patent.fyi
Applications  /  US 2026/0365782
United States Patent Application Publication

US 2026/0365782 A1

Published
Nov 19, 2026
Filed
Apr 24, 2024
Earliest date on the face
Apr 24, 2023
Classification
C08G 59/504
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Longer oligomeric repeat unit chains

What ifWhat if the repeating segment contains 8 to 20 units?
Claim language“n is 1-5”

Extending the repeat count to 8 to 20 oxyalkylene or alkylene units increases the chain length between crosslinks and lowers the glass transition temperature of the cured network. The longer flexible segments improve impact resistance and reduce internal stress during curing at 0 °C to 10 °C. The weight ratio of curing agent to epoxy resin is increased to maintain a 1:1 molar ratio of active amine hydrogens to epoxide rings.

1.2Bulky cyclic substituents on backbone positions

What ifWhat if the substituent positions carry cyclohexyl or phenyl rings?
Claim language“consisting of H, CH3, C2H5”

Attaching cyclohexyl or phenyl rings at the substituent positions introduces steric hindrance around adjacent reactive centers and increases backbone rigidity. The bulky hydrophobic rings reduce moisture uptake and surface carbamation during ambient or cold-temperature curing in humid environments. Higher aromatic or cycloaliphatic content raises the glass transition temperature and chemical resistance of the crosslinked epoxy matrix.

1.5Hydroxyalkyl side groups for self-acceleration

What ifWhat if the side substituent is a 2-hydroxyethyl or 2-hydroxypropyl group?
Claim language“independently methyl, or ethyl”

A 2-hydroxyethyl or 2-hydroxypropyl side group supplies an intramolecular hydroxyl hydrogen bond donor directly adjacent to the curing site. During mixing with a diglycidyl ether resin at 0 °C to 10 °C, the hydroxyl group polarizes the epoxide oxygen and accelerates nucleophilic ring opening without requiring an external phenolic accelerator. The polar side chains also improve adhesion to wet mineral or metallic substrates.

1.6Aromatic or cycloaliphatic divalent spacers

What ifWhat if the divalent spacer group is a meta-xylylene or 1,4-cyclohexylene ring?
Claim language“ethylene, propylene, isopropylene, butylene, isobutylene”

Replacing short aliphatic alkylene spacers with meta-xylylene or 1,4-cyclohexylene units stiffens the curing agent backbone while retaining primary amine reactivity at low temperatures. Meta-xylylene spacers promote fast gelation below 10 °C and limit water absorption in the cured thermoset. The rigid ring geometry increases tensile modulus and thermal stability of the crosslinked polymer.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cold-weather marine hull repair composite laminate

A marine composite repair system pairs a bisphenol-based liquid epoxy resin with the three-component modified amine curing agent for structural patching of vessel hulls at ambient water temperatures between 2 °C and 8 °C. Glass fiber reinforcement fabrics are saturated with the resin and curing agent mixture at a stoichiometric amine-to-epoxide ratio of 1.0 and applied directly onto abraded hull surfaces under vacuum bagging at 85 kPa. Crosslinking proceeds to full structural hardness within 24 hours without external heaters, forming a water-resistant thermoset laminate. At end of service life, immersion of the detached patch in a dilute acidic cleavage bath at 70 °C dissolves the cured matrix and recovers clean glass fibers for reuse.

Refrigerated storage facility seamless structural floor coating

The three-component modified curing agent and a bisphenol-F epoxy resin form a self-leveling floor coating applied inside active cold-storage warehouses operating at 4 °C without shutting down refrigeration units. Silica flour filler at 35 wt% is dispersed into the resin component using a high-shear mixer prior to combining with the curing agent at a 2:1 volume ratio. Installers spread the mixed slurry onto shot-blasted concrete slabs at a wet film thickness of 3 mm using notched squeegees and spiked aeration rollers. The coating reaches foot-traffic hardness in 14 hours at 4 °C and undergoes localized chemical stripping with a heated acidic gel when floor sections require resurfacing.

Combination with existing systems

Closed-loop filament winding and solvolysis recycling line

The recyclable low-temperature epoxy system integrates directly into a multi-axis wet filament winding machine equipped with a temperature-controlled resin bath held at 8 °C. Continuous carbon fiber tows pass through the chilled bath containing the epoxy resin and the three-component modified curing agent before winding onto a cylindrical mandrel to form pressure vessels. A dedicated post-life chemical recycling unit connects downstream, combining a mechanical shredder, a 500 L agitated solvolysis reactor operating with aqueous acetic acid at 90 °C, and a vacuum filtration skid. The filtration skid separates intact carbon fibers from the liquid cleavage stream, while a rotary evaporator recovers the dissolved thermoplastic-like epoxy oligomers for reformulation into secondary moldings.

Specific version of a part

Zero-unit direct linkage configuration

Setting n to 0 eliminates the intervening repeating segment and bonds the terminal functional group directly to the core structure. This compact molecular geometry lowers molecular weight per reactive site and increases crosslink density in the cured epoxy network. The shorter spacing yields higher compressive strength and faster initial tack-free times at 5 °C.

Three-unit oligomeric spacer segment

Selecting m as 3 builds a three-unit repeating spacer that balances chain flexibility with high reactive group concentration. The trimer-length segment lowers crystallization tendency during cold storage at 0 °C and keeps the curing agent pumpable without preheating. During cure, the three-unit span reduces shrinkage stress across bonded composite interfaces.

Cite aspatent.fyi, US 2026/0365782 A1, claim 1, first published 2026-11-23T16:17:13-05:00, https://patent.fyi/US20260365782/, SHA-256 102462be669ead7844ef1db187b47e715269c452cdd06982a223a4898da4fb0d
First published
Permanent addresshttps://patent.fyi/US20260365782/