Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Random propylene copolymer low-weight resin
What ifWhat if the low-molecular-weight polypropylene component is a random propylene-ethylene copolymer rather than a block polypropylene or a homo-polypropylene?
Claim language“block polypropylene or a homo-polypropylene”
A single-stage reactor copolymerizes propylene with 2 to 6 weight percent ethylene randomly distributed along the polymer backbone to form a resin with a weight average molecular weight of 200,000 to 380,000. The random comonomer units disrupt isotactic sequence length, lowering the crystalline melting temperature to between 135 °C and 150 °C and reducing melt viscosity during injection molding. Blending this random copolymer with the higher-molecular-weight matrix maintains mold flowability while reducing warpage in thin-walled molded parts.
1.1Ultra-low molecular weight flow modifier
What ifWhat if the lower-molecular-weight polypropylene has a weight average molecular weight of 50,000 to 150,000?
Claim language“weight average molecular weight of 200,000 to 380,000”
Controlled peroxide visbreaking or high-hydrogen chain-transfer polymerization produces a short-chain polypropylene fraction with a weight average molecular weight between 50,000 and 150,000. At loadings of 10 to 25 weight percent, these short chains act as an internal polymeric lubricant that lowers shear viscosity at shear rates above 1,000 reciprocal seconds. The reduced melt resistance enables filling of complex mold cavities at barrel temperatures below 210 °C while the high-molecular-weight phase sustains structural stiffness.
A twin-screw extruder melt-blends 15 to 30 weight percent polyamide 6 with the low-molecular-weight polypropylene and 3 to 5 weight percent maleic-anhydride-grafted polypropylene at 245 °C. The anhydride groups react with terminal amine groups on the polyamide chains at the phase interface to form in-situ graft copolymers that stabilize sub-micron dispersed domains. The rigid semicrystalline polyamide domains increase flexural modulus and heat deflection temperature without requiring an ultra-viscous polypropylene fraction.
What ifWhat if the homo-polypropylene fraction has a weight average molecular weight of 900,000 to 1,500,000?
Claim language“weight average molecular weight of 500,000 to 700,000”
Low-hydrogen slurry polymerization produces a homo-polypropylene component with a weight average molecular weight between 900,000 and 1,500,000 at a concentration of 5 to 15 weight percent of the total blend. Under extensional flow during molding or thermoforming, the long chains align to form row-nucleated crystalline structures that accelerate solidification and increase melt tension. Keeping the ultra-high-molecular-weight fraction at a low mass ratio preserves overall processability while elevating tensile strength and creep resistance.
1.3Beta-crystal nucleating agent without rubber
What ifWhat if the composition contains no rubber and relies on a beta-crystal nucleating agent for impact resistance?
Claim language“at least one rubber”
Compounding 0.05 to 0.3 weight percent of a calcium pimelate or aryl amide nucleating agent into the bimodal polypropylene blend induces crystallization into the trigonal beta-form during cooling between 100 °C and 130 °C. Under impact loading, the beta-phase lamellae undergo shear yielding and stress-induced phase transformation into the denser alpha-form, absorbing fracture energy through micro-cavitation. This crystalline toughening mechanism increases notched impact strength while retaining the surface hardness and stiffness of an unmodified polypropylene matrix.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Thermoformed food container sheet from bimodal polypropylene
A chill-roll sheet extrusion line processes the bimodal polypropylene and elastomer composition into monolayer sheets with a thickness of 0.4 mm to 1.2 mm for rigid food packaging trays. The high-molecular-weight polypropylene fraction increases melt strength during vacuum and pressure thermoforming at 155 °C to 168 °C, preventing sheet sag across wide mold cavities. The low-molecular-weight polypropylene fraction fills sharp corner radii and rim flanges during plug-assisted forming, while the dispersed elastomer domains maintain impact resistance at refrigerated storage temperatures of 0 °C to 4 °C. A nucleating agent based on sorbitol derivatives at 0.2 parts by mass per 100 parts total resin accelerates crystallization during roll cooling to reduce cycle time and optical haze.
A hydrogenated styrene-ethylene-butylene-styrene block copolymer replaces the olefinic post-added rubber at 15 parts to 35 parts by mass per 100 parts of the low-molecular-weight polypropylene. A co-rotating twin-screw extruder operating at 210 °C to 230 °C and a screw speed of 250 rpm disperses the styrenic elastomer into sub-micron domains within the bimodal polypropylene matrix. The ethylene-butylene midblocks interpenetrate the amorphous polypropylene regions while the polystyrene endblocks form physical crosslinks that increase elastic recovery under flexural strain. This phase structure maintains dimensional stability after injection molding and reduces stress whitening upon bending compared to uncrosslinked ethylene-alpha-olefin elastomers.
Parameter or scale variation
Expanded molecular weight split for large blow-molded tanks
The bimodal resin formulation shifts the low-molecular-weight polypropylene fraction to a weight average molecular weight of 120,000 to 190,000 and raises the high-molecular-weight polypropylene fraction to 750,000 to 1,100,000. The mass ratio of high-molecular-weight polypropylene to low-molecular-weight polypropylene sits between 25:75 and 45:55, with 10 parts to 25 parts by mass of copolymerized ethylene-propylene rubber. An accumulator-head extrusion blow molding machine extrudes a vertical parison at 200 °C to 215 °C with a die swell ratio of 1.3 to 1.5 and minimal drawdown over a 1.5 m parison length. Compressed air at 0.6 MPa to 0.8 MPa expands the parison against water-cooled aluminum molds to produce hollow chemical storage vessels with uniform 4 mm to 8 mm wall thickness.
Combination with existing systems
Co-injection molding with glass-fiber reinforced polypropylene core
A two-barrel co-injection molding machine combines the bimodal polypropylene and rubber composition as the outer skin layer with a 30 percent by mass short glass-fiber reinforced polypropylene core. A sequential hydraulic valve-gate nozzle injects the bimodal skin melt at 215 °C first to coat the mold cavity walls, followed immediately by the fiber-filled core melt at 230 °C. The skin layer encapsulates the glass fibers to produce a smooth, impact-resistant exterior surface while the rigid core carries structural bending loads. Shared polypropylene chains across the skin-core boundary diffuse during the 20 s to 35 s packing phase to form a continuous welded interface without tie-layer adhesives.
Microcellular foaming with supercritical nitrogen injection system
A supercritical fluid dosing unit injects nitrogen gas at 18 MPa to 24 MPa and 0.3 percent to 0.8 percent by mass directly into the molten bimodal polypropylene and elastomer blend inside an injection molding barrel. A static mixing section dissolves the supercritical nitrogen into a single-phase polymer-gas solution before a shut-off nozzle meters the shot into a mold cavity held at 45 °C. The rapid pressure drop during cavity filling nucleates closed microcells with diameters of 20 micrometers to 60 micrometers, while the high-molecular-weight polypropylene fraction resists cell wall rupture during expansion. This foamed structure reduces part density by 10 percent to 18 percent and eliminates sink marks opposite structural ribs without requiring high holding pressures.
Automated or data-driven variant
Closed-loop gravimetric blending using inline melt viscosity sensing
An automated compounding line feeds low-molecular-weight polypropylene pellets, high-molecular-weight polypropylene pellets, and elastomer pellets through three loss-in-weight gravimetric feeders into a twin-screw extruder. An inline slit-die capillary rheometer mounted at the extruder discharge continuously measures shear viscosity at two shear rates every 10 s and transmits the readings to a programmable logic controller. A multivariable regression model converts the dual-rate viscosity ratio into estimated weight average molecular weight and molecular weight distribution breadth in real time. When the computed viscosity ratio drifts outside a 2 percent tolerance band, the controller adjusts the feeder mass flow setpoints to restore the target bimodal balance without stopping production.
Specific version of a part
Isotactic homo-polypropylene from gas-phase polymerization
A gas-phase fluidized-bed reactor polymerizes propylene over a supported titanium-magnesium catalyst with an external alkoxysilane electron donor and controlled hydrogen partial pressure to yield a homo-polypropylene with a weight average molecular weight of 260,000 and an isotactic pentad fraction above 97 percent. The narrow chain-length distribution produces a melt flow rate of 25 to 40 grams per 10 minutes at 230 °C under a 2.16-kilogram load, supporting rapid thin-wall injection molding.
Multi-stage block polypropylene with ethylene-propylene phase
Two slurry loop reactors in series synthesize an isotactic polypropylene homopolymer matrix at low hydrogen concentration, followed by a gas-phase copolymerization reactor feeding a 50:50 molar ratio of ethylene and propylene to yield a block polypropylene with a weight average molecular weight of 550,000. The resulting heterophasic resin contains 12 to 18 weight percent dispersed ethylene-propylene copolymer domains with an intrinsic viscosity of 2.5 to 4.0 deciliters per gram in decahydronaphthalene at 135 °C. The high-molecular-weight chains entangle across phase boundaries to sustain creep resistance and low-temperature impact strength.
A co-rotating twin-screw extruder compounds 10 to 20 weight percent of a post-added ethylene-1-octene copolymer elastomer having a density of 0.865 to 0.875 grams per cubic centimeter and a 1-octene content of 25 to 35 weight percent into the molten polypropylene blend at 210 °C. High-shear kneading blocks break the elastomer into uniform droplets with a number-average diameter of 0.3 to 0.8 micrometers. Under impact stress, these soft elastomer particles cavitate and initiate localized shear banding in the surrounding polypropylene matrix.
A second-stage gas-phase reactor directly polymerizes an amorphous ethylene-propylene rubber component inside the porous granules of the low-molecular-weight polypropylene matrix using the active catalyst sites retained from the first stage. Controlling the ethylene-to-propylene gas feed ratio to maintain 40 to 55 weight percent ethylene in the copolymer phase yields a rubber fraction with a glass transition temperature near -50 °C. In-reactor synthesis produces intimate sub-micron dispersion of the rubber component without a separate elastomer pellet-blending step.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a low-molecular-weight polypropylene which is a block polypropylene or a homo-polypropylene having a weight average molecular weight of 200,000 to 380,000;
According to a first embodiment of the present invention, a process for preparing a high flow polypropylene composition is provided, comprising the following steps: (i) preparation of a low molecular weight propylene homopolymer with an MFR2 of at least 40 g/10 min;
B · US 2012/0015170 A1 · ¶ 63
1.2a high-molecular-weight polypropylene which is a block polypropylene having a weight average molecular weight of 400,000 to 700,000 or a homo-polypropylene having a weight average molecular weight of 500,000 to 700,000; and
(ii) preparation of a high molecular weight propylene copolymer with an MFR2 of not more than 15 g/10 min and having a comonomer content of not higher than 8 wt %; and compounding the polymers to receive the final polypropylene composition having an MFR2 of at least 5 g/10 min.
B · US 2012/0015170 A1 · ¶ 63
1.3at least one rubber selected from a rubber component copolymerized with the low-molecular-weight polypropylene, a rubber component copolymerized with the high-molecular-weight polypropylene, and a post-added rubber.
In the automobile parts comprising a polypropylene resin composition according to the first and second aspects of the present invention, it is preferred that the elastomer (B) be at least one elastomer selected from among a propylene/α-olefin random copolymer (B-1), an ethylene/α-olefin random copolymer (B-2), an ethylene/α-olefin/nonconjugated polyene random copolymer (B-3) and a hydrogenated block copolymer (B-4).
A · US 7,081,493 B2 · ¶ 21
In already indicated above, the polypropylene composition may comprise conventional adjuvants, such as additives, fillers and reinforcing agents or additional impact modifiers.
B · US 2012/0015170 A1 · ¶ 83
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document B has a passage for 1.11.2. Both have a passage for 1.3. Both are classified in CPC C08L, as is this patent.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
A rather low molecular weight improves processability and crystallinity, hence stiffness, however, the impact strength is deteriorated.
B · US 2012/0015170 A1 · ¶ 5
Related claim parts: 1.3
When an injection molding of the above polypropylene resin composition is conducted, there would occur such problems that the transfer of emboss pattern provided on the inside surface of the metal mold is poor to thereby fail to lower the gloss, and that the transferability is different between the vicinity of a gate of the metal mold and a position remote from the gate to thereby bring about a gloss difference.
A · US 7,081,493 B2 · ¶ 4
Therefore, the above polypropylene resin composition has a drawback in that the molding cycle cannot be shortened.
A · US 7,081,493 B2 · ¶ 5
Still further, materials subjected to visbreaking generally suffer from bad taste and odour which is a great disadvantage in the field of food packaging.
B · US 2012/0015170 A1 · ¶ 7
It is therefore an object of the present invention to provide a polypropylene composition with high flowability and hence processability, which at the same time has good mechanical and optical properties, particularly a good balance of stiffness and haze.
B · US 2012/0015170 A1 · ¶ 8
Cite aspatent.fyi, US 2026/0365839 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365839/, SHA-256 36b9036991c5ec7da4e6a2f8303f30ccc28426f06434e2e7c1599852ee97da6b