patent.fyi
Applications  /  US 2026/0365567
United States Patent Application Publication

US 2026/0365567 A1

Published
Nov 19, 2026
Filed
Mar 19, 2026
Earliest date on the face
May 16, 2025
Classification
C03C 17/32
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Inorganic metal mask replaces organic layer

What ifWhat if the first glass portion were protected by a sputtered chromium-free metal film patterned by lift-off, with no organic layer on that portion?
Claim language“forming a first organic layer”

A thin sputtered film of a corrosion-resistant metal, 100 to 300 nanometers thick, is deposited through a shadow mask onto the first glass portion. The film resists hydrofluoric acid etchant during the etching step. The film is later stripped with a selective metal etchant that does not attack the glass.

1.5Laser ablation removes glass

What ifWhat if the glass substrate were shaped by scanning a pulsed ultrashort laser over the exposed region to remove material, with no chemical etching?
Claim language“etching the glass substrate”

A femtosecond or picosecond laser beam is focused on the exposed glass surface and scanned along a programmed path. Each pass removes a thin layer by ablation, and the number of passes sets the depth. A brief polishing step with a mild flame or a light chemical rinse smooths the ablated surface.

1.4Keep the first layer in place

What ifWhat if the first organic layer were left on the first glass portion through the etching step, and only the second organic layer were removed afterward?
Claim language“removing the first organic layer”

The first organic layer is formed from an etchant-resistant polymer film, and the second layer covers the remaining area so only the intended region is exposed. Both layers withstand the etchant bath. After etching, a single stripping step removes the layers together.

1.1Single continuous glass region

What ifWhat if the glass substrate had one uniform surface region that is masked by a single patterned layer, with no separate adjacent portions defined?
Claim language“a second glass portion that is adjacent the first glass portion”

One organic resist layer is applied across the whole surface and patterned by photolithography to open the areas to etch. The etchant attacks only the openings. The resist is then stripped, and the substrate has the preset shape.

1.6Sacrificial layer consumed by etchant

What ifWhat if the second organic layer were a thin film that dissolves during the etching bath itself, so no separate removal step is run?
Claim language“removing the second organic layer”

The second layer is a thin water-soluble or acid-soluble polymer film of calibrated thickness. It protects the covered region for the first part of the bath and then dissolves at a known rate. The etch time is set so that the covered glass receives only a shallow etch while the open glass is etched deeper.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Selective etching of microfluidic glass chips

A borosilicate glass plate for a microfluidic device has a channel region as the first glass portion and a surrounding bonding surface as the second glass portion. A water-soluble polymer film is printed over the channel region. A UV-curable acrylic resin is then printed over the bonding surface and over the edge of the polymer film. The polymer film is rinsed away with warm water, which leaves the resin intact. The plate is immersed in a hydrofluoric acid bath, which cuts the channel to a depth of 50 micrometers, and the resin is then stripped with an organic solvent.

Component substitution

Dry plasma etching in place of wet acid

The etching step uses a reactive ion etching chamber fed with a fluorocarbon gas and argon in place of a liquid acid bath. The first organic layer is a water-soluble polyvinyl alcohol film and the second organic layer is a cross-linked photoresist-type polymer. After the water rinse removes the polyvinyl alcohol, the substrate is placed on a cooled electrode in the chamber. Radio-frequency power of 300 watts drives anisotropic etching of the exposed glass. The remaining polymer is stripped with an oxygen plasma ashing step, which gives near-vertical sidewalls.

Automated or data-driven variant

Vision-guided alignment of the second organic layer

A line-scan camera images the first organic layer after curing and sends the image to a processing unit. Image analysis locates the layer edge to within 5 micrometers and computes the offset to the target position. The processing unit corrects the inkjet head coordinates so that the second organic layer overlaps the edge by a set width of 30 micrometers. After etching, a second camera measures the etched profile. A regression model uses the measured depth to adjust etch time for the next substrate.

Closed-loop etch control with conductivity sensing

The etching bath contains a conductivity sensor, a fluoride ion probe and a temperature sensor wired to a controller. The controller doses fresh acid through a metering pump when the fluoride concentration falls below a set point of 5 percent by weight. It also holds the bath at 30 degrees Celsius with a heater and chiller. A trained gradient-boosting model predicts the etch rate from the sensor readings and sets the immersion time for each substrate. A thickness gauge at the exit verifies the removed depth and updates the model.

Specific version of a part

Adhesive laminated film as second mask

A polyolefin sheet with a pressure-sensitive adhesive is die-cut to the mask outline. A roller laminator presses the sheet onto the glass at a set pressure so the edge seals against the surface. After etching, the sheet is peeled off by hand or by a peeling roller.

Photocurable acrylic resist by screen printing

A photocurable acrylic resin is screen printed on the first glass portion at a thickness of 10 to 30 micrometers. Ultraviolet light at about 365 nanometers cures it. The cured film resists hydrofluoric acid etchant.

Inkjet-printed wax-based second layer

A piezo inkjet head deposits a hot-melt wax-based ink onto the second glass portion and over the edge of the first organic layer. The ink solidifies on contact with the glass held at 25 degrees Celsius. The overlap of 0.2 to 1 millimeter seals the boundary between the two layers.

Solvent stripping of the first layer

The substrate is dipped in a heated amine-based stripping solution at 60 degrees Celsius with ultrasonic agitation. The first organic layer swells and lifts from the glass. The second layer is made from a polymer that does not swell in this solution, so it stays in place.

Spray etching with buffered acid

A buffered hydrofluoric and ammonium fluoride solution is sprayed onto the substrate from oscillating nozzles in a conveyor chamber. The etchant temperature is held at 25 degrees Celsius and the line speed sets the etch depth. A water rinse and a nitric acid rinse follow to remove residue.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2023/0183130 A1
Published
Jun 15, 2023
Filed
Nov 28, 2022
Class
C03C 23/0025
Document BUS 2024/0426734 A1
Published
Dec 26, 2024
Filed
Jun 20, 2023
Class
G01N 15/088
Claim 1
Document A
Document B
1.1providing a glass substrate comprising a first glass portion and a second glass portion that is adjacent the first glass portion;
A method of manufacturing a glass substrate having a penetrating structure, the method includes: (1) preparing a glass substrate that has a first surface and a second surface opposite to each other, and includes 3 mol % to 30 mol % of B2O3 in terms of oxide;
A · US 2023/0183130 A1 · abstract
1.2forming a first organic layer on the first glass portion;
In one or more embodiments, photolithographically exposing sites for metal electrodes at block 301 includes applying a photoresist polymer coating to the substrate, then curing the photoresist coating.
B · US 2024/0426734 A1 · ¶ 23
1.3forming a second organic layer on the second glass portion and a portion of the first organic layer;
1.4removing the first organic layer;
1.5etching the glass substrate; and
(3) wet etching the glass substrate having the initial penetrating structure formed;
A · US 2023/0183130 A1 · abstract
After patterning the photoresist with the mask, dry etching may be performed to remove substrate material from the areas not covered by photoresist. Removal of the substrate material leads to patterning of the substrate.
B · US 2024/0426734 A1 · ¶ 25
1.6removing the second organic layer.
This method 400 includes coating a photoresist on a substrate, at block 401, baking out the photoresist, at block 403, removing portions of the photoresist with ultraviolet lithography, at block 405, depositing metal electrodes on exposed portions of the substrate, at block 407, exposing the photoresist and substrate to ultraviolet radiation with a mask to form a pattern in the photoresist, at block 409, dry etching the substrate to form a plurality of channels in the substra
B · US 2024/0426734 A1 · ¶ 26

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1. Only Document B has a passage for 1.2 1.6. Both have a passage for 1.5.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Such a bump portion may cause a problem when using the glass substrate for a glass interposer or the like.
A · US 2023/0183130 A1 · ¶ 6
Glass substrates having a penetrating structure such as a through hole have many applications including glass filters, glass interposers, substrate integrated waveguides (SIW), and post-wall waveguides.
A · US 2023/0183130 A1 · ¶ 3
However, for EEOR, there remains a need for equipment for laboratory testing and characterization to estimate the impact of electrical current on pore throat size to effectively design the electric current parameters and the treatment time for EEOR applications.
B · US 2024/0426734 A1 · ¶ 2
EEOR is one of the most promising EOR techniques because of its electrical efficiency and overall usefulness while minimizing environmental impact.
B · US 2024/0426734 A1 · ¶ 1
Cite aspatent.fyi, US 2026/0365567 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365567/, SHA-256 38d259c1d2682673973ed95ae45f3d9ed9aac38102ee689aa6be5497ed913a57
First published
Permanent addresshttps://patent.fyi/US20260365567/
Content fingerprint (SHA-256)38d259c1d2682673973ed95ae45f3d9ed9aac38102ee689aa6be5497ed913a57
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi