1.1Cellulose film from solution
A slit die feeds dissolved cellulose into a coagulation bath that regenerates the cellulose as a continuous film. Water washing removes residual processing chemicals, and drying under tension controls shrinkage.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
A slit die feeds dissolved cellulose into a coagulation bath that regenerates the cellulose as a continuous film. Water washing removes residual processing chemicals, and drying under tension controls shrinkage.
A screw extruder feeds molten polyethylene through an annular die, and internal air pressure expands the melt into a tube. A cooling air ring solidifies the tube before nip rolls flatten it for winding.
Hydrolysis of a microbial polyamide yields polyaspartate, and acidification converts the recovered salt to the acid form. Heating closes succinimide rings along the existing polymer chains as water leaves, and the resulting polymer is solution cast.
Alkaline hydrolysis opens the succinimide rings and produces water-soluble sodium polyaspartate with backbone amide bonds and pendant carboxylate groups. A release liner supports the aqueous coating during drying, and a small glycerol fraction improves flexibility in dry service.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A solution-cast polysuccinimide film covers a colored patch on a rigid backing mounted beneath a pipe joint. The film contains a water-soluble dye with a contrasting color, and a transparent cover with a drip inlet protects the patch from handling. Water entering the inlet extracts dye from the film and carries it into an adjacent absorbent strip, where the stain records a leak.
A copolymer of methyl methacrylate and N-vinylsuccinimide replaces the polysuccinimide in the film body. Free-radical solution polymerization incorporates the succinimide rings as side groups on a carbon-chain backbone. The copolymer solution is cast onto a release liner and dried, and the resulting film is peeled from the liner.
A 15 percent by mass solution of polysuccinimide in dimethylformamide feeds an adjustable casting knife over a smooth release liner. Wet gaps of 200 and 600 micrometers provide starting settings for dry films of 25 and 75 micrometers, respectively. A ventilated oven removes most of the solvent, a vacuum oven completes drying, and measured dry thickness guides adjustment of the casting gaps.
A rotary pin punch forms 0.5 millimeter holes in a dry polysuccinimide film supported by a sacrificial backing. Square grids with pitches of 2 and 4 millimeters give nominal open areas of 4.9 and 1.2 percent, respectively. The hole array provides paths for air exchange through the film, and the unperforated margins provide continuous surfaces for edge bonding.
A dry polysuccinimide film carries a pressure-sensitive acrylic adhesive on one face and a printable primer on the other. A release liner supports the adhesive during rotary die cutting, and the surrounding film is stripped from the liner after cutting. An automatic label applicator peels each label from the liner and presses the adhesive face against a paperboard carton.
A metering pump feeds polysuccinimide casting solution to a slot die above a moving release liner. A traversing optical gauge measures the dry coating after the oven, using a calibration that accounts for liner thickness. A controller averages each cross-web scan and adjusts pump speed against the thickness target while accounting for the web travel time from the die to the gauge.
A heated vacuum reactor polycondenses powdered aspartic acid and removes the water produced during chain growth and ring formation. The resulting polysuccinimide dissolves in dimethyl sulfoxide, and a doctor blade meters the solution onto a release liner for vacuum drying.
Phosphoric acid promotes thermal polycondensation of aspartic acid and formation of cyclic succinimide units. The resulting polymer is washed with water to remove residual acid, dried, and dissolved in dimethyl sulfoxide for film casting.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
One aspect of the invention relates to polymerizing aspartic acid to polysuccinimide in a supercritical fluid (SCF), such as liquid CO2 or supercritical CO2 in combination with an organic cosolvent.A · US 6,903,181 B2 · ¶ 16
Another advantage is that the succinimide moiety is not capable of a further transformation (after curing with an isocyanate) to form a hydantoin ring structure as do aspartate esters.B · US 7,307,140 B2 · ¶ 46
An empty cell means only that no passage was reproduced there.
Both have a passage for 1.1.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
The present invention relates to a process for the preparation of polysuccinimide, and derivatives; the polysuccinimide is formed in a supercritical fluid (SCF), such as liquid CO2 or supercritical CO2 in an organic cosolvent, starting with L-aspartic acid, and the derivatives are formed by a ring-opening reaction.A · US 6,903,181 B2 · ¶ 3
However, the reason that some aspartic acid residues persisted in the product polymers was that the temperatures of polymerization were too low to drive the reaction to completion, leading to inefficient processes.A · US 6,903,181 B2 · ¶ 9
The present invention relates to novel polyaspartimides, a process for preparing them from specific primary amines and maleimides and to their use as reactive components for polyisocyanates in two-component polyurethane coating compositions.B · US 7,307,140 B2 · ¶ 1
It would also be desirable to prepare an aspartate that would be less prone to hydantoin formation.B · US 7,307,140 B2 · ¶ 7
Thermal polycondensation of aspartic acid and aspartic acid precursors, such as maleic acid plus ammonia, to produce polysuccinimide, which is then converted to polyaspartate by mild alkaline hydrolysis (see scheme below), has been the subject of commercial research and development for more than two decades.C · US 7,053,170 B2 · ¶ 23
Related claim parts: 1.1
Document C: US 7,053,170 B2, published May 30, 2006. Cited for this statement only.
patent.fyi, US 2026/0365805 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365805/, SHA-256 42ebaa98462d1860311b225483aabe5123cfc12d7641fd18c6434421ffd874fa