Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Ethanol slurry medium

What ifWhat if ethanol replaces methanol as the liquid in the first slurry?
Claim language“a methanol”

An impeller disperses the interphase-coated NCM particles in ethanol. A small water fraction in the subsequent buffer feed keeps the tris salts and dopamine hydrochloride in solution during coating.

1.1Single-phase phosphate glass

What ifWhat if the interphase consists of a continuous lithium phosphate glass film with no dispersed ceramic particles?
Claim language“a plurality of ceramic particles dispersed within the glass phase layer”

A lithium phosphate precursor coats the NCM particles and converts to a thin amorphous film during heat treatment. The film separates the oxide from the electrolyte and provides a short path for lithium-ion transport.

1.2Equal speed with recirculation

What ifWhat if the wet mixer runs at the same rotation speed in both steps and an external loop distributes the buffer during the second step?
Claim language“the second rotation speed of the wet mixer is larger than the first rotation speed”

A pump draws slurry from the bottom of the vessel and returns it near the liquid surface. The tris buffer enters the pump discharge, and several vessel turnovers distribute it through the suspension.

1.3Polyethyleneimine and tannic acid coating

What ifWhat if polyethyleneimine and tannic acid replace dopamine hydrochloride as the coating precursors?
Claim language“a dopamine hydrochloride”

Separate feeds deliver tannic acid and branched polyethyleneimine to the particle suspension, where the polyphenol and polyamine associate at the particle surface. The deposited film contains nitrogen from the polyamine and forms a nitrogen-containing carbon residue during inert heat treatment.

1.4Drying a separated filter cake

What ifWhat if filtration separates the coated particles from the third slurry before a vacuum dryer dries the recovered filter cake?
Claim language“drying the third mixed slurry”

A pressure filter retains the coated particles and removes the bulk liquid along with soluble buffer components. A vacuum dryer removes residual solvent from the cake, which is then broken up and screened before heat treatment.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cathode for stationary grid storage

Use the glass–ceramic interphase and outer nitrogen-containing carbon coating on lithium nickel manganese cobalt oxide particles in a liquid-electrolyte cell for stationary grid storage. Mix the coated powder with conductive carbon and polyvinylidene fluoride binder in N-methyl-2-pyrrolidone, then coat, dry, and calender the mixture on aluminum foil. Stack the cathode with a porous separator and graphite anode, then fill the cell with a lithium hexafluorophosphate solution in carbonate solvents.

Component substitution

Ethanol as the slurry solvent

Disperse the interphase-coated oxide particles in a 70:30 ethanol–water mixture by volume. Dissolve tris(hydroxymethyl)aminomethane and its hydrochloride in the water fraction before combining it with the ethanol and powder. Add dopamine hydrochloride as an aqueous feed and stir under air to deposit a polydopamine film. Dry the coated powder and heat it under nitrogen to convert the film into nitrogen-containing carbon.

Parameter or scale variation

Shallow powder beds for carbonization

Spread the dried dopamine-coated powder in 2–3 mm beds on alumina trays inside a tube furnace. Purge with nitrogen, heat at 2 °C per minute to 500 °C, and hold for 60 minutes to carbonize the coating. Route nitrogen across the trays during heating and maintain the flow until the powder cools below 80 °C.

Combination with existing systems

Dry roll lamination of cathodes

Integrate the coated oxide powder into a dry electrode line that uses fibrillated polytetrafluoroethylene as the binder. Blend the powder with a sulfide solid electrolyte, conductive carbon, and binder under dry argon, then shear the blend until binder fibrils form a cohesive mixture. Roll the mixture into a sheet, laminate it onto aluminum foil, and press the exposed cathode face against a sulfide electrolyte separator.

Solvent recovery during slurry drying

Transfer the dopamine-coated slurry to a closed agitated vacuum dryer fitted with a fines filter and a chilled condenser. Stir the solids at low speed while the jacket supplies heat and the vacuum draws methanol-rich vapor through the filter to the condenser. Rectify the condensate, measure its water content, and blend it with fresh methanol to reach the solvent composition specified for the next batch. Backfill the dryer with nitrogen and discharge the powder to a sealed hopper feeding the calcination furnace.

Automated or data-driven variant

Automated buffer and dopamine dosing

Fit the stirred coating vessel with a solvent-compatible pH probe and separate metering pumps for tris base, tris hydrochloride, and dopamine hydrochloride solutions. A programmable controller uses the apparent pH reading to adjust the ratio of the two buffer feeds against a setpoint established for the slurry solvent composition. Once the reading stabilizes, the controller meters dopamine at a fixed mass per kilogram of oxide, holds the batch under agitation for a programmed interval, and transfers it to the dryer.

Specific version of a part

Phosphate glass with ceramic inclusions

A continuous lithium phosphate glass film surrounds each NCM particle and contains dispersed lithium zirconium phosphate crystallites. The glass separates the NCM surface from the electrolyte while the lithium-bearing phases provide paths for lithium-ion transport across the interphase.

Staged impeller speeds with buffer

A jacketed vessel fitted with a 50 mm pitched-blade impeller disperses the particles in methanol at 300 rpm. The impeller increases to 600 rpm as a premixed concentrate of tris and tris hydrochloride enters below the liquid surface.

Vacuum tray drying

Shallow trays hold the third slurry in layers approximately 5 mm deep. A vacuum oven heats the trays at about 50 °C, and a cold trap collects the solvent vapor as the slurry dries to a powder.

Argon calcination in a tube furnace

A shallow alumina boat holds the mixed powder in a tube furnace under flowing argon. The furnace ramps at 3 °C per minute to 450 °C, holds for one hour to carbonize the dopamine coating, and cools under argon.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 10,633,554 B2
Published
Apr 28, 2020
Filed
Dec 11, 2017
Class
C09D 165/00
Document BUS 11,387,053 B2
Published
Jul 12, 2022
Filed
Jul 4, 2018
Class
H01G 11/36
Claim 1
Document A
Document B
1.1step A: placing a plurality of NCM (lithium nickel manganese cobalt oxide) composite particles and a methanol into a wet mixer and then mixing the NCM composite particles and the methanol to form a first mixed slurry at a first rotation speed using the wet mixer; wherein each of the NCM composite particles includes a NCM particle and the interphase layer coated on an outer surface of the NCM particle; the interphase layer includes a glass phase layer and a plurality of ceramic particles dispersed within the glass phase layer; the interphase layer serves to protect a corresponding NCM particle and increase the lithium ion conducting effect; the glass phase layer serves to block a direct contact between the corresponding NCM particle and the electrolyte of the battery and reduce the interface side reaction; and the glass phase layer serves to reduce an interface impedance of lithium ions entering and exiting the corresponding NCM particle;
1.2step B: placing a tris (tris(hydroxymethyl)aminomethane, (HOCH2)3CNH2) material and a tris(hydroxymethyl)aminomethane hydrochloride (NH2C(CH2OH)3·HCl) into the wet mixer, and then stirring the first mixed slurry, the tris material and the tris(hydroxymethyl)aminomethane hydrochloride at a second rotation speed to form a second mixed slurry using the wet mixer; wherein after the stirring, an outer surface of each of the NCM composite particles is coated with a hydroxide ion (OH− ) layer containing a plurality of OH− ions; the second rotation speed of the wet mixer is larger than the first rotation speed in the step A; and the tris(hydroxymethyl)aminomethane hydrochloride serves to control a pH value of a chemical reaction in the step B;
In this example, dopamine aqueous solution (2 g/L) under weakly alkaline condition (Tris-HCl buffer solution) is applied to conduct surface coating and hydrophilization for PVDF microporous membranes.
A · US 10,633,554 B2 · ¶ 23
The method according to claim 1, wherein in step (1), a pH value of the aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride is 8.5, a reaction of the aramid fiber bundles, dopamine hydrochloride and trimethylolaminomethane hydrochloride is carried out with shaking at room temperature for 5 to 48 hours; in step (2), a reaction of the polydopamine-coated aramid fiber bundles, the solution C, and the aqueous glucose solution is a shaking
B · US 11,387,053 B2 · claim 3
1.3step C: placing a dopamine hydrochloride ((HO)2C6H3CH2CH2NH2·HCl) into the wet mixer and stirring the second mixed slurry and the dopamine hydrochloride to form a third mixed slurry using the wet mixer; wherein in the stirring, a polymerization triggered by dehydration is performed between OH− ions of the dopamine molecules in the dopamine hydrochloride and the OH− ions of the hydroxide ion layer to cause that each of the NCM composite particles is bound to a plurality of corresponding dopamine molecules; and the corresponding dopamine molecules are co-polymerized to form a dopamine layer coated on an outer side of the hydroxide ion layer on the corresponding NCM composite particle;
A method for preparing an aramid fiber electrode, comprising the following steps: (1) immersing aramid fiber bundles in an aqueous solution containing dopamine hydrochloride and trimethylolaminomethane hydrochloride to obtain polydopamine-coated aramid fiber bundles;
B · US 11,387,053 B2 · claim 1
1.4step D: drying the third mixed slurry having the NCM composite particles coated with the dopamine layer to obtain a mixed powder; and
3) After reaction in dopamine modification solution, membrane sample are transferred into deionized water to wash and remove unreacted dopamine molecules, and then heated for drying in an oven (60° C., 2 hours) to obtain the composite membranes with polydopamine coating layer.
A · US 10,633,554 B2 · ¶ 27
In the above technical solution, wherein in step (1), after the reaction is finished, the fibers are taken out, washed and dried to obtain polydopamine coated aramid fiber bundles; in step (2), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated with silver nanoparticles; in step (3), after the reaction is finished, the fibers are taken out, washed and dried to obtain aramid fiber bundles coated by silver nanopartic
B · US 11,387,053 B2 · ¶ 22
1.5step E: placing the mixed powder into a sintering furnace, and then performing a calcination in an inert atmosphere using the sintering furnace to form the NCM electrode particles; wherein in the calcination, a dehydration reaction is performed between the OH− ions and the oxygen in the hydroxide ion layer and the dopamine layer to form a plurality of nitrogen-contained carbon molecules; the nitrogen-contained carbon molecules are bound to the lone pairs of the oxygen ions of the interphase layer on each NCM composite particle by a van der Waals force, forming the nitrogen-contained carbon layer coated on the outer side of each NCM composite particle; each of the NCM electrode particles is formed by a corresponding NCM composite particle coated with the interphase layer and the nitrogen-contained carbon layer; and the nitrogen-contained carbon layer serves to increase the electrical conductivity of the NCM electrode particle.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.3. Both have a passage for 1.2 1.4.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

