Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Flexible polyester acrylate binder
What ifWhat if the coating uses a flexible polyester diacrylate binder with no urethane linkages?
Claim language“a urethane (meth)acrylate (X)”
Esterify both terminal hydroxyl groups of a polycaprolactone diol with acrylic acid. Ultraviolet exposure in the presence of a radical photoinitiator links the acrylate ends into a network with flexible polyester segments between junctions.
1.2Cyclic ether acrylate diluent
What ifWhat if tetrahydrofurfuryl acrylate serves as the reactive diluent and the formulation contains no acrylamide?
Claim language“an acrylamide derivative (Y)”
Tetrahydrofurfuryl acrylate reduces the viscosity of the urethane acrylate blend before application. Its acrylate group copolymerizes with the oligomer during ultraviolet curing, incorporating the diluent into the coating network.
1.3Difunctional polyether soft segment
What ifWhat if the urethane oligomer uses a polyether diol as its sole polyether polyol?
Claim language“a polyether polyol that is trifunctional”
React a polypropylene glycol diol with excess aliphatic diisocyanate and cap the terminal isocyanate groups with 2-hydroxyethyl acrylate. The difunctional diol forms linear soft segments, while terminal acrylates connect the oligomers during radical curing.
1.3Acrylate attachment through amine
What ifWhat if 2-aminoethyl acrylate supplies the terminal acrylate groups through urea linkages?
Claim language“a (meth)acrylic ester having at least one hydroxy group”
React free-base 2-aminoethyl acrylate with an isocyanate-terminated polyurethane prepolymer under dry conditions. The primary amine forms a urea linkage at each capped end, and the remaining acrylate double bonds polymerize during ultraviolet exposure.
1.4Single oxygen acrylamide diluent
What ifWhat if the acrylamide diluent is N,N-dimethylacrylamide, whose only oxygen atom belongs to the acryloyl group?
Claim language“contains at least one oxygen atom in addition”
Blend N,N-dimethylacrylamide with the urethane acrylate oligomer and a radical photoinitiator. The liquid amide lowers the blend viscosity, and its vinyl group copolymerizes with the oligomer acrylate groups during ultraviolet exposure.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Protective layer for flexible printed graphics
A clear topcoat covers printed graphics on flexible thermoplastic polyurethane sheets used for equipment labels. The resin contains a urethane acrylate based on a trifunctional polyether polyol with a number average molecular weight of 900 g/mol and N-(2-hydroxyethyl)acrylamide at a urethane acrylate to acrylamide mass ratio of 5:10. A reverse-roll coater applies the resin over the dried print, and ultraviolet light activates a photoinitiator in the topcoat. The cured layer protects the print from handling and cleaning as the sheet bends.
Component substitution
Polycarbonate triol in the urethane acrylate
A hydroxyl-terminated aliphatic polycarbonate triol with a number average molecular weight of about 1000 g/mol replaces the trifunctional polyether polyol. The triol reacts with excess linear aliphatic diisocyanate, and 2-hydroxyethyl acrylate caps the residual isocyanate groups. The resulting urethane acrylate is blended with N-(2-hydroxyethyl)acrylamide at a mass ratio of 5:10 and cured under ultraviolet light with a photoinitiator.
Parameter or scale variation
Two thicknesses at matched ultraviolet dose
A slot die coats a flexible web at wet thicknesses of 8 and 24 micrometers in separate runs using the same urethane acrylate and N-(2-hydroxyethyl)acrylamide formulation at a mass ratio of 5:10. At a web speed of 10 meters per minute, the metering pump delivers 80 or 240 milliliters per minute per meter of coated width. Both runs receive an incident ultraviolet dose of 1.2 joules per square centimeter under nitrogen, and infrared measurements track acrylate conversion at the exposed surface and the substrate interface.
Combination with existing systems
Ultraviolet embossing on a flexible web
A slot die feeds the urethane acrylate and N-(2-hydroxyethyl)acrylamide blend onto a transparent thermoplastic web upstream of an engraved embossing roll. A nip presses the wet layer into the roll texture while ultraviolet light passes through the web and activates a photoinitiator in the resin. The web peels from the roll after curing and carries the replicated texture into the rewinder.
Automated or data-driven variant
Feedback control of blend and cure
Separate mass-flow meters measure the urethane acrylate and N-(2-hydroxyethyl)acrylamide feeds upstream of a static mixer, and a controller trims the urethane acrylate pump to maintain a 5:10 mass ratio. An inline near-infrared sensor reads a residual acrylate band downstream of the ultraviolet station. A calibration against laboratory conversion measurements lets the controller adjust lamp power to hold the conversion setpoint as web speed changes.
Specific version of a part
Oligomer rich coating blend
Blend 200 parts urethane acrylate with 100 parts N-acryloylmorpholine by mass. Warm the blend to 40 °C for coating, then expose the applied layer to ultraviolet light in the presence of a radical photoinitiator.
Aliphatic urethane diacrylate oligomer
React a polycarbonate diol with an excess of hexamethylene diisocyanate to form an isocyanate-terminated urethane oligomer. Cap both ends with 2-hydroxyethyl acrylate to supply two polymerizable acrylate groups per ideal oligomer molecule.
Glycerol initiated polyether triol
Use a glycerol-initiated polypropylene glycol triol with a number-average molecular weight of 900 grams per mole. React the triol with isophorone diisocyanate to form a branched urethane intermediate, then cap the residual isocyanate groups with 2-hydroxyethyl acrylate.
Cyclic ether acrylamide monomer
Use N-acryloylmorpholine, which has a molecular weight of approximately 141 grams per mole and an ether oxygen in its six-membered ring. The acryloyl double bond copolymerizes with urethane acrylate groups during radical curing.
Four to ten blend ratio
Mix 40 grams of urethane acrylate oligomer with 100 grams of N-acryloylmorpholine to set the X/Y mass ratio at 0.40. Stir until homogeneous and incorporate a radical photoinitiator before applying and curing the coating.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
Especially suitable are, for example, esters of ethylenically unsaturated carboxylic acids and polyols or polyepoxides, and polymers having ethylenically unsaturated groups in the chain or in side groups, e.g. unsaturated polyesters, polyamides and polyurethanes and copolymers thereof, alkyd resins, polybutadiene and butadiene copolymers, polyisoprene and isoprene copolymers, polymers and copolymers having (meth)acrylic groups in side chains, and also mixtures of one or more
A · US 2007/0028805 A1 · ¶ 68
The photopolymerizable resin composition includes 40 to 80% by weight of a photopolymerizable urethane (meth)acrylate oligomer, 10 to 40% by weight of a low-viscosity multifunctional urethane acrylate oligomer, and 1 to 10% by weight of a photoinitiator.
B · US 2011/0159285 A1 · abstract
1.2an acrylamide derivative (Y), wherein
The invention encompasses an adhesive, coating or film composition comprising a polymer formed from at least one N-substituted acrylamide monomer, which monomer comprises at least one phosphonic or phosphinic acid or ester moiety.
A · US 2007/0028805 A1 · ¶ 21
1.3the urethane (meth)acrylate (X) comprises at least: a structural unit derived from an isocyanate; a structural unit derived from a polyether polyol that is trifunctional and that has a number average molecular weight of 1200 or lower; and a structural unit derived from a (meth)acrylic ester having at least one hydroxy group,
After the addition was finished, the NCO content of the reaction mixture whose theoretical NCO content is 8.67% was adjusted to 7.5-8.5%. 716.50 g (0.36 moles) of polypropylene glycol polyol (PPG) (Korea Polyol (Korea)) having an average molecular weight of 2,000 was added.
B · US 2011/0159285 A1 · ¶ 66
1.4the acrylamide derivative (Y) is a compound that has a molecular weight of 300 or lower and that contains at least one oxygen atom in addition to an oxygen atom in an acryloyl group, and
The photopolymerizable resin composition according to claim 12, wherein the photopolymerizable monomer is selected from the group consisting of phenoxyethyl acrylate, phenoxyethylene glycol acrylate, phenoxytetraethylene glycol acrylate, phenoxyhexaethylene glycol acrylate, isobornyl acrylate (IBOA), isobornyl methacrylate, N-vinylpyrrolidone (N-VP), N-vinylcaprolactam (N-VC), acryloyl morpholine (ACMO), ethoxylated bisphenol diacrylate, ethoxylated phenol monoacrylate, polye
B · US 2011/0159285 A1 · claim 13
1.5the mass ratio X/Y between the urethane (meth)acrylate (X) and the acrylamide derivative (Y) is 1/10 to 7.5/10.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.2. Only Document B has a passage for 1.31.4. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Other requirements of the composition for the outer coating film are sufficient flexibility for ease of handling of the optical fiber, low water absorption, stickiness, chemical resistance and sufficient adhesion to the inner coating film.
B · US 2011/0159285 A1 · ¶ 4
Related claim parts: 1.2
Incorporation of said monomers into adhesives, pigment dispersants, coatings or films for polar surfaces or polar particles gives improved adhesive, anti-corrosive, and flame retardant properties.
A · US 2007/0028805 A1 · ¶ 2
Conventional phosphorus-containing additives are non-polymerizable and suffer from several drawbacks such as migration and leaching, leading to modification of adhesive, coating or film properties over time.
A · US 2007/0028805 A1 · ¶ 3
However, conventional coating compositions do not ensure rapid curing owing to their high viscosity levels.
B · US 2011/0159285 A1 · ¶ 6
Particular disadvantages associated with the use of the reactive diluents are modification and poor adhesive strength of the compositions in hot water, resulting in low long-term reliability of optical fibers and bringing about a reduction in the ability of optical fibers to transmit signals.
B · US 2011/0159285 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0365773 A1, claim 1, first published 2026-11-23T16:17:13-05:00, https://patent.fyi/US20260365773/, SHA-256 b8588e4b9adbf0f620014478af8a9d99e24e47368c70a8163af6ef2b3088fed1