Other field of use
Molten basalt strip forming for mineral wool
A feed channel delivers a strip of molten basalt-based melt at a viscosity of 5 Pa·s to a rotating water-cooled steel drum. The drum surface speed is set to 110% of the strip velocity at the contact line. A set of spinner wheels downstream receives the sheet-like melt from the drum and converts it into fibers. A blower and a collection conveyor carry the fibers to a curing oven, where a binder sets the mat.
Glass-ceramic precursor strip for ceramic substrate production
A melting unit supplies a nucleating glass melt at 10 Pa·s through a slot nozzle to a pair of counter-rotating cooled rollers. Each roller surface speed is set to 100% of the strip velocity at the nip. The formed strip passes into a roller-hearth furnace, where a nucleation stage at 700 °C and a crystal growth stage at 850 °C convert it into glass-ceramic. A saw cuts the cooled strip into substrate plates.
Component substitution
Porous graphite belt replacing metal drum
A continuous belt of dense graphite runs over two driven rollers and replaces the cooled metal drum as the mobile discharge surface. The belt receives a glass strip at 20 Pa·s from a slot nozzle. A drive controller sets the belt speed to 100% to 120% of the strip velocity at the contact line. A nitrogen purge hood covers the belt to limit oxidation of the graphite. A scraper blade at the belt return side removes residual glass.
Parameter or scale variation
Narrow strip forming for thin glass ribbon
A platinum-alloy slot nozzle 150 mm wide delivers a strip 2 mm thick at a viscosity of 0.5 Pa·s and a flow rate of 30 kg per hour. A roller with a 300 mm diameter turns at a surface speed of 95% of the strip velocity, which is 0.04 m/s. The roller surface is held at 600 °C by internal oil circulation. The ribbon leaves the roller and passes through an annealing lehr about 6 m long to produce sheet 0.3 mm thick.
Combination with existing systems
Strip feed from a continuous electric melter
A continuous electric melting tank with submerged electrodes feeds a heated forehearth, which ends in a slot-shaped orifice. The orifice delivers a strip at 50 Pa·s to a moving discharge surface formed by a belt of heat-resistant steel links. A float bath of molten tin is placed after the belt, and the strip flows onto the tin to level its thickness. The belt speed is set to 105% of the strip velocity, and the bath leads into an annealing lehr and a cutting station.
Automated or data-driven variant
Camera-based closed-loop speed control of discharge surface
A line-scan camera and an infrared pyrometer observe the strip near the contact line and report strip width, edge position and temperature. A processor converts temperature into viscosity using a stored viscosity-temperature table and estimates strip velocity from the mass flow signal of a weighing system. A controller drives the discharge surface motor so that surface speed stays between 90% and 200% of the estimated strip velocity. The controller also adjusts nozzle heating power when the viscosity leaves the 0.01 Pa·s to 100 Pa·s range.