Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.2Calcium carbonate filler with alkali activator
What ifWhat if the composition had no lime material and used ground limestone together with a sodium silicate solution as the alkaline component?
Claim language“a lime material comprising a calcium oxide and/or a calcium hydroxide”
Ground limestone acts as a fine filler and nucleation surface. Sodium silicate solution with a silica modulus near 1.5 raises the pore solution pH and dissolves the pozzolan. The dissolved aluminosilicate forms a binding gel, so the lime is not needed.
1.3Inert mineral aggregate without a pozzolan
What ifWhat if the composition had no pozzolan and relied on a hydrated magnesium carbonate network formed around coarse and fine aggregate for strength?
Claim language“a pozzolan”
Magnesium oxide and lime are mixed with graded sand and crushed stone at a water-to-binder ratio of about 0.4. The mixture is placed in a mold and cured in a carbon dioxide atmosphere. Magnesium oxide hydrates to brucite, and brucite converts to hydrated magnesium carbonates that interlock and bond the aggregate particles.
1.4Sulfate supplied by a soluble salt
What ifWhat if the composition carried its set-regulating sulfate as a dissolved magnesium sulfate solution added to the mixing water, with no solid gypsum?
Claim language“comprises gypsum at a concentration no more than 1.5% by weight”
Magnesium sulfate heptahydrate is dissolved in the mixing water at a few percent by mass of the binder. The dissolved sulfate controls the early reaction of the aluminate phases in the pozzolan and the hydration rate of the magnesium oxide. The dry mix holds no calcium sulfate, and the sulfate enters only at the mixing step.
1.4Composition without any sulfate regulator
What ifWhat if the composition had no sulfate-bearing set regulator at all and relied on a retarding organic admixture to control early reactions?
Claim language“wherein the building material composition comprises gypsum”
A hydroxycarboxylic acid retarder is added at 0.1 to 0.3 percent of binder mass. The retarder adsorbs on the surfaces of reactive particles and slows dissolution during mixing and placing. The mix sets in a controlled time without a sulfate source.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Carbonating lime-magnesia plaster for interior wall finishing
A dry premix of magnesium oxide, hydrated lime and ground brick powder is blended with fine silica sand and a cellulose ether thickener. The premix is mixed with water to a trowelable paste and applied in two coats of 6 mm each to interior masonry. The plaster hardens as hydrated lime and magnesium hydroxide react with carbon dioxide from room air, and a gypsum content below 0.5% by weight keeps the matrix free of sulfate phases. A relative humidity of 55% to 75% is held in the room during the first 14 days to support carbonation.
Carbon absorbing pavement base stabilizer for road subgrade
A powder of magnesium oxide, quicklime and ground granulated blast-furnace slag is spread over a clay-rich road subgrade at 4% to 8% by dry soil weight. A rotary soil mixer blends the powder to a depth of 300 mm and water is added to reach optimum moisture content. A smooth drum roller compacts the layer, and the layer cures under a perforated membrane that admits air for carbon dioxide uptake. The binder contains no added gypsum, so the stabilized layer shows no sulfate-driven swelling.
Component substitution
Calcined clay pozzolan with magnesium hydroxide slurry
Magnesium oxide is replaced by a magnesium hydroxide slurry at 55% solids, produced by hydrating dead-burned magnesia in a stirred tank. Hydrated lime and a metakaolin pozzolan made by calcining kaolinitic clay at 750 °C are dry blended in a paddle mixer. The slurry is metered into the dry blend to form a mortar with a water-to-binder ratio of 0.55. The mortar contains 0.3% gypsum by weight or less and gains strength through pozzolanic reaction and carbonation of the magnesium hydroxide and lime.
Parameter or scale variation
High-magnesia precast block cured in carbon dioxide chamber
A binder of 40% magnesium oxide, 30% hydrated lime and 30% silica fume by weight is mixed with lightweight aggregate at a binder-to-aggregate ratio of 1:3. The mix is pressed in a hydraulic block machine at 15 MPa into hollow blocks of 400 x 200 x 200 mm. The blocks are placed in a sealed chamber held at 20 °C and 70% relative humidity with 10% carbon dioxide by volume for 24 hours. The gypsum content stays at 0% by weight, and the blocks are then stacked for 28 days of air curing.
Combination with existing systems
Binder paste fed by flue gas capture unit
A cement kiln or biomass boiler exhaust duct is connected to a gas conditioning unit that cools the gas to 40 °C and removes particulates. The conditioned gas is fed at 12% to 15% carbon dioxide by volume into a curing tunnel holding extruded boards made from magnesium oxide, hydrated lime and fly ash with gypsum at 1% by weight. Fans recirculate the gas through the tunnel and a vent line returns the depleted gas to the stack. Boards cure in 48 hours and take up carbon dioxide from the exhaust stream.
Automated or data-driven variant
Sensor-controlled curing with predictive mix adjustment
Carbon dioxide, humidity and temperature sensors in a curing room send readings every 60 seconds to a controller. The controller adjusts a gas valve, a humidifier and a heater to hold set points for each curing stage, and embedded temperature probes in sample panels estimate the degree of carbonation. A regression model trained on past batches predicts compressive strength at 28 days from mix proportions of magnesium oxide, lime and pozzolan, and from the sensor history. The batching software then changes the pozzolan dosage within a 0.5% to 75% range and keeps gypsum under 1.5% by weight for the next batch.
Specific version of a part
Lightly calcined magnesite reactive magnesia
Magnesite is calcined at 700 to 800 degrees Celsius and ground to a median particle size of about 10 micrometers. The product has a high specific surface area and a high citric acid reactivity. It hydrates to brucite in the wet mix and carbonates in air.
Metakaolin pozzolan from calcined kaolinitic clay
Kaolinitic clay is calcined in a flash calciner at 700 to 800 degrees Celsius to form amorphous aluminosilicate. The product is ground to a median size of 5 to 10 micrometers. It is used at 20 to 40 percent of binder mass and reacts with lime to form calcium aluminosilicate hydrates.
Gypsum-free blend with ground slag
The binder is made of magnesia, hydrated lime and ground granulated blast-furnace slag, with no added calcium sulfate. The slag content is 30 to 50 percent of binder mass. Residual sulfur in the slag is below 1.5 percent gypsum equivalent by mass, and the blend is tested for set time and carbonation depth.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1magnesium oxide or magnesium hydroxide, preferably magnesium oxide;
The resulting hydrated lime has highly reduced contents of calcium oxide and magnesium oxide.
A · US 2013/0213264 A1 · abstract
1.2a lime material comprising a calcium oxide and/or a calcium hydroxide; and
Through subsequent addition of water, quicklime is converted into the less caustic (but still strongly alkaline) slaked lime or hydrated lime (calcium hydroxide, Ca(OH)2).
A · US 2013/0213264 A1 · ¶ 1
These components may include calcium hydroxide, fly ash, among others.
B · US 11,746,051 B2 · ¶ 13
1.3a pozzolan,
The pozzolan material may include any pozzolan material as generally known in the art. For instance, the pozzolan material may include, but is not limited to, fly ash, blast furnace slag, metakaolin, silica fume, microsilica, or a mixture thereof.
B · US 11,746,051 B2 · ¶ 18
1.4wherein the building material composition comprises gypsum at a concentration no more than 1.5% by weight of the building material composition.
For example, the gypsum may be present in the core in an amount of 20 wt. % or less, such as 15 wt. % or less, such as 10 wt. % or less, such as 8 wt. % or less, such as 5 wt. % or less, such as 4 wt. % or less, such as 3 wt. % or less, such as 2 wt. % or less, such as 1 wt. % or less, such as 0.5 wt. % or less based on the weight of the core.
B · US 11,746,051 B2 · ¶ 19
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.1. Only Document B has a passage for 1.31.4. Both have a passage for 1.2.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The quality of raw lime materials vary with the quality of the rock formations from which it is mined.
A · US 2013/0213264 A1 · ¶ 4
Hydrated lime is a very well-known and understood material that has been used for many years as an additive into many different industrial applications.
A · US 2013/0213264 A1 · ¶ 3
Commonly used cement boards may have deficiencies regarding their waterproofing capabilities.
B · US 11,746,051 B2 · ¶ 2
As a result, there is a need to further improve the waterproof performance of cement boards while also maintaining its durability.
B · US 11,746,051 B2 · ¶ 3
For instance, the cement board includes a water-resistant additive that allows for an improvement with respect to the waterproof performance.
B · US 11,746,051 B2 · ¶ 6
For instance, features illustrated or described as part of one embodiment can be used with another embodiment to yield a still further embodiment.
B · US 11,746,051 B2 · ¶ 5
While it is well known that the addition of pozzolanic material to cementitious mixtures can enhance the curing reaction and result in stronger and more durable concrete at reduced cost, there are significant tradeoffs in material processing and properties which can limit the use of pozzolanic materials in HPC and UHPC.
C · US 10,081,573 B2 · ¶ 31
Related claim parts: 1.3
Document C: US 10,081,573 B2, published Sep 25, 2018. Cited for this statement only.
Cite aspatent.fyi, US 2026/0365574 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365574/, SHA-256 578594ee11025814fa474f5b5f1f3e17de855211216a3594666d648ff95e82cc