patent.fyi
Applications  /  US 2026/0365843
United States Patent Application Publication

US 2026/0365843 A1

Published
Nov 19, 2026
Filed
Nov 3, 2023
Earliest date on the face
Nov 4, 2022
Classification
C08L 53/00
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Co-continuous phase network morphology

What ifWhat if the composition forms a co-continuous interpenetrating phase network?
Claim language“a plurality of domain regions dispersed in the matrix region”

Two immiscible polymer phases are melt-blended at a volume ratio near 50:50 and a viscosity ratio near 1.0 in a twin-screw extruder at 190 to 230 degrees Celsius. Both phases remain continuous throughout the molded part in three dimensions, creating a high interfacial area without isolated islands. Impact energy transfers along the continuous elastomeric pathways and dissipates through shear yielding across the interconnected rigid phase.

1.2Polyamide matrix with elastomer domains

What ifWhat if the matrix region consists of an aliphatic polyamide rather than a polyolefin-based resin?
Claim language“a polyolefin-based resin”

Melt-compounding an aliphatic polyamide such as polyamide 6 with a maleic-anhydride-grafted elastomeric modifier at 240 to 270 degrees Celsius produces a tough engineering thermoplastic blend. Amine end groups on the polyamide react with anhydride groups on the modifier during extrusion to form covalent grafts at the phase boundary. The grafted interface stabilizes dispersion and promotes matrix shear yielding under low-temperature impact loading.

1.3Random olefin elastomer domains

What ifWhat if each dispersed domain consists of a random ethylene-octene copolymer with no block structure?
Claim language“a block copolymer”

A random ethylene-octene copolymer having an octene content of 20 to 38 weight percent and a density of 0.86 to 0.88 grams per cubic centimeter is melt-blended into the polyolefin matrix. Its glass transition temperature below minus 40 degrees Celsius keeps the dispersed rubbery droplets compliant under subzero impact. Interfacial adhesion arises directly from chain entanglement between the olefinic segments of the random copolymer and the surrounding polyolefin matrix.

1.3All-olefin multiblock copolymer domains

What ifWhat if the block copolymer replaces the aromatic vinyl-based polymer block with crystalline polyethylene hard blocks?
Claim language“an aromatic vinyl-based polymer block”

Chain-shuttling polymerization produces an all-olefin multiblock copolymer alternating between low-comonomer crystalline polyethylene blocks and high-comonomer amorphous ethylene-octene blocks. The crystalline polyethylene segments act as physical crosslinks at service temperatures while remaining free of aromatic monomers. During impact, the amorphous olefin segments cavitate and relieve triaxial stress while the crystalline blocks anchor the domains to the polyolefin matrix.

1.4Sub-micron elastomer domain sizing

What ifWhat if the dispersed domain regions have diameters between 150 nm and 500 nm?
Claim language“10 nm to 15 nm”

Compounding a higher-viscosity elastomer modifier into a polypropylene matrix at moderate shear rates produces sub-micron rubber particles averaging 200 to 400 nm in diameter. Under rapid impact, particles in this size range cavitate internally to release hydrostatic tension before brittle fracture initiates. The cavitated rubber particles then trigger localized shear banding across the surrounding matrix ligaments.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Cryogenic fluid transfer tubing with dispersed block domains

A flexible cryogenic transfer hose incorporates a high-density polyethylene matrix containing dispersed diblock copolymer domains of polystyrene and hydrogenated polybutadiene with domain diameters of 12 nm and inter-domain spacings of 35 nm. The composition is melt-extruded through an annular die at 200 degrees Celsius into a seamless inner liner wall with a thickness of 2.5 mm. During exposure to liquefied gas temperatures down to minus 160 degrees Celsius, the nanoscale elastomer domains arrest microcrack propagation across the semi-crystalline polyethylene matrix under bending loads. The liner maintains pressure containment during repeated thermal cycling between ambient storage and cryogenic transfer states.

Subterranean power cable jacket with nanoscale elastomer domains

An extruded outer jacket for buried electrical power cables uses a medium-density polyethylene matrix containing 25 wt % of a styrene-ethylene-butylene block copolymer dispersed as 11 nm to 14 nm domains at inter-domain spacings of 30 nm to 55 nm. A crosshead extrusion die applies a 3.0 mm continuous jacket over a metallic moisture shield and cross-linked polyethylene insulation core at a line speed of 18 meters per minute. The dispersed nanoscale domains dissipate impact energy from rocky trench backfill and resist environmental stress cracking during winter installation at minus 30 degrees Celsius. Carbon black pigment at 2.5 wt % is co-dispersed in the matrix phase to block ultraviolet degradation during outdoor reel storage prior to burial.

