Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Lower elastomer share with mineral filler
What ifWhat if the thermoplastic polyurethane accounts for 55 to 70 wt. % of the total composition?
Claim language“84-97 wt. %”
Reducing the elastomer fraction leaves 30 to 45 wt. % of the formulation for hydrated mineral fillers such as magnesium hydroxide or aluminum trihydroxide. At elevated temperatures, the mineral filler undergoes endothermic dehydration between 180 and 350 °C, absorbing heat and releasing water vapor to dilute combustible gases. The remaining continuous polyurethane matrix retains flexibility for cable jacketing and extruded profiles while the dense inorganic residue forms a thermal barrier.
1.1Thermoplastic copolyester elastomer base matrix
What ifWhat if the polymer matrix is a thermoplastic copolyester elastomer with no polyurethane segments?
Claim language“a thermoplastic polyurethane”
A block copolymer of crystalline polybutylene terephthalate hard segments and amorphous polytetramethylene ether glycol soft segments provides elastic recovery and melt processability. Compounding this matrix at 210 to 230 °C with a phosphorus-nitrogen flame retardant system produces a melt-extrudable compound for flexible tubing and connectors. During thermal decomposition, the aromatic ester hard segments contribute to char formation while the additive suppresses gas-phase combustion.
1.2High loading intumescent flame retardant
What ifWhat if the flame retardant loading is 22 to 30 wt. % of the total composition?
Claim language“3-16 wt. %”
An intumescent package combining ammonium polyphosphate, pentaerythritol, and melamine at 25 wt. % total loading operates through a solid-phase charring mechanism. Upon heating above 280 °C, the acid source esterifies the carbonific polyol while the blowing agent releases non-flammable ammonia and nitrogen gases to expand the char into an insulating foam layer. This higher solid loading delivers fire resistance without relying on low-dosage liquid synergists, using twin-screw extrusion with distributive mixing elements to maintain dispersion.
1.2Chemically bound reactive phosphorus backbone
What ifWhat if the composition omits any separate flame retardant additive and incorporates flame-inhibiting groups directly into the polyurethane backbone?
Claim language“a flame retardant”
During prepolymer synthesis, a reactive phosphorus-containing diol such as a phosphine oxide diol reacts with diisocyanate and polyester polyol to form covalent bonds within the polymer chain at 1.5 to 3.0 wt. % elemental phosphorus. Because the fire-inhibiting moiety is covalently integrated into the macromolecule, the polymer resists migration, blooming, and leaching during thermal aging or solvent contact. When exposed to flame, the modified chains cleave to release phosphorus-containing radicals in the gas phase and promote crosslinked char at the burning surface.
1.3Melamine cyanurate synergist without ionic liquid
What ifWhat if the flame retardant replaces the ionic liquid with a solid melamine cyanurate synergist?
Claim language“an ionic liquid”
Solid melamine cyanurate particles dispersed at 4 to 8 wt. % work alongside the phosphorus-containing ester without introducing mobile ionic salts into the polymer matrix. At temperatures above 320 °C, melamine cyanurate sublimes endothermically and dissociates into melamine and cyanuric acid, absorbing heat and releasing inert nitrogen-rich gases. Simultaneously, the phosphorus-containing ester catalyzes dehydration of the polyurethane into a cohesive surface char that limits melt dripping.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Flame retardant polyurethane jacketing for subterranean power cables
A flame retardant thermoplastic polyurethane composition containing 88 wt. % polyether-based thermoplastic polyurethane and 12 wt. % of a combined imidazolium ionic liquid and phosphonate ester additive forms the outer protective jacket of an underground power transmission cable. During extrusion, a single-screw extruder melts the compounded pellets at 195 °C and applies a 2.5 mm concentric layer over a cross-linked polyethylene insulation core and copper conductor bundle. Under fault-induced overheating, the phosphorus-containing ester promotes char layer formation on the jacket surface while the ionic liquid catalyzes cross-linking of the decomposing polymer melt to suppress dripping and flame propagation along the cable conduit. The polyether backbone resists hydrolysis and microbial degradation in damp soil environments while maintaining flexibility at installation temperatures down to -20 °C.
Component substitution
Nitrogen-based imidazolium ionic liquid with cyclic phosphonate ester
In place of a phosphorus-based ionic liquid and aromatic phosphate esters, the flame retardant package pairs 1-butyl-3-methylimidazolium tetrafluoroborate with a cyclic pentaerythritol diphosphonate ester. The composition combines 86 wt. % polyester-based thermoplastic polyurethane with 2.0 wt. % of the imidazolium salt and 12.0 wt. % of the cyclic phosphonate ester in a twin-screw extruder operating at 185 °C and 200 rpm. Upon thermal exposure, the cyclic phosphonate ester decomposes to generate phosphoric acid derivatives that dehydrate the polyurethane chains into a swollen carbonaceous barrier. Simultaneously, the tetrafluoroborate anion and imidazolium cation release non-combustible gas-phase radical scavengers that interrupt combustion reactions in the flame zone.
Bio-based sebacic acid polyurethane with ammonium ionic liquid
A bio-derived thermoplastic polyurethane synthesized from sebacic acid polyester polyols, 1,4-butanediol, and diphenylmethane diisocyanate replaces petroleum-derived polyurethane at 90 wt. % of the total formulation. The flame retardant system uses 1.5 wt. % of a quaternary ammonium bis(trifluoromethylsulfonyl)imide ionic liquid combined with 8.5 wt. % of a reactive diol-functional phosphonate ester. Melt blending in an internal mixer at 190 °C for 8 minutes disperses the ionic liquid and grafts a portion of the reactive phosphonate ester onto residual isocyanate end groups. Covalent incorporation of the phosphorus ester reduces additive migration to the molded surface during prolonged thermal aging while preserving tensile elongation above 400 percent.
Parameter or scale variation
High-loading flame retardant formulation for thin-wall molded parts
For injection-molded enclosures with wall thicknesses between 0.4 mm and 0.8 mm, the formulation shifts to 78 wt. % thermoplastic polyurethane and 22 wt. % total flame retardant comprising 4.0 wt. % ionic liquid and 18.0 wt. % oligomeric phosphate ester. The higher additive loading compensates for the reduced thermal mass of thin-wall sections by accelerating condensed-phase char formation within the first 5 seconds of direct flame impingement. Processing requires lowering the barrel temperature profile to 170 °C to 180 °C and increasing injection pressure to 110 MPa to limit thermal degradation of the elevated ionic liquid fraction during high-shear cavity filling. Post-molding annealing at 85 °C for 4 hours relieves residual molding stress and stabilizes dimensional tolerances to within 0.05 mm across the thin-wall geometry.
A 1.2 mm extruded sheet of thermoplastic polyurethane containing 91 wt. % polymer, 1.5 wt. % ionic liquid, and 7.5 wt. % phosphorus-containing ester is thermally laminated onto a 3.0 mm woven glass fiber mat and a 0.2 mm aluminum foil heat spreader. The composite sheet is die-cut into interlocking partitions and installed between prismatic lithium-ion battery cells inside a sealed aluminum module housing. During a single-cell thermal runaway event, the aluminum foil distributes localized heat laterally while the polyurethane layer intumesces against the glass fiber scaffold to form an insulating carbonaceous barrier. The mechanical resilience of the elastomer layer simultaneously accommodates cyclic cell swelling of up to 8 percent during charge and discharge cycles without cracking the thermal barrier.
Automated or data-driven variant
Closed-loop twin-screw compounding with inline spectroscopic monitoring
A gravimetric loss-in-weight feeder system meters thermoplastic polyurethane pellets, liquid phosphorus-containing ester, and ionic liquid into a co-rotating twin-screw extruder equipped with an inline near-infrared spectroscopic probe at the die adapter. The spectroscopic probe samples the melt stream at 2 Hz and transmits absorption spectra corresponding to phosphorus-oxygen and urethane carbonyl bands to a programmable logic controller running a multivariate regression model. When the predicted flame retardant concentration deviates by more than 0.15 wt. % from the target setpoint or melt viscosity shifts outside a 5 percent tolerance band, the controller automatically adjusts liquid pump speed and screw rotational speed. Continuous feedback regulation maintains uniform additive dispersion across multi-ton production runs and logs batch composition profiles to a plant manufacturing database for quality traceability.
The base polymer constitutes 90 wt. % of the composition and consists of a linear segmented polyurethane synthesized from 4,4'-methylene diphenyl diisocyanate, 1,4-butanediol chain extender, and poly(butylene adipate) diol with a number-average molecular weight of 2000 g/mol. The polymer exhibits an elongation at break above 400 percent, a glass transition temperature near -35 °C, and a melt processing window between 185 and 205 °C. Ester soft segments provide high tensile strength and oil resistance while interacting with acidic phosphorus decomposition products to build char.
Ten weight percent twin-screw compounded package
The flame retardant package accounts for 10 wt. % of the total composition, split at a 1:4 weight ratio between the ionic liquid and the phosphorus-containing ester. Liquid and low-melting components are metered into the mid-barrel zone of a co-rotating twin-screw extruder operating at 195 °C and 250 revolutions per minute via a heated gravimetric liquid-injection pump. Downstream vacuum degassing at -0.08 MPa removes residual moisture and volatiles before underwater pelletizing.
Imidazolium hexafluorophosphate and resorcinol diphosphate
The flame retardant pairs 1-butyl-3-methylimidazolium hexafluorophosphate as the ionic liquid with oligomeric resorcinol bis(diphenyl phosphate) as the phosphorus-containing ester. During melt blending at 190 °C, the imidazolium salt acts as a compatibilizing plasticizer that lowers melt viscosity and promotes uniform dispersion of the oligomeric aryl phosphate. Upon ignition, the phosphate ester generates metaphosphoric acid to catalyze polyurethane charring while the ionic liquid decomposes to release fluorinated and nitrogenous fragments that inhibit flame propagation.
Phosphonium sulfonate and cyclic phosphonate ester
The flame retardant combines tetrabutylphosphonium methanesulfonate as the ionic liquid with a cyclic neopentyl glycol methylphosphonate ester. The phosphonium cation provides thermal stability above 300 °C, preventing premature decomposition during extrusion or injection molding of the polyurethane. Under fire exposure, the cyclic phosphonate ester delivers high phosphorus density for gas-phase radical scavenging while the sulfonate anion accelerates condensed-phase carbonization.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.184-97 wt. % of a thermoplastic polyurethane, and
More preferably, the thermoplastic polyurethane is present in an amount greater than or equal to about 50 weight percent of the total thermoplastic polyurethane-based resin component; most preferably, it is present in an amount greater than or equal to about 70 weight percent of the total thermoplastic polyurethane-based resin component.
A · US 2011/0130490 A1 · ¶ 4
A thermoplastic polyurethane elastomer particle having a Shore hardness ranging from 45D to 80D is provided.
B · US 2022/0259771 A1 · abstract
1.23-16 wt. % of a flame retardant,
The present invention is a flame-retardant polyurethane composition comprising (a) a thermoplastic polyurethane-based resin component, (b) a phosphorus flame retardant particulate filler, and (c) a low melting temperature phosphorus flame retardant agent.
A · US 2011/0130490 A1 · abstract
1.3wherein the flame retardant comprises an ionic liquid and a phosphorus-containing ester.
Other useful low melting temperature phosphorus flame retardant agents include phosphate esters such as resorcinol bis(diphenylphosphate), resorcinol dixylenyl phosphate (both oligomeric and monomeric versions), trixylenyl phosphate, triethyl phosphate, and triphenyl phosphate.
A · US 2011/0130490 A1 · ¶ 8
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.21.3. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Desired composition performance will determine the selection of the TPU.
A · US 2011/0130490 A1 · ¶ 6
Related claim parts: 1.1
There is a need for a polyurethane-based composition and articles made therefrom, where the composition provides an excellent balance of burn performance, physical properties (including excellent heat deformation and flexibility), and extrusion performance.
A · US 2011/0130490 A1 · ¶ 1
It would be readily apparent that the invented composition would be useful in other applications where flexibility and/or burn resistance are desired.
A · US 2011/0130490 A1 · ¶ 2
However, in the dry spinning process, a great amount of the solvent is required, which causes environmental concerns.
B · US 2022/0259771 A1 · ¶ 5
In addition, since a step of dissolving the polyurethane is carried out after synthesizing, physical properties of the polyurethane fiber are weakened.
B · US 2022/0259771 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0365826 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365826/, SHA-256 01e55e4a54cffe1c92441a92a2c0fe1226ca7e8bb14a682fcb5f1c595246f5d0