductive carbon, binder solution, and solvent through separate feed ports. The slurry passes through a vacuum deaerator and is pumped to a slot die that coats moving aluminum foil before oven drying.
Automated or data-driven variant
Feedback control of powder classification
Two air classifiers prepare fine and coarse fractions from separately formed powders containing lithium, cobalt, nickel, aluminum, magnesium, oxygen, and fluorine. An automated sampler directs material from each classifier outlet to a laser diffraction analyzer using the same dispersion procedure for all samples. A controller adjusts each classifier rotor speed from the measured D50 error relative to its setpoint of 3 μm or 16 μm. Diverter valves route material to the blend hoppers when its D50 is within 0.3 μm of the fine setpoint or 1 μm of the coarse setpoint.
Specific version of a part
Classified three micrometer fraction
A jet mill deagglomerates fired lithium cobalt oxide powder containing nickel, aluminum, magnesium, and fluorine. An air classifier collects the fine fraction, and wet laser diffraction verifies a D50 of 3 μm after dispersion.
Spray dried coarse granules
A spray dryer granulates a suspension of lithium cobalt oxide containing nickel, aluminum, and magnesium, together with a lithium fluoride source. Heat treatment consolidates the granules, and laser diffraction verifies a D50 of 15 μm for the classified coarse fraction.
Low shear drum blending
A rotating drum repeatedly lifts and drops the two dry powder fractions to distribute the fine particles throughout the coarse fraction. Samples from different parts of the discharge are checked by laser diffraction for consistent contributions from the two size populations.
Fifteen percent fine fraction
A batch scale meters 15 kg of the first group and 85 kg of the second group on a dry powder basis. The first group accounts for 15 weight % of the combined active material before binder and conductive carbon are added.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1forming a first group of particles comprising lithium, cobalt, nickel, aluminum, magnesium, oxygen, and fluorine, the first group of particles having D50 of longer than or equal to 2 μm and shorter than or equal to 4 μm when particle size distribution is measured by a laser diffraction and scattering method;
The seventh embodiment of the present invention provides non-agglomerated spherical magnesium-containing microparticles that contain magnesium atom, aluminum atom, and alkoxy group having 1 to 20 carbon atoms, are insoluble in hydrocarbon solvents, and have a median diameter (d50) measured by laser diffraction scattering of 0.1 μm≦d50≦5 μm and a variation coefficient (Cv) of particle diameter of 20% or less.
A · US 7,601,423 B2 · ¶ 36
1.2forming a second group of particles comprising lithium, cobalt, nickel, aluminum, magnesium, oxygen, and fluorine, the second group of particles having D50 of longer than or equal to 9 μm and shorter than or equal to 25 μm when particle size distribution is measured by a laser diffraction and scattering method; and
The median diameter (d50) of produced polymer was 9.4 μm, and the Cv value was 13.9%. 100% of the particles passed through a 37-μm mesh screen.
A · US 7,601,423 B2 · ¶ 346
1.3forming a group of particles by mixing the first group of particles and the second group of particles,
In Example 1, a joining material paste was produced by mixing a first metal powder, a second metal powder, and a flux together.
B · US 2019/0001444 A1 · ¶ 73
1.4wherein a proportion of the first group of particles in the group of particles is greater than or equal to 5 weight % and less than or equal to 30 weight %.
In the joining material of the present invention, it is preferred that a proportion of the second metal powder to a weight of the first metal powder be 5 wt % or less.
B · US 2019/0001444 A1 · ¶ 15
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.11.2. Only Document B has a passage for 1.31.4.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
In more detail, it relates to ethylene-based polymer microparticles and functional group-containing ethylene-based polymer microparticles in which the particle diameter is smaller than those of conventional polyethylene fine-particles, microparticles do not agglomerate each other, the particle size distribution is extremely narrow, and the sphericity is high.
A · US 7,601,423 B2 · ¶ 1
Commonly to these uses as novel high-performance materials, for further functionalization and improvement in performances and quality, there is a demand for polyethylene-based spherical ultra-fine particles with smaller particle diameter and narrower particle size distribution free from inter-particle agglomeration.
A · US 7,601,423 B2 · ¶ 6
When such soldering material is cooled from a melted state and solidified, a crack is sometimes generated in a joined portion.
B · US 2019/0001444 A1 · ¶ 7
According to Patent Document 2, it is possible to prevent a propagation of a crack by micronizing crystal structure of Sn.
B · US 2019/0001444 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365531 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365531/, SHA-256 08e236ebcc068ae2f5329fee45496536644733dedf40f7dd6eaa6af99fcb290e