Component substitution

Hydrogenated diene triblock domains in cyclic olefin matrix

A rigid transparent polymer blend replaces the linear polyolefin matrix with an amorphous cyclic olefin copolymer having a glass transition temperature of 130 degrees Celsius and replaces the diblock copolymer with a triblock copolymer having terminal polystyrene blocks and a hydrogenated polyisoprene midblock. The two polymers are compounded in a twin-screw extruder at 240 degrees Celsius with a screw speed of 250 revolutions per minute to disperse triblock domains of 10 nm to 15 nm at inter-domain distances of 25 nm to 50 nm. Because the domain diameter remains below one-twentieth of visible light wavelengths, optical scattering stays low while the elastomeric midblock absorbs localized shear energy. The resulting molded part combines optical clarity with resistance to brittle fracture under drop impacts.

Parameter or scale variation

Eight-nanometer block domains with fifteen-nanometer spacing

A toughened polyolefin blend uses a low-molecular-weight aromatic-vinyl and olefin block copolymer with a weight-average molecular weight of 45,000 g/mol and a polydispersity index of 1.15 compounded at 12 wt % into a linear low-density polyethylene matrix. High-shear melt mixing at a shear rate of 1,200 reciprocal seconds and a barrel temperature of 190 degrees Celsius produces spherical block copolymer domains with a mean diameter of 7 nm to 8 nm and an inter-domain distance of 14 nm to 18 nm. Rapid water-bath quenching at a cooling rate of 80 degrees Celsius per second freezes the fine phase morphology before domain coalescence occurs. The higher number density of smaller domains increases the total interfacial area per unit volume and lowers the ductile-to-brittle transition temperature to minus 55 degrees Celsius.

Combination with existing systems

Multilayer coextruded barrier film with toughened skin layers

A five-layer coextruded packaging film integrates the nanoscale domain-dispersed polyolefin resin as two outer structural skin layers bonded through maleic-anhydride-grafted polyethylene tie layers to a central ethylene-vinyl alcohol oxygen-barrier core. Three extruders feed a flat feedblock die at 215 degrees Celsius to form a 120-micrometer sheet in which each 40-micrometer skin layer contains 12 nm block copolymer domains spaced 40 nm apart. During cold-chain handling at minus 20 degrees Celsius, the outer skin layers absorb puncture and flex-crack stresses before cracks reach the brittle barrier core. The central barrier core maintains low gas permeability across the full service temperature range of the laminated structure.

Automated or data-driven variant

Inline scattering feedback control for domain size regulation

A continuous twin-screw compounding line mounts an inline small-angle X-ray scattering sensor and a melt viscosity transducer immediately upstream of the pelletizing die to monitor domain size and inter-domain spacing in real time. A closed-loop controller runs a trained regression model that maps scattering peak positions, melt pressure, and die temperature to predicted domain diameter and spacing values every 2 seconds. When predicted domain diameter drifts outside the 10 nm to 15 nm target band or spacing leaves the 20 nm to 60 nm range, the controller adjusts screw rotation speed, barrel zone heaters, and the gravimetric block copolymer feeder ratio automatically. The feedback loop holds phase morphology within tolerance across feedstock viscosity fluctuations during continuous production runs.

Specific version of a part

Isotactic polypropylene homopolymer matrix resin

The matrix consists of an isotactic polypropylene homopolymer having a melt flow rate of 10 to 30 grams per 10 minutes at 230 degrees Celsius under a 2.16 kilogram load and an isotacticity index above 96 percent. High stereoregularity produces a crystalline spherulitic framework that supplies tensile stiffness and heat deflection resistance. Blending the elastomer domains into this rigid homopolymer base retains structural rigidity while elevating fracture toughness.

Hydrogenated styrene-ethylene-butylene-styrene triblock copolymer

Each dispersed domain consists of a selectively hydrogenated triblock copolymer with polystyrene end blocks and a saturated poly(ethylene-co-butylene) midblock. A styrene content of 13 to 30 weight percent and a number-average molecular weight of 50,000 to 120,000 grams per mole balance domain self-assembly with melt processability. Hydrogenation removes unsaturated double bonds from the olefinic midblock, improving thermal stability during compounding and compatibility with the polyolefin matrix.

High-shear twin-screw compounding for 12 nm domains

A co-rotating twin-screw extruder equipped with kneading block elements operates at 300 to 500 revolutions per minute and a barrel temperature profile of 190 to 220 degrees Celsius to disperse the block copolymer. Matching the melt viscosity ratio between the block copolymer and the polyolefin matrix near unity promotes droplet breakup into uniform spherical domains measuring 11 to 14 nm in diameter. Rapid cooling in an injection mold held at 30 to 50 degrees Celsius freezes the nanoscale morphology before droplet coalescence occurs.

