Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Sulfur conversion cathode
What ifWhat if the cathode active material used elemental sulfur as its redox material and contained no transition metal?
Claim language“a transition metal”
Porous carbon distributes sulfur through an electronically conductive network. In a lithium cell with an ether electrolyte, sulfur converts through lithium polysulfides to lithium sulfide on discharge, and charging regenerates sulfur.
1.1Organic carbonyl cathode
What ifWhat if the cathode active material stored charge at organic carbonyl groups and contained no transition metal?
Claim language“a transition metal”
A polyimide with electroactive imide carbonyl groups is mixed with conductive carbon and a binder. The carbonyl groups accept electrons and coordinate lithium ions on discharge, and charging releases the lithium ions.
1.2Higher surface carbonate content
What ifWhat if the cathode powder contained 1.2 wt % residual surface lithium carbonate on a powder mass basis?
Claim language“a residual lithium content on a particle surface is 1 wt % or less”
A layered lithium nickel manganese cobalt oxide powder retains surface lithium carbonate from synthesis and subsequent exposure to carbon dioxide. Dry handling and nonaqueous slurry processing limit moisture uptake, while the layered oxide supplies reversible capacity through lithium insertion and extraction.
1.2Dense single crystal particles
What ifWhat if the cathode powder had a BET surface area of 0.25 m²/g and consisted of dense single crystals?
Claim language“a BET is 0.4 m2/g or more”
Calcination forms dense, low-porosity lithium nickel manganese cobalt oxide crystals several micrometers across. Electrolyte contacts the outer crystal faces, and lithium ions diffuse through the layered lattice during charge and discharge.
1.2Dense layered cobalt oxide
What ifWhat if the cathode powder had a BET surface area of 0.20 m²/g and used dense lithium cobalt oxide grains?
Claim language“a BET is 0.4 m2/g or more”
High-temperature firing grows lithium cobalt oxide grains and reduces open porosity. Conductive carbon connects the grains to the current collector, and the oxide exchanges lithium ions with the electrolyte at exposed grain surfaces.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Cells for stationary backup power
Stationary backup cells use a transition-metal oxide powder with surface residual lithium of 1 wt % or less and a BET surface area of at least 0.4 m²/g. An aluminum current collector carries a dried coating of the powder, conductive carbon, and polyvinylidene fluoride. A porous separator soaked with lithium-ion electrolyte separates the cathode from a graphite anode. The cells connect in series in a backup module that supplies a direct-current bus during power interruptions.
Component substitution
Spinel oxide replaces layered oxide
Spinel lithium manganese oxide, LiMn₂O₄, replaces layered transition-metal oxide as the cathode active phase. Solid-state calcination of lithium carbonate and manganese dioxide forms the spinel, and milling and classification set the powder particle size. The finished powder has surface residual lithium of 1 wt % or less and a BET surface area of at least 0.4 m²/g. A dried coating of the powder, conductive carbon, and binder on aluminum foil stores and releases lithium through the spinel structure.
Parameter or scale variation
Fine powder with tighter release limits
The cathode uses a transition-metal oxide powder with a median particle diameter of 3–5 µm, a BET surface area of 0.8–1.2 m²/g, and surface residual lithium of 0.30 wt % or less. An air classifier selects the particle-size fraction after calcination. A brief deionized-water wash removes soluble surface lithium compounds, followed by filtration and vacuum drying. Laser diffraction, nitrogen adsorption, and aqueous extraction followed by acid titration verify the finished powder against the three limits.
Continuous washing with timed filtration
A continuous wash line feeds calcined transition-metal oxide powder and deionized water into a stirred contactor at a starting ratio of 0.5 kg of water per kilogram of powder. The contactor operates at 20–25 °C with a nominal residence time of 2 minutes and discharges onto a vacuum belt filter. A vacuum dryer dries the filter cake at 120 °C, and a screen breaks up loose agglomerates. Finished powder samples undergo surface residual lithium and BET measurements against limits of 1 wt % or less and 0.4 m²/g or more, respectively.
Combination with existing systems
Cathode powder in dry electrode coating
A roll-to-roll dry coating line blends transition-metal oxide powder with conductive carbon and polytetrafluoroethylene binder. The active powder has surface residual lithium of 1 wt % or less and a BET surface area of at least 0.4 m²/g. A high-shear mixer fibrillates the binder, and a roll press consolidates the blend into a continuous film. Heated rolls laminate the film onto carbon-coated aluminum foil, and a slitter cuts the coated foil to electrode width.
