patent.fyi
Applications  /  US 2026/0365562
United States Patent Application Publication

US 2026/0365562 A1

Published
Nov 19, 2026
Filed
Jul 23, 2026
Earliest date on the face
Jun 24, 2016
Classification
C03C 10/0027
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Lower lithium oxide content

What ifWhat if the glass batch contains 16 mol % Li2O and retains a silica-rich glass matrix after crystallization?
Claim language“18-40 mol % Li2O”

A batch containing 75 mol % SiO2, 16 mol % Li2O, 7 mol % ZrO2, 1 mol % Al2O3, and 1 mol % P2O5 supplies lithium and silica for lithium disilicate crystallization. A nucleation hold followed by a higher-temperature growth hold develops crystals while retaining a continuous silica-rich glass matrix.

1.1Alumina-free glass batch

What ifWhat if the glass batch omits Al2O3 and uses phosphate-assisted nucleation?
Claim language“>0-5 mol % Al2O3”

A batch containing 68 mol % SiO2, 25 mol % Li2O, 6 mol % ZrO2, and 1 mol % P2O5 forms a lithium silicate parent glass. A lower-temperature hold develops phosphate-rich nuclei, and a higher-temperature hold grows lithium silicate crystals within the glass.

1.1Low zirconia powder loading

What ifWhat if the bulk composition contains 1 mol % ZrO2 supplied as preformed zirconia particles?
Claim language“1.5-25 mol % ZrO2”

Submicrometer stabilized zirconia particles are dispersed in lithium silicate glass powder before consolidation. The glass powder densifies by viscous flow and then crystallizes lithium disilicate, which provides the main reinforcing phase at the low zirconia loading.

1.2Alumina platelets for crack deflection

What ifWhat if alumina platelets take the place of zirconia crystals as the dispersed reinforcement?
Claim language“crystals of zirconia”

Alumina platelets are blended with lithium silicate glass powder and consolidated under pressure while the glass flows around the platelets. During fracture, cracks deflect along platelet interfaces, increasing the fracture path length.

1.2Lithium metasilicate crystal phase

What ifWhat if lithium metasilicate serves as the lithium silicate crystal phase?
Claim language“crystals of lithium disilicate”

A lithium silicate parent glass undergoes a growth hold in the lithium metasilicate crystallization interval. Cooling after that hold arrests crystal growth and limits conversion to lithium disilicate, leaving fine metasilicate crystals dispersed in the residual glass.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Wear liners for ceramic slurry pumps

Form the zirconia and lithium disilicate glass-ceramic into curved segments that match the bore of a slurry pump casing. Grind the segment edges and bond the segments to the casing with a filled epoxy, keeping the joints flush with the wetted surface. The glass-ceramic lines the flow path while the casing carries the pressure load.

Component substitution

Titania in place of phosphorus pentoxide

Replace 1 mol % P2O5 in a starting batch with 1 mol % TiO2 supplied as rutile powder. Melt and homogenize the batch with the silica, lithium oxide, zirconia and alumina sources, then cast and anneal the precursor glass. Use differential scanning calorimetry to locate crystallization events, screen two-stage heat treatments around those events and use X-ray diffraction to select a treatment that produces zirconia and lithium disilicate crystals in residual glass.

Parameter or scale variation

Thin sheets with staged crystallization holds

Cast and anneal 2 mm precursor sheets from a batch with representative oxide contents of 68 mol % SiO2, 25 mol % Li2O, 4 mol % ZrO2, 2 mol % Al2O3 and 1 mol % P2O5. Support the sheets on flat alumina setters and screen crystallization schedules with heating rates of 2 to 5 °C per minute, first holds of 30 to 90 minutes and second holds of 15 to 60 minutes. Set the hold temperatures from the batch's thermal analysis and use diffraction and flatness measurements to select a schedule for the sheets.

Timed sodium exchange on polished plates

Polish 2 mm glass-ceramic coupons that contain zirconia and lithium disilicate crystals in a lithium-bearing residual glass. Immerse separate coupons in molten sodium nitrate at 400 °C for 1, 2 and 4 hours, then cool and rinse them. Sodium exchanges with lithium near the exposed surfaces, and measurements of the resulting surface stress and layer depth guide the choice of dwell time.

Combination with existing systems

Glass ceramic guide in a wire feeder

Diamond-grind a crystallized glass-ceramic blank into a guide bushing with a polished bore and radiused entries. Seat the bushing in a steel cartridge and align its bore with the outlet of the drive rollers and the inlet of the downstream feed tube. The rollers advance the wire through the bore while the glass-ceramic surface supports the wire at the transition.

Automated or data-driven variant

Diffraction feedback for furnace recipe selection

Place a witness coupon from each precursor glass batch beside the parts in a programmable furnace. After cooling, feed the coupon's X-ray diffraction pattern into a phase-fitting routine that estimates tetragonal zirconia, monoclinic zirconia and lithium disilicate fractions using an internal reference. Software compares the estimates with defined target bands and selects the next furnace recipe from a table of tested hold temperatures and durations.

