1.1Short chain glycol feed
Diethylene glycol has two hydroxyl groups and a molar mass of 106.1 g/mol. It reacts with urethane linkages in shredded polyurethane in a stirred vessel with an acetate catalyst, releasing polyol fragments.
Generated automatically. Not reviewed by a person. Not legal advice or an opinion.
Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
Diethylene glycol has two hydroxyl groups and a molar mass of 106.1 g/mol. It reacts with urethane linkages in shredded polyurethane in a stirred vessel with an acetate catalyst, releasing polyol fragments.
A stirred vessel holds finely shredded polyurethane in hot glycol at about 220 °C under nitrogen. The excess glycol supplies hydroxyl groups that cleave urethane linkages, and the hot hold continues until the insoluble polyurethane fraction reaches the batch endpoint.
An agitated pressure vessel heats a glycol-rich slurry of shredded polyurethane to 230 °C. The closed vessel retains volatile constituents during the hot hold, and a heat exchanger cools the outlet stream before phase separation.
A jacketed vessel agitates shredded polyurethane, excess glycol, and an acetate catalyst at 170 °C for five hours. The extended hold gives the glycol more time to react with urethane linkages at the lower end of the temperature range.
A settling vessel separates a polyol-rich layer from a glycol-rich layer that also carries soluble reaction by-products. The decanted polyol-rich liquid passes through a granular activated carbon bed to reduce residual color bodies.
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
A furniture cushion plant shreds flexible polyurethane foam from dismantled mattresses after removing fabric, metal, and adhesive-rich sections. A stirred reactor treats the foam with a catalyst and a molar excess of a long-chain glycol selected to be denser than the recovered polyol. A separator collects the polyol-rich, glycol-rich, and waste phases in separate receivers. The plant measures the recovered polyol's hydroxyl number and water content and uses those values to formulate flexible polyurethane seat cushions.
Propylene glycol with a molecular weight of 76.1 g/mol replaces the long-chain glycol in a stirred, jacketed reactor fitted with a reflux condenser. The reactor treats shredded flexible polyurethane foam with a glycolysis catalyst and a molar excess of propylene glycol at 185 °C for 120 minutes. After the reaction, a water wash transfers residual propylene glycol into an aqueous phase, and a three-phase decanter discharges the aqueous phase, the polyol-rich phase, and insoluble residue separately. A vacuum dryer removes water from the recovered polyol before it enters a polyurethane formulation.
Three jacketed, stirred reactors operate in series at 190 °C with a working volume of 60 L per reactor and a combined feed rate of 90 L/h at reactor conditions. A screw feeder delivers shredded polyurethane to the first reactor, where it joins a metered feed of catalyst and long-chain glycol in molar excess. The liquid level controls maintain a nominal total residence time of 120 minutes, and the third reactor discharges into a three-phase separator. Separate outlets collect the polyol-rich, glycol-rich, and waste phases, and the recovered polyol feeds a second polyurethane process.
A wiped film evaporator receives the recovered polyol phase downstream of a three-phase separator. A feed pump delivers the polyol to a heated vertical wall, where a rotor spreads it into a thin film under vacuum. A condenser collects water and light volatile compounds from the vapor outlet, and a bottom pump transfers the treated polyol to a blend tank. The measured hydroxyl number and water content of the treated polyol enter the formulation calculation for the second polyurethane.
A vacuum-vented twin-screw extruder receives shredded flexible polyurethane foam and a metered portion of the glycol charge. The screws compress and wet the foam, and a vacuum vent removes entrained air and moisture before the resulting paste enters a stirred reactor. The reactor receives the remaining glycol and the catalyst through separate metering pumps and holds the mixture at 190 °C for 120 minutes. A three-phase separator collects the recovered polyol for use in a second polyurethane formulation.
A gravity separator incorporates a vertical array of capacitance probes across its separation zone and dedicated outlets for the polyol-rich, glycol-rich, and waste phases. A controller uses probe readings calibrated against samples of the three phases to locate the two interfaces. The controller adjusts the glycol-rich and waste outlet valves to hold the interfaces within set bands and adjusts the polyol outlet valve to hold the total liquid level. A three-way valve diverts the polyol stream to a rework tank when an interface moves into the polyol draw zone.
An agitated tank contacts shredded polyurethane with a molar excess of polyethylene glycol with a number-average molar mass of about 400 g/mol. Potassium acetate promotes exchange between glycol hydroxyl groups and urethane linkages.
A jacketed stirred reactor holds the mixture at 195 °C for 90 minutes after the bulk liquid reaches the setpoint. An immersed temperature probe controls the jacket heat input while the impeller keeps the feed dispersed.
A temperature-controlled gravity settler holds the recycled mixture until the polyol-rich, glycol-rich, and waste-rich phases form distinct layers. A top draw and lower side draw collect the two liquid product streams, and a bottom drain removes the waste layer.
The dried recovered polyol supplies 10 percent by mass of the polyol blend for a rigid polyurethane foam. The formulation uses the blend’s measured hydroxyl number and water content to set the isocyanate charge.
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
The chemolysis, and more particularly glycolysis, may be understood essentially as an equilibration of the urethane, urea and isocyanurate bonds of the polyurethane material with glycols, such as propylene glycol, diethylene glycol and dipropylene glycol, in the presence of catalyst, such as potassium acetate and tin carboxylates, to form a liquid polyol product.B · US 8,962,704 B2 · ¶ 22
The glycolysis depolymerization is completed in a reactor at a temperature range of from about 180° C. when the process uses a high ratio of EG to polyester and the pressure of the reaction is atmospheric, to a temperature range of about 280° C. when the ratio of EG is lower and the reaction is performed at superatmospheric pressure, for a period of about one to five hours in either case.A · US 7,192,988 B2 · ¶ 30
A method of forming a polyurethane foam utilizing closed-loop recycling of polyurethane foam scrap comprising: forming a recycled polyol by subjecting polyurethane foam scrap to glycolysis; adding at least a portion of said recycled polyol to a virgin polyol to produce a polyol blend, wherein said polyol blend comprises 65-95 parts by weight of a virgin polyol, 5-25 parts by weight of said recycled polyol, and a viscosity reducer, wherein said polyol blend has a viscosity inB · US 8,962,704 B2 · claim 1
An empty cell means only that no passage was reproduced there.
Only Document A has a passage for 1.2. Only Document B has a passage for 1.1 1.4. Both are classified in CPC C08J, as is this patent.
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
However, it is known that certain types of contaminants generally present in waste PET are very difficult and expensive to remove from TA.A · US 7,192,988 B2 · ¶ 8
This process has significant advantages over methanolysis or hydrolysis primarily because the BHET may be used as a raw material in either a DMT or TA polyester production process without significant major modification of the production facility.A · US 7,192,988 B2 · ¶ 9
While use of the polyurethane foam trim waste in such foregoing manners may better protect the environment as opposed to discarding the trim waste into a landfill, it is desirable to incorporate the trim waste back into the manufacturing process from which it originated and not rely upon alternative recycling streams.B · US 8,962,704 B2 · ¶ 5
The present disclosure provides systems, methods and products to utilize trim waste and other scrap polyurethane, particularly rigid polyurethane foam, in the manufacturing process from which it originated, particularly as a reactive precursor component for the production of future polyurethane material.B · US 8,962,704 B2 · ¶ 6
patent.fyi, US 2026/0365818 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365818/, SHA-256 86bf5c24b52664099f9b7cdf6f529583af65b597f5b256e6519d80bb0383d087