Automated or data-driven variant
Automated powder lot release testing
An automated sampler collects a composite sample from each dried transition-metal oxide lot and divides it between two test stations. One station extracts soluble surface lithium compounds with water and measures the extract by automated acid titration. The second station degasses its subsample and measures BET surface area by multipoint nitrogen adsorption. Control software records both results and releases the lot when surface residual lithium is 1 wt % or less and BET surface area is at least 0.4 m²/g.
Specific version of a part
Layered nickel manganese cobalt oxide
A layered oxide has the composition LiNi₀.₈Mn₀.₁Co₀.₁O₂. Nickel supplies most of the reversible redox capacity as lithium ions enter and leave the layers.
Manganese spinel cathode particles
Lithium manganese oxide particles have the spinel composition LiMn₂O₄. Manganese changes between the +3 and +4 oxidation states as lithium ions move through three-dimensional channels in the lattice.
Washed porous oxide particles
A brief water wash followed by vacuum drying reduces surface lithium hydroxide and lithium carbonate on layered oxide particles. Acid titration of a water extract gives a combined surface residue of 0.50 wt % on a powder mass basis, and nitrogen adsorption gives a BET surface area of 0.65 m²/g.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The invention relates to nanoparticles of lithium metal oxides, in particular, in which the non-lithium metal includes, for example, cobalt, nickel, titanium, or combinations thereof with one or more additional metals.
A · US 2008/0131356 A1 · ¶ 2
Also, the lithium metal oxide may be represented by a formula selected from a group consisting of LixMn1-yM′yA2, LixMn1-yM′yO2-zXz, LixMn2O4-zXz, LixMn2-yM′yA4, LixCo1-yM′yA2, LixCo1-yM′yO2-zXz, LixNi1-yM′yA2, LixNi1-yM′yO2-zXz, LixNi1-yCoyO2-zXz, LixNi1-y-zCoyM′zAα, LixNi1-y-zCoyM′zO2-αXα, LixNi1-y-zMnyM′zAα, and LixNi1-y-zMnyM′zO2-αXα (where 0.95≤x≤1.1, 0≤y≤0.5, 0≤z≤0.5, and 0<α≤2), wherein, M′ is at least one element selected from a group consisting of aluminum (Al), nicke
B · US 2020/0194774 A1 · ¶ 11
1.2wherein a residual lithium content on a particle surface is 1 wt % or less, and a BET is 0.4 m2/g or more.
Also, BET surface areas were measured for the two precursor particle samples produced by laser pyrolysis under the conditions specified in columns 1 and 2 of Table 1 and for portions of the samples following heat treatment. The BET surface area was determined with an N2 gas absorbate.
A · US 2008/0131356 A1 · ¶ 151
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The growing use of portable electronic equipment has created ever increasing demand for improved power sources for these devices.
A · US 2008/0131356 A1 · ¶ 3
These lithium metal oxides are useful for the production of lithium-based secondary batteries.
A · US 2008/0131356 A1 · ¶ 5
Therefore, it is required to improve the lifetime characteristics of the cathode active material having a high nickel content by suppressing side reactions with the electrolyte penetrating into the grain boundaries and cracks.
B · US 2020/0194774 A1 · ¶ 6
In order to solve the above problems, the present disclosure provides a cathode active material for a lithium secondary battery having improved lifetime characteristics by suppressing side reactions with an electrolyte penetrating along grain boundaries and cracks of the cathode active material, a cathode and a lithium secondary battery each including the same, and a manufacturing method thereof.
B · US 2020/0194774 A1 · ¶ 7
(3) the ratio (amount of residual lithium/BET specific surface area) of the amount of residual lithium (mass %) contained in the lithium metal composite oxide to the BET specific surface area (m2/g) is 0.25 or less.
C · US 2021/0218022 A1 · ¶ 14
Related claim parts: 1.2
Document C: US 2021/0218022 A1, published Jul 15, 2021. Cited for this statement only.
Cite aspatent.fyi, US 2026/0365541 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365541/, SHA-256 1e5a6d53553f3a16f3243089f5d0df572fa1909af45279e5c9deecfdda656d6f