Specific version of a part

Phosphate-containing lithium silicate batch

The oxide composition is 65 mol % SiO2, 26 mol % Li2O, 7 mol % ZrO2, 1 mol % Al2O3, and 1 mol % P2O5. A premixed lithium phosphate precursor supplies P2O5 and part of the Li2O, and lithium carbonate supplies the remaining Li2O.

Batch with eleven mole percent zirconia

The oxide composition is 61 mol % SiO2, 25 mol % Li2O, 11 mol % ZrO2, 2 mol % Al2O3, and 1 mol % P2O5. Fine zirconia powder is mixed with the other batch materials before melting, and the melt is homogenized before casting.

Fine tetragonal zirconia dispersion

A nucleation hold followed by a short growth hold produces fine tetragonal zirconia crystals in a residual glass matrix containing lithium disilicate crystals. The growth hold limits zirconia coarsening, and stress near a crack tip drives local transformation of tetragonal zirconia to the monoclinic phase.

Interlocking lithium disilicate crystals

A growth hold develops elongated lithium disilicate crystals that impinge on one another within the residual glass. Zirconia crystals form a finer dispersion, and the elongated lithium disilicate crystals deflect cracks at crystal boundaries.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2014/0249016 A1
Published
Sep 4, 2014
Filed
May 9, 2014
Class
C03C 10/0027
Document BUS 2016/0060159 A1
Published
Mar 3, 2016
Filed
Nov 12, 2014
Class
C03C 10/0027
Claim 1
Document A
Document B
1.1a composition in terms of representative oxides comprising: 50-80 mol % SiO2; 18-40 mol % Li2O; 1.5-25 mol % ZrO2; >0-5 mol % Al2O3; and 0-5 mol % P2O5; and
Lithium silicate glass ceramic, which comprises at least 7.0 wt. % ZrO2 and which comprises more than 10 vol. % of crystal, wherein said crystal is selected from the group consisting of lithium metasilicate crystal and lithium disilicate crystal.
A · US 2014/0249016 A1 · claim 1
An exemplary embodiment of the present invention provides a lithium silicate glass composition for crystallizing to a lithium disilicate glass-ceramic having a crystobalite crystal phase, the lithium silicate glass composition including: a glass component including 11-13 wt % Li2O, 70.0-77.0 wt % SiO2, 2-3 wt % P2O5 as a nuclei formation agent, 2-5 wt % Al2O3 to increase glass transition temperature, softening temperature, and chemical durability of the glass component, 2.0-3
B · US 2016/0060159 A1 · ¶ 11
1.2crystalline and glass phases, the crystalline phase comprising: crystals of zirconia; and crystals of lithium disilicate.
With a second short crystallisation at 800° C. to 950° C. for 3 to 15 minutes, recrystallisation of the lithium metasilicate with amorphous SiO2 from the glass phase takes place to form lithium disilicate and the result is an increase in strength to 300 MPa to 450 MPa. In addition to the lithium disilicate phase, a subsidiary crystal phase with a zirconium oxide content can hereby be produced.
A · US 2014/0249016 A1 · ¶ 31
An exemplary embodiment of the present invention provides a method of forming cristobalite crystal phase and lithium disilicate crystal phase at the same time in the glass made from Li2O—Al2O3—SiO2—Li2O—K2O—Na2O—ZrO2—CaO—P2O5-coloring agents.
B · US 2016/0060159 A1 · ¶ 16

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1 1.2. Both are classified in CPC C03C, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Starting herefrom, it was the object of the present invention to provide a glass-ceramic which has improved mechanical and optical properties and also improved chemical stability relative to the (glass-) ceramics known from the state of the art.
A · US 2014/0249016 A1 · ¶ 8

Related claim parts: 1.1 1.2

The preparation method relates to a preparation of the high strength and aesthetic lithium disilicate crystalline glass-ceramics, dental restoration materials, and manufacturing methods which induce the growth of crystal phases or structures in a glass matrix with lithium disilicate crystal.
B · US 2016/0060159 A1 · ¶ 3

Related claim parts: 1.1 1.2

All known lithium disilicate glass-ceramics display inadequacies in the processing thereof to shaped products and/or in mechanical or visual properties and/or in chemical stability.
A · US 2014/0249016 A1 · ¶ 7
The invention relates to glass-ceramics based on the lithium disilicate system which can be mechanically machined easily in an intermediate step of crystallisation and, after complete crystallisation, represent a very strong, highly-translucent and chemically-stable glass-ceramic.
A · US 2014/0249016 A1 · ¶ 2
Although this crystalline glass has high aesthetic traits, the mechanical strength of monolithic crown manufactured by such method is low around 350 MPa, which is not adequate for posterior or bridges exposed to high stress.
B · US 2016/0060159 A1 · ¶ 8
An exemplary embodiment of the present invention provides dental lithium disilicate glass-ceramics containing cristobalite crystal with high strength as well as aesthetic traits.
B · US 2016/0060159 A1 · ¶ 9
Cite aspatent.fyi, US 2026/0365562 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365562/, SHA-256 8040ee8e397d686e5e0e0133a1e807bf5b016d08ebdb2dda07000e3c3edb4676
First published
Permanent addresshttps://patent.fyi/US20260365562/
Content fingerprint (SHA-256)8040ee8e397d686e5e0e0133a1e807bf5b016d08ebdb2dda07000e3c3edb4676
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi