patent.fyi
Applications  /  US 2026/0365821
United States Patent Application Publication

US 2026/0365821 A1

Published
Nov 19, 2026
Filed
Aug 6, 2025
Earliest date on the face
May 19, 2025
Classification
C08K 3/042
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Direct spray drying

What ifWhat if spray drying recovered the graphene oxide and rubber together as dry granules?
Claim language“adding a flocculant to flocculate the latex”

A two-fluid nozzle atomizes the stirred latex and graphene oxide dispersion into a stream of heated air. Water evaporates from the droplets, and a cyclone collects granules containing both rubber and graphene oxide.

1.1Dry filler incorporation

What ifWhat if dry graphene oxide entered the rubber during compounding after the latex was coagulated and dried?
Claim language“adding a certain amount of GO aqueous dispersion”

The latex is coagulated and dried as unfilled natural rubber. An internal mixer incorporates dry graphene oxide into the rubber under shear in several small additions before the curatives enter the compound.

1.2Cooled internal mixing

What ifWhat if a cooled internal mixer incorporated the curatives in a second mixing pass?
Claim language“using an open mill to open mill”

A water-jacketed internal mixer works the cooled compound at low rotor speed while sulfur and benzoyl peroxide enter in sequence. A stock temperature probe tracks heat buildup, and a vacuum-vented sheet extruder removes entrained air after discharge.

1.2Dicumyl peroxide cure

What ifWhat if dicumyl peroxide supplied the radicals for carbon–carbon crosslinking?
Claim language“the peroxide is benzoyl peroxide”

The mixer incorporates dicumyl peroxide on an inert mineral carrier during the cool final mixing stage. A cure rheometer sets the press cycle at a temperature that activates the peroxide and supports sulfur crosslinking.

1.2Vacuum extrusion for deaeration

What ifWhat if a vacuum-vented extruder removed entrained air from the mixed rubber?
Claim language“reducing a roller distance to reduce the thickness”

After curative mixing, a temperature-controlled screw carries the compound past a vacuum port that draws air out of the exposed rubber. A flat die sets the sheet thickness, and barrel cooling limits heat buildup before vulcanization.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Flexible skirt for grain hoppers

Natural rubber latex and aqueous graphene oxide form a coagulated masterbatch that is washed and dried before compounding. Sulfur and benzoyl peroxide are added in sequence on a cooled two-roll mill, and the compound is compression molded as a flexible skirt with a thick mounting flange and a thin contact lip. A clamp bar fastens the flange to a grain hopper so the lip flexes against a moving gate and limits grain leakage.

Component substitution

Twin screw compounding of masterbatch

A co-rotating twin-screw extruder replaces the internal mixer used for the initial dry compounding step. A crammer feeder delivers strips of dried graphene oxide and natural rubber masterbatch to the feed throat, and side feeders meter reinforcing filler and rubber additives upstream of the kneading blocks. The extruded strip cools to room temperature before a two-roll mill incorporates sulfur and benzoyl peroxide in sequence, followed by compression molding.

Vacuum belt drying of rubber crumb

A continuous vacuum belt dryer replaces the batch oven used to dry washed and dewatered graphene oxide and natural rubber crumb. A spreader distributes the crumb across a moving belt, heated platens supply heat through the belt, and a condenser collects water vapor from the vacuum line. Belt speed sets the residence time, and an outlet sample is weighed before and after additional drying to verify constant mass before compounding and sequential addition of sulfur and benzoyl peroxide.

Parameter or scale variation

Multi cavity molding of rubber pads

A heated compression mold has 16 cavities in a four-by-four array, each forming a pad 40 mm square and 3 mm thick. One weighed preform of the graphene oxide and natural rubber compound containing sulfur and benzoyl peroxide sits in each cavity, and shallow parting-line vents connect the cavity edges to flash gutters. Thermocouples in the mold near a center cavity and a corner cavity track temperature uniformity, and the closed mold holds all preforms under pressure for the compound's rheometer-based cure time.

Combination with existing systems

Masterbatch dewatering with belt filtration

A belt filter press receives the coagulated graphene oxide and natural rubber from a stirred latex flocculation vessel. The first belt drains free liquid and carries the rubber through a spray rinse, and a second belt compresses the washed rubber through a series of rollers. A scraper transfers the dewatered crumb to a dryer before internal mixing, sequential addition of sulfur and benzoyl peroxide on a two-roll mill, and mold curing.

Automated or data-driven variant

Rheometer controlled press dwell time

A moving-die rheometer measures the torque curve of a sample from each milled graphene oxide and natural rubber batch containing sulfur and benzoyl peroxide. Software calculates the time to reach 90 percent of the torque rise from minimum to maximum at the selected cure temperature and adds a heat-up allowance measured with an instrumented molding trial for the same part thickness. The press controller starts the resulting dwell timer when the mold reaches its closing pressure and opens the mold when the timer expires.

