Applications  /  US 2026/0365792
United States Patent Application Publication

US 2026/0365792 A1

Published
Nov 19, 2026
Filed
May 30, 2024
Earliest date on the face
May 31, 2023
Classification
C08G 75/23
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Free-radical vinyl end groups for polymerization

What ifWhat if each R1 is a vinyl group that undergoes free-radical chain-growth polymerization rather than a leaving group or a nucleophilic group?
Claim language“a leaving group or a nucleophilic group”

Both terminal positions of the diphenylsulfone core carry vinyl groups that react in the presence of a thermal radical initiator such as azobisisobutyronitrile at 65 to 80 degrees Celsius in a polar aprotic solvent. Chain-growth propagation links the vinyl groups into an all-carbon polymer backbone bearing pendant diphenylsulfone units with hydrophilic sidechains. The resulting copolymer dissolves in casting solvents and undergoes nonsolvent-induced phase separation to form a porous separation membrane.

1.2Ring-opened polyether sidechains on the core

What ifWhat if each grafted polymeric sidechain is a polyether produced by ring-opening polymerization of cyclic ethers rather than repeat units derived from an ethylenically unsaturated monomer?
Claim language“derived from an ethylenically unsaturated monomer”

Hydroxyl or amine initiator sites attached to the diphenylsulfone ring initiate anionic ring-opening polymerization of ethylene oxide at 80 to 120 degrees Celsius using an alkali metal alkoxide catalyst. Controlled monomer feed sets the poly(ethylene oxide) chain length between 20 and 100 repeat units per sidechain without carbon-carbon double bond polymerization. During membrane casting by phase inversion, the hydrophilic polyether segments migrate to the pore walls and establish a protein-resistant surface for biomolecule filtration.

1.2Discrete zwitterionic groups without polymeric chains

What ifWhat if each R2 is a single non-polymeric zwitterionic sulfobetaine moiety with no polymeric sidechain?
Claim language“a grafted polymeric sidechain”

An amino-substituted diphenylsulfone monomer reacts with 1,3-propanesultone in an aprotic solvent at 50 to 70 degrees Celsius to install a discrete quaternary ammonium-sulfonate group directly onto the aromatic ring. Polycondensation of this zwitterionic monomer with a dihalo diphenylsulfone and a bisphenol yields a hydrophilic sulfone copolymer with charge-balanced groups along the backbone. In aqueous phase-inversion casting, the zwitterionic moieties hydrate at the polymer-water interface and generate porous membranes that resist protein adsorption.

1.3Three or four sidechains per ring

What ifWhat if p is an integer equal to 3 or 4 so that one phenyl ring carries three or four sidechains?
Claim language“equal to 0, 1, or 2”

Exhaustive halogenation or nitration of one aromatic ring on the diphenylsulfone precursor installs three or four reactive anchor sites at the unsubstituted ring carbons. Subsequent coupling attaches three or four hydrophilic polymeric sidechains to that single ring, creating a densely branched comb architecture at a low molar ratio of modified monomer. Incorporating 2 to 5 mole percent of this multi-armed macromer into a polysulfone backbone supplies high hydrophilic segment density while preserving the mechanical strength of the hydrophobic matrix.

1.5Unmodified diphenylsulfone core with blended additive

What ifWhat if p+q equals 0 so that the diphenylsulfone monomer carries no grafted sidechains and hydrophilicity is imparted by blending a separate amphiphilic copolymer?
Claim language“equal to at least 1”

An unsubstituted dihalo diphenylsulfone undergoes step-growth polycondensation with a bisphenol at 150 to 180 degrees Celsius in dimethylacetamide with potassium carbonate to form a linear polyethersulfone homopolymer. The base polymer dissolves together with 5 to 15 weight percent of a separate amphiphilic block copolymer additive in a common casting solvent. During immersion precipitation in water, the hydrophilic blocks of the additive segregate to the pore surfaces and form a porous membrane for size-based biomolecule separation.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Proton exchange membrane for redox flow batteries

A dense ion-exchange membrane uses copolymers polymerized from diphenylsulfone macromers carrying grafted polymeric sidechains with sulfonic acid repeat units. The macromers polycondense with aromatic dihydroxyl monomers and activated dihalides in polar aprotic solvent at 160 °C to form a microphase-separated polyarylene ether sulfone film with a dry thickness of 50 micrometers. Installed between the positive and negative carbon felt electrodes of an aqueous vanadium redox flow cell, the hydrophobic sulfone backbone provides mechanical stability while the hydrated grafted sidechains form continuous proton-conducting channels. The membrane conducts hydrogen ions across the cell during charge and discharge cycles while limiting vanadium ion crossover between the two electrolyte half-cells.

Asymmetric gas separation membrane for flue gas capture

An integrally skinned asymmetric hollow fiber membrane spins from a copolymer of diphenylsulfone macromers bearing grafted poly(ethylene glycol) methyl ether methacrylate sidechains. Dry-jet wet spinning with a 15 centimeter air gap evaporates volatile cosolvent from the outer surface to form a dense selective skin layer 120 nanometers thick supported by a macroporous substructure. The membrane fibers assemble into a pressurized shell-and-tube module fed with humidified flue gas at 5 bar and 35 °C. The rigid aromatic sulfone matrix resists plasticization under feed pressure while the polar ether oxygen atoms along the grafted sidechains selectively solubilize and permeate carbon dioxide over nitrogen.

Component substitution

Polyoxazoline sidechains replacing ethylenically unsaturated grafted sidechains

A functionalized diphenylsulfone macromer carries grafted poly(2-ethyl-2-oxazoline) sidechains in place of sidechains derived from ethylenically unsaturated monomers. Halomethyl groups attached to the aromatic rings of the diphenylsulfone core initiate cationic ring-opening polymerization of 2-ethyl-2-oxazoline in acetonitrile at 80 °C, followed by nucleophilic termination with methanolic potassium hydroxide. The resulting amphiphilic macromer undergoes step-growth polycondensation with aromatic diol monomers to yield a graft copolymer that casts into porous ultrafiltration membranes through nonsolvent-induced phase separation. During aqueous filtration, the hydrophilic amide-bearing polyoxazoline chains segregate to the pore walls and form a hydrated surface layer that reduces protein adsorption.

Parameter or scale variation

Ultralong grafted sidechains with extended macromer substitution density

A heavily substituted diphenylsulfone macromer carries between 5 and 6 grafted polymeric sidechains distributed across both phenyl rings, with each sidechain containing 1500 to 3000 repeat units of a hydrophilic methacrylate monomer. The macromer copolymerizes at a 2 to 5 mole percent loading with unsubstituted dihalodiphenylsulfone and aromatic diol monomers in N-methyl-2-pyrrolidone at 185 °C for 14 hours to reach a weight-average molar mass above 180 kg/mol. A casting dope containing 14 weight percent of the copolymer extrudes through a spinneret with a bore fluid flow rate of 4 milliliters per minute into a 45 °C aqueous coagulation bath to form hollow fibers with an outer diameter of 1.8 millimeters. The long brush sidechains produce an open, interconnected sponge morphology with average pore diameters between 0.6 and 1.5 micrometers for high-flux cell harvesting.

Combination with existing systems

Hollow fiber membrane module inside tangential flow bioreactor

A bundle of porous hollow fiber membranes fabricated from the grafted diphenylsulfone copolymer sits potted in epoxy resin inside a cylindrical polysulfone housing equipped with feed, retentate, and permeate sanitary ports. The membrane module connects in an external recirculation loop to a stirred-tank perfusion bioreactor through a low-shear diaphragm pump that maintains a cross-flow velocity of 0.5 meters per second across the fiber lumens. Fresh nutrient medium enters the bioreactor at a rate matching cell-free permeate withdrawal through the membrane pores, retaining viable cells inside the vessel while harvesting secreted proteins continuously. Inline differential pressure transmitters across the feed and retentate ports trigger periodic reverse-flow permeate pulses to dislodge accumulated cell debris from the inner fiber walls.

Automated or data-driven variant

Closed-loop automated synthesis and phase inversion control system

An automated continuous-flow synthesis rig uses inline mid-infrared absorption spectroscopy probes and size-exclusion chromatography sampling valves to monitor monomer conversion and grafted sidechain length during diphenylsulfone macromer preparation. A trained regression model correlates real-time spectroscopic absorbance ratios, reaction temperature, and residence time to predict final copolymer molar mass and hydrophilic sidechain weight fraction. When predicted values drift outside target tolerances, a supervisory control program adjusts reagent syringe pump flow rates and jacket heater setpoints before feeding the resulting polymer dope into a flat-sheet casting line. During membrane formation, an optical laser micrometer and an inline bubble-point porometer measure wet film thickness and mean pore diameter, updating the casting knife gap and coagulation bath temperature automatically.

Specific version of a part

Para-fluoro leaving groups for nucleophilic substitution

Both R1 positions on the diphenylsulfone core carry fluorine atoms positioned para to the electron-withdrawing sulfone bridge. During step-growth polycondensation with an aromatic diol and potassium carbonate in N-methyl-2-pyrrolidone at 160 to 180 degrees Celsius, the sulfone group activates the carbon-fluorine bonds toward nucleophilic aromatic substitution. High-molecular-weight polyarylethersulfone copolymers form with high conversion and minimal side reactions.

Reversible addition-fragmentation poly(vinylpyrrolidone) sidechains

A thiocarbonylthio chain-transfer agent attaches to the diphenylsulfone ring through a benzyl ester linkage and mediates polymerization of N-vinylpyrrolidone in an organic solvent at 70 to 80 degrees Celsius. Controlled radical propagation grows hydrophilic poly(vinylpyrrolidone) sidechains with a number-average molecular weight between 5,000 and 20,000 grams per mole and a dispersity below 1.3. The resulting macromer copolymerizes into a polyethersulfone backbone that forms hydrophilic hollow-fiber membranes for protein separation.

Single sidechain attachment on one ring

Monobromination of one phenyl ring on 4,4'-difluorodiphenylsulfone sets p equal to 1 and leaves the remaining aromatic ring carbons unsubstituted. A single initiator handle attaches at the meta position relative to the sulfone bridge, limiting steric crowding during subsequent sidechain growth and polycondensation. This single-site substitution yields a comb copolymer with uniform sidechain spacing along the main chain.

Symmetric bis-substitution on the second ring

Setting q equal to 2 places two grafted polymeric sidechains at the 3- and 5-positions of the second phenyl ring while p remains 0 on the first ring. Dibromination of the precursor followed by palladium-catalyzed cross-coupling installs two identical polymerization initiators symmetrically around the R1 substituent. The resulting two-armed macromer doubles the local hydrophilic chain density per incorporated comonomer unit during membrane formation.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2009/0221787 A1
Published
Sep 3, 2009
Filed
Jul 10, 2006
Class
C08G 75/00
Document BUS 2012/0316337 A1
Published
Dec 13, 2012
Filed
Feb 17, 2011
Class
C07C 227/08
Claim 1
Document A
Document B
1.1each R1 is independently a leaving group or a nucleophilic group
Their derivatives) according to claim 1, caracterised in that they contain a broad substitution pattern of reactive halogen aromates (preferentially fluoro aromates) and can carry proton conducting groups (see FIG. 1 and FIG. 3), whereby as halogenated monomers are preferred: bis(pentafluorophenyl)sulfone, bis(pentafluorophenyl)sulfide, decafluorobiphenyle, 4,4′-difluorobiphenyle, decafluorobenzophenone, 4,4′-difluorobenzophenone, bis(4-fluorphenyl)phenylphosphinoxide), decaf
A · US 2009/0221787 A1 · claim 2
By “MNu”, we mean a reactant in which M is a metal and Nu is an independent nucleophile or a substituent of the aromatic ring of the benzoic acid derivative of general formula (II), said substituent being capable—or bearing a functional group capable—of reacting in the presence of a base and a metal to form MNu.
B · US 2012/0316337 A1 · ¶ 23
1.2each R2 comprises a grafted polymeric sidechain comprising a plurality of repeat units derived from an ethylenically unsaturated monomer
1.3p is an integer equal to 0, 1, or 2
1.4q is an integer equal to 0, 1, or 2
1.5p+q is an integer equal to at least 1.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The aim of this invention is to provide by nucleophilic aromatic substitution (SNAr) monomeric, oligomeric or polymeric sulfonic acids respective phosphonic acids or sulfonic acids derivatives or respective phosphonic acid derivates.
A · US 2009/0221787 A1 · ¶ 11
This method can be transferred surprisingly also to other suitable partly- or perhalogenated (preferentially partly- or perfluorinated) polymers.
A · US 2009/0221787 A1 · ¶ 11
Another known disadvantage of nucleophilic substitution is the need to protect/deprotect the carboxyl function (CO2H), necessary as a carbon anchoring point for subsequent chemical functionalization.
B · US 2012/0316337 A1 · ¶ 5
The invention has the industrial advantage of not requiring the use of metal catalysts, and therefore allows avoiding all of the current steps of purification/removal of precious metals, in particular palladium.
B · US 2012/0316337 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0365792 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365792/, SHA-256 4c0ceddd9683b43f7769d18af59563c0fbee10eed91e9f886ed10cbb262c58ee
First published
Permanent addresshttps://patent.fyi/US20260365792/
Content fingerprint (SHA-256)4c0ceddd9683b43f7769d18af59563c0fbee10eed91e9f886ed10cbb262c58ee
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi