Applications  /  US 2026/0365809
United States Patent Application Publication

US 2026/0365809 A1

Published
Nov 19, 2026
Filed
Sep 28, 2023
Earliest date on the face
Nov 4, 2022
Classification
C08J 7/06
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Amorphous oxide glass replaces crystalline structure

What ifWhat if the metal oxide is an amorphous glassy layer with no periodic crystal structure?
Claim language“a crystal structure of the metal oxide”

A sputtered amorphous alumina-silica film covers the substrate with disordered atomic positions and a dense population of dangling surface bonds. Oxygen-argon plasma treatment generates reactive hydroxyl groups across the disordered oxide surface. During hot pressing at 370 degrees Celsius, polar ketone groups along the polymer chains form hydrogen bonds and acid-base interactions with the amorphous surface without lattice periodicity.

1.1Organosilane coupling bridges wide spacing mismatch

What ifWhat if the relative difference between the benzene ring spacing and the metal atom spacing exceeds 15%?
Claim language“is 5% or less”

A bifunctional organosilane primer coats the metal oxide surface and hydrolyzes to form covalent metal-oxygen-silicon bonds independently of atomic spacing mismatch. The organic functional tails of the silane layer extend outward and react with plasma-oxidized polymer chains during thermal consolidation at 360 degrees Celsius. This covalent chemical bridge transfers interfacial stress across the joint without dimensional matching between polymer rings and metal atoms.

1.2Nanoporous oxide relies on mechanical infiltration

What ifWhat if the joined metal oxide plane has an atomic density below 12 atoms/nm2?
Claim language“is 17 atoms/nm2 or more”

Electrochemical anodization creates open nanopores 20 to 80 nanometers wide across the low-density oxide surface. Vacuum-assisted melt pressing at 390 degrees Celsius draws molten polyether ether ketone resin into the pore network. Upon cooling, the solidified polymer fibrils lock physically inside the oxide pores and resist peel and shear separation independently of planar atomic packing density.

1.2Intermediate tie-film separates resin from oxide

What ifWhat if an intermediate sulfonated polymer tie-film separates the polyether ether ketone resin from the metal oxide surface?
Claim language“a crystal plane joined to the polyether ether ketone resin”

A 15-micrometer film of sulfonated polyethersulfone sits between the polyether ether ketone resin and the metal oxide during hot pressing at 370 degrees Celsius. Polar sulfonic acid groups in the tie-film coordinate with metal cations on the oxide surface while the aromatic polymer backbone interdiffuses with the molten polyether ether ketone resin. This dual-interface transition layer bonds the two materials without direct contact between the resin and any metal oxide crystal plane.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

High-voltage power semiconductor insulating substrate assembly

A power electronics module uses a joined body of a polyether ether ketone resin layer bonded to a sintered polycrystalline metal oxide ceramic plate with oriented surface grains. The metal oxide crystal plane presents an atomic density of 17 atoms/nm2 or more and a metal-to-metal interatomic spacing within 5% of the benzene ring spacing along the polymer chain. Copper metallization traces adhere to the outer face of the resin layer while the opposite face of the ceramic plate mounts onto an aluminum liquid-cooled heat sink. During high-voltage switching, the matched interface transfers heat from semiconductor dies into the heat sink while maintaining dielectric isolation and resisting thermal-cycling delamination.

Component substitution

Polyether ketone ketone resin bonded to zirconia

A joined body substitutes a polyether ketone ketone resin for polyether ether ketone and pairs it with a yttria-stabilized tetragonal zirconia ceramic substrate. The zirconia substrate exposes a polished (101) crystal plane whose zirconium interatomic spacing matches the phenylene ring repeat spacing of the polyether ketone ketone chain within 5% and provides a surface atomic density above 17 atoms/nm2. Compression molding at 380 degrees Celsius and 10 MPa presses molten polyether ketone ketone onto the heated zirconia face, followed by controlled cooling at 5 degrees Celsius per minute to promote interfacial chain alignment. The higher glass transition temperature and keto-to-ether ratio of the substituted polymer raise the continuous operating temperature of the bonded joint while preserving high interfacial shear strength.

Crystalline zinc oxide interlayer on aluminum alloy

A structural laminate replaces a bulk ceramic oxide with a c-axis oriented wurtzite zinc oxide film deposited onto a grit-blasted aluminum alloy plate by radio-frequency magnetron sputtering. Sputtering parameters align the zinc oxide (002) crystal plane parallel to the surface, yielding a surface atomic density exceeding 17 atoms/nm2 and an interatomic spacing matched within 5% to the benzene ring interval of polyether ether ketone. An injection-molded polyether ether ketone layer fuses directly onto the sputtered zinc oxide coating at a melt temperature of 390 degrees Celsius and a mold surface temperature of 190 degrees Celsius. The thin oxide film acts as a lattice-matched adhesion bridge between the polymer and the metallic base, forming a lightweight metal-polymer hybrid component.

Parameter or scale variation

Sub-micron multilayer laminate with controlled interface spacing

A multilayer composite stacks 20 alternating polyether ether ketone films of 400 nm thickness and oriented metal oxide layers of 100 nm thickness to form a total laminate thickness of 10 micrometers. Each oxide layer is textured to achieve a surface atomic density between 22 and 28 atoms/nm2 and a relative interatomic distance difference between 0.5% and 2.5% with respect to the polymer benzene ring spacing. Vacuum hot pressing consolidates the stack at 375 degrees Celsius under a uniaxial pressure of 12 MPa for 15 minutes, followed by annealing at 260 degrees Celsius for 2 hours to reach 35% polymer crystallinity. Reducing individual layer thicknesses to the sub-micron scale multiplies total interfacial area per unit volume and raises flexural modulus and barrier resistance against gas permeation.

Combination with existing systems

Fused filament additive manufacturing with laser texturing

A hybrid additive manufacturing cell combines a heated-chamber fused filament printer with an integrated nanosecond pulsed laser and a six-axis robotic worktable. The laser scans a ceramic oxide insert clamped on the build plate to remove contaminants and recrystallize a surface zone exposing crystal planes with atomic density above 17 atoms/nm2 and interatomic spacing within 5% of polyether ether ketone benzene ring spacing. Immediately after laser conditioning, a heated extrusion nozzle operating at 410 degrees Celsius deposits continuous polyether ether ketone bead tracks directly onto the prepared oxide surface inside a 180 degrees Celsius build chamber. A heated compaction roller trailing the extrusion nozzle applies localized downward force to consolidate the molten polymer onto the crystal plane and build three-dimensional net-shape hybrid structures.

Automated or data-driven variant

Closed-loop crystal orientation inspection and bonding controller

An automated bonding line integrates a grazing-incidence X-ray diffraction sensor, an infrared thermography camera, and a programmable logic controller running a trained gradient-boosted regression model. Before polymer joining, the diffraction sensor maps the dominant crystal planes on each metal oxide substrate and computes the local metal-atom spacing and surface atomic density across a grid of measurement points. The regression model compares the measured lattice spacing against the benzene ring spacing of the incoming polyether ether ketone resin batch and outputs target press temperatures, dwell times, and cooling ramps for each zone of a segmented platen press. During consolidation, the infrared camera feeds real-time interface temperatures back to the controller, which adjusts heater power and hydraulic pressure to keep polymer chain alignment within specified tolerances.

Specific version of a part

Corundum alumina matched to aromatic spacing

A sintered alpha-alumina substrate is polished and thermally annealed at 1200 degrees Celsius to expose a flat crystalline surface with an inter-aluminum spacing of 0.476 nanometers. Polyether ether ketone resin having a 0.495-nanometer spacing between benzene rings along the polymer backbone is melt-pressed onto the alumina at 380 degrees Celsius, yielding a relative spacing difference of 3.8%. Slow cooling aligns the aromatic ring segments in register with the aluminum lattice positions.

Epitaxial rutile titania film on titanium

Reactive magnetron sputtering deposits a crystalline rutile titanium dioxide layer onto a titanium substrate at 450 degrees Celsius with a metal-atom spacing of 0.459 nanometers along the exposed face. Uniaxially oriented polyether ether ketone film with an inter-ring spacing of 0.478 nanometers is laminated against the titania layer at 370 degrees Celsius under 4 megapascals, maintaining a relative spacing difference of 4.0%. Annealing at 250 degrees Celsius for 30 minutes stabilizes the aligned crystalline interphase.

Close-packed basal plane of alpha-alumina

A textured alpha-alumina plate undergoes chemical-mechanical polishing to expose the close-packed (0001) basal plane with an atomic density above 20 atoms/nm2. Ultraviolet-ozone cleaning removes adsorbed hydrocarbons from the exposed plane while preserving surface crystallinity. Hot-pressing polyether ether ketone resin onto the cleaned basal plane at 385 degrees Celsius establishes dense contact between polymer carbonyl groups and closely packed surface atoms.

Cite aspatent.fyi, US 2026/0365809 A1, claim 1, first published 2026-11-23T16:39:40-05:00, https://patent.fyi/US20260365809/, SHA-256 5dabcab12cfa3c5486659669838337341360e9bc3ad60b58949bbf309fb7ebf5
First published
Permanent addresshttps://patent.fyi/US20260365809/
Content fingerprint (SHA-256)5dabcab12cfa3c5486659669838337341360e9bc3ad60b58949bbf309fb7ebf5