Specific version of a part

Formic acid coagulation

A metering pump adds dilute formic acid to the stirred mixture of natural rubber latex and aqueous graphene oxide dispersion until the latex coagulates. Water rinses the coagulum, squeeze rolls express retained water, and a forced-air oven dries the rubber to constant mass.

Baffled tank dispersion mixing

A jacketed tank holds natural rubber latex diluted with deionized water at 25 °C. An axial-flow impeller circulates the latex while a metering pump feeds the aqueous graphene oxide dispersion below the liquid surface, and wall baffles limit vortex formation.

Sequential curative addition

A water-cooled two-roll mill works the cooled compound into a continuous band on the front roll. Sulfur enters the rolling bank first, followed by benzoyl peroxide, with dosages set at 1.5 and 2.5 parts by mass per 100 parts natural rubber, respectively. The operator cross-cuts and folds the band between additions to distribute the curatives.

Compression molding a test sheet

A 2 mm steel cavity mold holds the conditioned rubber charge between heated hydraulic press platens. The press applies pressure while the compound cures at the selected mold temperature for a time set from a cure rheometer measurement at that temperature.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2008/0300354 A1
Published
Dec 4, 2008
Filed
May 14, 2008
Class
C08K 3/22
Document BUS 2012/0302684 A1
Published
Nov 29, 2012
Filed
May 25, 2011
Class
C08K 5/21
Claim 1
Document A
Document B
1.1step 1, adding a certain amount of deionized water to NR latex at a temperature T1, adding a certain amount of GO aqueous dispersion, mechanically stirring a mixture at a stirring speed v1 for a time t1, adding a flocculant to flocculate the latex, washing and dewatering the obtained raw rubber for many times, and drying the treated raw rubber to a constant weight at a temperature of T2 to obtain a GO/NR masterbatch;
The flocculation process comprises producing, harvesting or yielding a latex masterbatch before mixing a portion of the latex masterbatch with a coagulant and water to produce, harvest or yield raw natural rubber-based ABS powder. Subsequent process portions of flocculation include filtration and drying to produce, yield, harvest or give rise to the resultant or final product, natural rubber-based ABS powder.
B · US 2012/0302684 A1 · ¶ 22
1.2step 2, placing the GO/NR masterbatch obtained in step 1 in an internal mixer, mixing the GO/NR masterbatch at a temperature T3 for a time t2, discharging a rubber compound, and adding a rubber assistant and a reinforcing filler during this period; and cooling the discharged rubber compound to room temperature, using an open mill to open mill at a temperature T4 for a time t3, adding vulcanizing agents sulfur and peroxide in sequence during this period, after uniform mixing, reducing a roller distance to reduce the thickness until the rubber compound is free of bubbles, and obtaining a mixed rubber; wherein the peroxide is benzoyl peroxide, and a mass ratio of the NR to the sulfur to the peroxide in the GO/NR masterbatch is 100:1.5:2-3; and
A method for producing a cleaning blade, for use in an image-forming apparatus, comprising the steps of: roughly kneading a rubber component (1) containing rubber derived from acrylonitrile butadiene copolymer therein by supplying said rubber derived from acrylonitrile butadiene copolymer to a rubber-kneading apparatus; kneading said rubber component (1), a filler (2) essentially containing carbon black and zinc oxide therein, and a crosslinking agent (3) containing sulfur th
A · US 2008/0300354 A1 · claim 1
1.3step 3, placing the mixed rubber at a temperature t5 for a time t4, and vulcanizing the mixed rubber in a mold at a temperature T6 and a certain pressure P1 for a time t5, to obtain a GO/NR based on interpenetrating double crosslinked network structure constructed by dual vulcanizing agents.
The thermosetting elastomer composition obtained through the above-described steps is filled in a die and press-vulcanized at 160 to 170° C. for 20 to 40 minutes to mold the thermosetting elastomer composition into the cleaning blade 10.
A · US 2008/0300354 A1 · ¶ 118

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2 1.3. Only Document B has a passage for 1.1. Both are classified in CPC C08K, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The present invention relates to a method for producing a cleaning blade for use in an image-forming apparatus, and the cleaning blade.
A · US 2008/0300354 A1 · ¶ 3
As a result, unless the line pressure is increased, it is difficult to remove toner that remains on the surface of the photoreceptor, and the toner is liable to be removed defectively.
A · US 2008/0300354 A1 · ¶ 7
In particular, these existing methods, processes and techniques involve a number of complicated steps.
B · US 2012/0302684 A1 · ¶ 6
Furthermore, the use of polybutadiene (or any other types of synthetic rubbers) in conventional methods of producing ABS or ABS-based compositions or products has adverse effects on the environment.
B · US 2012/0302684 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0365821 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365821/, SHA-256 92023e7157ee5e2c35bc8b80ac05a47a0b0a1c370e7279cdc5186c26ee0fdd82
First published
Permanent addresshttps://patent.fyi/US20260365821/
Content fingerprint (SHA-256)92023e7157ee5e2c35bc8b80ac05a47a0b0a1c370e7279cdc5186c26ee0fdd82
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi