1.1Coupling carboxyl end groups
A twin-screw extruder disperses a multifunctional epoxy oligomer into dried, carboxyl-terminated polyester. The epoxy groups react with carboxyl end groups to couple polyester chains, increasing melt viscosity.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A twin-screw extruder disperses a multifunctional epoxy oligomer into dried, carboxyl-terminated polyester. The epoxy groups react with carboxyl end groups to couple polyester chains, increasing melt viscosity.
A stirred reactor dissolves polybutylene terephthalate in a phenolic solvent below TmA. Added 1,4-butanediol and a titanate catalyst promote ester exchange in solution. A nonsolvent precipitates the polyester for filtration and drying.
A wiped-film reactor holds the polyester at 10 to 20 °C above TmB and renews the exposed melt surface. Reduced pressure withdraws glycol vapor and shifts the polycondensation reaction toward chain growth.
A pressure vessel circulates supercritical carbon dioxide through polyester granules below TmB. The fluid extracts soluble low-molecular-mass constituents, which separate from the carbon dioxide when the downstream separator reduces the pressure.
A vacuum vent in the first treatment removes free glycol after a melt mixing zone provides residence time for ester exchange. A second heat treatment under dry nitrogen below TmB removes additional volatile material and supports solid-state polycondensation.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A jacketed stirred vessel mixes 100 parts by mass of polyethylene terephthalate with 1.0 part by mass of ethylene glycol and heats the mixture above the feed resin melting point. A cooled belt solidifies the discharged melt, and a granulator cuts it into chips. A liquid chromatography assay measures unreacted ethylene glycol in the chips and confirms a concentration from 0.05 to 4.76 mass percent before the second heating stage. A nitrogen-purged tray oven heats the chips below their measured melting point, and an injection molding machine uses the treated chips to form appliance housings.
A metering pump feeds 1,2-propanediol in place of ethylene glycol at 0.5 parts by mass per 100 parts by mass of polyethylene terephthalate. A stirred melt vessel operates above the feed resin melting point and discharges the treated melt onto a cooled belt. Gas chromatography measures free 1,2-propanediol in a cooled sample, and the operator adjusts the first-stage hold time on subsequent batches to maintain 0.05 to 0.30 mass percent free glycol. A nitrogen-purged oven heats the granulated discharge below its measured melting point.
A stirred batch reactor receives 1.00 kilogram of polyethylene terephthalate and 10 grams of ethylene glycol. The reactor holds the mixture for 5 minutes at 15 °C above the measured feed melting point and then discharges it onto a chilled plate. The cooled material is granulated to 2 to 3 millimeters, and a free-glycol assay checks that the intermediate contains 0.05 to 4.76 mass percent unreacted glycol. A nitrogen-purged oven holds the granules for 2 hours at 25 °C below the measured intermediate melting point.
A stirred melt vessel combines 100 parts by mass of polyethylene terephthalate with 0.75 parts by mass of ethylene glycol and heats the mixture above the feed melting point. A cooled belt solidifies the discharge for granulation, and a free-glycol assay verifies that the intermediate contains 0.05 to 4.76 mass percent unreacted glycol. A perforated conveyor carries the granules through a first nitrogen-purged zone for 30 minutes at 55 °C below the intermediate melting point. A second nitrogen-purged zone holds the granules for 90 minutes at 25 °C below that melting point, with belt speed and heated zone lengths setting the residence times.
A stirred melt vessel meters 1.0 part by mass of ethylene glycol per 100 parts by mass of polyethylene terephthalate and operates above the feed melting point. A gear pump sends the melt through a heated screen pack and into a pressurized underwater pelletizer. A centrifugal dryer removes surface water, and a chromatographic assay of the dried pellets checks for 0.05 to 4.76 mass percent unreacted glycol after water contact. A moving-bed heater then passes dry nitrogen through the pellets at a temperature below their measured melting point.
A controller uses load cells and a metering pump to add 1.0 part by mass of ethylene glycol per 100 parts by mass of polyester and a thermocouple to hold the stirred vessel above the measured feed melting point. An automated sampler cools a portion of the discharge and extracts free glycol for liquid chromatography. The controller releases intermediate batches to the second stage only when the measured free glycol concentration falls within 0.20 to 0.40 mass percent, and it adjusts the next batch's glycol dose within 0.1 to 5.0 parts by mass based on the measured deviation. The controller sets the second-stage oven 20 °C below the intermediate melting point entered from a differential scanning calorimetry measurement.
A metering pump feeds one part by mass of 1,4-butanediol per 100 parts by mass of dried polybutylene terephthalate into a pressurized twin-screw mixing zone. The zone holds the mixture above the measured TmA and disperses the glycol through the melt.
A stirred batch reactor combines 0.5 parts by mass of ethylene glycol with 100 parts by mass of polyethylene terephthalate. A heated jacket brings the mixture to 15 °C above its measured TmA, and an anchor agitator circulates the viscous melt.
Crystallized pellets of resin B enter a moving-bed vessel held at 20 °C below the measured TmB. Dry nitrogen flows countercurrent to the pellets and carries away glycol and other volatile reaction products.
The first melt treatment uses controlled residence time and vent pressure to produce resin B with 0.20 mass % free 1,4-butanediol. Solvent extraction and calibrated gas chromatography quantify the free glycol in a sample taken before the second heat treatment.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The glycolysis method is a method wherein a polyester is heated together with a depolymerization catalyst such as sodium carbonate in an excess alkylene glycol solvent to depolymerize the polyester and thereby form a bis(β-hydroxyalkyl)terephthalate and ethylene glycol (patent document 4, patent document 5).A · US 7,897,651 B2 · ¶ 7
Crosslinking also can be affected by heating the fused image to a temperature at which the toner will be crosslinked, for example in a post-fusing operation. In embodiments, crosslinking can be effected at temperatures of from about 160° C. or less, in embodiments from about 70° C. to about 160° C., in other embodiments from about 80° C. to about 140° C.B · US 8,829,149 B2 · ¶ 67
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.1. Only Document B has a passage for 1.2.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
This feedstock recycling is expected as a means capable of realizing reuse of resources because separation of impurities is feasible and the qualities of the raw materials do not differ so much from those of virgin materials.A · US 7,897,651 B2 · ¶ 3
Therefore, shortening of the reaction time has been desired.A · US 7,897,651 B2 · ¶ 8
Because toners are used in such great quantities worldwide, recycling the CO2 produced as a byproduct of preparing polyester resins used in the toners may reduce the amount of CO2 released into the environment.B · US 8,829,149 B2 · ¶ 5
There is a need to minimize the amount of carbon dioxide generated and released to the atmosphere.B · US 8,829,149 B2 · ¶ 5
patent.fyi, US 2026/0365785 A1, claim 1, first published 2026-11-23T16:17:13-05:00, https://patent.fyi/US20260365785/, SHA-256 ea0625d01f1b0bf2e1336260648be2d7699bc7a1b313f67921e7e4a1c0562f8d