1.1Nitric acid palladium leaching
Heated nitric acid oxidizes palladium and copper in a stirred vessel and transfers both metals into a nitrate liquor. Filtration removes the ceramic solids before metal separation.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Heated nitric acid oxidizes palladium and copper in a stirred vessel and transfers both metals into a nitrate liquor. Filtration removes the ceramic solids before metal separation.
Dissolved bromine oxidizes platinum and copper in a stirred hydrobromic acid slurry. Bromide stabilizes dissolved platinum as bromoplatinate, and filtration removes the ceramic solids.
An impeller suspends sulfur-functional resin beads in the chloride liquor as palladium loads onto the beads. A screen retains the loaded beads and drains the liquor containing most of the dissolved base metals.
A mixer disperses an organic phase containing a dialkyl sulfide in the chloride liquor so dissolved palladium transfers into the organic phase. A settling chamber separates the loaded organic phase from the aqueous phase containing most of the dissolved copper.
The carbon drains from the opened column and enters a furnace, where controlled air feed oxidizes the carbon. A particulate collector captures entrained platinum-bearing ash and combines it with the furnace residue for refining.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
The feed consists of discarded gas sensor elements with a platinum catalytic coating and base-metal contacts on a ceramic substrate. The elements are immersed in hydrochloric acid leachate, and the drained liquor passes through a particulate filter into a platinum-selective adsorption column. A separate eluent removes the platinum from the column, and ammonium chloride precipitates ammonium hexachloroplatinate from the concentrated eluate containing platinum in the +4 oxidation state.
A pair of mixer-settlers replaces the adsorption column and its elution circuit. The first mixer-settler contacts clarified hydrochloric acid leach liquor with di-n-octyl sulfide in a hydrocarbon diluent, then separates the palladium-bearing organic phase from the aqueous raffinate. The second mixer-settler strips palladium into aqueous thiourea and returns the separated organic phase to the extraction stage. A reduction vessel converts dissolved palladium in the strip liquor to a metal powder that a filter collects.
Two columns containing 5 L of adsorbent each operate in series at a leach liquor flow of 25 L/h, giving a nominal empty-bed contact time of 12 minutes per column. An interstage sample port measures palladium or platinum breakthrough, and valves isolate the lead column when the interstage concentration reaches 5 percent of the inlet concentration. The guard column then takes the lead position while the isolated column is eluted to a separate metal recovery vessel. A regenerated column returns to service in the guard position.
The adsorption column discharges its base-metal-bearing raffinate into a stirred wastewater neutralization tank. Sodium hydroxide raises the pH to precipitate the dissolved base metals as hydroxides, and a filter press dewaters the settled solids. A separate collection tank receives the palladium or platinum eluate and feeds it to the precious-metal recovery vessel.
A flow-through electrolysis cell receives a concentrated platinum-bearing chloride eluate from a recirculation tank. The cell pumps the eluate upward through conductive carbon granules that contact a cathode current feeder, while an ion exchange membrane separates the anode compartment. Platinum deposits on the moving granules as the eluate recirculates. The cell discharges the plated granules through a screened outlet for downstream platinum refining.
A flowmeter, an automated sampling valve, and an optical emission spectrometer connect the column outlet to a controller that operates a three-way collection valve. During elution, the controller combines measured palladium concentration with eluent flow to calculate the palladium mass passing through the outlet. The valve directs fractions above a configured concentration threshold to the recovery tank and routes dilute fractions to a separate tank. The controller ends elution when the outlet stays below the threshold for one bed volume.
A stirred reactor contacts crushed palladium and copper catalyst with hydrochloric acid while a metering pump feeds hydrogen peroxide. Peroxide oxidizes the metals, chloride stabilizes dissolved palladium, and filtration removes residual ceramic solids.
A packed column contains crosslinked polymer beads bearing thiol groups. The beads bind palladium from the chloride liquor, and outlet sampling tracks the rise in dissolved palladium as the bed loads.
An aqueous thiourea solution acidified with hydrochloric acid flows through the loaded resin bed. Thiourea forms soluble palladium complexes, and the outlet stream carries them into a collection tank.
Ammonium chloride added to a concentrated acidic solution of hexachloroplatinate precipitates ammonium hexachloroplatinate. Filtration collects the crystals, and thermal decomposition yields platinum sponge.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A rare metal recovery method according to the present invention comprises: a leaching step comprising: mixing, under a pressure of 1 atmosphere or less at a temperature of from 50° C. to 90° C., a hydrochloric acid mixture liquid obtained by mixing a waste material of rare metal comprising palladium, platinum and rhodium with hydrochloric acid; condensing steam obtained by the mixing; and flowing hydrochloric acid obtained by the condensing back to the hydrochloric acid mixtuA · US 8,974,572 B2 · ¶ 9
The present invention provides a preparation method of titanium pigment, where the Panxi ilmenite concentrate is leached by hydrochloric acid to obtain enriched titanium hydrochloric acid extract residue containing more than 90% of TiO2. Meanwhile, more than 90% of Ca, Mg, Fe and Mn impurities as well as more than 60% V and Al impurities can be removed during hydrochloric acid leaching.B · US 9,206,055 B2 · ¶ 28
An adsorption unit 2, which is used in the palladium adsorption step, the platinum adsorption step and the rhodium adsorption step by which the rare metal recovery method according to the embodiment of the present invention is comprised, includes, as shown in FIG. 3, a DHS-impregnated resin column 21 that is formed of a resin impregnated with di-n-hexyl sulfide (DHS) absorbing specifically palladium; an ion-exchange resin column 22 for platinum that is formed of an ion-exchanA · US 8,974,572 B2 · ¶ 36
Concerning the flow of the palladium elution step, the platinum elution step and the rhodium elution step in the structural system as described above, in case where the lapsed time for the steps of S1 to S7 reaches a predetermined time in Step S8 as described above in FIG. 1, the hydrochloric acid solution containing the thiourea is caused to flow from the hydrochloric acid tank 31 for palladium into the DHS-impregnated resin column 21 (S10).A · US 8,974,572 B2 · ¶ 47
The rare metal recovery method, according to the present invention may comprise, where appropriate, a palladium precipitation step of adding a sodium hydroxide solution to the palladium elution liquid obtained by the palladium elution step to precipitate a palladium oxide; a platinum precipitation step of adding a saturated ammonium chloride solution to the platinum elution liquid obtained by the platinum elution step to precipitate a platinum oxide; and a rhodium precipitatiA · US 8,974,572 B2 · ¶ 17
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.2 1.3 1.4. Both have a passage for 1.1.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, an effective method for recovering rare metals by a low temperature refining process has not as yet been established.A · US 8,974,572 B2 · ¶ 4
The method is performed without the need for external mechanical when separating and recovering the rare metal, thus controlling workload and enhancing the safety of operation.A · US 8,974,572 B2 · ¶ 7
There are difficulties in preparing synthetic rutile using Panxi ilmenite due to its low ore grade, high impurity and fine granularity.B · US 9,206,055 B2 · ¶ 6
The first technical problem resolved in the present invention is to provide enriched titanium hydrochloric acid extract residue which can be applied to prepare titanium pigment by sulfuric acid process.B · US 9,206,055 B2 · ¶ 8
The commercial process for separation/recovery of PGM from the above-described starting material containing them normally involves leaching in a solution and a subsequent separation process, e.g., solvent extraction or adsorption, by which they are separated mutually and refined.C · US 2005/0066774 A1 · ¶ 6
Related claim parts: 1.2 1.3 1.4
Document C: US 2005/0066774 A1, published Mar 31, 2005. Cited for this statement only.
patent.fyi, US 2026/0365542 A1, claim 1, first published 2026-11-23T13:37:42-05:00, https://patent.fyi/US20260365542/, SHA-256 6f462b49cadc871a892810683f55b876db3bbf4c1481970cc7c7af72d30d4d4b