1.1Dissolution in a hydrocarbon
Toluene dissolves shredded polystyrene under agitation at room temperature. A stainless steel screen removes insoluble debris before the solution enters the blending step.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Toluene dissolves shredded polystyrene under agitation at room temperature. A stainless steel screen removes insoluble debris before the solution enters the blending step.
A twin-screw extruder softens shredded polystyrene at 180 to 200 °C and disperses polycaprolactone through the melt. A flat die shapes the blend into a sheet that solidifies on chill rolls.
The polystyrene solution dries on a release liner to form a solid film. A corona discharge treats the film surface, and a heated roll nip bonds a separately formed polycaprolactone film to it at 65 to 75 °C.
Two metering pumps feed a dual-slot die with separate solutions of polystyrene and polycaprolactone in tetrahydrofuran. The die deposits the liquids as superposed layers on a moving release liner, and solvent removal solidifies the layers into a composite film.
A gear pump meters the solution through the die onto a smooth, rimless stainless steel belt. The coating dries as the belt travels through a ventilated enclosure, and a take-up roll collects the solid film.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Methyl ethyl ketone serves as the volatile solvent for chopped waste polystyrene. A covered stirred vessel dissolves the polymer before metered addition of oleic acid and continued mixing. A doctor blade spreads the mixture on a release liner, and an enclosed dryer removes the solvent to form a composite film.
Castor oil supplies the vegetable oil fraction in the composite. A covered stirred vessel dissolves waste polystyrene in toluene, then mixes in castor oil at 5 parts by mass per 100 parts of dry polymer. A casting blade spreads the mixture on a glass plate, and a ventilated drying enclosure removes the solvent before the film is peeled.
A stirred vessel holds a casting mixture with 10 mass percent waste polystyrene and 1 mass percent oleic acid in toluene. A casting blade set to gaps of 250 and 500 micrometers spreads aliquots of the same mixture on separate level glass plates. The plates dry at 23 degrees Celsius in a ventilated solvent enclosure until successive mass readings taken 30 minutes apart differ by less than 0.5 percent of the film mass.
A stirred feed tank holds waste polystyrene dissolved in toluene and blended with oleic acid. A metering pump supplies the mixture to a slot die that coats a moving silicone-coated release liner. The liner passes through an enclosed multizone dryer connected to a solvent recovery system. A peel roll separates the dry film from the liner, and a take-up roll winds the film.
A controller uses load cells to meter toluene and waste polystyrene into a covered mixing vessel. An optical transmission cell on a recirculation loop tracks polymer dissolution, and the controller starts the oleic acid dosing pump when transmission reaches a recipe threshold calibrated for the feedstock. After dosing, the controller tracks inline viscosity at a fixed temperature and opens the transfer valve when the reading stays within the recipe band for two minutes. The valve feeds a casting tray inside an enclosed dryer that removes the solvent.
Shredded waste polystyrene enters tetrahydrofuran at a loading of 5 to 10 percent by mass. A covered vessel and a paddle stirrer maintain agitation at room temperature until the polymer dissolves.
A syringe pump introduces liquid oleic acid below the surface of the polystyrene solution. The pump delivers 5 grams of oleic acid per 100 grams of dissolved polystyrene.
A 35 mm pitched-blade impeller circulates a 250 mL batch in a covered vessel at 300 revolutions per minute for 10 minutes. The inclined blades drive axial flow that distributes oleic acid throughout the polystyrene solution.
A level glass tray holds a 0.5 mm wet layer of the composite solution while toluene evaporates at 25 °C under controlled exhaust. After the film sets, a vacuum chamber at 40 °C removes residual toluene until the film reaches constant mass.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
In the recycling method of the present disclosure, the waste polystyrene is subjected to the first swelling and dissolving in water at 140° C. to 300° C.A · US 2024/0084092 A1 · ¶ 18
In the present disclosure, after obtaining the polystyrene solution, the polystyrene solution and a first surfactant is subjected to first mixing to obtain a first mixed material. In some embodiments, the first surfactant includes one or more selected from the group consisting of PVP, AES, a stearate, sodium palmitate, an oleate, an alkyl cellulose, CTAB, gelatin, SDBS, SDS, sodium polyacrylate, and a disproportionated rosinate.A · US 2024/0084092 A1 · ¶ 24
A rubber composition for tires, comprising a rubber component and a vegetable oil wherein the vegetable oil contains palmitic acid and oleic acid in a mass ratio ((palmitic acid)/(oleic acid)) of 0.65 or more and 1.2 or less.B · US 2024/0140139 A1 · abstract
In the present disclosure, after obtaining the polystyrene solution, the polystyrene solution and a first surfactant is subjected to first mixing to obtain a first mixed material.A · US 2024/0084092 A1 · ¶ 24
A method for blending the above components is not limited, and any one of the following methods may be used: a method in which components to be blended other than vulcanization-type compounding agents such as a vulcanizing agent and a vulcanization accelerator are previously kneaded to prepare a master batch, the remaining components are added to the master batch, and the resultant is further kneaded, a method in which components are added in any order and kneaded, and a methB · US 2024/0140139 A1 · ¶ 36
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.1. Both have a passage for 1.2 1.3.
Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Most of these organic solvents have strong toxicity, high cost, strong odor, and low recovery efficiency, thus limiting the application thereof.A · US 2024/0084092 A1 · ¶ 5
The recycling method according to the present disclosure does not use organic solvents, which avoids problems of toxicity, peculiar smell, and high cost in the organic solvent method.A · US 2024/0084092 A1 · ¶ 6
As a response to global environmental problems, it is desirable that sustainable raw materials are used also for a rubber composition for tires.B · US 2024/0140139 A1 · ¶ 2
Therefore, it is always desirable to provide a new method for recycling waste polymer resin packing materials, particularly the solid polystyrene packing materials, while overcome the problems existed in conventional recycling technologies.C · US 7,563,829 B2 · ¶ 7
Related claim parts: 1.1
Document C: US 7,563,829 B2, published Jul 21, 2009. Cited for this statement only.
patent.fyi, US 2026/0365813 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365813/, SHA-256 10464a03174bb88aeca6c2dab8f68796416cee8845b11b1613daf95e14ce9e49