Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
What ifWhat if the dianhydride component consists entirely of 3,3′,4,4′-biphenyltetracarboxylic dianhydride with no pyromellitic dianhydride?
Claim language“pyromellitic dianhydride (PMDA)”
Equimolar 3,3′,4,4′-biphenyltetracarboxylic dianhydride reacts with aromatic diamines in N,N-dimethylacetamide at 15 to 25 °C to form a high-molecular-weight polyamic acid precursor. Casting onto a stainless steel belt followed by thermal imidization up to 420 °C produces densely packed polymer chains stabilized by biphenyl ring stacking. The biphenyl linkage provides high chain rigidity and low in-plane thermal expansion without the rapid hydrolysis sensitivity of pyromellitic dianhydride.
1.1Phenylenediamine and bisaminophenoxybenzene diamine pair
What ifWhat if the diamine monomer consists of p-phenylenediamine and 1,4-bis(4-aminophenoxy)benzene with no 4,4′-diaminodiphenyl ether or m-tolidine?
Claim language“4,4′-diaminodiphenyl ether (ODA) and m-tolidine (m-TD)”
Rigid p-phenylenediamine units supply linear rod-like segments that raise tensile modulus and suppress thermal expansion along the film plane. Flexible 1,4-bis(4-aminophenoxy)benzene comonomer units introduce two ether linkages per repeat unit to preserve elongation and fold endurance during curing. Adjusting the molar ratio between 70:30 and 85:15 balances film toughness and dimensional stability across the 50 to 200 °C range.
1.1Multilayer laminate of homopolyimide films
What ifWhat if the film is a multilayer laminate of distinct homopolyimide layers?
Claim language“a copolymer”
A core layer of rigid biphenyltetracarboxylic dianhydride and p-phenylenediamine homopolyimide provides high stiffness and low thermal expansion. Outer skin layers of pyromellitic dianhydride and 4,4′-diaminodiphenyl ether homopolyimide are co-cast through a multilayer slot die onto the core polyamic acid gel. Simultaneous thermal imidization up to 400 °C fuses the interfaces into an integral film with composite mechanical strength and ductile surfaces.
1.2Copper-matched transverse thermal expansion
What ifWhat if the film has a transverse coefficient of thermal expansion between 15 and 20 ppm/°C to match copper foil?
Claim language“of −5 to 2.5 ppm/°C”
Increasing the molar fraction of flexible ether-linked diamines and reducing transverse tenter stretching during thermal curing lowers in-plane molecular orientation along the transverse axis. The resulting isotropic chain packing produces a transverse thermal expansion coefficient of 16 to 18 ppm/°C from 50 to 200 °C. During direct lamination with rolled copper foil at 300 °C, matched thermal contraction reduces curl and residual shear stress at the metal-polymer interface.
1.3Low-modulus compliant film for flexing
What ifWhat if the film has a tensile modulus between 2.5 and 4.5 GPa for dynamic folding applications?
Claim language“a modulus of 8 GPa or more”
Incorporating bent meta-linked diamines and flexible dianhydrides containing hexafluoroisopropylidene or oxydiphthalic linkages interrupts tight chain packing and lowers tensile stiffness. The resulting amorphous film exhibits a tensile modulus of 3.0 to 4.0 GPa and an elongation at break above 60 percent. Under repeated bending to a 1 mm radius, the lower modulus reduces outer-fiber tensile strain and lowers crack initiation.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Component substitution
Biphenyl tetracarboxylic dianhydride substitution in the copolymer backbone
A polyimide film replaces a portion of the pyromellitic dianhydride with 3,3',4,4'-biphenyltetracarboxylic dianhydride at a molar ratio of 20 to 50 percent of the total dianhydride content. The dianhydride mixture polymerizes with 4,4'-diaminodiphenyl ether and m-tolidine in N,N-dimethylacetamide at 15 to 25 °C to form a polyamic acid solution with a solid content of 15 to 20 weight percent. The solution casts onto an endless stainless steel belt, undergoes chemical imidization with acetic anhydride and isoquinoline, and cures in a tenter oven up to 450 °C while stretching in the transverse direction. The rigid biphenyl segments maintain an elastic modulus above 8 GPa while reducing moisture uptake and adjusting the transverse coefficient of thermal expansion within the -5 to 2.5 ppm/°C range.
Parameter or scale variation
Ultrathin film casting with elevated curing temperatures
The polyamic acid varnish derived from pyromellitic dianhydride, 4,4'-diaminodiphenyl ether, and m-tolidine is diluted to 8 to 12 weight percent solids in N-methyl-2-pyrrolidone and filtered through a 1-micrometer membrane filter. A slot-die coater deposits the solution onto a polished metal carrier at a wet thickness of 35 to 60 micrometers, yielding a finished dry film thickness between 4 and 8 micrometers. The cast gel film enters a multi-zone thermal imidization oven with zone temperatures stepping from 120 °C to a peak cure temperature of 480 to 510 °C over a residence time of 3 to 5 minutes under a transverse draw ratio of 1.15 to 1.30. This thin-gauge processing aligns polymer chains in the plane of the film, producing a tensile modulus of 10 to 13 GPa and a transverse coefficient of thermal expansion between -4 and 0 ppm/°C.
Combination with existing systems
Sputtered copper cladding for flexible printed circuits
The PMDA-ODA-m-TD polyimide film serves as the dielectric core in an adhesiveless flexible copper-clad laminate. Both surfaces of the film undergo argon-oxygen plasma etching to increase surface roughness and introduce polar functional groups before entering a roll-to-roll vacuum sputtering chamber. A 15-nanometer nickel-chromium tie layer and a 200-nanometer copper seed layer deposit sequentially onto the plasma-treated surfaces, followed by electroplating in an acid copper sulfate bath to build conductive copper layers of 9 to 18 micrometers. The low transverse thermal expansion and high modulus of the polyimide core limit dimensional distortion and warpage during photolithographic patterning and solder reflow at 260 °C.
Other field of use
Cryogenic multilayer insulation blankets for spacecraft thermal control
The low-expansion PMDA-ODA-m-TD polyimide film forms the reflective barrier sheets inside a vacuum multilayer insulation blanket for orbital spacecraft and cryogenic propellant tanks. A vacuum thermal evaporator deposits a 50-nanometer aluminum coating onto one or both sides of the film to provide low infrared emissivity. Ten to twenty metallized sheets stack alternately with spunbonded polyester net spacers, and edge-perforated vent holes allow trapped gas to evacuate during ascent. The high tensile modulus resists tearing during acoustic launch loads, while the near-zero transverse thermal expansion minimizes wrinkling across thermal cycles from -180 °C to 200 °C.
Flexible thin-film photovoltaic cell substrate web
The PMDA-ODA-m-TD polyimide film operates as a lightweight roll-to-roll substrate for thin-film copper indium gallium selenide photovoltaic modules. A sputtered molybdenum back-contact layer of 500 nanometers deposits directly onto the polyimide film, followed by vacuum co-evaporation of the semiconductor absorber layer at substrate temperatures between 400 °C and 450 °C. A cadmium sulfide buffer layer and a transparent zinc oxide front electrode complete the cell stack before laser scribing interconnects adjacent cells monolithically. The high modulus maintains flat web tracking through vacuum deposition chambers, and the low transverse thermal expansion matches the inorganic back-contact and absorber layers to prevent delamination upon cooling.
Automated or data-driven variant
Closed-loop optical birefringence control during film stretching
An inline polarization-sensitive optical sensor array spans the width of the tenter oven exit to measure real-time in-plane birefringence and molecular orientation across the moving PMDA-ODA-m-TD polyimide web. A supervisory controller feeds the spatial birefringence profile, web tension load cell readings, and infrared pyrometer temperatures into a trained regression model that predicts transverse coefficient of thermal expansion and tensile modulus. When predicted values drift outside target bounds of -5 to 2.5 ppm/°C or below 8 GPa, the controller automatically adjusts tenter clip rail divergence, line speed, and zonal air-impingement heater setpoints. This closed-loop feedback maintains uniform thermomechanical properties across the full web width during continuous roll-to-roll production.
Specific version of a part
Two-stage block-like diamine addition sequence
A molar ratio of 60:40 m-tolidine to 4,4′-diaminodiphenyl ether reacts sequentially with pyromellitic dianhydride in N,N-dimethylformamide at 20 °C. Adding m-tolidine first with a slight excess of dianhydride forms rigid anhydride-terminated oligomer blocks before introducing 4,4′-diaminodiphenyl ether to extend the chains to a rotational viscosity of 250 Pa·s. Chemical imidization with acetic anhydride and isoquinoline at a 2.5:1 molar ratio to amic acid groups converts the precursor into a self-supporting gel film.
Tenter-frame transverse stretching during imidization
A partially imidized gel film containing 35 weight percent residual solvent enters a pin-tenter oven with independent lateral rails. Transverse stretching of 1.25 to 1.40 times the initial width while ramping temperature from 250 to 450 °C aligns the rigid polymer backbones along the transverse axis. The oriented chain structure yields a transverse thermal expansion coefficient of −1.5 to 1.0 ppm/°C when measured by thermomechanical analysis under a 50 mN tensile load from 50 to 200 °C at 10 °C/min.
High-temperature annealing with inorganic nanofillers
Dispersing 3 to 5 weight percent surface-treated fumed silica nanoparticles with a primary particle diameter of 15 nm into the polyamic acid solution reinforces the polymer matrix without inducing haze. Final thermal annealing at 460 °C for 90 seconds under 15 MPa biaxial tension promotes intermolecular charge-transfer complexation and dense chain packing. Tensile testing at a crosshead speed of 50 mm/min confirms a tensile modulus between 9.5 and 11.5 GPa across both in-plane directions.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a copolymer in which a dianhydride monomer including pyromellitic dianhydride (PMDA) is copolymerized with a diamine monomer including 4,4′-diaminodiphenyl ether (ODA) and m-tolidine (m-TD),
However, in the method of the present invention, dianhydrides, which are used for preparing polyamic acid, include biphenylcarboxylic dianhydride or derivatives thereof, and pyromellitic dianhydride or derivatives thereof; and diamines, which are also used for preparing the polyamic acid, include phenylenediamine or derivatives thereof, and diaminophenylether or derivatives thereof. In this case, the diaminophenylether or the derivatives thereof may be 4,4-diaminophenylether.
A · US 2009/0069532 A1 · ¶ 23
According to an aspect, there is provided a polyimide film for a flexible metal clad laminate, which is derived from a polyimide precursor composition including an acid dianhydride and a diamine, in which the acid dianhydride includes 70% by mol or more of pyromellitic dianhydride (PMDA), and the diamine includes m-tolidine and dimer diamine.
B · US 2022/0135836 A1 · ¶ 12
1.2wherein the film has a coefficient of thermal expansion in a transverse direction (TD) (CTETD) of −5 to 2.5 ppm/°C measured at a temperature range of 50 to 200 °C and a heating rate of 10 °C/min, and
As a specific example, since the polyimide film according to the present disclosure may secure a coefficient of thermal expansion of 25 ppm/K or less in a temperature range of 100 to 200° C., and the copper foil may have a coefficient of thermal expansion of around 17 ppm/K in the same temperature range, dimensional stability may be improved by reducing the difference in the coefficient of thermal expansion with the copper foil when manufacturing a flexible copper clad lamina
B · US 2022/0135836 A1 · ¶ 75
1.3a modulus of 8 GPa or more.
Disclosed herein is a polyimide film having an elongation from 50 to 150%, a tensile elastic modulus from 4 to 8 GPa, a tensile strength from 150 to 500 MPa, and a hygroscopicity of 5% or less.
A · US 2009/0069532 A1 · abstract
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The reason is that dimensional changes can occur due to thermal contraction in a cooling process after the TAB and COF manufacturing processes, in which the polyimide film is bonded in a heated state, or a sputtering process, or dimensional changes can occur due to residual stress after an etching process.
A · US 2009/0069532 A1 · ¶ 5
Related claim parts: 1.2
The present invention relates to a polyimide film, useful for a flexible circuit board, and a base film for a Chip On Film (hereinafter, COF) and Tape Automated Bonding (hereinafter, TAB), which has low hygroscopicity, high elastic modulus, and improved elongation.
A · US 2009/0069532 A1 · ¶ 1
In order to overcome this problem, the polyimide film must have low hygroscopicity.
A · US 2009/0069532 A1 · ¶ 6
However, in the case of such a material, there are problems in that the interfacial bonding force is low due to a difference in organic and inorganic characteristics, it is difficult to control the dispersibility due to a difference in specific gravity, and it is difficult to secure the dimensions due to a difference in the coefficient of thermal expansion with a metal foil.
B · US 2022/0135836 A1 · ¶ 7
Therefore, it is necessary to develop a technology capable of improving dielectric properties of pure polyimide.
B · US 2022/0135836 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365804 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365804/, SHA-256 beb1a4d39c4546c05e662fc28739cbfb08e48e9696658602874f4a60f431be7b