1.1Fly ash in the binder
Blend low-calcium fly ash with ground hydraulic clinker and gypsum. Clinker hydration supplies calcium hydroxide, which reacts with the glassy fraction of the ash to form additional calcium aluminosilicate hydrate.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Blend low-calcium fly ash with ground hydraulic clinker and gypsum. Clinker hydration supplies calcium hydroxide, which reacts with the glassy fraction of the ash to form additional calcium aluminosilicate hydrate.
Blend metakaolin-rich calcined clay with ground hydraulic clinker and gypsum. The clay reacts with calcium hydroxide released by clinker hydration, and dissolved alumina reacts with calcium carbonate to form carbonate-bearing aluminate hydrates.
Mill calcitic limestone and combine it with an aqueous alkanolamine dose during batching. The fine calcite particles provide surfaces for hydrate growth and supply carbonate for reactions with dissolved aluminate.
Dissolve sodium sulfate in the batch water and disperse precipitated calcium carbonate in a binder containing granulated blast-furnace slag and hydraulic clinker. In the alkaline pore solution, sulfate reacts with calcium and dissolved aluminate to form ettringite as the slag hydrates.
Dose the solution into ground granulated blast-furnace slag and blend it with the batch water. The alkaline solution dissolves the slag glass, and soluble silicate combines with released calcium and alumina to form a calcium aluminosilicate hydrate gel.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Blend ground granulated blast furnace slag with precipitated calcium carbonate and an aqueous triethanolamine solution. Mix the activated binder with thickened mine tailings in a twin-shaft mixer and adjust the water content to the pumpable range measured for the tailings. Pump the paste through a backfill line into an underground void, where the binder hydrates and hardens.
Charge a 20 L planetary mixer with 5 kg of dry slag-containing binder and the weighed precipitated calcium carbonate. Dry-mix for 60 seconds at 60 revolutions per minute, then meter the alkanolamine solution and the remaining batch water over 30 seconds. Mix for another 120 seconds at 120 revolutions per minute and discharge the paste into molds.
Fit a continuous colloidal grout plant with separate loss-in-weight screw feeders for the slag-containing binder and precipitated calcium carbonate. Meter aqueous alkanolamine into the plant water line upstream of the high-shear mixing chamber, where the liquid meets both powder streams. Transfer the grout through an agitated holding tank to a positive-displacement pump for injection into masonry voids.
Install a gravimetric feeder for precipitated calcium carbonate and a liquid metering pump for alkanolamine on the pan mixer of a vibropress block line. Blend the carbonate with the slag-containing binder and graded aggregate, then spray the alkanolamine in the batch water over the moving solids to form a low-slump mix. Feed the mix into block molds, consolidate it under vibration and pressure, and transfer the demolded blocks to a humidity-controlled curing chamber.
Install a calibrated microwave moisture sensor at the outlet of the slag feed bin and weigh the incoming slag on a belt scale. A programmable controller calculates dry slag mass from the measured moisture fraction and uses it to set the precipitated calcium carbonate feeder rate and the alkanolamine solution pump rate. The controller subtracts the water in the incoming slag and alkanolamine solution from the batch water target and meters the balance into the mixer.
Water-granulate molten blast-furnace slag to produce glass-rich granules, then dry and grind them. Use the resulting powder as the slag fraction of a binder that also contains ground hydraulic clinker.
Recover entrained metal from crushed basic oxygen furnace slag by magnetic separation. Steam-condition the mineral fraction to hydrate free lime, then dry and grind it for blending with hydraulic clinker.
Use precipitated calcite with a median particle diameter of about 2 micrometres as the solid activator component. Dose triethanolamine as a dilute aqueous solution and count its water toward the batch water.
Dry-blend the slag-containing binder and precipitated calcium carbonate in a pan mixer. Add batch water containing dissolved alkanolamine while the paddles turn, then continue mixing until the paste is uniform.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The present disclosure also provides a method of manufacturing cement, comprising the step of mixing the above-mentioned granulated blast-furnace slag activator with granulated blast-furnace slag and activating the granulated blast-furnace slag.A · US 10,947,159 B2 · ¶ 9
This is the case of blast-furnace slag which a by-product of iron industry. By grinding this product into fine powder (GGBS) one can obtain a cementitious material that can be used in partial substitution of cement or used alone by adding some chemical activators (such as alkalis or sulfates).B · US 2021/0238094 A1 · ¶ 9
By grinding this product into fine powder (GGBS) one can obtain a cementitious material that can be used in partial substitution of cement or used alone by adding some chemical activators (such as alkalis or sulfates).B · US 2021/0238094 A1 · ¶ 9
An empty cell means only that no passage was reproduced there.
Only Document B has a passage for 1.3. Both have a passage for 1.1. Both are classified in CPC C04B, as is this patent.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Only in a certain alkaline environment to which a certain amount of sulfate is then added, granulated blast-furnace slag can be well activated, and higher cementation strength can be obtained.A · US 10,947,159 B2 · ¶ 2
Related claim parts: 1.3
The technical field of the invention relates to hydraulic mineral binders including at least one slag, for instance a Ground Granulated Blast furnace Slag (GGBS or slag), which are used in settable and hardenable compositions, such as mortar or concrete compositions.B · US 2021/0238094 A1 · ¶ 1
Related claim parts: 1.1
However, such cement has longer setting times, low early strength, and is prone to efflorescence, and it is, therefore, not widely used in China.A · US 10,947,159 B2 · ¶ 3
In the current situation where assemblization of buildings is being promoted in the state and mechanized assembly line for production has been performed in prefabrication factories, cement with high flexural strength is further needed.A · US 10,947,159 B2 · ¶ 4
Portland cement production has a strong and negative impact on the environment due to the emissions of large quantities of carbon dioxide.B · US 2021/0238094 A1 · ¶ 5
patent.fyi, US 2026/0365575 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365575/, SHA-256 2dcb80fad4fbc37d031cac74146b70df2ff4180fd1ef63be1e48dfadb7065a61