patent.fyi
Applications  /  US 2026/0365835
United States Patent Application Publication

US 2026/0365835 A1

Published
Nov 19, 2026
Filed
Sep 21, 2023
Earliest date on the face
Oct 5, 2022
Classification
C08L 23/0815
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Supported titanium catalyst

What ifWhat if a supported titanium chloride catalyst produces the linear low density polyethylene?
Claim language“metallocene catalyzed linear low density polyethylene”

Two gas-phase reactors in series use a magnesium chloride-supported titanium chloride catalyst activated by an alkylaluminum compound. The first reactor uses 1-butene and a higher hydrogen-to-ethylene ratio to form a higher-flow fraction, and the second uses 1-hexene and a lower hydrogen-to-ethylene ratio to form a lower-flow fraction.

1.3Ethylene octene copolymer fraction

What ifWhat if an ethylene–1-octene copolymer forms the lower-density fraction?
Claim language“the ethylene-1-hexene polymer component”

A solution reactor copolymerizes ethylene and 1-octene to target a density of 905 kg/m³ and a melt mass-flow rate of 0.2 g/10 min at 190 °C under 2.16 kg. The octene introduces six-carbon side branches that disrupt crystal packing, and the reactor uses a low hydrogen feed to retain high molecular weight.

1.4Lower melt flow ratio

What ifWhat if the multimodal polyethylene has a melt flow ratio of 30?
Claim language“35.0 to 60.0”

The reactors use a smaller difference in hydrogen feed relative to ethylene to bring the molecular weights of the two fractions closer together. The resin targets melt mass-flow rates of 0.6 and 18 g/10 min at 190 °C under loads of 2.16 and 21.6 kg, respectively.

1.6Lower density recycled feed

What ifWhat if the recycled polyethylene blend has a density of 940 kg/m³?
Claim language“950 to 970 kg/m3”

A compounder combines recycled high-density polyethylene from sorted rigid containers with recycled linear low-density polyethylene from sorted film. The compounder adjusts the feed proportions using density measurements on compounded pellets, then melt filters the blend before pelletizing it for film extrusion.

1.11Furnace ash measurement

What ifWhat if furnace ashing measures the inorganic residue?
Claim language“measured by TGA”

A dried pellet sample burns in air in a preweighed crucible at 600 °C. The crucible cools in a desiccator and undergoes repeated heating and weighing until its mass stabilizes, and the remaining ash mass is reported as a percentage of the starting sample mass.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Release film for composite layup

A cast film containing 85 wt % multimodal linear low density polyethylene and 15 wt % recycled high density polyethylene serves as a release sheet for room-temperature epoxy composite fabrication. The film lies between the release fabric and the breather cloth inside the vacuum bag. A pin roller perforates the film so air and excess resin pass into the breather cloth during consolidation. After cure, the operator lifts the breather cloth and film away before peeling off the release fabric.

Component substitution

Octene copolymer in the softer fraction

A metallocene-catalyzed ethylene–1-octene copolymer replaces the ethylene–1-hexene component. The octene copolymer has a density of 900 kg/m³ and a melt mass-flow rate of 0.10 g/10 min at 190 °C under a 2.16 kg load. A twin-screw extruder compounds equal masses of the octene and ethylene–1-butene copolymers, with the two copolymers together supplying 80 wt % of the blend and recycled high density polyethylene supplying 20 wt %. A flat die extrudes the compounded pellets onto a chilled roll to form film.

Parameter or scale variation

Three gauges from one film blend

A cast film line processes a blend of 75 wt % multimodal linear low density polyethylene and 25 wt % recycled high density polyethylene. A 500 mm flat die with a 0.6 mm lip gap feeds a chill roll held at 25 °C. At constant melt output, the operator increases the chill-roll speed to reduce film thickness from 80 to 50 and then 30 µm. A traversing thickness gauge measures each film across the web, and its mean reading guides the final speed adjustment at each gauge.

Combination with existing systems

Recycled blend core in pouch film

A three-layer blown film line places the multimodal linear low density polyethylene and recycled high density polyethylene blend in the core of a pouch web. A linear low density polyethylene layer forms the inner sealing surface, and a medium density polyethylene layer forms the outer surface. The three extruders feed a common annular die at an initial outer, core and inner thickness split of 20, 60 and 20 percent. A vertical form-fill-seal machine folds the web with the sealing surface inward and closes the longitudinal seam and pouch ends with heated jaws.

Recycled blend backing for woven sheeting

An extrusion coating line applies a blend of 85 wt % multimodal linear low density polyethylene and 15 wt % recycled high density polyethylene to woven polyethylene tape fabric. A flat die delivers the molten blend into the nip between a rubber pressure roll and a chilled steel roll, with the fabric entering on the pressure-roll side. The pressure roll presses the melt into the weave openings, and the chilled roll solidifies the exposed surface before winding. The resulting coated sheet serves as a waterproof backing for reusable equipment covers.

Automated or data-driven variant

Lot selection from pilot film measurements

A production controller stores the melt mass-flow rate at 190 °C under a 5 kg load and the inorganic residue content for each recycled polyethylene lot. A line-scan camera also records defect counts by size over 10 m² of pilot film made from each lot using a fixed base resin and recycled content. The controller checks the recorded values against the production recipe and issues eligible lot identifiers and blend setpoints to two gravimetric feeders. The feeders meter the base resin and selected recycled lot into the film extruder and record actual mass flow against the production run.

Specific version of a part

Higher flow butene fraction

A gas-phase reactor copolymerizes ethylene and 1-butene with a supported metallocene catalyst to produce a fraction with a density of 945 kg/m³. Hydrogen feed controls molecular weight to give a melt mass-flow rate of 40 g/10 min at 190 °C under 2.16 kg.

Recycled pellets with controlled flow

Recycled polyethylene pellets make up 20 wt % of the film composition and have a melt mass-flow rate of 2.0 g/10 min at 190 °C under 5.0 kg. A piston forces the molten sample through a heated die under this load, and the mass collected over a timed interval is reported in grams per 10 minutes.

Recycled blend rich in homopolymer

The recycled polyethylene blend contains an 86 wt % homopolymer fraction. Cross-fractionation chromatography first separates the dissolved polymer by crystallizability and then separates each temperature fraction by molecular size, and integration of the assigned homopolymer region gives its mass fraction.

One percent isotactic polypropylene fraction

The recycled blend contains 1 wt % isotactic polypropylene, 85 wt % polyethylene homopolymer, and 14 wt % polyethylene copolymer by cross-fractionation chromatography. The analysis assigns the polymer eluting at 104 °C and above to the isotactic polypropylene fraction.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,317,054 B2
Published
Jan 8, 2008
Filed
Jul 22, 2005
Class
C08L 23/00
Document BUS 9,388,303 B2
Published
Jul 12, 2016
Filed
Sep 4, 2014
Class
C08L 23/06
Claim 1
Document A
Document B
1.1(I) 50.0 to 99.0 wt %, based on the total weight of the composition, of a metallocene catalyzed linear low density polyethylene (mLLDPE), which consists of: (i) 30.0 to 70.0 wt %, based on the total weight of the mLLDPE, of an ethylene-1-butene polymer component (A) and (ii) 70.0 to 30.0 wt %, based on the total weight of the mLLDPE, of an ethylene-1-hexene polymer component (B),
A HDPE blended composition comprising at least two components wherein the first component is a low molecular weight (LMW) linear polyethylene having a melt index (MI) from about 1.0 to about 20 grams per 10 minutes, wherein said first component is linear low density (LLDPE), medium density (MDPE) or high density (HDPE) polyethylene and a second component is a high molecular weight (HMW) HDPE, wherein said blend contains a major portion of HDPE and only minor amounts of LLDPE
A · US 7,317,054 B2 · claim 12
The polyethylene resin composition according to the above [1], wherein the ethylene homopolymer comprises: 30 to 70% by mass of a component (A) composed of an ethylene homopolymer having a melt flow rate of 3.0 to 300 g/10 min and a density of 962 to 974 kg/m3, and 70 to 30% by mass of a component (B) composed of an ethylene homopolymer having a melt flow rate different from the melt flow rate of the component (A).
B · US 9,388,303 B2 · ¶ 22
1.2wherein the ethylene-1-butene polymer component (A) comprises: a density (ISO 1183) in the range of 925 to 960 kg/m3 and a MFR2 (190 °C, 2.16 kg, ISO 1133) in the range of 1.0 to 100.0 g/10 min;
1.3the ethylene-1-hexene polymer component (B) comprises: a density (ISO 1183) in the range of 880 to 915 kg/m3 and a MFR2 (190 °C, 2.16 kg, ISO 1133) in the range of 0.001 to 1.0 g/10 min; and
TABLE 2 Example Example Example Example Example Example 1 2 3 4 5 6 Component MFR (g/10 min) 49.8 20.1 4.93 4.80 4.43 5.09 (A) Density (kg/cm3) 969 968 965 966 966 966 Content (% by weight) 50 50 50 60 70 70 Kind of a Catalyst Ziegler Ziegler Ziegler Ziegler Ziegler Ziegler Z1 Z1 Z1 Z2 Z2 Z2 Component MFR (g/10 min) (calculated 0.015 0.017 0.028 0.010 0.013 0.002 (B) value) Content (% by weight) 50 50 50 40 30 30 Kind of a Catalyst Ziegler Ziegler Ziegler Ziegler Ziegler Zieg
B · US 9,388,303 B2 · ¶ 208
1.4wherein the multimodal linear low density polyethylene (mLLDPE) comprises: a density (ISO 1183) in the range of 910 to 923 kg/m3, a MFR2 (190 °C, 2.16 kg, ISO 1133) in the range of 0.1 to 1.2 g/10 min and a MFR21 (190 °C, 21.6 kg, ISO 1133) in the range of 5.0 to 75.0 g/10 min and a ratio MFR21/MFR2 in the range of 35.0 to 60.0; and
To adjust processability and performance, a mixture of low molecular weight HDPE homopolymers and copolymers 13 (FIG. 6) having a narrow molecular weight is blended with the HMW HDPE copolymer 12 in FIG. 6 to obtain the desired MI and density of the blend 14 shown in FIG. 7.
A · US 7,317,054 B2 · ¶ 47
A polyethylene resin composition comprising an ethylene homopolymer and having: a melt flow rate of 0.10 to 0.60 g/10 min; a molecular weight distribution (Mw/Mn) of 6.0 to 20; a density of 956 to 970 kg/m3; and in a cross-fractionation chromatography measurement using orthodichlorobenzene, a cumulative elution volume of 40° C. or more and less than 91° C. of 2.0% by mass or more and 15% by mass or less of a total elution volume; a cumulative elution volume of 91° C. or more
B · US 9,388,303 B2 · claim 1
1.5(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (i) a MFR5 (ISO1133, 5.0 kg; 190 °C) in the range of 0.1 to 10.0 g/10 min, and
This application discloses compositions having specific range of molecular properties, densities, and melt flow index (MI), and the methods for selecting, formulating, and melt blending said compositions composed of prime, wide and off specification virgin and post consumer and industrial recycled, reprocessed and regrind HDPE in order to comply with the performance standards of AASHTO.
A · US 7,317,054 B2 · ¶ 2
1.6(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (ii) a density (ISO1183) in the range of 950 to 970 kg/m3, and
1.7(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (iii) a C2 fraction in an amount of above 95.0 wt %, as measured by NMR of the d2-tetrachloroethylene soluble fraction, and
1.8(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (iv) a homopolymer fraction (HPF) content, based on the total weight of the PCR, determined according to Chemical Composition Analysis by Cross Fractionation Chromatography (CFC) in the range of 80.0 to 91.0 wt %, and
1.9(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (v) a copolymer fraction (CPF) content, based on the total weight of the PCR, determined according to Chemical Composition Analysis Cross Fractionation Chromatography (CFC) in the range of 9.0 to 20.0 wt %, and
1.10(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (vi) optionally an iso-PP fraction (IPPF) content, based on the total weight of the PCR, determined according to Chemical Composition Analysis Cross Fractionation Chromatography (CFC) in the range of 0.0 to 2.0 wt %, whereby said iso-PP fraction (IPPF) is defined as the polymer fraction eluting at a temperature of 104 °C and above, whereby said homopolymer fraction (HPF), said copolymer fraction (CPF), and said iso-PP fraction (IPPF) add up to 100 wt %, and
1.11(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (vii) inorganic residues (measured by TGA) in the range of 0.01 to 2.00 wt % with respect to the total polyethylene recycling blend, and
1.12(II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (viii) OCS gels of size 100 to 299 micrometer measured on 10 m2 of a film by an OCS count instrument within the range of 500 to 5000 counts per squaremeter; wherein: (II) 1.0 to 50.0 wt %, based on the total weight of the composition, of a polyethylene recycling blend (PCR) comprising: (ix) the polyethylene blend comprises a CIELAB color space (L*a*b*) measured according to DIN EN ISO 11664-4 of: L* from 75.0 to 86.0; a* from −5.0 to 0.0; b* from 5.0 to below 25.0 or (x) the polyethylene blend comprises a CIELAB color space (L*a*b*) measured according to DIN EN ISO 11664-4 of: L* from above 86.0 to 97.0; a* from −5.0 to 0.0; b* from 0.0 to below 5.0.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.5. Only Document B has a passage for 1.3. Both have a passage for 1.1 1.4. Both are classified in CPC C08L, as is this patent.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Patent Literature 2 discloses a method of using a kind of polyethylene having a specific molecular weight, or as required, concurrently using a polyethylene having a higher molecular weight, to thereby improve permeation and mechanical properties.
B · US 9,388,303 B2 · ¶ 4

Related claim parts: 1.5

The benefit of this method is that it provides, a priori, a means of determining the ESCR of HDPE blends utilizing wide and off specification virgin HDPE resins as well as post consumer and post industrial recycled HDPE components.
A · US 7,317,054 B2 · ¶ 3
This means that existing polyethylene resins and blends of polyethylene resins are not capable of providing sufficiently enhanced ESCR.
A · US 7,317,054 B2 · ¶ 6
Polyolefin microporous films are broadly used as separation and permselective separation membranes, separator materials and the like for various types of substances, and broadly utilized in medical applications such as microfiltration membranes, electric material applications such as separators for fuel cells and separators for capacitors, and the like.
B · US 9,388,303 B2 · ¶ 2
However, technical progresses advance the downsizing of batteries and the thickness reduction of microporous films, and higher air permeation, mechanical strength and high processability have been demanded on separators.
B · US 9,388,303 B2 · ¶ 9
Cite aspatent.fyi, US 2026/0365835 A1, claim 1, first published 2026-11-23T17:00:00-05:00, https://patent.fyi/US20260365835/, SHA-256 fe8d8ece681256364ca0ded181b5cee33c6ac56aa8bee596d0b7580b6059f458
First published
Permanent addresshttps://patent.fyi/US20260365835/
Content fingerprint (SHA-256)fe8d8ece681256364ca0ded181b5cee33c6ac56aa8bee596d0b7580b6059f458
Methodv2026-11-18.2 · automated, not reviewed by a person