patent.fyi
Applications  /  US 2026/0365837
United States Patent Application Publication

US 2026/0365837 A1

Published
Nov 19, 2026
Filed
Dec 3, 2025
Earliest date on the face
May 13, 2025
Classification
C08L 23/12
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1High-density polyethylene as the rigid matrix

What ifWhat if the rigid matrix is a high-density polyethylene resin with no polypropylene resin?
Claim language“a polypropylene resin”

High-density polyethylene at a density of 0.955 g/cm3 to 0.965 g/cm3 forms the continuous crystalline phase and provides structural stiffness and heat resistance up to 110 C. The ethylene-rich backbone of the matrix co-crystallizes with the ethylene-based blocks of the elastomeric phase during injection molding, creating direct interfacial bonding without compatibilizers. Mold shrinkage and low-temperature ductility are balanced by adjusting the melt flow rate of the polyethylene between 15 g/10 min and 35 g/10 min.

1.1Lower polypropylene content for softer housings

What ifWhat if the polypropylene resin content is lowered to 25 wt % to 35 wt %?
Claim language“from 40 wt % to 70 wt %”

At 25 wt % to 35 wt % polypropylene resin, the elastomeric components form a co-continuous morphology with the polypropylene phase during twin-screw extrusion at 200 C. This phase structure reduces flexural modulus to between 300 MPa and 550 MPa while maintaining tear resistance during rapid deployment at minus 35 C. Wall thickness of the molded housing is increased by 0.5 mm to 1.0 mm to preserve geometric rigidity under cabin heat aging.

1.2Dynamically vulcanized rubber phase

What ifWhat if the elastomeric phase is a dynamically vulcanized ethylene-propylene-diene rubber with no olefin block copolymer?
Claim language“an olefin block copolymer”

Ethylene-propylene-diene terpolymer rubber is crosslinked in situ with a phenolic curing agent during high-shear melt mixing with the polypropylene resin at 190 C to 210 C. The resulting crosslinked rubber domains, measuring 1 micrometer to 3 micrometers in diameter, remain dispersed within the thermoplastic matrix and absorb impact energy without flowing at elevated temperatures. Compression set and dimensional recovery improve because the covalent crosslinks prevent permanent chain slippage under sustained load.

1.2Low olefin block copolymer loading

What ifWhat if the olefin block copolymer is present at 5 wt % to 12 wt %?
Claim language“from 15 wt % to 50 wt %”

Reducing the olefin block copolymer to between 5 wt % and 12 wt % leaves the polypropylene resin and polyolefin plastomer to carry the primary stiffness and impact balance. The small block copolymer fraction concentrates at the phase boundary between the polypropylene matrix and the plastomer droplets, functioning as an interfacial compatibilizer rather than the bulk elastomer. This lowers melt viscosity and allows thin wall sections to fill at injection pressures below 60 MPa.

1.3Hydrogenated styrenic triblock copolymer modifier

What ifWhat if the impact-modifying component is a hydrogenated styrene-ethylene-butylene-styrene triblock copolymer with no polyolefin plastomer?
Claim language“a polyolefin plastomer”

The hydrogenated midblock of the styrenic triblock copolymer entangles with the polypropylene and olefin block copolymer phases, while the glassy polystyrene endblocks form physical crosslink domains at service temperatures. Blending 10 wt % to 20 wt % of this triblock copolymer at a styrene content of 18 wt % to 30 wt % provides low-temperature ductile fracture resistance down to minus 40 C. The glassy endblocks also restrict post-molding crystalline contraction, keeping linear mold shrinkage below 1.2 percent.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Low-temperature flexible cable jacketing for industrial robotics

The polyolefin thermoplastic elastomer blend containing polypropylene resin, an olefin block copolymer, and a polyolefin plastomer forms an extruded outer jacket around insulated copper conductor bundles in articulated robotic harnesses. A single-screw extruder with a temperature profile of 190 °C to 220 °C feeds the molten blend through a crosshead die onto a braided shield layer at a wall thickness of 0.8 mm to 1.5 mm. The elastomeric phase dispersed within the polypropylene matrix absorbs repeated torsional and bending stresses at operating temperatures down to -40 °C without surface cracking. The resulting jacket provides abrasion resistance and dimensional stability during continuous multi-axis flexing cycles.

Component substitution

Hydrogenated styrenic block copolymer replacing olefin block copolymer

A styrene-ethylene-butylene-styrene triblock copolymer replaces the olefin block copolymer at 15 wt % to 45 wt % in the blend with polypropylene resin and a polyolefin plastomer. The triblock copolymer has a styrene content of 20 wt % to 33 wt % and a solution viscosity of 800 mPa·s to 2,500 mPa·s at 25 °C in a 20 wt % toluene solution. During twin-screw compounding at 200 °C to 230 °C, the ethylene-butylene midblocks co-crystallize with the polyolefin plastomer while the glassy polystyrene endblocks form physical crosslink domains throughout the polypropylene matrix. This physical network increases elastic recovery and lowers compression set at elevated service temperatures up to 90 °C.

Propylene-ethylene random elastomer replacing ethylene-based polyolefin plastomer

A semi-crystalline propylene-ethylene copolymer elastomer containing 10 wt % to 16 wt % randomly distributed ethylene units replaces the polyolefin plastomer at 10 wt % to 30 wt % of the total composition. The propylene-ethylene elastomer has a density of 0.860 g/cm3 to 0.875 g/cm3 and a melting peak temperature between 50 °C and 75 °C. During melt blending with the polypropylene resin and olefin block copolymer at 210 °C, the high propylene sequence compatibility reduces interfacial tension between the continuous matrix and the dispersed elastomer domains. The resulting blend exhibits finer domain dispersion below 1.2 micrometers in diameter and higher weld-line tensile retention in thin-walled injection-molded housings.

Parameter or scale variation

High-elastomer soft-touch formulation with reduced polypropylene content

The composition shifts to 20 wt % to 35 wt % polypropylene resin, 45 wt % to 60 wt % olefin block copolymer, and 15 wt % to 30 wt % polyolefin plastomer to produce a soft elastomeric material with a durometer A hardness of 55 to 75. Compounding occurs in a co-rotating twin-screw extruder having a length-to-diameter ratio of 44:1 at a screw speed of 350 rpm to 450 rpm and a barrel temperature gradient from 175 °C to 205 °C. Injection molding uses a melt temperature of 195 °C, a mold surface temperature of 30 °C, and a packing pressure of 45 MPa for 6 seconds to control shrinkage below 0.9%. The higher elastomeric fraction yields a tensile elongation at break above 500% and a flexural modulus below 120 MPa for compliant sealing profiles.

Combination with existing systems

Two-shot overmolding onto glass-fiber reinforced polypropylene substrates

The thermoplastic elastomer composition is integrated with a rigid structural housing molded from 30 wt % short glass-fiber reinforced polypropylene using a rotary-platen two-shot injection molding press. In the first stage, the rigid substrate is molded at 240 °C and cooled to a surface temperature of 70 °C to 85 °C before the platen indexes 180 degrees to the second cavity. The molten thermoplastic elastomer is injected directly onto the warm substrate at 215 °C and 55 MPa, creating a 2.0 mm perimeter gasket or grip layer. Interdiffusion of polypropylene chains across the molten interface forms a continuous fusion bond with a peel strength exceeding 4.5 N/mm without primers or mechanical interlocks.

Automated or data-driven variant

Inline spectroscopic feedback control for twin-screw compounding

A near-infrared optical probe mounted in the die adapter of a twin-screw compounding extruder continuously collects melt spectra between 1,100 nm and 2,500 nm at 2 Hz during production of the three-component blend. A partial least squares regression model calibrated on offline rheological and compositional datasets converts each spectrum into real-time estimates of polypropylene fraction, olefin block copolymer fraction, polyolefin plastomer fraction, and melt flow rate. A proportional-integral-derivative controller compares the predicted melt flow rate and component ratios against target setpoints every 5 seconds and adjusts gravimetric loss-in-weight feeder speeds and screw rotation rate. Closed-loop adjustment holds the melt flow rate within 1.5 g/10 min of the target value and compensates for lot-to-lot feedstock viscosity drift.

Specific version of a part

High-flow heterophasic impact polypropylene copolymer

The polypropylene resin is a reactor-grade heterophasic impact copolymer with a melt flow rate of 30 g/10 min to 60 g/10 min at 230 C under a 2.16 kg load. It consists of an isotactic polypropylene homopolymer matrix containing 10 wt % to 18 wt % finely dispersed ethylene-propylene rubber particles synthesized directly in a multi-stage gas-phase reactor. This internal rubber phase pre-toughens the rigid matrix while the high melt flow rate enables rapid filling of thin-walled chute geometries.

Nucleated isotactic polypropylene homopolymer matrix

The polypropylene resin is an isotactic homopolymer with an isotacticity index above 96 percent, compounded with 0.1 wt % to 0.3 wt % of an organic phosphate ester nucleating agent. The nucleating agent accelerates spherulite formation during cooling, raising the crystallization temperature to 125 C to 130 C and shortening injection molding cycle times. Fine, uniform spherulites increase tensile yield strength above 35 MPa and reduce isotropic shrinkage variation across the molded part.

Chain-shuttled ethylene-octene multiblock copolymer

The olefin block copolymer is a statistical multiblock ethylene-octene copolymer produced by dual-catalyst chain-shuttling polymerization using a dialkyl zinc shuttling agent. Alternating crystalline ethylene-rich hard segments with a melting point of 118 C to 124 C and amorphous octene-rich soft segments with a glass transition near minus 60 C form a thermally reversible physical network. At a density of 0.875 g/cm3 to 0.885 g/cm3 and a melt index of 1 g/10 min to 5 g/10 min at 190 C, the copolymer maintains elastic recovery at cabin temperatures up to 105 C.

Single-site catalyzed ethylene-octene plastomer

The polyolefin plastomer is a random ethylene-1-octene copolymer synthesized with a single-site metallocene catalyst to achieve a narrow molecular weight distribution with a polydispersity index near 2.0. It has a density between 0.865 g/cm3 and 0.875 g/cm3, a 1-octene comonomer content of 28 wt % to 35 wt %, and a melt index of 5 g/10 min to 15 g/10 min at 190 C under a 2.16 kg load. Its uniform comonomer distribution and low shear viscosity promote dispersion into sub-micrometer droplets inside the polypropylene phase, lowering low-temperature brittle transition temperatures.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,361,720 B2
Published
Apr 22, 2008
Filed
Oct 7, 2003
Document BUS 2010/0081756 A1
Published
Apr 1, 2010
Filed
Oct 1, 2008
Class
C08L 23/16
Claim 1
Document A
Document B
1.1a polypropylene resin in an amount ranging from 40 wt % to 70 wt %;
In a third aspect, the invention is an impact modified polypropylene copolymer composition comprised of a first polymer component comprising a high crystalline homopolymer or copolymer resin in accordance with the first and/or second aspect of this invention. This high crystalline resin is blended with an impact modifier.
A · US 7,361,720 B2 · ¶ 18
In one embodiment, the invention is a resin composition comprising about 70% to about 95% by weight of a polypropylene homopolymer having less than 3% by weight xylene solubles and a crystallinity of at least 55%.
B · US 2010/0081756 A1 · ¶ 9
1.2an olefin block copolymer in an amount ranging from 15 wt % to 50 wt %; and
No. 5,460,884 to Kobylivker describes a composition comprising a homopolymer and an ethylene/propylene random block copolymer.
B · US 2010/0081756 A1 · ¶ 18
1.3a polyolefin plastomer in an amount ranging from 5 wt % to 30 wt %.
The more preferred impact modifiers are ethylene/alpha-olefin copolymers made with single-site or metallocene catalysts wherein the units within the impact modifier derived from ethylene are greater than 50% by weight and the alpha-olefin is selected from olefins having at least three carbon atoms, preferably at least 4 carbon atoms, more preferably from 4 to 12 carbon atoms, further more preferably from 4 to 8 carbon atoms.
A · US 7,361,720 B2 · ¶ 19

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.3. Only Document B has a passage for 1.2. Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

What is desired is a polypropylene that exhibits a relatively narrow molecular weight distribution, but also exhibits high flexural modulus and low xylene solubles.
A · US 7,361,720 B2 · ¶ 4
Still another object of the invention is to provide a polypropylene homopolymer that provides the above properties and also exhibits excellent optical properties, such as improved contact clarity and lower values for haze than comparable commercially available polypropylene homopolymers.
A · US 7,361,720 B2 · ¶ 7
There thus exists a long felt, but unmet need in the art for a BOPP grade resin that maintains the processability of the high xylene solubles homopolymer, but exhibits enhanced characteristics when processed into a BOPP film.
B · US 2010/0081756 A1 · ¶ 5
The present invention provides a polypropylene polymer suitable for use in producing BOPP film.
B · US 2010/0081756 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0365837 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365837/, SHA-256 4f588a95f0710d223fe6bfad9b8a2e9654c9be2cbc54ca9a98f1f107b910bc97
First published
Permanent addresshttps://patent.fyi/US20260365837/
Content fingerprint (SHA-256)4f588a95f0710d223fe6bfad9b8a2e9654c9be2cbc54ca9a98f1f107b910bc97
Methodv2026-11-18.2 · automated, not reviewed by a person