Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Omission of internal disubstituted ethylene units

What ifWhat if the copolymer contains only pendant vinyl groups and saturated backbone linkages with no 1,2-substituted ethylene units?
Claim language“a 1,2-substituted ethylene group-containing unit”

Living anionic copolymerization of divinylbenzene and ethylvinylbenzene using an organolithium initiator at minus 40 to 20 °C suppresses proton-transfer side reactions that form internal disubstituted alkene linkages. The resulting branched polymer carries exclusively terminal vinyl groups on the aromatic rings and saturated hydrocarbon chain ends after protic termination. Because terminal vinyl groups react faster than sterically hindered internal alkenes, the resin cures at lower temperatures with higher double-bond conversion.

1.1Benzocyclobutene thermal ring-opening reactive unit

What ifWhat if the copolymer carries strained benzocyclobutene rings as its curing sites?
Claim language“a vinyl group-containing unit”

Copolymerization of a benzocyclobutene-substituted styrene monomer with a monovinyl aromatic monomer yields a soluble hydrocarbon polymer devoid of free vinyl double bonds. Heating the resin above 200 °C triggers electrocyclic ring opening of the four-membered cyclobutene ring to form a reactive ortho-quinodimethane intermediate. These intermediates undergo [4+2] thermal cycloaddition and dimerization without added radical initiators or volatile byproducts, forming a low-dielectric cross-linked network.

1.2High-molecular-weight thermoplastic elastomer film matrix

What ifWhat if the copolymer is synthesized at a number-average molecular weight above 25,000 to form a self-supporting film?
Claim language“a number-average molecular weight of 300 to 10,000”

Controlled radical polymerization with a low chain-transfer rate grows the vinyl aromatic chains to a number-average molecular weight between 25,000 and 80,000 while keeping branching low enough to prevent gelation. Chain entanglements above the critical entanglement molecular weight impart mechanical toughness and allow casting of dry, tack-free dielectric films without glass-cloth reinforcement. During press lamination at 180 to 210 °C, residual unsaturated groups cross-link the entangled chains to lock in dimensional stability.

1.2Insoluble cross-linked microgel particle dispersion

What ifWhat if the copolymer is formed as solvent-insoluble cross-linked microgel particles dispersed in a liquid reactive monomer?
Claim language“soluble in toluene, xylene, tetrahydrofuran, dichloroethane, or chloroform”

Emulsion or precipitation polymerization at high divinyl aromatic concentration produces internally cross-linked polymer nanoparticles with diameters of 50 to 300 nanometers that swell slightly but do not dissolve in aromatic or chlorinated solvents. Surface-exposed residual vinyl groups allow the particles to be dispersed into a liquid acrylate or styrene reactive diluent to form a low-viscosity varnish. Upon thermal curing, the liquid diluent polymerizes around and covalently grafts to the microgel surfaces, reducing cure shrinkage and thermal expansion.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Optical waveguide cladding films for planar photonics

A planar photonic device uses the soluble polyfunctional vinyl aromatic copolymer as a low-birefringence upper cladding film over silicon nitride waveguide cores on a fused silica wafer. A toluene solution containing 25 wt% of the copolymer and 1.5 wt% of a thermally activated peroxide cross-linker deposits by spin coating at 2,000 rpm to form a uniform 3 micrometer film. Baking the coated wafer in a nitrogen oven at 110 °C for 5 minutes evaporates the solvent, and a subsequent thermal cure at 190 °C for 60 minutes cross-links the pendant vinyl and 1,2-substituted ethylene groups into an optically transparent network. The cured aromatic hydrocarbon matrix exhibits a refractive index near 1.59 at 1,550 nanometers and seals the waveguide sidewalls against moisture ingress.

Component substitution

Divinylnaphthalene monomer substitution in copolymer backbone synthesis

The copolymer synthesis replaces divinylbenzene with 1,4-divinylnaphthalene as the divinyl aromatic monomer alongside 4-tert-butylstyrene as the monovinyl aromatic comonomer. Cationic copolymerization runs in cyclohexane using boron trifluoride diethyl etherate as a fluorine-containing acid catalyst and ethyl acetate as an electron-pair donor modifier to control branching and preserve solubility in tetrahydrofuran. The resulting fused-ring aromatic backbone retains pendant vinyl units, cross-linked bridges, and internal 1,2-substituted ethylene groups while raising the glass transition temperature of the cured network above 240 °C. Bulky tert-butyl substituents along the monovinyl segments increase free volume between polymer chains and maintain room-temperature solubility in aromatic and cyclic ether solvents.

Solid acid catalyst bed replacing homogeneous acid catalysts

A packed-bed reactor replaces the soluble homogeneous acid catalyst and electron-pair donor additive with a fixed bed of perfluorinated sulfonic acid ion-exchange resin beads supported on porous silica. A preheated solution of divinylbenzene and styrene in toluene flows upward through the 95 °C catalyst bed at a liquid hourly space velocity of 2.0 inverse hours. Acidic sites on the solid beads initiate cationic chain growth and controlled intramolecular cyclization while leaving pendant vinyl and 1,2-substituted ethylene groups along the soluble chains. Because the catalyst remains immobilized inside the column, the exiting polymer solution requires no alkaline neutralization or water extraction and maintains chlorine and bromine impurity levels below 1 part per million.

Parameter or scale variation

Continuous tubular polymerization at elevated pressure and temperature

A continuous jacketed tubular reactor with a 12 millimeter internal diameter and a 40 meter length polymerizes a monomer feed containing 12 mol% divinylbenzene and 88 mol% ethylvinylbenzene at 135 °C and 0.8 megapascals. Static mixing elements spaced every 0.5 meters maintain plug flow over a 6 minute residence time, yielding 25 kilograms per hour of soluble copolymer after inline catalyst quenching with methanol. The isolated copolymer has a number-average molecular weight of 14,500 grams per mole, a polydispersity index (Mw/Mn) of 3.2, and an average of 5.4 unsaturated vinyl and 1,2-substituted ethylene groups per molecule. Lowering the divinyl monomer ratio to 12 mol% prevents gelation at the elevated molecular weight while keeping the polymer soluble in xylene at 40 wt% solids.

Combination with existing systems

Integration with roll-to-roll glass fabric prepreg impregnation

A continuous vertical treater line combines a varnish of the soluble polyfunctional vinyl aromatic copolymer, polyphenylene ether oligomer, and spherical fused silica filler at 60 wt% of total solids with woven low-dielectric alumino-borosilicate glass cloth. The glass fabric passes through a dip pan at 4 meters per minute, moves between metered doctor rolls that set the resin pickup to 52 wt%, and travels through a three-zone convection oven held at 110 °C, 135 °C, and 155 °C to produce tack-free semi-cured prepreg sheets. Four stacked prepreg sheets positioned between 18 micrometer electrodeposited copper foils enter a vacuum hydraulic press at 2.5 megapascals and cure at 210 °C for 90 minutes. During lamination, the melted copolymer flows into the glass fiber bundles and co-cures with the polyphenylene ether oligomer to form a copper-clad composite board with low dielectric loss and low linear thermal expansion.

Automated or data-driven variant

Closed-loop infrared control of copolymer unsaturated group ratios

An inline attenuated total reflectance infrared probe and a vibrating-tube viscometer mount directly on a recirculation loop connected to the stirred polymerization reactor. The probe samples absorption bands for terminal vinyl groups near 1,630 inverse centimeters and internal 1,2-substituted ethylene groups near 1,655 inverse centimeters every 15 seconds and sends the spectra to a partial least-squares regression model. The model estimates real-time number-average molecular weight, polydispersity, and unsaturated group concentrations, passing those values to a model-predictive controller. The controller adjusts mass-flow valves for the acid catalyst solution, electron-pair donor modifier, and jacket cooling oil to hold the target vinyl-to-internal-alkene ratio and quench the reaction automatically before cross-linking reaches the gel point.

Specific version of a part

Controlled chain-transfer synthesis of diphenylethylene units

Polymerizing divinylbenzene and styrene with a trifluoromethanesulfonic acid catalyst in the presence of a controlled amount of an aromatic ether modifier promotes selective beta-proton elimination alongside vinyl propagation. This balance yields both pendant vinyl aromatic units and internal trans-1,2-diphenylethylene units within the branched chain and at chain termini. Proton nuclear magnetic resonance spectroscopy verifies the ratio of pendant vinyl protons at 5.2 to 6.8 parts per million to internal disubstituted alkene protons near 7.0 parts per million.

Fluorinated catalyst purification for halogen-free resin

Using boron trifluoride or trifluoromethanesulfonic acid as the polymerization initiator eliminates chlorine- and bromine-containing catalyst residues from the reaction mixture. Following polymerization, the organic phase is neutralized with aqueous sodium hydroxide, washed repeatedly with deionized water until neutral conductivity is reached, and passed through an activated alumina column. Ion chromatography confirms that residual chlorine and bromine concentrations remain below 2 parts per million while fluorine-derived species are removed or kept within target limits.

