patent.fyi
Applications  /  US 2026/0365578
United States Patent Application Publication

US 2026/0365578 A1

Published
Nov 19, 2026
Filed
May 14, 2026
Earliest date on the face
May 14, 2025
Classification
C04B 24/405
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.2Cellulose nanofibril reinforcement

What ifWhat if the composition used a dispersion of cellulose nanofibrils as the nanoscale additive and contained no graphene additive?
Claim language“a graphene additive”

An aqueous suspension of cellulose nanofibrils with a solids content of 2% to 3% is added to the mixing water. High-shear mixing breaks up fibril bundles before the cement is added. The fibrils bridge microcracks and retain water near cement grains, which supports hydration and raises flexural strength.

1.2Dosing per volume of concrete

What ifWhat if the additive dose were set in grams per cubic metre of fresh concrete and metered by a liquid dispenser, so that the cement mass plays no part in the dose?
Claim language“by mass of cement”

A dispensing pump meters a stock dispersion into the mixer according to the batch volume reported by the batching controller. The dose in grams per cubic metre stays fixed when the cement content of the mix design changes. A flow meter on the dispenser line records each delivered dose.

1.2Graphene only in a surface layer

What ifWhat if the graphene were absent from the bulk mix and applied only as a thin sprayed layer on the surface after curing?
Claim language“present in an amount ranging from about 0.01% to about 0.04%”

A hardened cement-based element is cured for 28 days and its surface is cleaned. An aqueous graphene dispersion is sprayed on at a set coverage in grams per square metre and dried. The coating forms a conductive, low-permeability skin that slows chloride and moisture ingress, while the bulk matrix carries no additive.

1.2Nano-silica sol as the additive

What ifWhat if the additive were a colloidal nano-silica sol?
Claim language“selected from fractal graphene (FG) or reactive fractal graphene (RG)”

A colloidal silica sol with particles of 10 to 30 nanometres is added to the mixing water at a low solids dose. The particles react with calcium hydroxide released by hydration and form extra calcium silicate hydrate. The paste densifies and compressive strength rises at early ages.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Graphene-modified refractory castable for furnace linings

A refractory castable contains calcium aluminate binder, alumina aggregate and a carbon nanoplatelet additive at 0.02% by mass of binder. The additive is dispersed in mixing water by ultrasonic treatment before the water is added to the dry blend in a paddle mixer. The cast lining is cured for 24 hours at 25 °C, dried at 110 °C and fired to 800 °C. The nanoplatelets act as nucleation sites for hydrate phases and reduce the pore volume of the dried lining.

Parameter or scale variation

Graphene dose ladder for blended cement pastes

A paste contains a blended cement with 30% fly ash replacement and a graphene additive at 0.005%, 0.01%, 0.04% or 0.08% by mass of binder, at a water-to-binder ratio of 0.40. Each dose is dispersed in the mixing water by bath sonication for 15 minutes at 40 kHz. Cubes of 50 mm edge length are cast and cured at 20 °C. Compressive strength is measured at 3, 7 and 28 days to relate dose to strength gain.

Combination with existing systems

Graphene suspension dosing in a ready-mix batching plant

A batching plant includes a storage tank holding an aqueous graphene suspension at 1% solids, an agitator, a metering pump and a flow meter. The controller doses the suspension into the mixing water line so that the graphene mass equals 0.02% of the cement mass of each batch. The water line discharges into a truck mixer that also receives cement, aggregate and the remaining water. The agitator keeps the suspension uniform during the production day.

Specific version of a part

Sulfate-resistant calcium silicate cement

The cement is a hydraulic calcium silicate cement with a tricalcium aluminate content below 5% by mass. It is ground to a fineness of about 380 square metres per kilogram. The low aluminate content limits ettringite formation in sulfate-bearing environments.

Cement blended with fly ash

The cement is a blend of 75% calcium silicate clinker cement and 25% class F fly ash by mass. The fly ash reacts pozzolanically with calcium hydroxide and refines the pore structure over time. The blend lowers heat of hydration in mass pours.

Pre-dispersed fractal graphene in water reducer

Fractal graphene powder is dispersed in an aqueous solution of a polycarboxylate ether superplasticizer by probe ultrasonication for 20 minutes. The dispersion is added to the mixing water so that the graphene dose is 0.02% by mass of cement. The polymer adsorbs on the sheets and keeps them separated in the alkaline pore solution.

Reactive fractal graphene with oxygen groups

The reactive fractal graphene carries hydroxyl and carboxyl groups on its edges and is supplied as a 1% aqueous paste. The paste is diluted in the mixing water and sheared at high speed for five minutes before cement is added. The dose is 0.03% by mass of cement, and the oxygen groups bind to calcium ions on hydrating cement grains.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 10,138,164 B2
Published
Nov 27, 2018
Filed
Mar 18, 2016
Class
C04B 14/361
Document BUS 2024/0034680 A1
Published
Feb 1, 2024
Filed
Dec 8, 2021
Class
C04B 28/16
Claim 1
Document A
Document B
1.1cement; and
A supplementary cementitious material used in combination with an activator such as Portland cement to produce a hydraulic binder.
A · US 10,138,164 B2 · abstract
In concrete and mortars, cement is used as a hydraulic binder.
B · US 2024/0034680 A1 · ¶ 2
1.2a graphene additive selected from fractal graphene (FG) or reactive fractal graphene (RG), wherein the graphene additive is present in an amount ranging from about 0.01% to about 0.04% by mass of cement.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1. Both are classified in CPC C04B, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The supplementary cementitious material is based on physico-chemically treated filter cake product extracted from dredged sediments and can partially replace Portland cement clinker in conventional concrete applications.
A · US 10,138,164 B2 · ¶ 2

Related claim parts: 1.1

A classical way to reduce the CO2 footprint of cement is to replace a part of the milled clinker by secondary cementitious material (SCM) with a lower CO2 footprint, thus reducing the clinker factor of the cement.
B · US 2024/0034680 A1 · ¶ 4

Related claim parts: 1.1

Considering the scale of production it is estimated that 5-8% of man-made CO2 emissions are related to cement manufacture.
A · US 10,138,164 B2 · ¶ 4
Since most conventional, high-quality SCMs such as blast-furnace slags are practically entirely consumed, further incremental reductions of the environmental impact of cement production will need to come from new, alternative materials.
A · US 10,138,164 B2 · ¶ 5
It is therefore critical to reduce the cement's carbon footprint.
B · US 2024/0034680 A1 · ¶ 3
As limestone is a cheap and widely available product, which has a very low CO2 footprint, it allows further reducing the CO2 footprint and the cost of the binder, when part of the Portland clinker is replaced by the mix of calcined clay and limestone (LS, CaCO3).
B · US 2024/0034680 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0365578 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365578/, SHA-256 76dbe8fcd013f21b63d129b54ece1f8da95b3cba5f476b6496396bbcd33f930c
First published
Permanent addresshttps://patent.fyi/US20260365578/
Content fingerprint (SHA-256)76dbe8fcd013f21b63d129b54ece1f8da95b3cba5f476b6496396bbcd33f930c
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi