patent.fyi
Applications  /  US 2026/0365539
United States Patent Application Publication

US 2026/0365539 A1

Published
Nov 19, 2026
Filed
May 14, 2025
Earliest date on the face
May 14, 2025
Classification
C01G 53/44
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Ethanol slurry medium

What ifWhat if an ethanol-rich liquid carries the composite particles during initial mixing?
Claim language“a methanol”

A wet mixer disperses the interphase-coated particles in ethanol. The tris reagents and dopamine hydrochloride enter as aqueous concentrates, and the water fraction supports buffer action and dopamine deposition.

1.1Crystalline phosphate interphase

What ifWhat if a continuous crystalline lithium phosphate film forms the interphase matrix?
Claim language“a glass phase layer”

A lithium phosphate precursor film crystallizes during a heat treatment before slurry processing and surrounds dispersed ceramic particles. The crystalline film separates the oxide surface from the electrolyte and conducts lithium ions across its thickness.

1.2Constant speed buffer dosing

What ifWhat if the mixer holds the initial rotation speed during buffer addition?
Claim language“the second rotation speed of the wet mixer is larger”

A metering pump delivers a premixed tris buffer below the liquid surface near the impeller. The impeller runs at the initial slurry speed until the measured pH stabilizes.

1.3Oxidative dopamine polymerization

What ifWhat if dissolved oxygen initiates dopamine polymerization through oxidation?
Claim language“a polymerization triggered by dehydration”

In a mildly alkaline, oxygenated slurry, dissolved oxygen oxidizes dopamine to quinone intermediates. Oxidative coupling and aggregation deposit a polydopamine film on the suspended particles.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Coated cathodes for flooded test cells

Prepare lithium nickel manganese cobalt oxide particles with a ceramic-filled glass interphase and a dopamine-derived nitrogen-containing carbon outer layer. Mix the coated powder with conductive carbon and polyvinylidene fluoride and cast the mixture onto aluminum foil. Place a disc of the dried electrode opposite lithium metal in a laboratory half-cell with a porous separator and excess liquid electrolyte. Cycle the cell to measure capacity and interfacial impedance under flooded conditions.

Component substitution

Aqueous carbonate buffer for dopamine deposition

Disperse the glass-and-ceramic-coated oxide particles in deionized water and use sodium bicarbonate and sodium carbonate in place of the two tris reagents. Set the aqueous slurry to pH 8.5 and add dopamine hydrochloride under agitation with air exposure so that oxidative polymerization deposits polydopamine on the particles. Filter the solids and rinse them with deionized water to remove soluble salts. Vacuum-dry the recovered powder and heat it under nitrogen to form the nitrogen-containing carbon layer.

Parameter or scale variation

Shallow powder beds for batch carbonization

Feed the dried dopamine-coated powder into alumina trays and level it to a bed depth of 2 to 3 mm. Place the trays on separate shelves in a batch furnace with clearance for nitrogen flow over each bed. Under flowing nitrogen, ramp to 400 °C at 3 °C per minute and hold for 2 hours. Cool the trays under nitrogen before unloading the coated powder.

Combination with existing systems

Coated particles in dry electrode lamination

Feed the carbon-coated oxide powder into a dry blending system with a sulfide solid electrolyte, conductive carbon, and polytetrafluoroethylene binder. Shear the mixture until the binder forms a fibril network that holds the powders together. Calender the mixture into a free-standing cathode film and laminate it onto aluminum foil. Perform blending and lamination in a dry inert enclosure to limit sulfide exposure to moisture.

Closed solvent recovery during slurry drying

Transfer the dopamine-coated particle slurry from the wet mixer to a sealed agitated vacuum dryer fitted with a condenser and solvent receiver. Apply vacuum and jacket heat while stirring to evaporate methanol and collect it as liquid condensate. Check the recovered solvent for water content and distill it before reuse in the initial dispersion step. Discharge the dry powder into a sealed vessel for transfer to the inert-atmosphere furnace.

Automated or data-driven variant

Feedback control of dopamine deposition

Fit the wet mixer with a temperature probe, a glass electrode suitable for alcohol-water mixtures, and metering pumps for tris base and tris hydrochloride solutions. A controller samples the electrode signal after each dosing increment and holds the slurry in a process-specific apparent pH band established at the same methanol-to-water ratio and temperature. Once the signal stabilizes in the band, the controller starts the dopamine hydrochloride feed and runs the mixer at the programmed speed for the deposition interval. The controller records reagent mass, temperature, mixer speed, and apparent pH for each batch.

Specific version of a part

Solvent exchange into carbon dioxide

A centrifuge separates the dopamine-coated particles from the bulk slurry. Ethanol displaces the liquid retained in the cake, and supercritical carbon dioxide extracts the ethanol to yield a powder before calcination.

Phosphate glass with zirconia

A lithium phosphate glass forms a continuous film on the lithium nickel manganese cobalt oxide particles. Submicrometer zirconia particles sit within the glass matrix, which provides a path for lithium ions through the film.

Staged stirring with tris buffer

A baffled wet mixer disperses the particles in methanol at 200 revolutions per minute and increases to 400 revolutions per minute after addition of tris base and its hydrochloride salt. In the aqueous methanol mixture, the base-to-salt ratio controls the measured pH and establishes alkaline conditions at the particle surface.

Low temperature vacuum drying

Shallow trays hold the third slurry in a vacuum dryer at a shelf temperature of 45 °C. A condenser collects solvent vapor, and the trays remain under vacuum until the powder reaches constant mass.

Argon tube furnace calcination

An alumina boat holds the mixed powder in a tube furnace under flowing argon. The furnace heats the powder to 500 °C at 2 °C per minute and holds it there for two hours to carbonize the dopamine coating.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2021/0171713 A1
Published
Jun 10, 2021
Filed
Nov 25, 2020
Class
C08G 73/026
Document BUS 2022/0001354 A1
Published
Jan 6, 2022
Filed
Nov 11, 2019
Class
B01J 20/22
Claim 1
Document A
Document B
1.1step A: placing a plurality of NCM (lithium nickel manganese cobalt oxide) composite particles and a methanol into a wet mixer and then mixing the NCM composite particles and the methanol to form a first mixed slurry at a first rotation speed using the wet mixer; wherein each of the NCM composite particles includes a NCM particle and the interphase layer coated on an outer surface of the NCM particle; the interphase layer includes a glass phase layer and a plurality of ceramic particles dispersed within the glass phase layer; the interphase layer serves to protect a corresponding NCM particle and increase the lithium ion conducting effect; the glass phase layer serves to block a direct contact between the corresponding NCM particle and the electrolyte of the battery and reduce the interface side reaction; and the glass phase layer serves to reduce an interface impedance of lithium ions entering and exiting the corresponding NCM particle;
1.2step B: placing a tris (tris(hydroxymethyl)aminomethane, (HOCH2)3CNH2) material and a tris(hydroxymethyl)aminomethane hydrochloride (NH2C(CH2OH)3·HCl) into the wet mixer, and then stirring the first mixed slurry, the tris material and the tris(hydroxymethyl)aminomethane hydrochloride at a second rotation speed to form a second mixed slurry using the wet mixer; wherein after the stirring, an outer surface of each of the NCM composite particles is coated with a hydroxide ion (OH−) layer containing a plurality of OH− ions; the second rotation speed of the wet mixer is larger than the first rotation speed in the step A; and the tris(hydroxymethyl)aminomethane hydrochloride serves to control a pH value of a chemical reaction in the step B;
4 g of montmorillonite (MMT) was dispersed in 200 ml of aqueous solution, and they were stirred quickly, concentrated and a concentrated MMT solution was collected for use. 4 g of dopamine hydrochloride was added to a buffer solution to prepare a dopamine hydrochloride solution, and then 8 wt % hydrogen peroxide (oxidant) was added to the dopamine hydrochloride solution, and the pH value of the resulting solution was adjusted to 8-9.
A · US 2021/0171713 A1 · ¶ 51
According to the blending amounts shown in Table 10, a uniform slurry was obtained, in which Tris Base was added and dissolved in city water, and an adhesive and two pre-mixed spherical silica having different particle sizes “Sunsphere H-31” (average particle size: 3.7 μm) and “Sunsphere H-201” (average particle size: 23.1 μm) were dispersed, and dopamine hydrochloride was added to this slurry to prepare a coating solution.
B · US 2022/0001354 A1 · ¶ 112
1.3step C: placing a dopamine hydrochloride ((HO)2C6H3CH2CH2NH2·HCl) into the wet mixer and stirring the second mixed slurry and the dopamine hydrochloride to form a third mixed slurry using the wet mixer; wherein in the stirring, a polymerization triggered by dehydration is performed between OH− ions of the dopamine molecules in the dopamine hydrochloride and the OH− ions of the hydroxide ion layer to cause that each of the NCM composite particles is bound to a plurality of corresponding dopamine molecules; and the corresponding dopamine molecules are co-polymerized to form a dopamine layer coated on an outer side of the hydroxide ion layer on the corresponding NCM composite particle;
The method increases the surface area of montmorillonite by the mechanical force of a ball mill, and uses dopamine to chemically modify the montmorillonite nanomaterials while physically modifying the montmorillonite, so that active functional groups are formed in the interlayer and on the surface of the montmorillonite, improving the surface activity of montmorillonite nanomaterials.
A · US 2021/0171713 A1 · ¶ 6
In the dopamine hydrochloride contained in the coating solution of the present invention, dopamine self-polymerizes under weak alkaline conditions to form polydopamine, which coats the surface of the fine particles, and the adhesion between the fine particles in the dust collecting layer formed on the surface of the element material by the application of the coating solution is exhibited by the interaction with the water-soluble adhesive blended in the coating solution.
B · US 2022/0001354 A1 · ¶ 44
1.4step D: drying the third mixed slurry having the NCM composite particles coated with the dopamine layer to obtain a mixed powder; and
The solid product was separated by a ultrasonic centrifugation, then washed with deionized water, and lyophilized at a temperature of −40° C. to −50° C. for 48 hours, obtaining a polydopamine-modified MMT (Bal-MMT30min).
A · US 2021/0171713 A1 · ¶ 51
applying the carbon coating solution on the surface of a filter element material consisting of a resin sintered body and then drying the coating solution to form a conductive carbon layer, and then
B · US 2022/0001354 A1 · ¶ 9
1.5step E: placing the mixed powder into a sintering furnace, and then performing a calcination in an inert atmosphere using the sintering furnace to form the NCM electrode particles; wherein in the calcination, a dehydration reaction is performed between the OH− ions and the oxygen in the hydroxide ion layer and the dopamine layer to form a plurality of nitrogen-contained carbon molecules; the nitrogen-contained carbon molecules are bound to the lone pairs of the oxygen ions of the interphase layer on each NCM composite particle by a van der Waals force, forming the nitrogen-contained carbon layer coated on the outer side of each NCM composite particle; each of the NCM electrode particles is formed by a corresponding NCM composite particle coated with the interphase layer and the nitrogen-contained carbon layer; and the nitrogen-contained carbon layer serves to increase the electrical conductivity of the NCM electrode particle.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.2 1.3 1.4.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Researchers have vigorously developed this effective surface modification technology, and used properties of polydopamine such as adhesion, hydrophilic properties and subsequent functionalization to implement secondary modifications on the modified substrate to perform surface functionalization, thereby obtaining a variety of materials with different functional properties respectively.
A · US 2021/0171713 A1 · ¶ 4

