patent.fyi
Applications  /  US 2026/0365573
United States Patent Application Publication

US 2026/0365573 A1

Published
Nov 19, 2026
Filed
Nov 13, 2023
Earliest date on the face
Nov 25, 2022
Classification
C04B 20/04
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Low iron clay feed

What ifWhat if the feed is kaolinite-rich clay with 0.5 wt.-% iron expressed as Fe2O3 on a 950 °C loss-on-ignition-free basis?
Claim language“an iron content of at least 2 wt.-%”

The process forms the clay into lumps and heats them at 750 °C to dehydroxylate the kaolinite into metakaolin. The cooled material is ground to a powder for blending with hydraulic cement.

1.2Pan granulation of clay

What ifWhat if a rotating pan rolls moist clay powder into near-spherical granules?
Claim language“by extrusion, by pressing, or by compacting in a mold”

Water sprays onto a rolling bed of clay powder, and successive layers of powder adhere to the moist nuclei. A screen selects granules between 10 and 16 mm, and a dryer removes free moisture before calcination.

1.2Thin sheets within extrudates

What ifWhat if a multichannel die forms clay pieces with a surface-to-volume ratio above 1.00 mm−1?
Claim language“a surface to volume ratio in the range from 0.05 to 1.00 mm−1”

A die forms 20 mm wide pieces with open longitudinal channels separated by webs about 1 mm thick. The channel walls contribute to the exposed surface, and kiln gas flows through the channels during calcination.

1.2Three millimeter clay wafers

What ifWhat if the smallest dimension of each clay piece is 3 mm?
Claim language“the minimum extension of the lumps from 5 to 25 mm”

A slot die extrudes a 3 mm thick clay ribbon, and a cutter divides it into 30 mm square wafers. A perforated belt carries the dried wafers through the heated zone in a single layer, exposing both broad faces to kiln gas.

1.3Calcination under nitrogen

What ifWhat if the clay lumps are calcined in a nitrogen atmosphere?
Claim language“under oxidizing conditions”

An indirectly heated rotary retort tumbles the lumps at about 750 °C. A nitrogen sweep limits oxygen ingress and carries away water vapor released as the clay minerals dehydroxylate.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Calcined clay grog for bricks

A screw extruder forms iron-bearing clay into 12 mm diameter cylinders that a wire cutter cuts to 20 mm lengths. A kiln calcines the cylinders in air, and a cooler lowers their temperature before a roll mill grinds them. A screen collects the 0.25 to 1 mm fraction for use as grog in a brick body. A paddle mixer blends the grog with plastic clay before the brick body is formed, dried and fired.

Component substitution

Roller compaction with ribbon cutting

A pocketless roller compactor replaces the extruder or mold press and consolidates moist iron-bearing clay between two counter-rotating rolls. The roll gap and feed rate produce a continuous ribbon 10 mm thick. Slitting discs divide the ribbon into 15 mm strips, and a cross-cutting knife cuts the strips into 20 mm pieces. An air-fired kiln calcines the pieces before cooling and grinding.

Parameter or scale variation

Two-stage drying and calcination

A perforated conveyor carries 12 mm thick clay pieces in a single layer through a drying zone supplied with air at 150 °C. The conveyor provides 20 minutes of drying residence time before transferring the pieces to a separate calcination zone. The calcination zone uses a 750 °C air setpoint and provides 40 minutes of residence time. A forced-air cooler lowers the temperature of the calcined pieces before grinding.

Combination with existing systems

Cooler heat recovery for drying

A forced-air cooler receives calcined clay lumps and sends its hot exhaust through a cyclone to the hot side of an air-to-air heat exchanger. A separate fan drives clean air through the cold side and into a belt dryer upstream of the calciner. A mixing damper blends ambient air into the dryer supply to hold its temperature setpoint. The cooled lumps leave the cooler through a chute that feeds the grinding mill.

Automated or data-driven variant

Sensor feedback for oxidizing calcination

A thermocouple measures gas temperature in the calcination zone, and an extractive oxygen analyzer samples gas at the zone outlet. A programmable controller adjusts burner firing to maintain the temperature setpoint and trims the combustion air-to-fuel ratio to maintain the outlet oxygen setpoint. If oxygen falls below the configured lower limit, the controller pauses incoming lump feed while the exhaust fan maintains draft. Feed resumes when oxygen and temperature return to their operating bands.

Three-dimensional inspection of clay lumps

A singulating conveyor spreads formed clay lumps beneath laser triangulation heads that scan their exposed surfaces. A transfer between two scan stations turns the lumps over so the second station captures the belt-contact face. Software combines the scans into a closed surface mesh and calculates surface area, enclosed volume and minimum caliper dimension. A timed diverter returns pieces outside the configured dimension or surface-to-volume limits to the forming feed and sends accepted pieces to the calciner.

