Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.5High-soda melt with acid leaching
What ifWhat if the batch carried 10 to 15 weight percent Na2O for easy melting, and the sodium were removed from the fibers after forming?
Claim language“Na2O 0-0.2 weight percent”
A sodium-rich borosilicate melt fiberizes at a low temperature through a conventional bushing. The drawn fibers are treated in a hot mineral acid bath, which dissolves the alkali and boron phases and leaves a porous high-silica skeleton. The fibers are washed, dried and heat-treated to densify them.
1.4Barium and strontium oxide modifiers
What ifWhat if the batch held no magnesium oxide, and heavier alkaline earth oxides such as BaO and SrO supplied the network modification?
Claim language“MgO 7-17 weight percent”
The batch uses 6 to 12 weight percent combined BaO and SrO from carbonate raw materials, with the silica and alumina contents adjusted to hold the viscosity-temperature curve. The heavier ions lower the liquidus temperature and raise density and refractive index. The melt is drawn through a platinum alloy bushing in the usual way.
1.11Gas bubbling for melt refining
What ifWhat if the melt were refined mechanically, with no tin oxide in the batch?
Claim language“SnO2 0-4 weight percent”
A bubbler array in the refining zone of the furnace injects fine oxygen bubbles into the melt. The bubbles collect dissolved gases and carry them to the surface. A deep, slow-flow refining channel then gives residual bubbles time to rise before the melt reaches the bushings.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Specific version of a part
Calcined alumina and kaolin supply
Al2O3 at 14 to 15 weight percent is supplied by a blend of calcined alumina powder and washed kaolin. The calcined alumina sets the target level and the kaolin adds fine silica and promotes batch granulation. Particle size is held below 75 micrometers so the batch melts without unmelted alumina stones.
Lithium oxide from spodumene
Li2O at 1 to 2 weight percent is supplied by a lithium aluminosilicate mineral concentrate with low iron content. The concentrate also supplies part of the alumina and silica, and the batch is rebalanced to hold the target composition. The lithium lowers the melt viscosity at the bushing and widens the forming temperature range.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
More particularly, the aluminosilicate proppant particles typically have a silica (SiO2) content of between about 54 and about 57 weight percent, an alumina (Al2O3) content of between 32 and about 38 weight percent.
A · US 8,722,590 B2 · ¶ 12
This is primarily due to their relatively high silica and boron oxide content.
B · US 8,728,964 B2 · ¶ 3
1.2Al2O3 11 to less than 18 weight percent
1.3CaO 5.1 to 12 weight percent
1.4MgO 7-17 weight percent
1.5Na2O 0-0.2 weight percent
More than 2 weight percent alkalis can also worsen devitrification behavior.
B · US 8,728,964 B2 · ¶ 22
1.6K2O greater than 0-1 weight percent
1.7Li2O 0-5 weight percent
1.8TiO2 0-2 weight percent
A sintered, generally spherical ceramic body, comprising: an alumina content between about 32 and about 39 weight percent distributed substantially homogeneously throughout the body; a silica content between about 52 and about 58 weight percent distributed substantially homogeneously throughout the body; an iron oxide content of about 3 weight percent; a titania content of about 2 weight percent titania; with the remainder being alkali and alkali earth metal oxides; having an
A · US 8,722,590 B2 · claim 1
1.9B2O3 0-3 weight percent
Thus, boron oxide is preferably used within a range of about 3 to about 10 weight percent, preferably 4 to 6 weight percent, and most preferably, about 5 weight percent +/− about 0.25 weight percent.
B · US 8,728,964 B2 · ¶ 18
1.10Fe2O3 0-1 weight percent
1.11SnO2 0-4 weight percent
1.12ZnO 0-4 weight percent at least one rare earth oxide in an amount not less than 0.05 weight percent other constituents 0-11 weight percent total.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.8. Only Document B has a passage for 1.51.9. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, denser, heavier proppants are harder to pump, more expensive to transport, and are less permeable than lighter, more porous agents.
A · US 8,722,590 B2 · ¶ 3
Lowering the alumina content of the material generally results in a lower density proppant with corresponding lower strength, since the higher silica content results in significant loss of strength.
A · US 8,722,590 B2 · ¶ 7
In addition, these glasses tend to have relatively low elastic moduli (<70 GPa) and as a result are a poor choice for applications that require rigidity and high dimensional stability.
B · US 8,728,964 B2 · ¶ 3
The low CTE fibers are particularly suitable for use in insulating layers of PCB, chip carrier substrates and/or controlled collapse (C4) ball grid array (BGA) connectors.
B · US 8,728,964 B2 · ¶ 7
Cite aspatent.fyi, US 2026/0365563 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365563/, SHA-256 a7ed3f4b2ccd9d92b9074a91e55fed8a5c80e29ad5ddc96efd6eef0a595bc282