Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Solid catalyst filtration without chemical neutralization
What ifWhat if the thiol-epoxide reaction stops by filtering out a solid-supported catalyst with no neutralizing agent added?
Claim language“adding a neutralizing agent to terminate the reaction”
A polymer-bound tertiary amine resin or solid metal-oxide catalyst drives the ring-opening addition of thiol groups to epoxide rings in a stirred reactor at 60 to 90 °C. Once titration confirms complete epoxide conversion, the reaction mixture passes through a 5 μm sintered stainless steel filter that retains the solid catalyst particles and stops further catalysis. Omitting a liquid neutralizing agent eliminates dissolved neutralization salts from the resulting hydroxyl-terminated prepolymer.
1.2Secondary diamine chain extender in mixture
What ifWhat if the epoxide-derived prepolymer mixes with a linear secondary aliphatic diamine rather than a branched polythiol?
Claim language“mixing the epoxide-derived prepolymer with a branched polythiol”
The hydroxyl-terminated thioether prepolymer blends with a linear secondary aliphatic diamine such as N,N'-di-sec-butyl-1,6-hexanediamine at 40 to 50 °C under dry nitrogen. Upon isocyanate addition, the secondary amine groups react with isocyanate groups to generate substituted urea linkages alongside the urethane bonds formed by the prepolymer hydroxyls. Hydrogen bonding between the urea groups increases cohesive tensile strength while the thioether prepolymer backbone maintains solvent and moisture resistance.
1.3Multifunctional acrylate crosslinking by conjugate addition
What ifWhat if the thiol-rich mixture reacts with a multifunctional acrylate monomer via base-catalyzed conjugate addition with no isocyanate?
Claim language“mixing the mixture with an isocyanate”
The mixture of hydroxyl-terminated prepolymer and branched polythiol blends with a trifunctional acrylate such as trimethylolpropane triacrylate at a 1:1 molar ratio of thiol groups to acrylate double bonds. A tertiary amine or phosphine catalyst at 0.1 to 0.5 weight percent initiates nucleophilic conjugate addition of thiolate anions across the electron-deficient carbon-carbon double bonds at 25 to 60 °C. This step-growth crosslinking forms a dense thioether-ester adhesive network without generating carbon dioxide gas from ambient moisture.
What ifWhat if step (1) uses pentaerythritol tetrakis(3-mercaptopropionate) as the branched polythiol outside the listed three-compound group?
Claim language“2,3-bis((2-mercaptoethyl)thio)-1-propanethiol, trimethylolpropane tris(3-mercaptopropionate), and 1,3,5-tris(mercaptomethyl)benzene”
Pentaerythritol tetrakis(3-mercaptopropionate) supplies four primary thiol arms attached to a central neopentyl carbon core. Reacting this tetrafunctional polythiol with the epoxide compound yields a four-arm hydroxyl-terminated thioether prepolymer with a higher branching density than a trifunctional core. When crosslinked with isocyanate, the four-arm architecture increases network crosslink density and raises shear strength on coated fabric substrates.
1.6Aromatic glycidyl ether for prepolymer synthesis
What ifWhat if the prepolymer reaction uses phenyl glycidyl ether rather than ethylene oxide, propylene oxide, or epoxypentane?
Claim language“ethylene oxide, propylene oxide, and epoxypentane”
Phenyl glycidyl ether reacts with the branched polythiol in the presence of a base catalyst at 70 to 100 °C to open the oxirane ring and generate beta-hydroxy thioether linkages bearing pendant phenoxymethyl groups. Because phenyl glycidyl ether is a low-volatility liquid at room temperature, the reaction proceeds in an atmospheric-pressure vessel without a pressurized autoclave. The pendant aromatic rings increase glass transition temperature and increase resistance to nonpolar organic solvents.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Marine composite hull bonding with sulfur-containing polyurethane adhesive
The solvent-free sulfur-containing polyurethane adhesive bonds glass-fiber reinforced unsaturated polyester hull panels to structural foam cores in marine vessel construction. After degassing at 500 Pa to remove entrained air, the liquid adhesive is metered through a dual-component static mixer onto abraded composite surfaces at a wet film thickness of 0.3 mm to 0.8 mm. The bonded assembly cures under a vacuum bag pressure of 80 kPa at 40 °C for 6 hours to form a hydrolytically stable, thioether-linked urethane bond line. The resulting joint resists saltwater ingress, cyclic hull flexing, and subzero deck temperatures.
Component substitution
Tetrafunctional thiol and cycloaliphatic epoxide prepolymer synthesis
Pentaerythritol tetrakis(3-mercaptopropionate) replaces the trifunctional branched polythiol in both the prepolymer synthesis step and the subsequent chain-extension mixing step, while cyclohexene oxide replaces the linear aliphatic epoxide compound. The four thiol groups per monomer react with the cycloaliphatic epoxide rings in the presence of a phosphazene base catalyst at 65 °C to form a higher-functionality hydroxyl-terminated thioether prepolymer, followed by neutralization with solid-supported sulfonic acid resin beads that are removed by filtration. Mixing this prepolymer with additional pentaerythritol tetrakis(3-mercaptopropionate) and reacting the blend with isophorone diisocyanate produces a densely crosslinked polyurethane network with an increased glass transition temperature.
Hexamethylene diisocyanate trimer and glycidyl ether prepolymer formulation
Butyl glycidyl ether replaces the simple alkylene oxide in the first reaction stage, and a hexamethylene diisocyanate isocyanurate trimer replaces the monomeric isocyanate in the final stage. The branched polythiol undergoes ring-opening addition with butyl glycidyl ether using a zinc carboxylate catalyst at 75 °C, and the catalyst is deactivated by adding a chelating beta-diketone compound instead of a mineral acid. The resulting hydroxyl-functional thioether prepolymer is blended with the branched polythiol and reacted with the aliphatic trimer at an isocyanate-to-active-hydrogen molar ratio of 1.05:1. Degassing the reacted product under a vacuum of 200 Pa at 50 °C yields a non-yellowing polyurethane adhesive suited for outdoor exposure.
Parameter or scale variation
High-ratio hydroxyl prepolymer synthesis in continuous microreactors
The prepolymer synthesis operates in a continuous stainless-steel plate microreactor with internal channel diameters of 0.8 mm and a residence time of 180 seconds at 95 °C and 0.6 MPa gauge pressure. The branched polythiol and epoxide compound enter through separate mass-flow-controlled inlets at a thiol-to-epoxy molar ratio of 1:18 to produce a high-molecular-weight polyether-thioether prepolymer. Downstream, a static inline mixer combines the neutralized prepolymer with additional branched polythiol at a hydroxyl-to-thiol molar ratio of 3.5:10, and a second mixing zone injects the isocyanate at an isocyanate-to-active-hydrogen molar ratio of 1.25:1. A continuous thin-film vacuum degasser operating at 150 Pa and 55 °C removes dissolved gases at a throughput of 25 kg per hour.
Combination with existing systems
Integration with roll-to-roll slot-die textile lamination lines
The solvent-free adhesive preparation vessel connects directly through heated stainless-steel transfer hoses maintained at 45 °C to a precision slot-die coater on a continuous roll-to-roll textile lamination line. A progressive-cavity metering pump feeds the degassed polyurethane adhesive from a nitrogen-blanketed day tank into the die manifold to deposit a uniform 40-micrometer layer onto a moving woven polyester base fabric. Immediately downstream, a heated nip roller pair applies 0.4 MPa line pressure at 80 °C to laminate a thermoplastic elastomer backing film onto the coated fabric. The laminated web passes through a 12-meter infrared and convective curing tunnel at 90 °C before winding onto a tension-controlled take-up roll.
