patent.fyi
Applications  /  US 2026/0365566
United States Patent Application Publication

US 2026/0365566 A1

Published
Nov 19, 2026
Filed
Nov 22, 2023
Earliest date on the face
Nov 25, 2022
Classification
C03C 17/30
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Direct grafting to glass

What ifWhat if the water-repellent layer bonds directly to the glass after oxygen plasma treatment?
Claim language“forming a primer layer”

An oxygen plasma removes organic residue from the glass, and exposure to water vapor provides surface silanol groups. Hydrolyzed octyltrimethoxysilane condenses with those groups during curing to form siloxane bonds and leave octyl groups at the exposed surface.

1.2Adhesive lamination of fluoropolymer film

What ifWhat if a pressure roller laminates a transparent fluoropolymer film onto the primed glass using an optically clear adhesive?
Claim language“grafting of a layer”

A clear acrylic pressure-sensitive adhesive bonds the treated back face of a fluorinated ethylene propylene film to the primer. A roller presses the laminate against the glass and drives out trapped air, while the exposed fluoropolymer surface repels water.

1.3Butoxy groups on silicon

What ifWhat if each hydrolyzable substituent on the octylsilane is an n-butoxy group?
Claim language“a C1-3 alkoxy group”

Water and a mild acid catalyst hydrolyze the butoxy groups of octyltributoxysilane to silanols and release butanol. The silanols condense with hydroxyl groups on a silica primer during curing, leaving octyl groups at the coating surface.

1.3Ten-carbon alkyl chain

What ifWhat if the alkyltrialkoxysilane carries a ten-carbon alkyl chain?
Claim language“where n=3-8”

Decyltrimethoxysilane hydrolyzes in an acidified ethanol and water mixture. The resulting silanols condense with surface hydroxyl groups on a silica primer, and the exposed decyl chains reduce water wetting.

1.4Acetoxy groups on silicon

What ifWhat if the octylsilane carries three acetoxy groups on silicon?
Claim language“a chlorine atom”

Moisture hydrolyzes octyltriacetoxysilane to silanols and releases acetic acid. The silanols condense with hydroxyl groups on the primer and with neighboring silanols to form an octyl-bearing siloxane layer.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Exterior coating for rail cab glazing

A transparent primer covers the weather-facing surface of a laminated rail cab windshield. An octyltrimethoxysilane layer grafts onto the dried primer through condensation with surface hydroxyl groups. The treated face sits outside the cab, where surface alkyl groups reduce wetting by rain.

Component substitution

Sputtered alumina as the primer layer

A transparent alumina film replaces the silica primer on the selected glass face. Reactive magnetron sputtering deposits the film from an aluminum target in an argon and oxygen atmosphere. Water vapor exposure hydroxylates the alumina surface. Hydrolyzed hexyltrimethoxysilane condenses with surface hydroxyl groups during warm drying and leaves hexyl groups at the exposed surface.

Parameter or scale variation

Heated primer drying on glass coupons

A wire-wound drawdown rod spreads a 10 µm wet layer of colloidal silica dispersion on one face of a 100 mm by 150 mm glass coupon. A forced-air oven dries the primer at 80 °C for 10 minutes. After the coupon cools to 25 °C, an applicator spreads hydrolyzed propyltrimethoxysilane over the primer. A second oven hold at 80 °C for 30 minutes promotes condensation at the primer surface.

Hydrophobic coating on both glass faces

An edge-grip fixture holds a 300 mm by 300 mm glass pane vertically and exposes both main faces. Opposed spray heads apply colloidal silica primer to both faces in one pass, and filtered air dries the films. A second pair of spray heads applies hydrolyzed octyltrimethoxysilane over the two primer films. The fixture holds the pane by its edges during a 30-minute cure at 80 °C.

Combination with existing systems

Hydrophobic cover for a heated camera

An outdoor camera looks through a glass cover with a transparent resistive heater on the interior face. The exterior face carries a silica primer and a grafted octyltriethoxysilane layer. A thermistor at the cover edge feeds a controller that switches current to the heater when the glass approaches freezing. The heater warms the cover while the exterior coating reduces wetting by rain and meltwater.

Automated or data-driven variant

Optical feedback for primer deposition

A conveyor carries each glass sheet beneath a metered spray head that applies a silica primer to the upper face. After drying, a spectral reflectometer samples the primer at three positions across the sheet and estimates dry thickness using a calibrated film model. A controller adjusts the primer pump rate for subsequent sheets using the difference between the mean measured thickness and the target. A downstream head applies hexyltrimethoxysilane to the dried primer, and a heated zone promotes grafting.

Specific version of a part

Dip-coated silica primer

Clean glass is dipped into an acid-catalyzed silica sol prepared from tetraethoxysilane, ethanol, and water. Controlled withdrawal and drying form a transparent silica primer with surface silanol groups.

Spray grafting followed by curing

A fine spray applies dilute hydrolyzed octyltriethoxysilane in ethanol and water to a hydroxylated silica primer. A warm cure promotes condensation between silanols in the applied layer and silanols on the primer.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 10,185,057 B2
Published
Jan 22, 2019
Filed
Nov 8, 2012
Class
G02B 1/14
Document BUS 2019/0062564 A1
Published
Feb 28, 2019
Filed
Aug 24, 2018
Class
C09D 5/038
Claim 1
Document A
Document B
1.1forming a primer layer on one of the main surfaces of the glass substrate,
In some cases, a primer coating is applied to the substrate surface prior to application of the porous sol-gel layer. The primer coating is interposed between the substrate and the sol-gel layer, and serves as a barrier coating and/or as an adhesive layer to promote adhesion of the sol-gel layer to the substrate surface.
A · US 10,185,057 B2 · ¶ 44
1.2grafting of a layer of C3-C8 alkyltrialkoxysilane and/or C3-C8 alkyltrichlorosilane onto the primer layer,
The sealant layer may be deposited onto the porous sol-gel layer from a solution of alkyltrihalosilane in an aprotic solvent, such as a 5 percent by weight solution of alkyltrihalosilane in ISOPAR L, a mixture of isoparaffins available from ExxonMobil Chemicals, or in SOLVESSO 100, a mixture of aromatic solvents, also available from ExxonMobil Chemicals.
A · US 10,185,057 B2 · ¶ 42
The invention is characterised in that the filler comprises particles which have a surface coating, the particles comprising a siliceous or carbonatic component and having a basic pH value in aqueous solution, and the surface coating of the particles comprising one of the substances alkyltrimethoxysilane, alkyltriethoxysilane and/or alkyl siloxane.
B · US 2019/0062564 A1 · ¶ 5
1.3wherein the C3-C8 alkyltrialkoxysilane is an alkyltrialkoxysilane of formula CnH2n+1SiR3, where n=3-8, each R representing a C1-3 alkoxy group, and
The alkoxysilane has the general formula R1mSi(OR2)4-m, wherein each R1 may be the same or different and represents an organic radical; each R2 may be the same or different and represents a C1 to C4 alkyl group, and m is 0 to 3. R1 can be C1 to C6 alkyl, vinyl, methoxyethyl, phenyl, γ-glycidoxypropyl, or γ-methacryloxypropyl.
A · US 10,185,057 B2 · ¶ 47
1.4wherein the C3-C8 alkyltrichlorosilane is an alkyltrichlorosilane of formula CnH2n+1SiR3, where n=3-8, each R representing a chlorine atom.
Examples of suitable alkyltrichlorosilanes include methyltrichlorosilane, vinyltrichlorosilane, ethyltrichlorosilane, n-propyltrichlorosilane, i-propyltrichlorosilane, γ-chloropropyltrichlorosilane, i-butyltrichlorosilane, n-butyltrichlorosilane, pentyltrichlorosilane, hexyltrichlorosilane, heptyltrichlorosilane, n-octyltrichlorosilane, i-octyltrichlorosilane, hexadecyltrichlorosilane, 10-undecenyltrichlorosilane, 13-tetradecenyltrichlorosilane, 14-pentadecenyltrichlorosilane
A · US 10,185,057 B2 · ¶ 41

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1 1.3 1.4. Both have a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

According to at least one further embodiment, the surface coating comprises a hydrophobic component.
B · US 2019/0062564 A1 · ¶ 7

Related claim parts: 1.3 1.4

Polymeric organic materials that typically are used to make optical elements, transparent sheets and films, often have surfaces that are susceptible to abrasion and chemical attack.
A · US 10,185,057 B2 · ¶ 2
It would be desirable to provide articles having coatings that provide abrasion resistance approaching that of glass while allowing for lower cost, light weight, impact performance, moisture barrier and easy removal.
A · US 10,185,057 B2 · ¶ 4
However, materials having high pH values which could prevent or slow the growth of algae, mold and many plants, as well as corrosion, are not suitable for many applications owing to the other material properties thereof.
B · US 2019/0062564 A1 · ¶ 4
The hydrophobic component, also referred to as the active component, makes it possible for the filler, i.e. the particle comprising the surface coating, to be set so as to be more hydrophobic than the uncoated carrier particle.
B · US 2019/0062564 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365566 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365566/, SHA-256 e7f1ea350c972f42ce4b2e7bf6172eb7a1910a80f71037993c8eb93b360cfa1b
First published
Permanent addresshttps://patent.fyi/US20260365566/
Content fingerprint (SHA-256)e7f1ea350c972f42ce4b2e7bf6172eb7a1910a80f71037993c8eb93b360cfa1b