Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Lower stress with closer spacing
What ifWhat if the glass spacer has 500 MPa of surface compression and the support array uses a closer pitch?
Claim language“about 700 MPa to about 1,000 MPa”
A potassium and sodium ion exchange bath produces a surface compressive stress of 500 MPa in the glass. A square array with a pitch of 20 mm carries about 40 N per interior spacer at a pressure difference of 100 kPa.
1.1Higher compression at the surface
What ifWhat if the surface compressive stress is 1,200 MPa?
Claim language“about 700 MPa to about 1,000 MPa”
A sodium exchange stage forms a deeper compressive layer in lithium aluminosilicate glass, and a short potassium exchange stage sets the surface compression at 1,200 MPa. The shallow potassium enriched layer resists the opening of small surface flaws, and the flat end faces transfer the compressive load between the panes.
1.2Lower tension with shallow exchange
What ifWhat if the peak central tensile stress is 20 MPa?
Claim language“about 40 MPa to about 90 MPa”
A short potassium exchange forms a shallow compressive layer in a polished sodium aluminosilicate spacer. The shallow layer limits the integrated compressive stress that the core balances, and the spacer's flat end faces carry the pane load in axial compression.
1.2Higher tension with deeper exchange
What ifWhat if the peak central tensile stress is 120 MPa?
Claim language“about 40 MPa to about 90 MPa”
A longer sodium exchange in lithium aluminosilicate glass deepens the compressive layer. The larger integrated surface compression is balanced by a core stress profile that peaks at 120 MPa, and a flat cylinder with rounded contact edges transmits the pane load in axial compression.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Vacuum jacket for a microscope chamber
A temperature-controlled microscope chamber has a double-pane window in its observation port. Transparent, ion-exchanged glass pillars sit between the panes on a square grid, with the central observation area between four adjacent pillars. A perimeter seal encloses the evacuated gap, and the pillars carry the pressure load while the microscope images the specimen through the central area.
Component substitution
Fused silica pillars with polished ends
Short cylinders of fused silica replace the chemically strengthened glass pillars between the panes. Both ends of each cylinder are lapped flat and parallel, and the perimeter of each end has a small polished bevel. The cylinders transmit visible light and carry the pressure load in axial compression. Cylinder diameter and pitch are selected from compression tests on representative pane and cylinder assemblies.
Parameter or scale variation
Closer pillar spacing near panel corners
A 600 mm square prototype uses two 4 mm glass panes separated by transparent, ion-exchanged glass pillars with a height of 0.25 mm. The central field uses a 25 mm square pitch, and a 50 mm square zone near each corner uses a 12.5 mm pitch. The closer spacing divides the atmospheric load near the corners among more contacts. Evaluation uses a gradual pressure reduction while measuring pane deflection and inspecting the glass at the pillar contacts.
Combination with existing systems
Vacuum glazing with radiant defogging
A transparent conductive oxide coating is deposited on the exposed face of one pane in a vacuum glazing assembly supported by transparent, ion-exchanged glass pillars. Busbars along opposite edges of the coating connect to a low-voltage supply, and a surface temperature sensor sits near the edge of the viewing area. A controller regulates current through the coating to keep the exposed glass above the dew point on that side. The wiring stays outside the evacuated gap.
Automated or data-driven variant
Machine vision for pillar placement
A telecentric camera with oblique illumination locates the edges of transparent, ion-exchanged glass pillars on a feeder tray. Software registers the lower pane from its edge coordinates and directs a vacuum pick head to place a pillar at each position in the panel layout. A second image measures each pillar's position after placement, and the pick head corrects positions outside the assembly tolerance before the upper pane is fitted.
Sensor guided ion exchange bath control
Transparent glass pillar blanks sit in shallow perforated trays that keep the pieces separated during two successive molten salt exchanges. Thermocouples monitor bath temperature, and an ion analyzer measures sodium and potassium concentrations in cooled bath samples. A controller uses these readings to hold the bath temperatures and schedule salt replenishment, and a timed lift transfers the trays between stages. Stress measurements on witness pieces of matching glass composition and thickness provide feedback for adjusting the stage durations between batches.
Specific version of a part
Surface compression at 780 mpa
A potassium nitrate bath exchanges potassium for sodium in a polished sodium aluminosilicate spacer. Bath temperature and dwell time set the surface compressive stress at 780 MPa.
Surface compression at 950 mpa
A sodium nitrate bath replaces lithium near the surface of a lithium aluminosilicate spacer and forms a deep compressive layer. A subsequent potassium nitrate bath enriches the outer layer in potassium and sets the surface compressive stress at 950 MPa.
Central tension at 65 mpa
A 0.30 mm thick glass spacer undergoes ion exchange on both bearing faces to produce a symmetric stress profile through its thickness. Exchange time controls the depth of compression and sets the peak tensile stress at the midplane to 65 MPa.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1wherein the spacer comprises a compressive surface stress in a range of about 700 MPa to about 1,000 MPa, and
In contrast, ion exchange (IX) techniques can produce high levels of compressive stress in the treated glass, as high as about 1000 MPa at the surface, and is suitable for very thin glass.
A · US 2016/0280591 A1 · ¶ 8
1.2wherein the spacer comprises a central tension maximum stress in a range of about 40 MPa to about 90 MPa.
After the anneal of 6 hours at 455° C., the final compression stress (fCS) was about 227 MPa, the final depth of compressive layer (fDOL) was about 100 μm, and the final central tension (CT) was 42 MPa.
A · US 2016/0280591 A1 · ¶ 60
The value of this CT1 is proposed as an upper limit of the value of the central tension CT and defined as a critical value of the onset of unacceptable frangible behavior.
B · US 2018/0230045 A1 · ¶ 3
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Both have a passage for 1.2. Both are classified in CPC C03C, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Although the conventional single step ion exchange processes may employ a long ion exchange step to achieve a higher depth of compressive layer (DOL), such lengthy durations also result in a rise in the central tension (CT) past a chosen frangibility limit of the glass, resulting in undesirable fragmentation of the glass.
A · US 2016/0280591 A1 · ¶ 9
Related claim parts: 1.2
Indeed, although a DOL of about 101 μm was achieved, a relatively high CT of 65 MPa results, which was higher than the desired frangibility limit (48 MPa) of the subject glass sheet.
A · US 2016/0280591 A1 · ¶ 9
Related claim parts: 1.2
The embodiments disclosed herein relate to methods for producing ion exchanged glass, especially such glass with characteristics of moderate compressive stress, high depth of compressive layer, and/or desirable central tension.
A · US 2016/0280591 A1 · ¶ 3
However, as expressed in the equation (1), by increasing the value of CS or DOL, the central tension (CT) became large, too, a value of which was limited by the upper limit expressed by the equation (2).
B · US 2018/0230045 A1 · ¶ 5
In consequence, the upper limits of CS and DOL were also substantially limited.
B · US 2018/0230045 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0365568 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365568/, SHA-256 ae9434112df0988fd8c4bf0e3bf2393ceaca893f7a30129839046efba13bd2a5