1.1Carbide from calcium oxide
An electric arc furnace heats lime and coke to about 2,000 °C. The reaction produces molten calcium carbide and carbon monoxide, and the furnace taps the molten carbide for cooling.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
An electric arc furnace heats lime and coke to about 2,000 °C. The reaction produces molten calcium carbide and carbon monoxide, and the furnace taps the molten carbide for cooling.
A flowing mixture of methane and hydrogen passes over heated tungsten powder. Methane dissociates at the particle surface, and carbon diffuses into the tungsten to form tungsten carbide.
A cooled hydrolysis vessel contacts granular calcium carbide with water and draws acetylene from the headspace. The calcium hydroxide slurry passes to a separate neutralization vessel, where hydrochloric acid converts it to calcium chloride solution.
Steam reacts with aluminum carbide in a heated vessel to release methane and form a solid aluminum oxide residue. A condenser removes residual steam from the gas, and a separate acid leach converts the oxide to aluminum chloride solution.
A membrane cell electrolyzes aqueous sodium chloride and withdraws chlorine from the anode compartment. Sodium ions cross the membrane and combine with hydroxide generated by water reduction at the cathode, producing sodium hydroxide solution and a separate hydrogen stream.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A steel pickling line supplies spent hydrochloric acid to an acid recovery unit that separates a hydrogen chloride gas stream from dissolved iron salts. An acid-resistant gas conditioning train separates entrained liquid and water vapor before the hydrogen chloride enters a calcium carbide reactor. The reactor sends acetylene to a separate collection header and calcium chloride to a molten salt cell that produces chlorine and calcium. The calcium returns to the carbide furnace, where it reacts with solid carbon.
A high-temperature furnace contacts elemental aluminum with solid carbon to form aluminum carbide, which a sealed transfer vessel delivers to a separate gas-solid reactor. Dry hydrogen chloride reacts with the carbide to generate methane and aluminum chloride. A cooled solids collector captures aluminum chloride from the reactor effluent while methane passes to the gas outlet. A molten chloride cell receives the collected salt and produces chlorine and aluminum, which returns to the furnace.
Three sealed fixed-bed vessels hold calcium carbide from a common furnace and share a dry hydrogen chloride supply. Two beds receive hydrogen chloride at half the total feed rate each, while the third bed is isolated for purging, calcium chloride removal, and fresh carbide loading. When the outlet of an operating bed reaches the hydrogen chloride breakthrough threshold, the inlet manifold brings the loaded bed online and isolates the spent bed. A common gas header collects acetylene, and sealed hoppers deliver calcium chloride to the halide conversion cell.
A calcium carbide reactor receives hydrogen chloride and sends the resulting calcium chloride to a molten salt cell that produces chlorine and calcium for recycle. A particulate filter and a dry acid guard bed condition the acetylene-rich gas before a mixer adds hydrogen. The gas passes through a staged palladium catalyst bed with intercooling, where acetylene reacts with hydrogen to form ethylene. An outlet analyzer measures residual acetylene and controls the hydrogen feed.
A carbide furnace discharge chute feeds hot calcium carbide through an enclosed indirect moving-bed cooler before the carbide enters the hydrogen chloride reactor. A circulating nitrogen loop carries heat from the cooler to a separate waste heat boiler, where it generates steam for plant use. The carbide reactor produces acetylene and calcium chloride, and a molten salt cell converts the calcium chloride to calcium and chlorine. The calcium returns to the furnace for reaction with solid carbon.
A vertical moving-bed reactor receives calcium carbide through an upper lock hopper and hydrogen chloride through a lower gas distributor. An infrared analyzer measures hydrogen chloride in the acetylene outlet, and a controller increases fresh carbide feed when the measured concentration rises above its setpoint. A bed level sensor controls the lower solids discharge valve, and a sealed intermediate hopper transfers calcium chloride to the halide conversion cell. A high-high outlet concentration closes the hydrogen chloride feed valve and routes the remaining outlet gas to an acid scrubber.
A sealed reactor heats calcium metal in contact with graphite under argon. Calcium reacts at the graphite surface to form calcium carbide.
A cooled, stirred reactor feeds calcium carbide granules into excess aqueous hydrochloric acid. Acetylene leaves through the gas outlet, and calcium chloride remains in the liquid.
A stirred acid reactor contacts crushed aluminum carbide with aqueous hydrochloric acid. Methane leaves the headspace, and aluminum chloride remains dissolved in the reactor liquor.
A divided electrolysis cell holds anhydrous magnesium chloride in a molten chloride bath operated above the melting point of magnesium. Liquid magnesium forms at the cathode and floats into a collection zone, while chlorine forms at the graphite anode and exits through a separate gas outlet.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
It is well known to harden steels by heat treatment at elevated temperatures under a carbon rich atmosphere followed by tempering at higher temperatures. During the heat treatment process iron carbide is formed at elevated concentrations.A · US 8,118,949 B2 · ¶ 3
Treatment of the reduced (metallic) cobalt catalysts with pure CO at 220° C. leads to cobalt carbide (Co2C) formation which is inactive towards FTS.B · US 2015/0273443 A1 · ¶ 3
An empty cell means only that no passage was reproduced there.
Both have a passage for 1.1.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
While cobalt additions have been successful in promoting secondary carbide precipitation, the attendant cost of such additions has been burdensome.A · US 8,118,949 B2 · ¶ 3
The present invention provides advantages and/or alternatives over the prior art by providing a method of promoting the precipitation of secondary metal carbides in a carbon enriched zone of a carburized steel part with the reduced or eliminated use of cobalt.A · US 8,118,949 B2 · ¶ 5
It is known that the activation conditions can be adapted to improve the activity of the eventual catalyst.B · US 2015/0273443 A1 · ¶ 3
No improvements were observed in the formation of the cobalt hcp phase at the higher temperatures, but it was most unexpectedly found that when this cobalt carbide was treated with hydrogen at a temperature above 300° C., the catalyst so formed had a higher FTS catalyst activity and/or lower methane selectivity.B · US 2015/0273443 A1 · ¶ 5
patent.fyi, US 2026/0365595 A1, claim 1, first published 2026-11-23T14:44:57-05:00, https://patent.fyi/US20260365595/, SHA-256 6824cc867b013174b43e2059f9e0178d3e1b00e1f55dd632eec868e8e6145c34