Related claim parts: 1.3

In view of the current situation that the existing solution modification method cannot produce multifunctional nano-montmorillonite materials in batches, and the shortcoming that deposition of dopamine is insufficient for the solution method, one object of the present disclosure is to provide a mechanical ball milling method for preparing a polydopamine-modified montmorillonite nanomaterial.
A · US 2021/0171713 A1 · ¶ 6
The method increases the surface area of montmorillonite by the mechanical force of a ball mill, and uses dopamine to chemically modify the montmorillonite nanomaterials while physically modifying the montmorillonite, so that active functional groups are formed in the interlayer and on the surface of the montmorillonite, improving the surface activity of montmorillonite nanomaterials.
A · US 2021/0171713 A1 · ¶ 6
The present invention relates to a coating solution which contains various fine particles as a main component, and is useful as a material for a dust collecting filter and the like.
B · US 2022/0001354 A1 · ¶ 1
In addition, a conductive carbon layer may be added depending on the specifications of the filter element.
B · US 2022/0001354 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0365539 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365539/, SHA-256 a050043f6c0fc6426826a10e879d257f4fd049e88542a3bc8a575840e7a851fd
First published
Permanent addresshttps://patent.fyi/US20260365539/
Content fingerprint (SHA-256)a050043f6c0fc6426826a10e879d257f4fd049e88542a3bc8a575840e7a851fd
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi