Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Liquid organic solvent swelling without gas
What ifWhat if the polymer is swollen with a volatile liquid organic solvent at atmospheric pressure with no gas impregnation?
Claim language“with said gas”
Solid polymer granules are immersed in a stirred bath of ethyl acetate at 25 °C and 1 bar until the solvent softens the amorphous regions and increases chain mobility. The swollen granules are transferred into a bath containing the lipophilic liquid active agent, which diffuses into the expanded polymer structure. Vacuum drying at 40 °C then removes the volatile solvent while retaining the low-volatility active agent.
1.1Supercritical fluid plasticization above critical point
What ifWhat if the gas is held in the supercritical state above its critical temperature and pressure during polymer impregnation?
Claim language“in the non-supercritical state”
A high-pressure pump compresses carbon dioxide to 120 bar inside a heated autoclave maintained at 45 °C, placing the fluid above its critical point of 31.1 °C and 73.8 bar. The dense supercritical fluid diffuses rapidly into the thermoplastic polymer, lowering its glass transition temperature and expanding intermolecular spacing. Controlled depressurization to ambient pressure prepares the expanded polymer for active agent uptake.
1.1Condensable hydrocarbon gas for polymer plasticization
What ifWhat if a condensable hydrocarbon gas such as n-butane plasticizes the polymer in place of carbon dioxide or dinitrogen?
Claim language“carbon dioxide (CO2) or dinitrogen (N2)”
An explosion-proof pressure vessel exposes polyolefin pellets to gaseous n-butane at 25 °C and 2 bar, below the vapor pressure where bulk liquefaction occurs. Because n-butane has high solubility in nonpolar hydrocarbon chains, it swells the polymer matrix at lower operating pressures than inert gases. After active agent incorporation, a heated vacuum cycle strips residual hydrocarbon gas from the loaded pellets.
1.2Sub-ambient ultrasonic incorporation below 30 °C
What ifWhat if the active agent is incorporated into the gas-impregnated polymer at a chilled temperature between 5 °C and 20 °C?
Claim language“between 30 °C and 100 °C”
The gas-plasticized polymer pellets are immersed in a jacketed cooling tank holding the lipophilic liquid active agent at 15 °C. An ultrasonic transducer operating at 40 kHz generates acoustic microstreaming at the solid-liquid boundary to accelerate diffusion into the softened polymer surface. Low-temperature operation preserves thermally labile active agents that oxidize or volatilize above 30 °C.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Agricultural pheromone dispensers formed from gas-impregnated polymer pellets
A pressurized stainless-steel autoclave holds thermoplastic elastomer pellets alongside a gas manifold supplying non-supercritical carbon dioxide at 20 bar and 25 °C for 90 minutes to swell the polymer free volume. After venting the chamber at a controlled rate of 2 bar per minute, a heated rotary tumbler transfers the swollen pellets into a sealed mixing drum containing a liquid insect sex pheromone formulation maintained at 55 °C. The liquid pheromone diffuses into the expanded amorphous regions of the polymer over 4 hours before cooling to 20 °C locks the volatile compound inside the matrix. Field applicators distribute the loaded pellets across orchard rows, where gradual diffusion through the polymer walls releases the pheromone over 90 days to disrupt pest mating.
Self-lubricating polymer bearings loaded with synthetic ester oils
Molded acetal homopolymer bearing bushings sit inside a batch pressure vessel charged with non-supercritical dinitrogen at 30 bar and 20 °C for 3 hours to expand the intermolecular spacing in the amorphous phase. After controlled venting, an automated basket transfers the bushings into a nitrogen-blanketed oil bath containing a synthetic polyol ester lubricant heated to 80 °C for 5 hours. The low-viscosity ester oil permeates the gas-expanded subsurface layer to a depth of 400 micrometers, after which ambient air cooling contracts the polymer chains around the trapped lubricant droplets. During mechanical rotation against a steel shaft, frictional heating drives slow exudation of the embedded oil to the sliding interface without an external lubrication supply.
Component substitution
Argon and nitrous oxide as non-supercritical swelling gases
A high-pressure gas blending manifold replaces pure carbon dioxide or dinitrogen with a binary mixture of 70 mol% nitrous oxide and 30 mol% argon held in the subcritical gas phase at 18 bar and 22 °C. Because nitrous oxide exhibits higher solubility in polar acrylic and polycarbonate thermoplastics than dinitrogen while argon regulates total chamber pressure without reacting with hydrolytically sensitive chains, the gas blend plasticizes the polymer glass transition temperature uniformly. Once gas saturation reaches equilibrium after 60 minutes, the vessel depressurizes to atmospheric pressure and a heated jacket raises the polymer bed to 65 °C while a metering pump injects a lipophilic ultraviolet light stabilizer. The stabilizer penetrates the temporarily plasticized polymer chains, and subsequent vacuum degassing removes residual dissolved argon and nitrous oxide to yield a stabilized thermoplastic resin.
Parameter or scale variation
Multi-stage cyclic pressurization for thick extruded polymer sheets
A 500-liter horizontal autoclave accommodates stacked 6 mm thick thermoplastic sheets separated by perforated metal spacers to maintain gas contact across both faces. Instead of a single static soak, a programmable pressure controller cycles carbon dioxide between 8 bar and 32 bar at 12 °C over four 45-minute pulses with 10-minute intermediate holds to drive gas deeper into the core of the thick cross-sections. Following the final depressurization, a conveyor moves the sheets into an oil-heated immersion bath containing a lipophilic antimicrobial agent held at 85 °C for 6 hours. Cooling rollers press the exiting sheets at 18 °C to consolidate the surface skin and achieve uniform active loading across the full 6 mm thickness.
Combination with existing systems
Inline gas impregnation chamber coupled to twin-screw extrusion
A continuous lock-hopper gas impregnation column sits directly upstream of a gravimetric feeder mounted on the feed throat of a co-rotating twin-screw extruder. Polymer pellets enter the pressurized vertical column at 25 bar and 28 °C under a countercurrent flow of non-supercritical carbon dioxide before exiting through a rotary airlock into a heated pre-conditioning hopper at 70 °C. A heated positive-displacement pump sprays a metered stream of lipophilic liquid flame retardant onto the gas-swollen pellets inside the pre-conditioning hopper immediately prior to entry into the extruder barrel. The extruder screws homogenize the impregnated pellets at low shear and 95 °C, then discharge the loaded polymer through a strand die and water-cooled pelletizer for downstream injection molding.
Automated or data-driven variant
Closed-loop spectroscopic monitoring of gas sorption and loading
An inline near-infrared reflectance probe and a quartz crystal microbalance sensor sit inside the impregnation vessel and the heated incorporation drum, streaming real-time spectra and mass uptake readings to a programmable logic controller. A regression model trained on historical sorption curves calculates the instantaneous dissolved gas concentration and polymer swelling state from the spectral shift of the carbon dioxide absorption band. When the predicted swelling reaches a target setpoint, the controller triggers automated depressurization valves, activates the thermal oil circulator to reach the target incorporation temperature between 40 °C and 90 °C, and adjusts the liquid dosing pump rate. Continuous feedback from the near-infrared probe terminates the incorporation stage as soon as the active agent absorption peak plateaus, reducing cycle time and batch-to-batch concentration variance.
Specific version of a part
Subcritical carbon dioxide in jacketed autoclave
A stainless-steel batch autoclave fitted with an external glycol cooling jacket holds the polymer pellets at 25 °C while a piston compressor feeds gaseous carbon dioxide to 25 bar. A back-pressure regulator and platinum resistance thermometer hold pressure within 0.5 bar and temperature within 1 °C for a 90-minute soak. This subcritical regime keeps carbon dioxide in the gaseous phase below its critical temperature of 31.1 °C and critical pressure of 73.8 bar.
Pressurized dinitrogen impregnation in fluidized bed
A vertical pressure column with a sintered metal distributor plate circulates dinitrogen gas upward through a bed of fine thermoplastic powder at 20 °C and 30 bar. Continuous gas circulation prevents particle agglomeration and exposes the full surface area of each grain to the pressurized gas for 60 minutes. A closed-loop gas blower and heat exchanger recycle the dinitrogen while removing compression heat to keep the bed below 40 °C.
Heated tumbling drum with spray nozzles
Gas-impregnated polymer pellets are transferred into a heated rotary tumbling drum maintained at 65 °C by an electric band heater. Atomizing spray nozzles meter the lipophilic liquid active agent onto the cascading pellet bed over 20 minutes while the drum rotates at 15 revolutions per minute. Tumbling continues for an additional 40 minutes at 65 °C until surface liquid absorbs completely into the polymer interior, yielding dry, free-flowing loaded pellets.
Cite aspatent.fyi, US 2026/0365800 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365800/, SHA-256 e2eca99c36e2d0fd4cbeece3bac1c04dca8bc591f61301e34fb9a2cb72ac4498