Narrow-dispersity oligomer fractionation by solvent precipitation

Gel permeation chromatography using polystyrene calibration monitors the copolymer during synthesis so the reaction terminates at a number-average molecular weight of 1,500 to 4,000 and a polydispersity index between 2.0 and 8.0. Adding a nonsolvent such as methanol or hexane to a 20 weight percent toluene solution of the crude copolymer selectively precipitates the target oligomer while leaving unreacted monomers and low-boiling dimers in the supernatant. Vacuum drying at 60 °C produces a resin with 2.5 to 3.5 unsaturated functional groups per molecule that dissolves readily in toluene or tetrahydrofuran.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2011/0105638 A1
Published
May 5, 2011
Filed
Mar 3, 2009
Class
C08L 33/06
Document BUS 11,130,861 B2
Published
Sep 28, 2021
Filed
Mar 29, 2018
Class
C08L 71/12
Claim 1
Document A
Document B
1.1wherein the structural unit derived from a divinyl aromatic compound (a) has a vinyl group-containing unit represented by the following formula (a1), a 1,2-substituted ethylene group-containing unit represented by the following formula (ta2), a cross-linked structural unit represented by the following formula (a2), and a structural unit represented by the following formula (ta1) containing both a vinyl group and a 1,2-substituted ethylene group; and the structural unit derived from a monovinyl aromatic compound (b) has a structural unit represented by the following formula (b1) and a 1,2-substituted ethylene group-containing terminal unit represented by the following formula (tb1), and
The structural unit derived from the divinyl aromatic compound contains a vinyl group as a crosslinking component for expressing heat resistance. Meanwhile, the structural unit derived from the monovinyl aromatic compound is free of a vinyl group involved in a curing reaction, and hence imparts molding property and the like.
A · US 2011/0105638 A1 · ¶ 61
Disclosed herein is a soluble polyfunctional vinyl aromatic copolymer containing structural units derived from a divinyl aromatic compound (a), styrene (b), and a monovinyl aromatic compound (c) other than styrene.
B · US 11,130,861 B2 · abstract
1.2wherein the polyfunctional vinyl aromatic copolymer has a total number of unsaturated bond functional groups (excluding an unsaturated bond group in an aromatic ring) in one molecule of 2.1 or more and less than 4.0, a functional group equivalent of 1,2-substituted ethylene groups derived from the following formulae (ta1), (ta2), and (tb1) of 1,000 or more, a number-average molecular weight of 300 to 10,000, and a molecular weight distribution (Mw/Mn) represented by a ratio of a weight-average molecular weight to a number-average molecular weight of 50 or less, and is soluble in toluene, xylene, tetrahydrofuran, dichloroethane, or chloroform, and does not comprise a halogen element other than fluorine as an impurity in an amount of 5 ppm or more:
Preferred examples of the soluble polyfunctional vinyl aromatic copolymer include a copolymer obtained by allowing the following compounds to react with each other: 5 to 75 mol % of a divinyl aromatic compound; 35 to 5 mol % of a monovinyl aromatic compound; and 60 to 20 mol % of an aromatic ether compound, in which: the copolymer has, at the end, a end group derived from the aromatic ether compound represented by the above-mentioned formula (1), has a number average molecula
A · US 2011/0105638 A1 · ¶ 89
The copolymer has a number-average molecular weight Mn of 300 to 100,000, and a molecular weight distribution (Mw/Mn) represented by a ratio of the weight-average molecular weight Mw to the number-average molecular weight Mn, of 100 or lower. The copolymer is soluble in toluene, xylene, tetrahydrofuran, dichloroethane or chloroform solvents.
B · US 11,130,861 B2 · ¶ 31

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1 1.2. Both are classified in CPC C08L.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

One of the reasons is that a thermal characteristic such as heat resistance or thermal stability and processability such as solvent solubility or film moldability cannot be attained simultaneously.
A · US 2011/0105638 A1 · ¶ 3

Related claim parts: 1.1 1.2

Furthermore, materials that exhibit high heat resistance, i.e. a high glass transition temperature are desired due to the fact that a printed board or electronic component in which such electrical insulating materials are used is exposed to high-temperature solder reflow during mounting.
B · US 11,130,861 B2 · ¶ 3

Related claim parts: 1.1 1.2

The present invention relates to an end-modified soluble polyfunctional vinyl aromatic polymer having improved heat resistance, compatibility, and heat discoloration resistance, and a production method for the soluble polyfunctional vinyl aromatic polymer.
A · US 2011/0105638 A1 · ¶ 1
From the viewpoints of compatibility during copolymerization of the soluble polyfunctional vinyl aromatic copolymer with any other radical polymerizable monomer, and heat discoloration resistance after curing, the compatibility or solubility with a highly versatile (meth)acrylate compound is insufficient, and the thermal stability to high process temperatures is also insufficient.
A · US 2011/0105638 A1 · ¶ 6
The present invention relates to a novel soluble polyfunctional vinyl aromatic copolymer having improved heat resistance, compatibility, dielectric properties, wet heat reliability, and resistance to thermal oxidative degradation, to a method for producing the copolymer, and to a curable resin composition containing the copolymer.
B · US 11,130,861 B2 · ¶ 2
In order to have more excellent electrical characteristics, in particular, to reduce transmission loss at high-frequency bands, electrical insulating materials that have low permittivity and low dielectric tangent and, in particular, exhibit small changes in dielectric properties after absorption of moisture have been demanded.
B · US 11,130,861 B2 · ¶ 3
Cite aspatent.fyi, US 2026/0365768 A1, claim 1, first published 2026-11-23T16:17:13-05:00, https://patent.fyi/US20260365768/, SHA-256 89dcfa5d0e8167ee534df17560bb292f7ce6fc58e27fb3d967eb7cbe2d0bdc3d
First published
Permanent addresshttps://patent.fyi/US20260365768/
Content fingerprint (SHA-256)89dcfa5d0e8167ee534df17560bb292f7ce6fc58e27fb3d967eb7cbe2d0bdc3d