Automated or data-driven variant
Closed-loop spectroscopic monitoring and automated reagent dosing
An inline attenuated total reflectance infrared probe mounted in the reactor wall tracks the epoxide ring absorption band near 910 cm⁻¹ and the isocyanate stretching band near 2270 cm⁻¹ at 5-second intervals. A programmable logic controller reads the real-time spectral peak areas together with reactor temperature and torque viscosity measurements from an inline rotational viscometer. A trained gradient-boosted regression model predicts residual epoxide conversion and hydroxyl value, automatically opening the metering valve for the neutralizing agent when conversion reaches 99.2 percent. During the final stage, the controller adjusts the isocyanate feed pump rate to hold the molar ratio of isocyanate groups to active hydrogen groups within 0.01 of the target setpoint before routing the batch to an automated vacuum degassing cycle.
Specific version of a part
Alkali hydroxide catalysis with phosphoric acid neutralization
Aqueous potassium hydroxide at 0.2 to 0.5 weight percent based on total reactants catalyzes the ring-opening addition of the branched polythiol and epoxide compound at 80 to 110 °C under a nitrogen blanket. Upon reaching target hydroxyl value, stoichiometric 85 percent phosphoric acid neutralizes the alkali catalyst to form insoluble potassium phosphate salts. Vacuum filtration through a diatomaceous earth filter aid followed by vacuum stripping at 100 °C removes the precipitated salts and residual water.
Aliphatic polyisocyanate curing with thin-film vacuum degassing
The prepolymer-polythiol mixture reacts with a solvent-free hexamethylene diisocyanate isocyanurate trimer in the presence of 0.05 weight percent dibutyltin dilaurate at 55 to 70 °C under dry nitrogen. The viscous reaction product then flows as a 1 to 2 millimeter film down the heated inner wall of a wiped-film degasser operating at 0.5 to 2 kPa absolute pressure. Thin-film exposure under reduced pressure extracts entrapped nitrogen and trace carbon dioxide bubbles within 2 to 5 minutes before packaging.
Semi-batch epoxide feeding at 1:6 molar ratio
The reactor initially charges the entire mass of branched polythiol and catalyst, then meters liquid epoxide continuously over 3 hours until the cumulative molar ratio of thiol groups to epoxy groups reaches 1:6. Staged addition controls the exothermic ring-opening enthalpy of 85 to 95 kJ/mol of epoxide and maintains reactor temperature between 85 and 95 °C via an external cooling jacket. This 1:6 ratio yields oligomeric polythioether-polyether arms averaging six oxyalkylene repeat units per original thiol site, balancing low-temperature flexibility with sulfur content.
Static-mixer blending at 3:10 hydroxyl-to-thiol ratio
Positive-displacement gear pumps meter the epoxide-derived prepolymer and the branched polythiol at a fixed hydroxyl-to-thiol molar ratio of 3:10 into a jacketed 18-element helical static mixer heated to 45 °C. Heating reduces the viscosity of the prepolymer below 500 mPa·s so the two streams homogenize without entraining air. The resulting uniform mixture supplies both hydroxyl groups for urethane formation and abundant thiol groups for thiourethane bond formation in the subsequent isocyanate reaction.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(1) mixing a branched polythiol with an epoxide compound, adding a catalyst to conduct a reaction, and then adding a neutralizing agent to terminate the reaction, thereby obtaining an epoxide-derived prepolymer;
A process for producing a plastic lens described above in 1., wherein the prepolymer comprising sulfur is prepared by bringing at least one compound having epithio group, sulfur and a portion of a polythiol compound into reaction with each other in presence of a vulcanization catalyst; 3.
A · US 8,193,303 B2 · ¶ 24
1.2(2) mixing the epoxide-derived prepolymer with a branched polythiol, thereby obtaining a mixture; and
The process for mixing the prepolymer comprising sulfur and the rest of the polythiol compound is not particularly limited as long as the components can be sufficiently mixed together.
A · US 8,193,303 B2 · ¶ 71
1.3(3) mixing the mixture with an isocyanate and conducting a reaction, thereby obtaining a product, and subjecting the product to degassing treatment to obtain the high-strength polyurethane adhesive;
According to the present invention, isocyanate-terminated urethane-containing prepolymers can comprise the reaction product of reactants comprising: the polythiol adduct provided by the present disclosure; a thiol-terminated sulfur-containing prepolymer; and a diisocyanate.
B · US 2018/0112025 A1 · ¶ 35
1.4in step (1), the branched polythiol and the epoxide compound are mixed according to a molar ratio of thiol groups to epoxy groups of 1:(0.1-25);
1.5in step (1), the branched polythiol is one selected from the group consisting of 2,3-bis((2-mercaptoethyl)thio)-1-propanethiol, trimethylolpropane tris(3-mercaptopropionate), and 1,3,5-tris(mercaptomethyl)benzene;
A process for producing a plastic lens described above in any one of 1. to 6., wherein the polythiol compound is at least one compound selected from bis(mercaptomethyl)-1,4-dithiane, bis(mercaptoethyl)sulfide, bis(mercaptoethyl)disulfide, 1,2-bis(mercaptoethyl)thio-3-mercapto-propane, pentaerythritol tetrakismercaptoacetate, pentaerythritol tetrakismercaptopropionate, trimethylolpropane trismercaptoacetate, trimethylolpropane trismercaptopropionate and trimercaptopropane; 8.
A · US 8,193,303 B2 · ¶ 24
1.6the epoxide compound is one selected from the group consisting of ethylene oxide, propylene oxide, and epoxypentane;
1.7in step (2), the epoxide-derived prepolymer and the branched polythiol are mixed according to a molar ratio of hydroxyl groups in the epoxide-derived prepolymer to thiol groups in the branched polythiol of (2-4):10; and
In the polyaddition reaction between a thiol-terminated sulfur-containing prepolymer, a polythiol adduct and a diisocyanate, the reactants can comprise an equivalent ratio of thiol-terminated sulfur-containing prepolymer from about 2:5 to about 1.5:4, from about 1:3 to about 1:5, or about 1:3.
B · US 2018/0112025 A1 · ¶ 311
1.8in step (3), the mixture and the isocyanate are mixed according to a molar ratio of —N═C═O groups in the isocyanate to active hydrogen groups in the mixture of 0.8-1.3.
The total diisocyanate equivalent to thiol equivalent index can be from about 2.0 to about 2.1, and the equivalent ratio of diisocyanate to thiol can be from about 5:1 to about 2:1.
B · US 2018/0112025 A1 · ¶ 311
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.11.21.5. Only Document B has a passage for 1.31.71.8. Both are classified in CPC C08G, as is this patent.
Additional background
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, CR-39 has a refractive index of about 1.50 which is smaller than those of inorganic glasses, and a drawback arises in that the thickness of the lens is increased at edge portions in minus-power lenses and at the central portion in plus-power lenses.
A · US 8,193,303 B2 · ¶ 5
The present invention relates to a process for producing a plastic lens and, more particularly, to a process for producing a plastic lens which exhibits excellent weatherability in combination with a great refractive index, a great Abbe number and excellent transparency.
A · US 8,193,303 B2 · ¶ 2
Low density aerospace coatings and sealants having homogenously dispersed fillers, improved adhesion, and enhanced flexibility are desired.
B · US 2018/0112025 A1 · ¶ 5
Isocyanate-terminated urethane-containing prepolymers of the present invention can be combined with a polyamine curing agent and a low density filler to provide low density coatings and sealants that meet the requirements of aerospace sealant applications.
B · US 2018/0112025 A1 · ¶ 6
For example, by using a specific aliphatic isocyanate or a specific alicyclic isocyanate, it is possible to obtain a urethane resin-based optical material or a thiourethane resin-based optical material and a plastic lens including a photochromic compound without causing deterioration in performance of the photochromic compound (Patent Document 1).
C · US 12,275,813 B2 · ¶ 6
Related claim parts: 1.3
Document C: US 12,275,813 B2, published Apr 15, 2025. Cited for this statement only.
Cite aspatent.fyi, US 2026/0365778 A1, claim 1, first published 2026-11-23T16:17:13-05:00, https://patent.fyi/US20260365778/, SHA-256 5f8c59a65ae972338aed684fca56cdc67a9f3937c02904587977978c82cfac8c