Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Mixing with hydrochloric acid
What ifWhat if the mineral is mixed with hydrochloric acid to produce a lithium chloride liquor?
Claim language“with nitric acid”
A jacketed, acid-resistant stirred tank contacts finely ground, acid-leachable sedimentary silicate with aqueous hydrochloric acid. After removal of insoluble solids and dissolved impurities, sodium carbonate precipitates lithium carbonate from the lithium chloride liquor and leaves sodium chloride in the mother liquor.
1.2Sulfate roasting and water leaching
What ifWhat if a sulfate roast converts mineral-bound lithium to a water-soluble sulfate before leaching?
Claim language“is leached as lithium nitrate”
An oxidizing kiln roasts ground lithium-bearing clay with gypsum and limestone to convert mineral-bound lithium to lithium sulfate. Water dissolves the lithium sulfate from the cooled calcine, and sodium carbonate precipitates lithium carbonate from the clarified and purified leach liquor.
1.3Lithium capture within the slurry
What ifWhat if screened ion exchange beads remove dissolved lithium directly from the leach slurry?
Claim language“separating the solution comprising lithium nitrate from a residue of insoluble solids”
After adjustment to the sorbent's operating pH, a stirred tank contacts the unclarified slurry with coarse beads containing a lithium-selective inorganic sorbent. A screen retains the loaded beads while the fine mineral residue and spent liquor pass together. A separate elution vessel strips lithium from the washed beads with dilute nitric acid to produce a lithium nitrate liquor.
1.4Carbonation with ammonium carbonate
What ifWhat if ammonium carbonate supplies the carbonate for lithium carbonate precipitation?
Claim language“adding sodium carbonate”
A stirred crystallizer doses aqueous ammonium carbonate into purified, concentrated lithium nitrate liquor and maintains an alkaline pH to supply carbonate ions. Lithium carbonate crystallizes, and filtration separates the crystals from an ammonium nitrate mother liquor.
1.7Dosing dissolved ammonium bicarbonate
What ifWhat if an aqueous ammonium bicarbonate feed supplies bicarbonate to the sodium nitrate liquor?
Claim language“with carbon dioxide”
A metering pump feeds concentrated ammonium bicarbonate solution into an agitated vessel containing the concentrated sodium nitrate stream. Cooling and seeding crystallize sodium bicarbonate, and filtration recovers the crystals from the ammonium nitrate mother liquor.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Lithium recovery from glass manufacturing scrap
A glass finishing line collects offcuts from lithium silicate glass before lamination or coating. A mill grinds the offcuts, and an agitated nitric acid leach transfers lithium into solution as lithium nitrate. A filter removes the silica-rich residue, and a stirred vessel precipitates lithium carbonate from the filtrate with sodium carbonate. A filter recovers the carbonate, and the sodium nitrate filtrate passes through ammonia dissolution and carbon dioxide contacting.
Component substitution
Potassium carbonate as the precipitation reagent
An aqueous potassium carbonate feed replaces sodium carbonate in the stirred lithium precipitation vessel. A filter collects the lithium carbonate and sends the potassium nitrate filtrate to an ammonia dissolution vessel. A separate gas contactor mixes the ammoniated filtrate with carbon dioxide to form a solution containing potassium bicarbonate and ammonium nitrate.
Parameter or scale variation
Two-stage hot lithium carbonate precipitation
Two jacketed stirred tanks in series hold the clarified lithium nitrate liquor at 85 to 90 °C with a nominal liquid residence time of 30 minutes per tank. The first tank receives 70% of the sodium carbonate dose, and the second receives the remaining 30%. The total dose supplies 1.05 moles of carbonate per 2 moles of dissolved lithium. A heated filter collects the lithium carbonate, and the cooled filtrate feeds the ammonia and carbon dioxide stages.
Combination with existing systems
Nitric acid recovery with membrane electrodialysis
A polishing filter and a cation exchange bed remove suspended solids and residual divalent ions from a sodium nitrate filtrate sidestream upstream of ammonia addition. A bipolar membrane electrodialysis stack converts the polished sodium nitrate into separate nitric acid and sodium hydroxide streams. The nitric acid returns to the mineral leach, and a carbon dioxide contactor converts the sodium hydroxide into sodium carbonate for lithium precipitation. The rest of the sodium nitrate filtrate feeds the ammonia and carbon dioxide stages.
Countercurrent washing of insoluble leach residue
A primary thickener receives the nitric acid leach slurry and sends its lithium nitrate overflow through a polishing filter to carbonate precipitation. The thickener underflow passes through two countercurrent wash thickeners, with fresh water entering the second washer and its overflow feeding the first washer. The first washer returns its lithium-bearing overflow to the primary thickener feed, and the final washed residue goes to a filter press. The lithium carbonate filter sends its separate sodium nitrate filtrate to ammonia dissolution and carbon dioxide contacting.
Automated or data-driven variant
Analyzer-controlled carbonate dosing and slurry recycle
An automated sampler filters and dilutes clarified leach liquor for lithium measurement by flame emission, while a flowmeter measures the liquor feed rate. A controller calculates the sodium carbonate feed from the measured lithium flow and trims the metering pump using dissolved lithium readings from a filtered crystallizer outlet sample. An inline slurry density meter adjusts a recycle pump that returns part of the crystallizer underflow as seed. A product filter separates the remaining slurry and sends its sodium nitrate filtrate to ammonia dissolution and carbon dioxide contacting.
Specific version of a part
Metered acid addition under agitation
A glass-lined baffled tank suspends ground mineral in water with an axial-flow impeller. A metering pump adds nitric acid below the liquid surface, and a cooling jacket removes heat during mixing.
Pressure filtration with cake washing
A recessed-plate filter press passes lithium nitrate liquor through acid-resistant cloth and retains the insoluble mineral residue in the plate chambers. A displacement wash recovers lithium nitrate held in the cake pores, and the wash liquor joins the primary filtrate.
Hot centrifugal crystal separation
A perforated-basket centrifuge separates lithium carbonate crystals from hot sodium nitrate mother liquor. A short wash with hot water displaces residual mother liquor while limiting dissolution of the lithium carbonate.
Ammonia absorption in a packed column
A cooled packed column passes sodium nitrate liquor downward over inert packing as ammonia gas flows upward. The packing provides gas–liquid contact area, and a slipstream pH measurement controls the ammonia feed.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1i. mixing the mineral comprising lithium with nitric acid, forming a mixture;
The process comprises mixing the silicate mineral with nitric acid.
B · US 10,131,968 B2 · abstract
1.2ii. subjecting the mixture to a leaching process in which lithium in the mineral comprising lithium is leached as lithium nitrate and a solution comprising lithium nitrate is formed;
The process as disclosed herein can comprise subjecting the mixture of silicate mineral with nitric acid to a leaching process. The leaching process can take place in one or more stages, and may be conducted under conditions such that lithium values in the silicate mineral are leached into an aqueous phase as lithium nitrates.
B · US 10,131,968 B2 · ¶ 17
1.3iii. separating the solution comprising lithium nitrate from a residue of insoluble solids;
The pulp 4 formed is then subjected to a solid/liquid separation method 5 such as thickening and filtration in order to obtain a brine depleted in magnesium 7; as well as depleted in salts Mg(OH)2 and CaSO4.2H2O 6.
A · US 8,691,169 B2 · ¶ 28
In one variation (described in detail below with reference to FIG. 4), where a primary solids-liquids separation sub-stage has been employed, and prior to a final filtration stage, any remaining solids residue in the process solution/slurry can first be subjected to a clarification stage (e.g. in one or more settling vessels). This can ensure that the resultant clarified liquor that is passed onto subsequent stages of the process is essentially free of solids residue.
B · US 10,131,968 B2 · ¶ 116
1.4iv. adding sodium carbonate to the solution comprising lithium nitrate, such that lithium carbonate precipitates therefrom to form a lithium carbonate precipitate in a solution comprising sodium nitrate;
The resultant brine is then further purified by reaction with an aqueous solution of sodium carbonate, also known as soda ash (Na2CO3) at 80 to 100° C. in order to precipitate the lithium carbonate.
