Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
What ifWhat if the primary resin component is a cycloaliphatic diepoxide containing no aromatic rings?
Claim language“aromatic liquid epoxy resin”
A cycloaliphatic diepoxide such as 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexanecarboxylate provides the primary crosslinkable matrix with low viscosity at 25 °C. During curing at 140 °C to 180 °C with a liquid anhydride hardener and a tertiary amine catalyst, the internal cyclohexyl epoxide rings open to form an aliphatic network. The absence of aromatic rings prevents ultraviolet discoloration while maintaining thermal stability above 200 °C.
1.2Non-epoxy ester plasticizer for flexibility
What ifWhat if the composition omits the second liquid epoxy resin and reduces viscosity and modulus using a non-epoxidized dibenzoate ester plasticizer?
Claim language“at least one liquid epoxy resin A2”
A dipropylene glycol dibenzoate ester with a boiling point above 300 °C blends directly into the aromatic epoxy resin at 10 to 25 parts by weight per 100 parts of resin. The ester solvates the polymer chains during compounding and reduces paste viscosity for pumpable dispensing without participating in epoxide ring-opening reactions. Its low vapor pressure prevents outgassing and bubble formation during curing at 210 °C while increasing elongation at break of the cured seal.
1.3Dicyandiamide and substituted urea curing system
What ifWhat if the latent curing agent is micronized dicyandiamide combined with a substituted urea accelerator rather than a dihydrazide?
Claim language“where the curing agent B is a dihydrazide”
Micronized dicyandiamide with a median particle size below 10 micrometers remains insoluble in the liquid epoxy matrix at storage temperatures up to 55 °C. Adding 1 to 3 percent by weight of a dimethyl-phenyl substituted urea lowers the onset curing temperature from 180 °C to 130 °C. Heating in the curing oven melts and dissolves the dicyandiamide, initiating nitrile and amine addition across the epoxide rings to form a crosslinked thermoset.
1.4Omission of polymeric toughness improver
What ifWhat if the composition contains no polymeric toughness improver and relies on the aliphatic epoxy resin and mineral fillers for mechanical resilience?
Claim language“at least one toughness improver D”
Increasing the proportion of epoxidized polyether polyol within the epoxy blend lowers the crosslink density and glass transition temperature of the cured network. Finely divided precipitated calcium carbonate and fumed silica at 20 to 35 percent by weight deflect propagating microcracks and control thixotropic sag during heating. Eliminating elastomeric polymers lowers paste viscosity and removes high-molecular-weight phases that increase mixing torque.
1.5High aromatic-to-aliphatic resin weight ratio
What ifWhat if the weight ratio of aromatic liquid epoxy resin to aliphatic liquid epoxy resin is between 8.0 and 15.0?
Claim language“(A1/A2) is from 0.25-5.0”
Formulating the resin blend with 89 to 94 percent by weight of aromatic liquid epoxy resin and 6 to 11 percent by weight of aliphatic liquid epoxy resin raises the crosslink density and glass transition temperature above 110 °C. The minor aliphatic fraction reduces paste viscosity enough for automated bead extrusion at 40 °C without softening the cured network. The resulting high-modulus thermoset withstands high shear loads in structural metal-to-metal joints.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Potting compound for electric motor stator windings
The one-component epoxy composition serves as a thermally conductive potting material for encapsulating copper windings in electric motor stators. Liquid aromatic diglycidyl ether and aliphatic polyol glycidyl ether resins at an aromatic-to-aliphatic weight ratio of 1.5 are blended with a micronized dihydrazide curing agent, core-shell rubber particles, and 45 weight percent fused silica filler. The uncured paste flows into stator slots under vacuum at 50 °C to displace trapped air and wet the enameled wire bundles. Heating the potted assembly in a convection oven at 180 °C for 45 minutes crosslinks the resin matrix without outgassing voids, yielding a crack-resistant dielectric barrier.
Component substitution
Latent dicyandiamide curing agent with encapsulated amine
A micronized dicyandiamide hardener replaces the dihydrazide curing agent in the one-component aromatic and aliphatic epoxy resin blend. Dicyandiamide powder with a median particle diameter below 5 micrometers is dispersed at 6 parts per hundred resin alongside 2 parts per hundred resin of a thermally rupturable microencapsulated tertiary amine catalyst. During storage at 55 °C, the crystalline dicyandiamide remains insoluble in the liquid resin mixture and the polymer shell isolates the catalyst from the epoxy groups. Exposure to 190 °C melts the microcapsule walls and dissolves the dicyandiamide, initiating rapid ring-opening polymerization across the aromatic and aliphatic epoxy network.
An epoxidized linseed oil having an average of 5.5 oxirane rings per triglyceride molecule replaces the synthetic aliphatic glycidyl ether component in the resin blend. The epoxidized triglyceride is mixed with liquid bisphenol F diglycidyl ether at an aromatic-to-aliphatic weight ratio of 2.0, along with a blocked polyurethane toughener and isophthalic dihydrazide. Because the internal oxirane groups on the fatty acid chains react more slowly than terminal glycidyl ethers, the composition exhibits extended viscosity stability during 60 °C storage. At a curing temperature of 210 °C, the dihydrazide opens both the terminal aromatic and internal triglyceride oxirane rings to form a flexible, hydrophobic crosslinked network.
Parameter or scale variation
High aromatic ratio formulation for structural rigidity
The weight ratio of the liquid aromatic epoxy resin to the liquid aliphatic epoxy resin is increased to a range of 6.0 to 12.0 to raise the glass transition temperature and tensile modulus. The formulation combines 72 parts by weight of bisphenol A diglycidyl ether, 8 parts by weight of 1,6-hexanediol diglycidyl ether, 12 parts by weight of a carboxyl-terminated butadiene-acrylonitrile adduct, and 8 parts by weight of sebacic dihydrazide. Curing proceeds in a two-stage thermal profile consisting of 20 minutes at 160 °C followed by 30 minutes at 220 °C to achieve full conversion without thermal runaway. The resulting cured network exhibits a glass transition temperature above 135 °C while retaining bubble-free cross-sections in bondlines up to 4 millimeters thick.
Combination with existing systems
Induction-cured seam sealant with ferromagnetic filler particles
The one-component epoxy resin composition integrates with a high-frequency electromagnetic induction heating system by incorporating 15 to 25 weight percent iron oxide susceptor particles. Magnetite particles with a diameter of 1 to 10 micrometers are dispersed uniformly into the blend of aromatic epoxy, aliphatic epoxy, dihydrazide hardener, and blocked polyurethane toughener via a three-roll mill. After automated bead extrusion onto overlapping sheet metal flanges, an induction coil operating at 25 kilohertz induces eddy currents and hysteresis heating directly within the sealant layer. Internal heat generation raises the bead core to 195 °C within 15 seconds, initiating rapid partial gelation that holds the joint geometry prior to downstream thermal baking.
Automated or data-driven variant
Closed-loop dispensing with inline dielectric cure monitoring
A robotic metering and dispensing cell applies the one-component epoxy composition using real-time viscosity feedback from an inline ultrasonic sensor and a regression model. As barrel temperature fluctuates between 40 °C and 55 °C, the control algorithm adjusts positive-displacement pump pressure and nozzle travel speed to maintain a constant bead cross-section of 3.0 millimeters. During the thermal curing stage, an interdigitated dielectric sensor embedded in a witness coupon measures ion viscosity continuously as the dihydrazide crosslinks the resin blend. A supervisory controller compares the measured log ion viscosity curve against a target cure profile and modulates oven zone temperatures to hold peak curing exotherm below 210 °C.
Specific version of a part
Bisphenol-A and bisphenol-f liquid epoxy blend
The aromatic liquid epoxy resin A1 consists of a 70:30 weight mixture of liquid bisphenol-A diglycidyl ether and liquid bisphenol-F diglycidyl ether. Blending the bisphenol-F fraction lowers the dynamic viscosity at 25 °C from 12 Pa·s to 6 Pa·s and suppresses crystallization during cold storage. Both resins carry an average of 1.9 to 2.0 epoxy groups per molecule with a molar mass per epoxy group of 170 to 190 g/mol.
Epoxidized polypropylene glycol diglycidyl ether
The aliphatic liquid epoxy resin A2 is a diglycidyl ether of a difunctional polypropylene glycol with a number-average molecular weight of 400 to 650 g/mol. The flexible ether backbone lowers the glass transition temperature of the cured matrix and increases elongation at break above 15 percent. Its low vapor pressure at 210 °C prevents volatile release and void formation during high-temperature baking.
Micronized adipic acid dihydrazide curing agent
The curing agent B is jet-milled adipic acid dihydrazide having a melting point of 180 °C and a particle size distribution with D90 below 15 micrometers. The fine crystalline powder disperses uniformly in the liquid epoxy phase and remains chemically inert during storage at 50 °C to 60 °C for several weeks. When the applied bead reaches 170 °C to 210 °C, the dihydrazide melts and its four active amino-hydrogen atoms react with epoxide rings to crosslink the matrix.
The toughness improver D is a terminally blocked polyurethane polymer prepared by reacting a polytetramethylene ether glycol of 2000 g/mol molecular weight with hexamethylene diisocyanate and capping the terminal isocyanate groups with o,o'-diallylbisphenol A. The blocked prepolymer dissolves in the epoxy blend at 10 to 20 percent by weight without premature reaction during warm storage. Upon heating above 160 °C, the phenolic blocking groups react into the epoxy network and phase-separate into flexible domains that absorb impact energy.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a) at least one liquid epoxy resin A1 having an average of more than one epoxy group per molecule, that is an aromatic liquid epoxy resin;
The coating composition may, if desired, contain reactive additives or coupling agents in addition to the blocked polyurethane prepolymer such, for example, other types of blocked or microencapsulated isocyanates (e.g., oxime-blocked hexamethylene diisocyanate trimer), epoxy resins (e.g., glycidyl ethers of polyphenols such as diglycidyl ethers of bisphenol A or bisphenol F), polyaminoamides (e.g., the reaction products of polymerized or dimerized fatty acids and epoxy resins
A · US 7,019,102 B2 · ¶ 24
In addition to the polyfunctional aliphatic glycidyl ether compounds having a total chlorine amount of less than 0.7% by mass, the thermosetting resin composition of the present invention may be blended with epoxy compounds having at least two epoxy groups in one molecule as a thermosetting component in order to improve the adhesion with a substrate.
B · US 2009/0093595 A1 · ¶ 70
1.2b) at least one liquid epoxy resin A2 having an average of more than one epoxy group per molecule, that is selected from the group consisting of: glycidyl ethers of difunctional saturated, branched or unbranched, cyclic or open-chain C2-C30 alcohols; glycidyl ethers of tri- or polyfunctional, saturated, branched or unbranched, cyclic or open-chain alcohols; and epoxidized di- or trifunctional polyether polyols;
The thermosetting resin composition of the invention comprises (A) a thermosetting resin, preferably a carboxyl group containing resin, and (B) a polyfunctional aliphatic glycidyl ether compound having a total chlorine amount of less than 0.7% by mass.
B · US 2009/0093595 A1 · abstract
1.3c) at least one curing agent B for epoxy resins, where the curing agent B is a dihydrazide; and
known and usual curing agents or curing accelerators such as an equimolar reactant of phenyl isocyanate and dimethyl amine, equimolar reactants of dimethyl amine and organic polyisocyanates such as tolylene diisocyanate or isophorone diisocyanate.
B · US 2009/0093595 A1 · ¶ 87
1.4d) at least one at least one toughness improver D selected from the group consisting of terminally blocked polyurethane polymers D1, liquid rubbers D2 and core-shell polymers D3,
Blocked polyurethane prepolymers obtained by reacting at least one polyol, a first polyisocyanate comprising diphenylmethane diisocyanate, a second polyisocyanate having a viscosity at 25° C. of less than about 250 mPa·s, a phenol blocking agent, and an oxime blocking agent, wherein the weight ratio of second polyisocyanate:first polyisocyanate is not more than 0.65:1.
A · US 7,019,102 B2 · abstract
1.5wherein the weight ratio of the at least one liquid epoxy resin A1 to the at least one liquid epoxy resin A2 (A1/A2) is from 0.25-5.0.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.4. Only Document B has a passage for 1.21.3. Both have a passage for 1.1.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
That is, it would be highly desirable to develop blocked polyurethane prepolymers that not only are sufficiently low in viscosity to enable the prepolymers and coating compositions containing such prepolymers to be applied easily to substrate surfaces by spraying but also exhibit good stability during storage (e.g., no phase separation).
A · US 7,019,102 B2 · ¶ 4
Such compositions are relatively low in viscosity, are comparatively inexpensive to produce, are storage-stable, and are capable of providing cured coatings upon heating that are highly adhesive and chip-resistant.
A · US 7,019,102 B2 · ¶ 2
However, conventional polyfunctional aliphatic glycidyl ether compounds contain about 5 to 20% by mass of chlorine and thereby have problems that defect in curing is caused or corrosion of copper wirings is caused by the influence of chlorine impurities to lower the electric insulating properties.
B · US 2009/0093595 A1 · ¶ 3
The present invention is intended to solve the problems associated with the prior arts, and it is an object of the invention to provide a thermosetting resin composition having excellent low temperature curing properties, tack properties, flexibility and electric properties.
B · US 2009/0093595 A1 · ¶ 11