Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Lower silica main frit
What ifWhat if the main ink contains 25% silica by weight?
Claim language“30-50% SiO2”
A bismuth borosilicate frit supplies the silica and acts as the fired binder for the black pigment. A second frit with 8% silica and a higher bismuth oxide content lowers the silica fraction and softening temperature of the blended deposit.
1.2Zinc borosilicate main frit
What ifWhat if the main ink uses a bismuth-free zinc borosilicate frit as its binder?
Claim language“20-40% Bi2O3”
The main ink carries milled zinc borosilicate frit and black spinel pigment in an organic printing vehicle. A lower-softening bismuth borate frit in the second ink forms a liquid phase during firing that wets the glass and binds the pigment.
1.8Lithium oxide flux
What ifWhat if the compensating ink uses 2% lithium oxide by weight?
Claim language“2-7% of ZnO”
Lithium carbonate enters the frit batch and supplies lithium oxide during melting. The frit is quenched and milled, then dispersed in a printing vehicle so the lithium-bearing bismuth borosilicate softens during firing and promotes flow.
1.9Phosphate based compensating frit
What ifWhat if the compensating ink uses a boron-free bismuth zinc phosphate frit?
Claim language“3-20% B2O3, and”
Phosphorus pentoxide supplies the glass-forming oxide in the compensating frit. The milled phosphate frit softens during firing and supplies a liquid phase that wets the glass and binds the pigment in the blended coating.
1.10Higher pigment compensating ink
What ifWhat if the compensating ink carries 18% ceramic black pigment by weight?
Claim language“0.2-15% ceramic black pigment”
The main ink carries 20% black spinel pigment by weight, and both inks use the same pigment. At equal deposited masses on the same composition basis, the blend contains 19% pigment and gains a lower-softening binder from the bismuth-rich compensating frit.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Fired markings on glass laboratory vessels
A rotary fixture holds borosilicate laboratory vessels beneath two inkjet heads that receive separate feeds of the main ink and the compensating ink. The fixture indexes each vessel while the heads deposit overlapping droplets to form graduation marks and identification text. The controller uses a blend ratio established on coupons of the vessel glass by firing test marks and measuring adhesion and optical contrast. The marked vessels pass through a firing oven that fuses the ceramic deposit to the glass.
Component substitution
Static mixer feeding one printhead
Two metering pumps deliver the main ink and the compensating ink to a helical static mixer upstream of a single recirculating piezoelectric printhead. The pump flow ratio sets the wet blend composition, and the mixer homogenizes the feeds before the ink enters the printhead circuit. At a ratio change, a divert valve routes the transitional blend to a collection vessel until the new blend displaces the ink in the mixer and supply circuit. The valve then returns the flow to the printing circuit.
Sequential screen printing of both inks
Two registered flatbed screen stations replace the inkjet heads and use ceramic screen-printing vehicles for the main and compensating compositions. The first screen prints the main ink pattern, and an intermediate dryer removes enough vehicle to prevent pickup at the second screen. The second screen deposits the compensating ink through matching openings, with stencil thickness and mesh selection setting its dry deposit mass relative to the first layer. The firing cycle fuses the overlapping deposits into a single ceramic coating.
Parameter or scale variation
Five blend levels on test strips
Two independently metered ink channels print five 15 × 15 mm patches on a 25 × 120 mm glass strip. The patches contain 0%, 10%, 20%, 30%, and 40% compensating ink by deposited dry solids mass, with equal total dry solids mass per unit area. The controller calculates the drop count for each channel from its measured drop mass and solids fraction. The strip passes through one firing cycle, and the fired patches provide a side-by-side comparison of adhesion, gloss, and optical density.
Combination with existing systems
Blend selection on a bottle line
A two-channel ceramic ink station sits between a machine-vision inspection station and the firing oven on a rotary bottle decoration line. The inspection station reads an embossed mold identifier under angled illumination and associates it with the bottle's carrier position using a conveyor encoder. At the print station, the controller retrieves a stored blend recipe for that identifier and commands the two heads to deposit registered droplets on the rotating bottle. The recipe table stores the blend established by firing and inspecting sample bottles from each mold.
Automated or data-driven variant
Fired gloss and density feedback
The two ink channels print a control patch on a witness coupon that travels through the oven with each production batch. After cooling, a fixed-angle gloss sensor and a reflectance densitometer measure the fired patch. The controller compares those readings with a calibration table generated from fired coupons at known blend ratios and deposited solids loads. It selects the ratio and solids load for the next batch from entries that meet the minimum optical density and minimizes the difference from the target gloss.
Specific version of a part
Boric acid batch source
Boric acid supplies boron for a main ink formulated to contain 12% B₂O₃ by weight. The batch mass accounts for water released by the boric acid during heating, and the boron enters the glass network during frit melting.
Copper chromite black pigment
The main ink contains 15% copper chromite spinel pigment by weight. The pigment is milled separately from the frit and dispersed into the ink to control the size of pigment agglomerates.
Eight percent silica frit
Fine quartz powder supplies silica for a compensating ink formulated to contain 8% SiO₂ by weight. The quartz dissolves in the frit melt before quenching and milling.
Seventy percent bismuth oxide
The compensating ink contains 70% Bi₂O₃ by weight, supplied by its frit. Bismuth oxide powder is melted with the other frit oxides, and the quenched glass is milled before dispersion in the printing vehicle.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
An optical glass comprises: germanium oxide (GeO2) content of 14 wt % to 21 wt %; niobium oxide (Nb2O5) content of 14 wt % to 23 wt %; bismuth oxide (Bi2O3) content of 40 wt % to 52 wt %; tungsten oxide (WO3) content of 0 wt % to 5 wt %; phosphoric acid (P2O5) content of 7 wt % to 14 wt %; potassium oxide (K2O) content of 0 wt % to 4 wt %; barium oxide (BaO) content of 0 wt % to 5 wt %; lithium oxide (Li2O) content of 0 wt % to 3 wt %; sodium oxide (Na2O) content of 0 wt % to
A · US 2008/0242528 A1 · abstract
1.33-20% B2O3, and
1.410-20% ceramic black pigment,
1.5wherein the compensating ink comprises:
1.65-10% SiO2,
1.765-75% Bi2O3,
1.82-7% of ZnO,
1.93-20% B2O3, and
1.100.2-15% ceramic black pigment,
1.11wherein addition of the compensating ink to the main ink results in a reduction in percentage composition of SiO2 and the ceramic black pigment to achieve a lower melting temperature, and wherein the addition of the compensating ink to the main ink results in an increase in the percentage composition of Bi2O3 to also achieve the lower melting temperature.
Specifically, the glass frits formed by firing the wavelength conversion glass frit composition at the glass frit temperature may be uniformly melted at a temperature lower than the temperature at which the wavelength conversion glass frit composition is fired. That is, a melting point of the glass frits may be lowered.
B · US 2018/0370847 A1 · ¶ 50
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Only Document B has a passage for 1.11. Both are classified in CPC C03C, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, a decrease in the size of the image pickup lens and a high performance have recently been noticeable, and thus a higher refractive index of the optical glass and an easier processing operation have been further demanded.
A · US 2008/0242528 A1 · ¶ 9
Related claim parts: 1.11
The invention is made in view of such problems, and an object of the invention is to provide an optical glass which has higher refractive index and is excellent in a molding property.
A · US 2008/0242528 A1 · ¶ 10
Therefore, it is necessary to develop a wavelength conversion glass that exhibits high transmittance and excellent thermal stability.
B · US 2018/0370847 A1 · ¶ 5
A purpose of the present disclosure is to provide a wavelength conversion glass exhibiting high transmittance, excellent thermal stability, and wavelength conversion efficiency.
B · US 2018/0370847 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0365565 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365565/, SHA-256 f1b1ca7f985122faf4f540b191b025b1b0910714ecafac9487d6f14014f0798d