patent.fyi
Applications  /  US 2026/0365533
United States Patent Application Publication

US 2026/0365533 A1

Published
Nov 19, 2026
Filed
Nov 28, 2023
Earliest date on the face
Nov 28, 2022
Classification
C01F 11/181
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Soluble calcium salt feed

What ifWhat if calcium chloride solution supplies the calcium ions?
Claim language“an alkaline calcium source”

Dissolve calcium chloride and glycine in water. Feed the solution and an aqueous sodium carbonate stream into a stirred vessel to generate supersaturation and precipitate vaterite.

1.1Supersaturation through rapid mixing

What ifWhat if rapid mixing controls initial precipitation without a separate additive in the calcium feed?
Claim language“with an additive”

Feed aqueous calcium chloride and sodium carbonate into an impinging-jet mixer at room temperature. Rapid mixing creates high supersaturation that favors vaterite formation, and prompt filtration limits conversion to calcite in the mother liquor.

1.2Dissolved carbonate ion feed

What ifWhat if a sodium carbonate solution supplies carbonate ions directly to the precipitation reactor?
Claim language“with a CO2 source”

Meter sodium carbonate solution and calcium chloride solution into a stirred tank. Mix rapidly to reach high calcium carbonate supersaturation, then separate the vaterite-rich precipitate from the sodium chloride liquor.

1.3Stabilization by drying

What ifWhat if removing the mother liquor and drying the powder preserve the vaterite during storage?
Claim language“adding a stabilizing agent”

Recover the vaterite-rich solid by vacuum filtration immediately after precipitation and dry the cake under reduced pressure. Store the powder in a sealed dry container to suppress the dissolution and reprecipitation that drive conversion to calcite.

1.3Polymer present before precipitation

What ifWhat if the stabilizing polymer enters the calcium slurry before carbonation begins?
Claim language“to the solid CaCO3 product of step (ii)”

Disperse sodium carboxymethyl cellulose in the aqueous calcium hydroxide slurry before introducing carbon dioxide. The dissolved polymer adsorbs onto calcium carbonate particles as they form and slows their conversion from vaterite to calcite in the slurry.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Vaterite pigment for paper coating

A stirred vessel combines calcium hydroxide and magnesium hydroxide in water. A sparger feeds carbon dioxide into the slurry to precipitate calcium carbonate containing vaterite. A metering pump adds sodium polyacrylate to the wet precipitate after carbonation. A mixer blends the pigment slurry with cooked starch, and a blade coater applies the mixture to paper.

Component substitution

Ethanol as the carbonation additive

Ethanol replaces magnesium hydroxide as the additive in a stirred calcium hydroxide suspension containing 30 percent ethanol by volume in the liquid phase. A submerged sparger feeds carbon dioxide into the suspension to precipitate calcium carbonate containing vaterite. A filter collects the wet solids, which are resuspended in water and treated with sodium polyacrylate. A distillation unit recovers ethanol from the filtrate for reuse in slurry preparation.

Parameter or scale variation

Staged carbonation in two stirred tanks

Two 10 L working-volume stirred tanks in series receive 1 L/min of aqueous calcium hydroxide slurry premixed with magnesium hydroxide. Separate spargers feed carbon dioxide to both tanks, with the gas flow adjusted to hold the first tank at pH 10.5 and the second at pH 9.0. Each tank provides a nominal liquid residence time of 10 minutes. A static mixer blends aqueous sodium polyacrylate into the vaterite-containing slurry downstream of the second tank.

Combination with existing systems

Carbonation supplied by digester gas upgrading

A membrane system separates methane from digester gas and supplies a carbon dioxide-rich stream. A condensate separator and a sulfur removal bed condition the stream before a blower feeds it to the carbonation vessel. The gas enters through a submerged sparger and reacts with an agitated slurry of calcium hydroxide and magnesium hydroxide to form calcium carbonate containing vaterite. A separate stirred tank receives the precipitate slurry and mixes in sodium polyacrylate.

Wet stabilization on a vacuum belt

A stirred tank carbonates an aqueous mixture of calcium hydroxide and magnesium hydroxide and discharges the vaterite-containing slurry onto a continuous vacuum belt filter. The first vacuum zone removes bulk liquid, and a spray bar in the next zone distributes aqueous sodium polyacrylate over the wet cake. Suction draws the stabilizer solution through the cake, and a final vacuum zone removes excess liquid. A discharge scraper transfers the treated solids to an enclosed hopper.

Automated or data-driven variant

Raman control of the carbonation endpoint

A stirred batch reactor combines calcium hydroxide and magnesium hydroxide in water and receives carbon dioxide through a mass-flow controller. An immersion Raman probe measures spectra during carbonation, and software fits the carbonate bands using reference spectra for vaterite, calcite and aragonite. The controller closes the gas valve when the estimated vaterite fraction and the slurry pH enter their programmed endpoint bands. The controller then starts a metering pump that doses sodium polyacrylate into the wet solids while agitation continues.

Specific version of a part

Amorphous carbonate followed by crystallization

Combine cooled calcium chloride and sodium carbonate solutions and promptly recover the amorphous precipitate by centrifugation. Redisperse the wet solid in water, monitor crystallization by powder X-ray diffraction, and isolate the powder when vaterite is the dominant crystalline phase.

Glycine in lime slurry

Prepare an aqueous suspension of finely powdered calcium hydroxide and dissolve glycine in the liquid phase under agitation. Keep the calcium hydroxide suspended while transferring the mixture to the carbonation vessel.

Carbon dioxide through a sparger

Feed a carbon dioxide and nitrogen mixture through a porous sparger below the impeller in a stirred calcium hydroxide slurry. Track pH during gas addition and use powder X-ray diffraction to verify vaterite in the recovered precipitate.

Carbonation in a recirculation loop

Pump the calcium hydroxide slurry through a venturi that draws carbon dioxide into the recirculation line. Return the gas and slurry to the vessel for continued absorption, then filter the suspension at the pH endpoint established for vaterite formation.

Polymer addition after carbonation

Meter an aqueous sodium polyacrylate solution into the stirred suspension immediately after carbonation. The polymer adsorbs onto the vaterite particle surfaces and slows conversion to calcite during wet handling.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2013/0192783 A1
Published
Aug 1, 2013
Filed
Mar 14, 2013
Class
D21H 17/66
Document BUS 2019/0002301 A1
Published
Jan 3, 2019
Filed
Sep 6, 2018
Class
C01F 11/02
Claim 1
Document A
Document B
1.1(i) combining an alkaline calcium source with an additive to form a reactant mixture;
Unfortunately, these additives are in many cases undesirable for the end user as they result in the addition of an “impurity” in the milk of lime and therefore in the process of the end user or in the finished product, not to mention that sometimes an active interference between the dispersant and the process or the final application has to be reckoned with, mainly because of the nature of the active surface of the majority of these additives.
B · US 2019/0002301 A1 · ¶ 36
1.2(ii) carbonating the reactant mixture with a CO2 source to form a solid CaCO3 product comprising vaterite; and
In some embodiments, there is provided a method for producing a paper product, the method comprising a) contacting CO2 with a solution comprising proton removing agent, alkaline earth-metal ions, and pulp under one or more precipitation conditions to make the carbonate additive comprising reactive vaterite in situ; b) transforming the reactive vaterite to aragonite in situ, and c) forming a paper product.
A · US 2013/0192783 A1 · ¶ 5
This slaked lime may also contain calcium oxide that would not have been hydrated during slaking, just as it may contain calcium carbonate CaCO3. The calcium carbonate may be from either the initial limestone from which the slaked lime is derived according to the invention (unburnt), or from a reaction of partial carbonation of the slaked lime in contact with air.
B · US 2019/0002301 A1 · ¶ 6
1.3(iii) adding a stabilizing agent to the solid CaCO3 product of step (ii) thereby producing the stabilized vaterite.
In some embodiments of the foregoing aspect and embodiments, the method further comprises contacting a stabilizer with the water comprising alkaline earth-metal ions wherein the stabilizer stabilizes the reactive vaterite.
A · US 2013/0192783 A1 · ¶ 5

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.3. Only Document B has a passage for 1.1. Both have a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

There exists a need for making environmentally safe products that sequester CO2.
A · US 2013/0192783 A1 · ¶ 2
In some embodiments of the foregoing aspect and embodiments, the composition is for a paper product; polymeric product; lubricant; adhesive; rubber; chalk; asphalt product; paint; abrasive for paint removal; personal care product; cosmetic; cleaning product; personal hygiene product; ingestible product; agricultural product; environmental remediation product; or combinations thereof.
A · US 2013/0192783 A1 · ¶ 3
The factors limiting the use of milk of lime in comparison with other potential reactants are generally linked to its viscosity and its rate of reaction or neutralisation in the reaction medium of the application.
B · US 2019/0002301 A1 · ¶ 8
Also, a process for converting gypsum into precipitated calcium carbonate including providing a mixture comprising i) gypsum ii) a seed, a mineral acid, or both iii) at least one additive selected from the group consisting of ammonium sulfate, an organic acid, or an iron material, and reacting the mixture with at least one carbonate source to produce precipitated calcium carbonate in the form of vaterite.
C · US 2018/0265370 A1 · abstract

Related claim parts: 1.3

Document C: US 2018/0265370 A1, published Sep 20, 2018. Cited for this statement only.

Cite aspatent.fyi, US 2026/0365533 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365533/, SHA-256 0fe0819c277fc0def2460e4540f4c354de353b7c6f0beb759d2b9549a803493c
First published
Permanent addresshttps://patent.fyi/US20260365533/
Content fingerprint (SHA-256)0fe0819c277fc0def2460e4540f4c354de353b7c6f0beb759d2b9549a803493c
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi