Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Coarser sol for polishing
What ifWhat if the sol uses a particle diameter D50 of 75 nm?
Claim language“5 nm or more and less than 50 nm”
An aqueous dispersion of zirconia particles with a D50 of 75 nm feeds the contact between a polishing pad and a workpiece. An adsorbed polyacrylate dispersant limits aggregation, and the pad carries the particles across the surface for abrasive removal.
1.1Sub-five-nanometer film particles
What ifWhat if the sol uses a particle diameter D50 of 3 nm?
Claim language“5 nm or more and less than 50 nm”
A carboxylate-stabilized dispersion delivers zirconia particles with a D50 of 3 nm by spin coating. Solvent evaporation packs the particles into a thin layer, and firing removes the stabilizer and consolidates the oxide.
1.2Rounded particles for coating
What ifWhat if X is 10% or less?
Claim language“40% or more”
Hydrothermal growth produces predominantly rounded zirconia particles, and transmission electron microscopy confirms that at most 10% of the isolated particles reach the circle diameter ratio of 2.0. The rounded particles disperse in water and deposit as a particulate coating during solvent evaporation.
1.2Projected aspect ratio percentile
What ifWhat if particle shape is specified by the 90th percentile of fitted ellipse aspect ratios?
Claim language“a proportion X attained by the following procedure”
Image analysis software segments isolated particles in transmission electron micrographs and fits an ellipse to each projected silhouette. The software divides the major axis length by the minor axis length and reports the 90th percentile across 100 particles.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Zirconia wear coatings for glass
An aqueous zirconia sol with D50 from 5 nm to below 50 nm and X of at least 40% supplies the ceramic phase of a wear coating for glass. A wire-wound coating rod spreads the sol over cleaned glass in a uniform wet layer. Drying removes water, and firing consolidates the zirconia particles into a ceramic film.
Component substitution
Scanning transmission imaging for particle outlines
A scanning transmission electron microscope with a high-angle annular dark-field detector replaces conventional bright-field transmission imaging. A rastered electron probe records zirconia particles on a thin carbon support, and the resulting intensity map supplies outlines for at least 20 isolated particles. For each outline, the minimum enclosing circle sets the center, and the shortest distance from that center to the outline sets the inscribed radius. X is the percentage of isolated particles whose enclosing diameter is at least twice their inscribed diameter.
Parameter or scale variation
Narrower size band with larger sampling
The zirconia sol has a D50 of 12 to 20 nm, and the image analysis uses 200 isolated particles sampled across at least 10 nonoverlapping fields. Each particle contributes one ratio between its minimum enclosing diameter and its concentric inscribed diameter. The counts from all fields are pooled, and 100 or more ratios of at least 2.0 give an X of at least 50%.
Combination with existing systems
Crossflow concentration of zirconia sol
A stirred feed vessel, a recirculation pump, and a crossflow ultrafiltration module form a loop that returns retentate to the vessel. The membrane retains zirconia particles while water and dissolved ions exit through the permeate line. Concentration ends when the retentate reaches the target solids content. Particle sizing and transmission electron micrographs of the feed and retentate track changes in D50 and X during concentration.
Zirconia top layers on ceramic membranes
A dip coater deposits an aqueous zirconia sol onto the fine-pored intermediate layer of a porous alumina membrane. The feed sol has a D50 from 5 nm to below 50 nm and an X of at least 40%, measured before coating. A constant withdrawal speed meters the wet film, followed by controlled drying and firing to form a porous zirconia separation layer. The finished membrane operates with a pressure difference across the support to drive liquid through the zirconia layer.
Automated or data-driven variant
Automated measurement from particle masks
A trained instance segmentation model converts transmission electron micrographs into individual particle masks, and software filters masks that touch another mask or the image border. A minimum enclosing circle algorithm sets the center and outer diameter for each remaining mask. The software measures the shortest distance from that center to the mask boundary and assigns an inscribed diameter of zero when the center lies outside the mask. With at least 20 isolated masks, the software reports the percentage for which the enclosing diameter is at least twice the inscribed diameter.
Specific version of a part
Sol with 12 nm median
Controlled hydrolysis of zirconium propoxide followed by hydrothermal aging produces zirconia nanoparticles with a D50 of 12 nm. Ultrafiltration removes soluble reaction residues while retaining the dispersed oxide particles.
Sol with 35 nm median
Seeded hydrothermal growth deposits zirconia onto preformed zirconia particles until the dispersion reaches a D50 of 35 nm. The cooled dispersion passes through an ultrafiltration membrane for washing and concentration.
Sol with sixty percent X
A sol contains elongated zirconia particles, and a transmission electron micrograph contains 50 isolated particle projections. For each projection, the analysis divides the circumscribed circle diameter by the diameter of the largest inscribed circle with the same center. Thirty projections have a ratio of at least 2.0, giving X of 60%.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a particle diameter D50 is within a range of 5 nm or more and less than 50 nm, and
Regarding the inorganic raw materials, the talc, preferably platy (i.e., having a platelet particle morphology), has a median particle size of between 5 and 35 μm, the silica has a median particle size of between 1 and 35 μm, and the alumina source has a median particle size of between 1 and 18 μm.
A · US 7,494,613 B2 · ¶ 23
From the viewpoint of handling properties and insulating properties, the volume median particle diameter (D50) of the particles (B) is preferably in a range of 5 nm to 28 nm, more preferably in a range of 10 nm to 26 nm, still more preferably in a range of 12.5 nm to 24 nm, and still more preferably in a range of 15 nm to 22 nm.
B · US 2015/0228414 A1 · ¶ 42
1.2a proportion X attained by the following procedure is 40% or more:
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention relates to diesel particulate filters, and in particular to cordierite wall-flow diesel particulate filters having high filtration efficiency, high strength and low pressure drops for catalyzed and uncatalyzed applications.
A · US 7,494,613 B2 · ¶ 2
A high-porosity cordierite DPF that provides a lower pressure drop in both the catalyzed and uncatalyzed state relative to filters that have been previously demonstrated, while maintaining high filtration efficiency and sufficient mechanical strength, would be an advancement in the art.
A · US 7,494,613 B2 · ¶ 8
In a case in which the porous light reflective layer and the porous insulation layer are provided as described above, the gap between the conductive layer and the power generation layer becomes long, and thus the diffusion resistance of an electrolyte increases and there are cases in which the photoelectric conversion efficiency decreases.
B · US 2015/0228414 A1 · ¶ 7
The present invention has been made in consideration of the problems of the related art, and provides dye-sensitized solar cell paste which has both high light reflectivity and excellent insulation properties and is capable of improving the photoelectric conversion efficiency, a porous light reflective insulation layer obtained by firing the same, and a dye-sensitized solar cell.
B · US 2015/0228414 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365534 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365534/, SHA-256 1e253989262f7d7d837fcbf1d439501c73e8856143aa20df6171829ac8228a1c