Specific version of a part

Iron reporting after ignition

A laboratory determines loss on ignition by heating a dried clay aliquot to 950 °C and measures total iron in the ignited residue by X-ray fluorescence. It reports iron as Fe2O3 by mass of the ignited residue and selects feed at or above 2 wt.-% on that basis.

Cut cylindrical clay extrudates

A screw extruder pushes plastic clay through a 12 mm circular die, and a wire cutter divides the strand into 15 mm lengths. The nominal cylinders have a minimum dimension of 12 mm and a surface-to-volume ratio of about 0.47 mm−1.

Rotary kiln with excess air

A gas-fired rotary kiln tumbles dried clay lumps through a zone held at 750 °C for kaolinite dehydroxylation. A flue gas oxygen analyzer provides feedback to the combustion air controls to maintain excess oxygen.

Air cooling and ball milling

A forced-air cooler lowers the calcined lump temperature below 80 °C before milling. A ball mill reduces the lumps to powder, and a dynamic air classifier returns coarse particles to the mill.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2009/0075824 A1
Published
Mar 19, 2009
Filed
Aug 11, 2006
Class
H01L 39/12
Document BUS 2020/0331806 A1
Published
Oct 22, 2020
Filed
Dec 26, 2018
Class
C04B 28/12
Claim 1
Document A
Document B
1.1providing a clay raw material with an iron content of at least 2 wt.-%, calculated as Fe2O3 on a loss on ignition at 950 °C free basis with respect to the total clay raw material,
Selecting marl (clayed lime-stone), comprising at least 70% CaCO3, as the raw material, b.
B · US 2020/0331806 A1 · ¶ 7
1.2forming lumps from the clay raw material with a surface to volume ratio in the range from 0.05 to 1.00 mm−1 and a size in the minimum extension of the lumps from 5 to 25 mm by extrusion, by pressing, or by compacting in a mold, wherein forming spherical particles by granulation is not used,
1.3calcining the lumps at a temperature from 450 to 1100 °C under oxidizing conditions to provide calcined lumps, and
Next, the mixture is calcined in an atmosphere (for example, air) containing 10 to 30% oxygen (hereinafter in the description this is also referred to as the oxygen-containing atmosphere) to obtain a calcined powder. The mixture is heated under a calcination condition of 880° C. to 960° C., more preferably 900° C. to 950° C. for 5 to 20 hours.
A · US 2009/0075824 A1 · ¶ 58
Calcining marl (clayed lime-stone), selected as the raw material, between temperatures 1000-1200° C., d.
B · US 2020/0331806 A1 · ¶ 7
1.4cooling and grinding the calcined lumps to provide calcined clay.
The calcined powder is put in a ceramic pot together with a zirconia ball and an organic solvent such as toluene and ball pulverization is performed to this calcined powder. The calcined powder is more finely pulverized by this ball pulverizing operation, thus making it possible to improve uniformity of the calcined particles and increasing thermal reactivity of the calcined particles in the next sintering step.
A · US 2009/0075824 A1 · ¶ 59
Re-grinding marl (clayed lime-stone), selected as the raw material, after the calcination process, e. Reducing the d90 particle size of the calcined marl to 486 nm after the grinding process, f.
B · US 2020/0331806 A1 · ¶ 7

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document B has a passage for 1.1. Both have a passage for 1.3 1.4.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Then, in each case of applying this wire material to a cable and applying it to a coil magnet, at least 1 km or more continuous superconducting thin film is desired, thus involving a technical problem that must be solved to improve a film forming speed of the superconducting thin film.
A · US 2009/0075824 A1 · ¶ 3
Similarly to sputtering methods as described above, the target bonded to the backing plate can be used as a laser ablation target in laser ablation methods.
A · US 2009/0075824 A1 · ¶ 7
By means of injection materials produced by using nano-sized lime, the repair of much thinner cracks is easily realized.
B · US 2020/0331806 A1 · ¶ 2
By means of the present art, it is difficult to provide the penetration, volume fixedness and resistance values which are required for reinforcing historical buildings.
B · US 2020/0331806 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0365573 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365573/, SHA-256 d07f60b495ae315b351d1f2b7308dacdcebefd225abf5d2a5bf32a527d921686
First published
Permanent addresshttps://patent.fyi/US20260365573/
Content fingerprint (SHA-256)d07f60b495ae315b351d1f2b7308dacdcebefd225abf5d2a5bf32a527d921686
Methodv2026-11-18.2 · automated, not reviewed by a person