A · US 8,691,169 B2 · ¶ 18
In one embodiment, sodium carbonate (i.e. soda ash) can be employed. As is known, the soda ash causes the lithium values to precipitate as sparingly soluble lithium carbonate, leaving additional sodium/potassium nitrate in solution.
B · US 10,131,968 B2 · ¶ 52
1.5v. separating the lithium carbonate precipitate from the solution comprising sodium nitrate;
The resultant brine is then further purified by reaction with an aqueous solution of sodium carbonate, also known as soda ash (Na2CO3) at 80 to 100° C. in order to precipitate the lithium carbonate. After washing and filtering the lithium carbonate cake, said cake is re-dissolved in cold water saturated with CO2 containing carbonic acid which reacts with the lithium carbonate to produce soluble bicarbonate of lithium.
A · US 8,691,169 B2 · ¶ 18
The lithium carbonate precipitate can be removed by conventional solids-liquids separation processes, such as by vacuum filtration and washing with hot water.
B · US 10,131,968 B2 · ¶ 162
1.6vi. mixing the solution comprising sodium nitrate with ammonia such that the ammonia dissolves therein;
In this embodiment the ammonium carbonate may be made by using an aqueous ammonia solution (ammonia can be used elsewhere in the process) to scrub a portion of the flue gases from the lithium silicate mineral concentrates calcination reactor.
B · US 10,131,968 B2 · ¶ 55
1.7vii. mixing the resultant solution from vi. with carbon dioxide;
The lithium carbonate cake 5 is then added to reactor 2 which is a conventional reactor having a conventional stirrer 3, and in which carbon dioxide 6 is injected at a pressure of 1 to 5 atmospheres through the use of a conventional diffuser 26, such as a perforated plate or a porous plate, for a reaction time from 1 to 120 minutes so that the carbon dioxide becomes dissolved and forms carbonic acid which continues to react with the dissolved lithium carbonate to form bicarbo
A · US 8,691,169 B2 · ¶ 40
1.8viii. subjecting the solution from vii. to reaction conditions such that a solution comprising sodium bicarbonate and ammonium nitrate is formed.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.7. Only Document B has a passage for 1.11.21.6. Both have a passage for 1.31.41.5. Both are classified in CPC C22B.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Spodumene is a pyroxene (double aluminum and lithium silicate) and has been an important source material in the production of different lithium compounds and is the principle lithium mineral exported at present.
A · US 8,691,169 B2 · ¶ 6
Related claim parts: 1.11.2
The main chemical consumed in the process can be carbon dioxide that is recovered from flue gas streams, including any that arise from process equipment used elsewhere in the process of converting lithium silicate minerals to products in demand by users of lithium chemicals (in particular lithium carbonate and lithium hydroxide).
B · US 10,131,968 B2 · ¶ 2
Related claim parts: 1.7
The present invention relates to a process that produces battery grade highly purified lithium carbonate from naturally occurring or industrial brines.
A · US 8,691,169 B2 · ¶ 1
Generally, chloride brines contain significant quantities of magnesium that has to be removed before the lithium is precipitated.
A · US 8,691,169 B2 · ¶ 8
A process, system and apparatus are disclosed for the recovery of lithium from silicate minerals that include lithium, including hard-rock minerals, and clay and micaceous minerals.
B · US 10,131,968 B2 · ¶ 2
However, until recently, there was little interest in exploring for hard-rock lithium mineral deposits, firstly because perceptions have been that there was an abundance of lithium in the salars of the Lithium Triangle; and, secondly, because current hard-rock lithium ore refining processes (largely unchanged since before World War II) are expensive, complicated, hazardous and environmentally challenging.
B · US 10,131,968 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0365532 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365532/, SHA-256 63dc4e7f474365582eb665bc6b6b808c6f0f160773e0f0dd6cc5ccfbb6576f49