United States Patent Application Publication

US 2026/0365822 A1

Published
Nov 19, 2026
Filed
Jun 26, 2026
Earliest date on the face
Dec 28, 2023
Classification
C08K 3/22
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Continuous ceramic dielectric layer

What ifWhat if the dielectric material is a continuous ceramic sheet bonded between two resin films?
Claim language“dielectric particles dispersed in the matrix resin”

Heat and pressure bond a dense barium titanate sheet between two epoxy films. Copper electrodes on the outer faces establish an electric field through the three dielectric layers, and the thickness and permittivity of each layer determine the capacitance.

1.2Amorphous glass dielectric beads

What ifWhat if the dielectric particles are solid amorphous glass beads?
Claim language“an aggregate of ferroelectric particles”

Solid soda-lime glass beads with diameters of 20–40 µm are mixed into liquid epoxy and held in place by curing. The glass polarizes in an applied electric field and contributes to the permittivity of the cured composite.

1.3Micrometer scale ferroelectric particles

What ifWhat if the ferroelectric particles have diameters of 2–4 µm?
Claim language“10 nm or more and 1,000 nm or less”

Spray granulation groups the barium titanate particles into granules with diameters of 25–50 µm. Light sintering bonds neighboring particles, and the resulting granules are mixed into epoxy before curing.

1.4Larger ferroelectric granules

What ifWhat if the aggregate particles have diameters of 150–200 µm?
Claim language“1 μm or more and 100 μm or less”

Sieving selects the 150–200 µm fraction of granules made from submicrometer barium titanate particles. A viscous epoxy suspension holds the granules in a 3 mm mold cavity during cure, and the embedded granules contribute to the molded plate's permittivity.

1.5Higher dielectric filler loading

What ifWhat if the cured resin member contains 15 mass % dielectric particles?
Claim language“0.1 mass % or more and 10 mass % or less”

Barium titanate granules make up 15% of the combined mass of the granules, epoxy resin, and hardener. The mixture is deaerated under vacuum and cured in a mold, where the epoxy forms a continuous phase around the granules.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Dielectric liner for grain moisture sensing

A 50 mm by 30 mm by 2 mm epoxy liner contains 5 mass % ferroelectric ceramic aggregates. The 10–30 μm aggregates consist of 200–500 nm primary particles. Two coplanar electrodes sit against the back of the liner, and grain passes over the opposite face. An alternating voltage across the electrodes produces a fringing electric field through the liner and grain, and the readout maps measured capacitance and temperature to moisture content using a calibration for the grain type.

Component substitution

Potassium sodium niobate as the dielectric

Potassium sodium niobate replaces barium titanate as the ferroelectric ceramic in an epoxy member. Spray drying an aqueous slurry of 200–500 nm potassium sodium niobate particles produces granules, and a heat treatment creates interparticle necks that hold the granules together. Sieving after heat treatment selects 15–40 μm granules, and low-shear mixing disperses them in epoxy at 6 mass %. The mixture cures in a 40 mm by 25 mm by 2 mm mold to form a dielectric insert between electrodes.

Parameter or scale variation

Thick panel with submicrometer ceramic aggregates

A 60 mm by 40 mm by 5 mm epoxy panel contains 4 mass % ceramic aggregates with diameters of 0.4–0.8 μm. Suspension drying consolidates 50–100 nm barium titanate primary particles into clusters, and centrifugal classification selects the target cluster size. A low-shear mixer disperses the classified clusters in the epoxy, which is vacuum degassed and cured in a flat mold. Electrodes on the broad faces establish an electric field through the 5 mm thickness.

Layered panel with graded ceramic loading

A 60 mm by 40 mm by 3 mm epoxy panel contains three 1 mm layers with ceramic loadings of 1, 5, and 9 mass %. Each layer uses 10–25 μm aggregates formed from 150–400 nm ferroelectric primary particles. Successive batches are cast after the preceding layer gels, and the stack receives a common final cure. Electrodes on the outer faces place the three dielectric layers electrically in series, and the local field in each layer depends on its effective permittivity.

Combination with existing systems

Embedded capacitors in a printed circuit board

A 100 mm by 80 mm by 0.25 mm cured epoxy sheet contains 8 mass % ceramic aggregates with diameters of 5–15 μm and primary particle diameters of 100–300 nm. The sheet is cast and cured between copper foils, and the upper foil is etched into capacitor pads while the lower foil forms a common return plane. The copper-clad sheet is laminated into a multilayer printed circuit board, where vias connect separate pads to local supply nets and the return plane to ground. Each pad and the corresponding area of the return plane form a shunt capacitor through the composite sheet.

Automated or data-driven variant

Automated filler dosing and dispersion inspection

A loss-in-weight feeder meters 10–30 μm ferroelectric aggregates made from 100–300 nm primary particles into a low-shear mixer supplied by an epoxy pump. A controller adjusts feeder speed from measured mass flow to maintain 5 mass % ceramic in the total formulation. At fixed intervals, an automated sampler spreads a thin film between glass plates, and a transmitted-light camera measures the area fraction of clusters larger than 60 μm. The controller diverts material when the measured area fraction exceeds a preset limit and fills 40 mm by 30 mm by 2 mm molds when the measurement is within the limit.

Specific version of a part

Dielectric granules in epoxy

An impeller disperses barium titanate granules throughout a liquid epoxy and hardener mixture. Vacuum deaeration removes entrained air, and curing fixes the granules in the epoxy matrix.

Submicrometer barium titanate particles

Barium titanate powder is wet classified to select particles with diameters of 200–400 nm. The classified powder is suspended in water and spray dried to form granules.

Five percent granule loading

A batch combines 50 g of dielectric granules with 950 g of solvent-free epoxy resin and hardener. The granules account for 5 mass % of the cured composite.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2007/0042286 A1
Published
Feb 22, 2007
Filed
Aug 22, 2005
Class
G03G 9/08
Document BUS 2013/0329179 A1
Published
Dec 12, 2013
Filed
Dec 12, 2012
Class
C09K 19/54
Claim 1
Document A
Document B
1.1a matrix resin and dielectric particles dispersed in the matrix resin,
(ii) shearing the pigment dispersion with a latex mixture comprised of a counterionic surfactant with a charge polarity of opposite sign to that of the ionic surfactant, a nonionic surfactant, and resin particles, thereby causing a flocculation or heterocoagulation of the formed particles of pigment, resin, and charge control agent; and (iii) stirring.
A · US 2007/0042286 A1 · ¶ 15
Liquid crystal compositions may include the ferroelectric nanoparticles in combination with a liquid crystal.
B · US 2013/0329179 A1 · abstract
1.2wherein the dielectric particles are aggregate particles each of which is an aggregate of ferroelectric particles,
When the turbine is driven at a speed such as 60,000 rpm, for example, the high speed airflow within the gas turbine separates the agglomerated nanoparticles into monoparticulates through a combination of impact with the turbine blades and the housing walls.
B · US 2013/0329179 A1 · ¶ 39
1.3wherein a particle diameter of the ferroelectric particles is 10 nm or more and 1,000 nm or less,
The methods may include size-reducing a starting material comprising particles of a bulk intrinsically nonferroelectric glass to form glass nanoparticles having an average size of less than 20 nm, the glass nanoparticles comprising ferroelectric nanoparticles.
B · US 2013/0329179 A1 · ¶ 8
1.4wherein a particle diameter of the aggregate particles is 1 μm or more and 100 μm or less, and
A toner process comprising aggregating or coagulating a latex emulsion comprising a resin, a colorant and wax particles using an amount of polymetal ion coagulant to provide core particles; heating the core particles to provide micron size aggregates; optionally adding a second resin emulsion; adding a sequestering or complexing component and a base to remove the polymetal ion in a controlled manner; further heating the mixture to provide toner particles; and optionally, isol
A · US 2007/0042286 A1 · abstract
1.5wherein a contained amount of the dielectric particles is 0.1 mass % or more and 10 mass % or less.
In some embodiments, to avoid flocculation when an electric field gradient is created, the suspension or dispersion may contain a small amount of glass nanoparticles such as from about 0.05 wt. % to about 0.2 wt. %, preferably about 0.08 wt. %, based on the total weight of the suspension or dispersion.
B · US 2013/0329179 A1 · ¶ 41

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.4. Only Document B has a passage for 1.2 1.3 1.5. Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents (and from a third earlier document, Document C) that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The resulting toners can be selected for known electrophotographic imaging, digital, printing processes, including color processes, and lithography.
A · US 2007/0042286 A1 · ¶ 2
With the present processes, small average particle sizes of, for example, from about 3 microns to about 9 microns, and more specifically, about 4 to about 6 microns or about 5 microns, are attained without resorting to classification processes, and wherein narrow geometric size distributions are attained, such as from about 1.14 to about 1.30, or from about 1.14 to about 1.25.
A · US 2007/0042286 A1 · ¶ 5
Unfortunately, common production methods such as chemical precipitation and spark plasma production cannot ensure that the resulting nanoparticles have strong ferroelectric dipole moments or that the material is even ferroelectric for smaller size particles, due to the size dependence of the ferroelectric effect.
B · US 2013/0329179 A1 · ¶ 4
Thus, there remain ongoing needs for versatile ferroelectric materials that may be used in applications such as liquid-crystal media.
B · US 2013/0329179 A1 · ¶ 7
Particle agglomerates are typically not easily dispersed.
C · US 2018/0215964 A1 · ¶ 41

Related claim parts: 1.2

Document C: US 2018/0215964 A1, published Aug 2, 2018. Cited for this statement only.

Cite aspatent.fyi, US 2026/0365822 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365822/, SHA-256 594d793c0647fa4472e050610527b6512dd40687bc21f3d875fbb7ab66824c69
First published
Permanent addresshttps://patent.fyi/US20260365822/
Content fingerprint (SHA-256)594d793c0647fa4472e050610527b6512dd40687bc21f3d875fbb7ab66824c69