What ifWhat if the flexible substrate is an ultra-thin aluminosilicate glass sheet with no organic polymer matrix?
Claim language“a transparent resin film”
An alkali aluminosilicate glass sheet drawn to a thickness of 30 μm to 50 μm undergoes molten potassium nitrate ion exchange to form a compressive surface stress layer. This inorganic sheet transmits over 91 percent of visible light and bends to a radius below 2 mm without plastic creasing. Surface coatings bond to hydroxyl groups on the glass through silane coupling agents.
1.2Surface densification by plasma ion implantation
What ifWhat if the second principal surface achieves scratch resistance through plasma-assisted surface cross-linking without any separate coating layer?
Claim language“a hard coat layer”
A vacuum chamber exposes the second principal surface of the polymer film to an argon and nitrogen plasma beam at accelerating voltages between 1 kV and 5 kV. Ion bombardment cleaves outer polymer chains and forms a cross-linked, carbon-rich surface skin 50 nm to 200 nm deep directly inside the substrate. This modified surface zone raises nanoindentation modulus and resists abrasion without an added coating interface.
1.3Sub-20 micrometer film on carrier laminate
What ifWhat if the transparent resin film has a thickness between 10 μm and 20 μm?
Claim language“has a thickness of 26 μm or more”
A thin polymer solution casts onto a temporary stainless steel belt and cures to a final film thickness of 15 μm to reduce bending strain during folding. A pressure-sensitive optical adhesive bonds the first principal surface to a 25 μm transparent support layer in the final display stack to maintain structural stiffness. The reduced thickness lowers total optical path length and keeps yellow index below 1.5.
1.3Single-resin cyclic olefin polymer film
What ifWhat if the transparent resin film consists of a single melt-extruded cyclic olefin polymer with no polyimide and no second blended resin?
Claim language“comprises a polyimide-based resin and a solvent-soluble resin”
Cyclic olefin polymer pellets melt at 260 °C to 290 °C and pass through a flat slot die onto mirror-finished chill rolls to form a single-phase film. The amorphous saturated hydrocarbon backbone transmits over 92 percent of visible light with low birefringence and low moisture uptake. Melt extrusion eliminates organic casting solvents and drying ovens from the film-forming line.
1.3Dual-sided hard coat layers for curl balance
What ifWhat if both the first principal surface and the second principal surface carry cured hard coat layers?
Claim language“no hard coat layer is provided on the first principal surface”
A roll-to-roll slot-die coater deposits an ultraviolet-curable urethane acrylate formulation onto both principal surfaces of the resin film in sequential passes. Matching coating thicknesses of 5 μm on each side balances curing shrinkage stress across the neutral plane and keeps the film flat. Both surfaces resist scratching during downstream lamination and display assembly.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Protective optical cover for flexible photovoltaic modules
A transparent resin film composed of a polyimide-based resin blended with a polycarbonate resin forms the outer frontsheet of a flexible thin-film solar module. A urethane-acrylate hard coat layer is disposed on the outward-facing second principal surface of the transparent resin film to resist abrasion from airborne particulates and cleaning brushes. The uncoated first principal surface has an arithmetic mean roughness Sa of 0.8 nm and bonds directly to an ethylene-vinyl acetate encapsulant layer above the photovoltaic absorber stack without interfacial light scattering. During thermal cycling between -40 °C and 85 °C, a glass transition temperature above 280 °C in the polyimide-based blend limits dimensional warping while maintaining optical transmittance above 88 percent across the visible spectrum.
Optical inspection window for microfluidic diagnostic cartridges
A 40 μm transparent resin film containing a polyimide-based resin and a solvent-soluble polysulfone resin serves as the top optical interrogation window of an injection-molded polymer microfluidic cartridge. The uncoated first principal surface with an arithmetic mean roughness Sa of 0.5 nm faces the fluid microchannels and seals against the channel walls via ultrasonic welding to minimize nonspecific protein adsorption and laminar flow disturbance. A fluoropolymer-modified polyurethane hard coat layer on the outward-facing second principal surface protects the cartridge window from scratching during automated handling in optical fluorescence readers. Low autofluorescence and chemical resistance to aqueous buffer reagents allow repeated optical absorbance measurements at 450 nm and 530 nm wavelengths without clouding.
Component substitution
Polyethersulfone resin blend with cationic epoxy hard coat
The transparent resin film consists of a colorless polyimide-based resin blended with 15 weight percent of solvent-soluble polyethersulfone resin cast from a polar aprotic solvent onto a polished stainless steel belt. A cationic-cured alicyclic epoxy hard coat layer containing 30 weight percent of 15 nm colloidal silica particles is applied to the second principal surface of the transparent resin film via slot-die coating and cured under ultraviolet radiation at 800 mJ/cm². The first principal surface remains free of any hard coat layer and retains an arithmetic mean roughness Sa of 0.6 nm from contact with the casting belt. Ring-opening polymerization of the epoxy network produces curing shrinkage below 2 percent, limiting film curl while providing a nanoindentation hardness of 0.45 GPa on the coated surface.
Parameter or scale variation
Thick substrate film with multi-pass hard coat
The transparent resin film is cast to a dry thickness of 120 μm using a solution containing 70 weight percent polyimide-based resin and 30 weight percent solvent-soluble polymethyl methacrylate resin in N,N-dimethylacetamide. Solvent evaporation proceeds through a three-zone thermal oven at 80 °C, 140 °C, and 220 °C for a total residence time of 18 minutes, producing an uncoated first principal surface with an arithmetic mean roughness Sa of 0.4 nm. A hard coat layer with a cured thickness of 65 μm is deposited onto the second principal surface in two sequential wet-on-dry passes of 32.5 μm each to relieve internal stress. The resulting laminate exhibits a flexural modulus of 4.2 GPa and supports structural span loads across transparent instrument enclosures without an underlying glass carrier.
Combination with existing systems
Integration with capacitive touch sensor and antireflection stack
The transparent resin film and hard coat assembly is laminated into a capacitive touch-display module by bonding the uncoated first principal surface to an optically clear adhesive layer of 25 μm thickness. A patterned indium tin oxide electrode array on a separate dielectric carrier sits directly beneath the optically clear adhesive, separated from the hard coat layer by the 50 μm polyimide-blend substrate. A four-layer vacuum-sputtered silicon dioxide and niobium pentoxide antireflection stack with a total thickness of 280 nm is deposited directly onto the outer surface of the hard coat layer. The smooth first principal surface with an arithmetic mean roughness Sa of 0.7 nm prevents micro-bubble trapping during vacuum lamination of the optically clear adhesive, while the antireflection stack reduces specular reflectance to below 0.5 percent at 550 nm.
Automated or data-driven variant
Closed-loop optical interferometry control during film casting
A roll-to-roll solution casting line incorporates an inline white-light interferometry profilometer positioned downstream of the peeling roller to measure the arithmetic mean roughness Sa of the uncoated first principal surface continuously across the web width. A real-time feedback controller compares the measured roughness profile against a 0.9 nm upper threshold and runs a gradient-boosted regression model trained on historical drying logs to predict surface roughening from solvent evaporation rates. When predicted Sa exceeds the threshold, the controller adjusts zone heater temperatures in 1 °C increments, modulates air-knife exhaust flow, and regulates casting-belt tension to restore surface smoothness. A second inline spectral reflectometer downstream of the ultraviolet curing chamber measures hard coat layer thickness on the second principal surface and tunes the slot-die metering pump speed to hold thickness variation within 0.5 μm.
Specific version of a part
Solution-cast optically clear resin film
A slot-die coater casts a filtered polymer solution onto a mirror-polished stainless steel endless belt inside a particle-filtered cleanroom oven. Stepwise drying from 80 °C to 220 °C removes residual solvent to below 0.5 weight percent while keeping total visible light transmittance above 88 percent and haze below 0.8 percent. Peeling the cured web at controlled tension produces a transparent resin film with two distinct principal surfaces.
A coating liquid combines multifunctional urethane acrylate oligomers, 35 weight percent surface-modified colloidal silica nanoparticles of 15 nm diameter, and a photoinitiator in methyl ethyl ketone. Wet-coating onto the second principal surface, flashing off solvent at 80 °C, and irradiating with 365 nm ultraviolet light at 600 mJ/cm² forms a 10 μm cross-linked hard coat layer. The inorganic-organic network achieves a surface indentation modulus above 6 GPa while bending around a 3 mm radius without cracking.
Fluorinated polyimide blended with acrylic polymer
A fluorinated colorless polyimide synthesized from an alicyclic dianhydride and a trifluoromethyl-substituted diamine dissolves in dimethylacetamide together with 15 weight percent of a solvent-soluble poly(methyl methacrylate) resin. Casting and thermal curing at 200 °C yield a 50 μm transparent resin film with a tensile modulus above 4.5 GPa. The acrylic component reduces phase-separated domain size and suppresses surface undulation during solvent evaporation.
Mirror-belt casting for sub-nanometer smoothness
The casting dope deposits onto a chrome-plated steel belt polished to an arithmetic mean roughness Sa of 0.4 nm so the belt-contact side replicates the mirror topography as the first principal surface. Leaving the first principal surface uncoated eliminates coating-induced orange peel and keeps its Sa at 0.6 nm and maximum height Sz below 50 nm. In a display module, this smooth first principal surface bonds directly to an optical adhesive layer without interfacial light scattering.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a transparent resin film having a first principal surface and a second principal surface; and
A film of an amorphous olefin polymer (Cyclo-Olefin-Polymer: COP) having an alicyclic structure may also be used as the light-transmitting substrate.
A · US 2013/0295390 A1 · ¶ 95
As the substrate film, any polymer film having transparency can be used.
B · US 2018/0066152 A1 · ¶ 24
1.2a hard coat layer disposed on the second principal surface of the transparent resin film,
A hard coat film including a transparent substrate and a hard coat layer formed on the surface of the transparent substrate is known as an optical layered body (see Patent Literatures 1 and 2).
A · US 2013/0295390 A1 · ¶ 3
The first hard coating composition prepared in Preparation Example 1 was coated on one surface of an optical polyimide film (100 μm) as a substrate so as to have a thickness of 5 μm after drying, dried in a 80° C. oven for 5 minutes and then irradiated with UV light of 0.5 J/cm2 in a high pressure mercury lamp to form a first hard coating layer.
B · US 2018/0066152 A1 · ¶ 91
1.3wherein: the transparent resin film has a thickness of 26 μm or more and comprises a polyimide-based resin and a solvent-soluble resin other than the polyimide-based resin, no hard coat layer is provided on the first principal surface of the transparent resin film, and an arithmetic mean roughness Sa of the first principal surface of the transparent resin film is 1 nm or less.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Both have a passage for 1.11.2.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
A hard coating film has been used for protecting the surface of various image displays including a liquid crystal display device (LCD), an electroluminescence (EL) display device, a plasma display (PD), a field emission display (FED) and the like.
B · US 2018/0066152 A1 · ¶ 3
Related claim parts: 1.11.2
Therefore, a hard coat film needs to have restorability, which is an ability to restore the surface to its original flat surface when a depression is formed on the surface of a hard coat film by pencils or the like.
A · US 2013/0295390 A1 · ¶ 6
In recent years, a hard coat film having higher hardness tends to be needed, and a hard coat film having high hardness as well as excellent restorability tends to be needed.
A · US 2013/0295390 A1 · ¶ 8
However, in the case of such a hard coating composition with high hardness, there was a problem that bending resistance and/or scratch resistance are not sufficient and curling occurs.
B · US 2018/0066152 A1 · ¶ 6
It is an object of the present invention to provide a hard coating film capable of suppressing the occurrence of curling while having excellent bending resistance and scratch resistance.
B · US 2018/0066152 A1 · ¶ 7
Cite aspatent.fyi, US 2026/0365808 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365808/, SHA-256 ae3d94990c7354c57bc01fbd12bd73c7b9aff00023bf24031b91a4056f728adf