It is a new direction for fabricating high performance composite materials, and the foundation is the oxidative auto-polymerization of dopamine and/or its derivatives on substrate surface.
A · US 10,633,554 B2 · ¶ 3

Related claim parts: 1.3

The stability of the polydopamine in organic solvents (or aqueous solutions containing organic solvents) and acidic/alkalic environments is poor, which is an bottleneck restricting polydopamine modification in practical application.
A · US 10,633,554 B2 · ¶ 4
After the cross-linking solidification, the polydopamine coating layer could be stable and effective for long-term utilization in severe environments, e.g., organic solvents and acidic/alkalic environments, and thereby greatly expand the application scope of the surface modification method based on dopamine polymerization.
A · US 10,633,554 B2 · ¶ 6
However, like other polymer fiber capacitors, aramid fiber capacitors also have two problems, their capacitance performance as well as their adhesion with the inorganic coating remain to be solved.
B · US 11,387,053 B2 · ¶ 6
In order to overcome the shortcomings of the prior art, an object of the present invention is to provide aramid fiber electrodes and electrochemical capacitors with high specific capacitance, high energy density, high mechanical properties, high stability, good flexibility and wearability, moreover, the preparation method is suitable for large-scale applications.
B · US 11,387,053 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0365540 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365540/, SHA-256 f444a7a2fd712c5f44b2398588432307f057856eb34eed331265cec210e9cb24
First published
Permanent addresshttps://patent.fyi/US20260365540/
Content fingerprint (SHA-256)f444a7a2fd712c5f44b2398588432307f057856eb34eed331265cec210e9cb24
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi