patent.fyi
Applications  /  US 2026/0365569
United States Patent Application Publication

US 2026/0365569 A1

Published
Nov 19, 2026
Filed
Mar 25, 2026
Earliest date on the face
Apr 9, 2025
Classification
C03C 21/007
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Scribed groove instead of perforations

What ifWhat if the edge contour were defined by a continuous mechanically scribed groove with a controlled median crack depth, and not by a row of perforations through the interior?
Claim language“a plurality of perforations that extend in a first direction”

A hardened wheel or a diamond tool cuts a shallow score line along the contour, which creates a median crack. The scored sheet is steam treated so that moisture enters the crack faces, and the sheet is then separated by applying bending moment along the score. The crack faces become the new edges and carry the hydrogen-enriched layer.

1.2Etched channels in place of damaged volumes

What ifWhat if each contour were formed by a through-hole produced by laser-induced modification followed by wet chemical etching, so that each hole is an open, smooth-walled channel with no void or micro-fissure population?
Claim language“each perforation comprises a volume of the glass or glass-based material having a plurality of voids and/or micro-fissures”

A focused ultrashort-pulse laser modifies a thin line through the glass thickness along the contour. The sheet is immersed in an alkaline or hydrofluoric-based etchant that preferentially removes the modified track and widens it into an open hole with smooth walls. The sheet is then steam treated and separated along the hole row.

1.5Ion-exchanged alkali layer for compression

What ifWhat if the compressive layers carried an enriched larger-alkali-ion concentration produced by molten salt immersion, with no raised hydrogen content relative to the interior?
Claim language“an increased hydrogen concentration compared to a concentration of the interior”

The perforated sheet, which contains smaller alkali ions, is immersed in a molten potassium salt bath at a temperature below the strain point for several hours. Larger ions replace smaller ions in all exposed surfaces, including the walls of perforations. The crowding of ions creates compressive layers on the surfaces and along the perforation walls.

1.4Single-sided strengthening with a bonded backing

What ifWhat if only one surface were strengthened, and the opposite surface were joined to a separate laminated polymer or glass ply that carries the bending load?
Claim language“a second compressive layer extending from the second surface toward the first surface”

A single strengthened sheet is bonded to a backing ply with a transparent interlayer film in a heated pressure cycle. The backing ply takes the tensile stress that would otherwise load the unstrengthened surface. Edge flaws are shielded by the bonded ply and an edge seal.

1.1Polymer-core sandwich body

What ifWhat if the interior between the two surfaces were a polymer or honeycomb core, with thin glass skins on the outer faces and no glass in the interior?
Claim language“defines an interior comprising a glass or glass-based material”

Two thin strengthened glass skins are bonded to a lightweight core of cellular polymer or aluminum honeycomb with a structural adhesive. The assembly is pressed and cured at a set temperature. The core carries shear while the skins carry bending.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Strengthened glass edges for automotive sensor covers

A thin glass cover plate for a vehicle-mounted optical sensor is cut from a perforated sheet that is steam treated before separation. The perforations follow a closed rounded-rectangle contour, and each perforation carries a lateral compressive layer with increased hydrogen concentration. The plate is bonded over a lens aperture in a housing and sees repeated impacts from road debris and thermal cycling. The hydrogen-enriched edge layers lower the rate of edge chips that would otherwise scatter light into the sensor field of view.

Perforated and steam treated glass for microfluidic chips

A microfluidic chip substrate is formed from a glass sheet carrying perforation contour lines that outline many chip outlines, together with interior perforation lines that outline fluid ports. The sheet is steam treated so that the surfaces, the outer edges and the port walls each carry a compressive layer with increased hydrogen concentration. The sheet is then separated along the contours into chips, and the ports are opened by pushing out the enclosed plugs. A cover layer is bonded to each chip, and the strengthened port walls resist cracking when external tubing is pressed into the ports.

Component substitution

Ultrafast burst laser replaced by filamentation with bessel beam optics

The perforations are formed by a picosecond pulsed laser with an axicon lens that produces an elongated Bessel-like focal line, in place of a burst-mode laser with a standard focusing lens. The focal line is 0.5 mm long and is positioned through the full thickness of a 0.5 mm glass sheet. Each pulse group creates a filament track containing voids and micro-fissures. The sheet then goes into the steam treatment, which diffuses hydrogen laterally from the track walls to form the lateral compressive layer.

Parameter or scale variation

Fine pitch perforations in ultrathin glass

A glass sheet 100 µm thick is perforated with a pitch of 3 µm along a contour line, with each perforation extending through the full thickness. The sheet is steam treated at 300 °C and 8 bar saturated pressure for 4 hours in a sealed pressure vessel. The first, second and lateral compressive layers each reach a depth of about 15 µm. The separated parts have strengthened edges with sub-micron roughness, and they can be bent around a roll of 10 mm radius.

Combination with existing systems

Integration with roll-to-roll flexible glass display line

A continuous ribbon of flexible glass is unwound and passes through a laser perforation station that writes contour lines for display cover panels. The ribbon then passes through a segmented steam chamber with inlet and outlet seals, where the dwell time is set by the line speed and the chamber length. A separation station applies a localized thermal or mechanical stress that splits the ribbon along the contours. The finished panels pass to a coating station that applies an anti-reflective layer to the hydrogen-enriched surfaces.

Automated or data-driven variant

Closed-loop steam treatment controlled by edge strength model

A machine vision system images each perforated sheet and measures perforation pitch, void size and micro-fissure length. A trained regression model uses these measurements and the glass thickness to predict the steam temperature, pressure and duration needed to reach a target lateral depth of layer. A controller sets the setpoints of the steam vessel, and humidity and temperature sensors log the cycle. Sample coupons from each batch are tested by a bend test, and the results retrain the model to update later setpoints.

Specific version of a part

Thermally tempered surface layer

The sheet is heated near its softening range and cooled by opposed air nozzles at high heat-transfer rate. The outer regions solidify first and the interior contracts later, which leaves the surfaces in compression and the center in tension. The edge is then ground or laser finished to remove flaws, and the sheet thickness must be large enough to sustain the thermal gradient.

Bessel-beam filament perforation line

An ultrashort-pulse laser with a pulse duration under 10 ps is shaped by an axicon lens into a line focus of about 1 mm length. Pulses fire in bursts of several sub-pulses at a pitch of about 5 to 10 micrometers along the contour. Each burst produces a filament track with voids and micro-fissures through the sheet thickness.

Pressurized steam autoclave treatment

The perforated sheet is held in a sealed vessel in saturated steam at a temperature of about 100 to 200 degrees Celsius and elevated pressure for several hours. Water diffuses into the glass network through the surfaces and perforation walls and forms silanol groups. The result is a hydrogen-enriched layer several hundred nanometers to micrometers deep.

Aluminosilicate sheet with alkali content

The substrate is a down-drawn alkali aluminosilicate sheet with a thickness of 0.3 to 1.1 mm. The composition contains silica, alumina, sodium oxide and a small amount of magnesium oxide. The high alumina content raises the water diffusion rate and the network response to hydrogen uptake.

Perforation pitch and depth selection

The perforations are spaced at a center-to-center pitch of 4 to 12 micrometers along a closed contour, such as a rounded rectangle. Each perforation extends through the full thickness of the sheet. The tight pitch lets a mechanical bending or thermal stress step separate the part, and the steam reaches every edge wall through the open spaces.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2019/0352227 A1
Published
Nov 21, 2019
Filed
Aug 5, 2019
Class
C03C 21/002
Document BUS 2024/0360032 A1
Published
Oct 31, 2024
Filed
Jul 10, 2024
Class
C03C 21/002
Claim 1
Document A
Document B
1.1a first surface and a second surface, wherein the second surface is positioned opposite to the first surface and defines an interior comprising a glass or glass-based material;
A mirror finish polishing process was performed on both surfaces of the ground pieces of glass, and a glass plate with a thickness of 0.8 mm was obtained.
A · US 2019/0352227 A1 · ¶ 94
1.2a plurality of perforations that extend in a first direction from the first surface toward the second surface and through at least a portion of the interior, wherein each perforation comprises a volume of the glass or glass-based material having a plurality of voids and/or micro-fissures, and wherein the plurality of perforations form one or more contour lines in at least one of the first and second surfaces;
1.3a first compressive layer extending from the first surface toward the second surface;
A chemically strengthened glass includes a compressive stress layer. A compressive stress is 200 MPa or more at a surface of the chemically strengthened glass.
A · US 2019/0352227 A1 · abstract
In the ion exchange treatment, ion exchange occurs between alkali metal ions contained in the glass and alkali metal ions having a greater ion radius contained in the inorganic salt composition, and the compressive stress layer is formed on the surface portion of the glass.
B · US 2024/0360032 A1 · ¶ 5
1.4a second compressive layer extending from the second surface toward the first surface; and
1.5a lateral compressive layer extending in a second direction from each of the perforations within the interior, wherein the first, second, and lateral compressive layers each comprise an increased hydrogen concentration compared to a concentration of the interior at a midpoint between the first and second surfaces.
The hydrogen concentration after the chemical strengthening is highest at the outermost surface and gradually decreases toward a deeper portion (bulk) where no compressive stress layer is formed.
B · US 2024/0360032 A1 · ¶ 104

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1. Only Document B has a passage for 1.5. Both have a passage for 1.3. Both are classified in CPC C03C, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Display units and casings of electronic devices, such as mobile phones or smartphones often include chemically strengthened glasses in which surface layers are formed by ion exchange processes.
A · US 2019/0352227 A1 · ¶ 3

Related claim parts: 1.5

Patent Application Publication No. 2015/0239775 has a problem that when an electronic device falls on an asphalt surface, the chemically strengthened glass breaks easily despite the great depth of the compressive stress layer (DOL).
A · US 2019/0352227 A1 · ¶ 5
The present invention has been made in view of the above-described problem, and aims to provide a chemically strengthened glass that is less likely to break than conventional chemically strengthened glasses when the glass falls on an asphalt surface, by controlling a balance between the surface compressive stress (CS) and the depth of the compressive stress layer (DOL).
A · US 2019/0352227 A1 · ¶ 6
In this way, when an instantaneous external impact is applied due to the collision of a flying stone or the like, the stress during the collision is not alleviated and the stress is concentrated, which may damage the glass as the protective member and the sensor.
B · US 2024/0360032 A1 · ¶ 8
Therefore, an object of the present invention is to provide a chemically strengthened glass exhibiting flying stone resistance, drop ball strength, and scratch resistance more excellent than those in the related art, and a production method therefor.
B · US 2024/0360032 A1 · ¶ 9
Cite aspatent.fyi, US 2026/0365569 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365569/, SHA-256 8824cd33a656ed1aa0169dbe8006f821c78bd7d74b40c2fc8ce4410a0982d841
First published
Permanent addresshttps://patent.fyi/US20260365569/
Content fingerprint (SHA-256)8824cd33a656ed1aa0169dbe8006f821c78bd7d74b40c2fc8ce4410a0982d841
Methodv2026-11-18.2 · automated, not reviewed by a person