Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
No entries.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Radical-grafted polyolefin dispersant for fuel additives
A stirred, jacketed reactor holds polyisobutylene that is heated to 190 °C under a nitrogen blanket. A dosing pump then meters a peroxide initiator, and a separate feed line supplies maleic anhydride. The grafted anhydride product is reacted with a polyamine in a second vessel to form a succinimide. The succinimide is blended at 0.01 to 0.1 weight percent into a gasoline or diesel fuel as a detergent that limits injector deposits.
Grafted succinate ester as metalworking fluid emulsifier
Polyisobutylene is heated to 180 °C in a glass-lined reactor, and a radical initiator and an unsaturated acylating agent are dosed in. The resulting anhydride-functional product is esterified with a polyol such as pentaerythritol at 200 °C while water is stripped. The ester is blended at 1 to 3 weight percent into a mineral oil concentrate for water-miscible cutting fluid. The ester acts as an oil-in-water emulsifier and corrosion inhibitor in the diluted fluid.
Component substitution
Azo initiator replacing peroxide in grafting step
The reactor holds polyisobutylene at 160 °C, and an azo-type initiator with a ten-hour half-life near 100 °C replaces the peroxide initiator. A liquid mixture of the initiator and itaconic anhydride dissolved in a hydrocarbon solvent is fed through a dip tube over 2 hours. Nitrogen purge carries off the gaseous decomposition products. The grafted product is reacted with tetraethylenepentamine to give a succinimide dispersant.
Parameter or scale variation
Pilot to production scale grafting at higher temperature
A 5,000 liter jacketed reactor with a pitched-blade agitator is charged with 3,000 kg of polyisobutylene of 2,300 number-average molecular weight. The charge is heated to 220 °C, and 60 kg of a peroxide initiator is metered over 4 hours. Maleic anhydride at 1.5 mole per mole of polymer is fed in parallel through a sparge line. A vacuum stage at 10 kPa then strips unreacted anhydride before the amine step.
Combination with existing systems
Grafting reactor integrated with continuous polymerization unit
A polyisobutylene polymerization unit discharges stripped polymer into a heated buffer tank held at 200 °C. A pump moves the polymer through a continuous plug-flow reactor with static mixers and injection ports for initiator and acylating agent. The outlet flows to a thin-film evaporator that removes residual anhydride. The product goes directly to an amidation reactor and then to a lubricant blending line with a base oil header and an additive metering skid.
Automated or data-driven variant
Model-controlled initiator dosing with inline spectroscopy
An infrared probe in a reactor recirculation loop measures the anhydride carbonyl band intensity during grafting. A controller compares the reading with a trained regression model that predicts grafting level from temperature, feed rates and band intensity. The controller adjusts the initiator pump rate and the jacket oil temperature every 30 seconds within 150 to 225 °C. A software interlock holds the initiator feed until a temperature sensor confirms the polymer has reached its setpoint.
Cite aspatent.fyi, US 2026/0365602 A1, claim 1, first published 2026-11-23T14:44:57-05:00, https://patent.fyi/US20260365602/, SHA-256 5f40c7012e9de7bb59a728284f4924e0e77717a950d4795d647700bcb8da3ffb