Controlled loading for 35 nm inter-domain spacing

Formulating the blend with 10 to 18 weight percent of the block copolymer relative to the polyolefin matrix sets the mean edge-to-edge distance between adjacent nanoscale domains to 30 to 45 nm. Gravimetric loss-in-weight feeders meter both pellets into the extruder throat within 0.5 percent mass accuracy to keep spatial distribution uniform across the melt. The narrow ligament spacing ensures continuous stress-field overlap between neighboring domains during high-rate impact deformation.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,479,590 B1
Published
Jan 20, 2009
Filed
Jan 3, 2008
Class
D01F 9/12
Document BUS 2013/0123413 A1
Published
May 16, 2013
Filed
Apr 15, 2011
Class
C08L 53/00
Claim 1
Document A
Document B
1.1a matrix region; and a plurality of domain regions dispersed in the matrix region,
Probably the matrix of the heterophasic propylene copolymers form a continuous phase being the matrix of the composition wherein the elastomeric copolymer(s), the styrenic block copolymer (SBC), and optionally the high density polyethylene (HDPE) form together or individually inclusions dispersed therein.
B · US 2013/0123413 A1 · ¶ 30
1.2wherein the matrix region comprises a polyolefin-based resin;
Examples of the organic polymer are polyacetals, polyolefins, polyacrylics, polycarbonates, polystyrenes, polyesters, polyphenylene oxides, polyamides, polyamideimides, polyarylates, polyarylsulfones, polyethersulfones, polyphenylene sulfides, polyvinyl chlorides, polysulfones, polyimides, polyetherimides, polytetrafluoroethylenes, polyetherketones, polyether etherketones, polyether ketone ketones, polybenzoxazoles, polyvinyl ethers, polyvinyl thioethers, polyvinyl alcohols,
A · US 7,479,590 B1 · ¶ 37
Such heterophasic propylene copolymers (HECO's) comprise a matrix being either a propylene homopolymer or a random propylene copolymer in which an elastomeric copolymer is dispersed.
B · US 2013/0123413 A1 · ¶ 2
1.3each of the domain regions comprises a block copolymer comprising an aromatic vinyl-based polymer block and an olefin-based polymer block;
Preferably the styrenic block copolymer (SBC) can be a styrene-ethylene/butylene-styrene (SEBS) block copolymer and/or a hydrogenated styrene-vinyl isoprene (SIS) block rubber.
B · US 2013/0123413 A1 · ¶ 109
1.4a size of the domain region is 10 nm to 15 nm; and
Disclosed herein is a printed circuit board comprising a laminate that comprises a copper foil; inorganic or metallic nanoparticles having an average diameter of less than 100 nanometers disposed on a surface of the copper foil; the nanoparticles being arranged in domains; the domains having average domain sizes of about 10 to about 100 nanometers and average interdomain spacings of 10 to about 1,000 nanometers; the nanoparticles not facilitating the transfer of an electrical
A · US 7,479,590 B1 · abstract
1.5a distance between the each of the domain regions is 20 nm to 60 nm.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.4. Only Document B has a passage for 1.1 1.3. Both have a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

Unfortunately, very smooth copper foils exhibit reduced peel strength when bonded to a polymeric material that is used in a laminate.
A · US 7,479,590 B1 · ¶ 3
It is therefore desirable to provide a single adhesive solution to the peel strength issue currently plaguing smooth copper foils.
A · US 7,479,590 B1 · ¶ 3
However such demanding properties cannot be fulfilled by classical heterophasic propylene copolymers.
B · US 2013/0123413 A1 · ¶ 4
Accordingly, the object of the present invention is to provide a polymer composition exhibiting an impact behavior of at least 5.0 kJ/m2 (Izod notched at −30° C.), a full ductile failure behavior at high speed multiaxial impact test as well as a stiffness (flexural modulus) of at least 1750 MPa.
B · US 2013/0123413 A1 · ¶ 5
Cite aspatent.fyi, US 2026/0365843 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365843/, SHA-256 c2a4b23c98f8225c8a379fc4f09d631291c0f766c582eac42b7a7648f69cd38f
First published
Permanent addresshttps://patent.fyi/US20260365843/
Content fingerprint (SHA-256)c2a4b23c98f8225c8a379fc4f09d631291c0f766c582eac42b7a7648f69cd38f
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi