Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Surface profiling by secondary ions
What ifWhat if secondary ion mass spectrometry measures the vinyl chloride-based polymer fraction at the surface?
Claim language“measured by XPS analysis”
A pulsed bismuth ion beam releases secondary ions from the particle surface, and a time-of-flight analyzer records chlorine-bearing organic fragments. Reference films with known polymer and dispersant fractions relate fragment intensities to surface composition.
1.1Bulk composition from combustion
What ifWhat if polymer content is determined across the full particle volume?
Claim language“in a surface layer”
A pulverized resin sample undergoes oxygen combustion, and ion chromatography quantifies the chloride captured in the absorption solution. For a formulation in which the polymer supplies all chlorine, the repeat-unit composition converts the measured chlorine mass to a bulk polymer mass fraction.
1.1Lubricant rich particle surface
What ifWhat if the vinyl chloride-based polymer accounts for 35% to 45% of the analyzed surface layer?
Claim language“50% or more”
A fluidized bed deposits polyethylene wax from an aqueous dispersion onto vinyl chloride-based polymer particles, and warm air dries the coating. The wax-rich surface lowers friction against metal during processing, and the particle cores supply the resin that consolidates under heat and shear.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Resin for electrical cable insulation
Use vinyl chloride-based resin powder with a surface-layer polymer content of at least 50% as measured by X-ray photoelectron spectroscopy. Dry-blend the powder with a plasticizer, a heat stabilizer, and a lubricant, then compound the blend in an extruder. Feed the compound to a crosshead die that coats a moving copper conductor, and cool the coated conductor in a water trough.
Component substitution
Dispersant with a lower hydrolysis grade
Replace the highly hydrolyzed polyvinyl alcohol in the dispersant premix with a partially hydrolyzed grade containing 87 to 89 mol% hydrolyzed units. Dissolve the replacement grade in water, mix the solution with the metal carbonate, and charge the premix to the suspension reactor before polymerization. Wash and dry the recovered particles, then verify a surface-layer vinyl chloride-based polymer content of at least 50% by X-ray photoelectron spectroscopy.
Parameter or scale variation
Particle size fractionation after drying
Stack a 180 μm screen above a 125 μm screen in an enclosed vibratory classifier. Feed dried resin powder to the upper screen and collect the fraction that passes through the upper screen and remains on the lower screen. Take a composite sample of the collected fraction and verify a surface-layer vinyl chloride-based polymer content of at least 50% by X-ray photoelectron spectroscopy.
Timed dispersant premix addition
Dissolve the polyvinyl alcohol in water, add the metal carbonate, and circulate the premix for 10 minutes in an agitated tank. Meter the premix into the stirred suspension reactor over 5 minutes before initiating polymerization. Recover, wash, and dry the particles, then verify a surface-layer vinyl chloride-based polymer content of at least 50% by X-ray photoelectron spectroscopy.
Combination with existing systems
Countercurrent washing before resin drying
Connect the suspension reactor discharge to two stirred wash vessels, each followed by a screen centrifuge. Transfer the solids from the first stage to the second, add fresh water to the second vessel, and return the second centrifuge filtrate to the first vessel as wash water. Send the second centrifuge cake to a dryer and verify that the dried powder has a surface-layer vinyl chloride-based polymer content of at least 50% by X-ray photoelectron spectroscopy.
Automated or data-driven variant
Automated surface composition lot verification
Take powder increments at fixed intervals during dryer discharge, combine them into a lot sample, and press the powder into a clean sample holder. Use a programmed X-ray photoelectron spectrometer to collect survey and high-resolution carbon, chlorine, and oxygen spectra at five positions. Use software to fit the spectra against reference spectra for the resin and dispersant residues, calculate the mean surface-layer polymer content using a fixed calibration, and flag lots below 50%.
Specific version of a part
Chlorine signal with carbon correction
X-ray photoelectron spectroscopy measures the carbon 1s and chlorine 2p peak areas on dried resin powder. A calibrated composition model uses sensitivity-corrected signals and the copolymer repeat-unit composition to estimate surface polymer content and check it against 50%.
Organic chlorine peak separation
High-resolution X-ray photoelectron spectra resolve the chlorine 2p doublets from polymer-bound chlorine and residual inorganic chloride using reference spectra. A calibrated model excludes the inorganic chloride contribution when calculating the polymer fraction, which is at least 50%.
Cite aspatent.fyi, US 2026/0365764 A1, claim 1, first published 2026-11-23T15:54:04-05:00, https://patent.fyi/US20260365764/, SHA-256 e35508153e82a45fa880cc72b8754f0af6b0e857879adee0db1c060b4b5c428f