Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.2Colloidal silica replaces fume
What ifWhat if an aqueous colloidal silica dispersion supplies the reactive silica?
Claim language“of silica fume”
Meter the dispersion into the mixing water and count its carrier water toward the total batch water. The dispersed silica particles provide surfaces for hydrate nucleation and react with calcium hydroxide to form calcium silicate hydrate.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Cast bases for precision instruments
The dry binder contains 65% cement, 15% silica fume, 15% ground feldspar and 5% limestone filler by mass. The binder is mixed with graded sand, water, a water-reducing admixture and short steel fibers, then cast around threaded inserts held in a fixture. The inserts secure instrument mounts to the cured base, and ground bearing pads provide a flat seating surface.
Component substitution
Ground quartz replaces silica fume
Micronized quartz flour replaces silica fume in a dry blend containing 70% cement, 10% quartz flour, 15% ground feldspar and 5% limestone filler by mass. The quartz flour has a median particle diameter of 3 to 5 μm and fills spaces between coarser binder particles. The dry blend is mixed with graded sand, water and a polycarboxylate water reducer to produce a castable mortar.
Parameter or scale variation
Low water content with staged mixing
The dry binder contains 65% cement, 15% silica fume and 20% ground feldspar by mass and is used at a total water-to-binder mass ratio of 0.19 to 0.22. The mixer blends the binder and sand for 60 seconds, then adds 80% of the batch water and mixes for 90 seconds. The remaining water and a polycarboxylate water reducer enter over 30 seconds, with water in the admixture counted in the total. Short steel fibers enter the flowing mix over 60 seconds to limit clumping.
Combination with existing systems
Binder grout for precast deck joints
The dry binder contains 60% cement, 15% silica fume, 20% ground feldspar and 5% limestone filler by mass. The binder is mixed with fine sand, water, a water-reducing admixture and short steel fibers to form a flowable grout. Adjacent precast deck panels have roughened joint faces and projecting reinforcement that overlaps within the joint. Temporary forms retain the grout around the reinforcement as it cures, and the hardened joint transfers load between panels.
Fiber mortar films for textile panels
The dry binder contains 65% cement, 15% silica fume, 15% ground feldspar and 5% limestone filler by mass and is mixed with fine sand, water and a water reducer. A first mortar layer is spread in a shallow mold, an open carbon textile grid is pressed into it, and a second mortar layer covers the grid. The fresh mortar passes through the grid openings and surrounds the yarns so that the embedded textile carries tensile load when the cured panel bends.
Automated or data-driven variant
Sensor control of batch water
Load cells proportion a dry binder containing 65% cement, 15% silica fume, 15% ground feldspar and 5% limestone filler by mass. A calibrated moisture probe in the sand feed measures moisture, and the controller subtracts free water carried by the sand from the target batch water. At fixed mixer speed, the controller compares motor torque with a band established by trial batches and meters small additions of water reducer when torque stays above that band after wetting. The controller records sand moisture, water addition, admixture dose and final mixing torque for each batch.
Specific version of a part
Silica fume at ten percent
Use undensified silica fume at 10% of the dry binder mass. Disperse it in the mixer with water and a high-range water reducer so the fine particles fill gaps between cement grains and react with calcium hydroxide.
Ground feldspar primary filler
Use ground feldspar at 15% of the dry binder mass for filler A1. Select a grade with a median particle size of about 5 micrometres to fill spaces between larger cement grains.
Ground limestone secondary filler
Use ground limestone at 10% of the dry binder mass for filler A2. Select a grade with a median particle size of about 8 micrometres to contribute to powder packing and provide surfaces for hydrate nucleation.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
A hydraulic binder includes, as percentage by mass: from 17 to 55% of a Portland cement, the particles of which have a D50 of from 2μm to 11 μm; at least 5% of silica fume; from 36 to 70% of a mineral addition A1, the particles of which have a D50 of from 15 to 150 μm; the sum of these percentages being from 80 to 100%; the sum of the percentages of cement and of silica fume being greater than 28%; the mineral addition A1 being selected from slags, pozzolanic additions or sil
A · US 2017/0152183 A1 · abstract
The cement compositions are comprised of Ordinary Portland Cement, or blended cements or non-Portland cements made with Supplementary Cementitious Materials (SCMs).
B · US 9,731,999 B2 · ¶ 2
1.2from 3% to 25% of silica fume;
(ii) Fly ash Class C (cementitious and pozzolanic), fly ash Class F (pozzolanic), and natural (raw or calcined) pozzolans such as diatomaceous earths, opaline cherts and shales, tuffs, volcanic ashes, and calcined clays and shales; and (iii) Silica fume (pozzolanic).
B · US 9,731,999 B2 · ¶ 8
1.3from 5% to 30% of a filler A1 selected from crushed glass, milled E-glass, ground feldspar filler, or mixtures thereof; from 0% to 25% of a filler A2 selected from siliceous mineral addition or limestone addition;
The hydraulic binder according to the invention comprises a mineral addition Al selected from among slags, pozzolanic additions or siliceous additions such as quartz, siliceous limestone mineral additions, limestone additions such as calcium carbonate or mixtures thereof.
A · US 2017/0152183 A1 · ¶ 55
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1. Both are classified in CPC C04B, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
With suitable formulation and additives, OPC can be partially or completely replaced by a variety of minerals and industrial byproducts, collectively referred to as Supplementary Cementitious Materials (SCMs, also known as Mineral Admixtures), the resultant products being referred to as blended cements and non-Portland cements respectively.
B · US 9,731,999 B2 · ¶ 7
Related claim parts: 1.3
The invention relates to hydraulic binders which give the possibility of obtaining an ultra-high performance concrete with low cement content, and to mixtures comprising this binder.
A · US 2017/0152183 A1 · ¶ 1
There is therefore a strong need for a method allowing ultra-high performance concrete to be produced with a reduction in associated emissions of carbon dioxide.
A · US 2017/0152183 A1 · ¶ 8
This invention generally relates to a new class of chemical admixtures for hydraulic cement compositions such as pastes, mortars, grouts and concretes.
B · US 9,731,999 B2 · ¶ 2
The admixtures improve the properties of cement compositions, including setting, hardness, compressive strength, shrinkage, and freeze-thaw resistance.
B · US 9,731,999 B2 · ¶ 2
Cite aspatent.fyi, US 2026/0365579 A1, claim 1, first published 2026-11-23T14:06:49-05:00, https://patent.fyi/US20260365579/, SHA-256 1420f2f37bc95b8f54c83913fd058d79043afe9cff1c8e0274b283b5849830ff