patent.fyi
Applications  /  US 2026/0365846
United States Patent Application Publication

US 2026/0365846 A1

Published
Nov 19, 2026
Filed
Oct 31, 2023
Earliest date on the face
Oct 31, 2022
Classification
C08L 67/02
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Aromatic tetracarboxylic dianhydride chain extender

What ifWhat if the composition uses a small-molecule aromatic tetracarboxylic dianhydride in place of an acrylic styrene copolymer?
Claim language“an acrylic styrene copolymer”

Pyromellitic dianhydride dosed at 0.1 to 0.8 wt % reacts with terminal hydroxyl groups on recycled polyethylene terephthalate chains during melt processing at 270 to 290 °C. Each dianhydride molecule couples two polyester chains through ester linkages and forms pendant carboxyl groups that undergo further condensation under vacuum devolatilization. This coupling raises intrinsic viscosity from 0.65 dL/g to above 0.80 dL/g within a melt residence time of 1 to 3 minutes.

1.1High-density fluorinated copolymer above 1.45

What ifWhat if the acrylic styrene copolymer has a specific gravity of 1.45 to 1.65 rather than a specific gravity of 0.9 to 1.4?
Claim language“a specific gravity of 0.9 to 1.4”

Copolymerizing 2,2,2-trifluoroethyl methacrylate, glycidyl methacrylate, and styrene produces a fluorinated acrylic styrene copolymer with a solid specific gravity of 1.45 to 1.65. The pendant glycidyl groups react with recycled polyester end groups at 270 to 285 °C to rebuild chain length and intrinsic viscosity. The elevated density closely matches heavy recycled polyester flake streams in gravimetric hoppers and limits segregation during dry blending.

1.2Porous mineral powder carrier

What ifWhat if the reactive copolymer is supported on a porous inorganic mineral powder in place of a carrier resin?
Claim language“a carrier resin”

Precipitated amorphous silica particles with a pore volume of 1.2 to 1.8 cm³/g absorb molten or solution-applied reactive copolymer at a 50 to 70 wt % active loading to form a free-flowing dry powder. Gravimetric loss-in-weight feeders meter this mineral-supported concentrate directly into the recycled polyester feed throat at 0.5 to 1.5 wt %. Melt shear in the extruder releases the copolymer from the silica pores to extend the polyester chains while the dispersed silica acts as a nucleating and anti-blocking agent.

1.2Neat compacted additive pastilles without carrier

What ifWhat if the composition consists of neat compacted pastilles of the reactive copolymer with no carrier resin?
Claim language“a carrier resin”

A chilled steel belt flaker or rotary dropformer solidifies molten reactive copolymer at 100 wt % active concentration into uniform dust-free pastilles measuring 2 to 4 mm in diameter. A micro-dosing gravimetric feeder meters the neat pastilles into the main extruder hopper at 0.2 to 1.0 wt % relative to the recycled polyester stream. Because the copolymer melts near 80 to 110 °C, it liquefies early in the feed section and coats the polyester flakes before full plastication occurs.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Masterbatch dosing in recycled polyester textile fiber spinning

A melt-spinning line blends a masterbatch containing an acrylic styrene copolymer with a specific gravity of 1.05 and a polybutylene terephthalate carrier resin into post-consumer polyethylene terephthalate flakes at a 2.5 weight percent letdown ratio. The blended stream enters a single-screw extruder at 280 degrees Celsius and passes through a melt gear pump and a 20-micrometer sintered metal filter pack before reaching a multi-hole spinneret. The acrylic styrene copolymer increases melt elasticity and stabilizes melt viscosity during high-speed drawdown at 3,200 meters per minute, reducing filament breaks during continuous multifilament yarn production. Drawn filaments pass over heated godet rollers at 110 degrees Celsius and wind onto bobbins as continuous textile yarn.

Masterbatch formulation for recycled polyester additive manufacturing filament

A filament extrusion line blends a masterbatch of acrylic styrene copolymer with a specific gravity of 1.08 in a glycol-modified polyester carrier resin into ground post-consumer polyester bottle flake at a 3.0 weight percent dosing ratio. The compound melts in a single-screw extruder equipped with a static mixer at 255 degrees Celsius and exits a 2.2-millimeter circular die into a two-stage water bath held at 60 degrees Celsius and 25 degrees Celsius. A dual-axis laser micrometer monitors filament diameter at 1.75 millimeters plus or minus 0.03 millimeters and regulates the haul-off capstan speed to maintain dimensional stability. The acrylic styrene copolymer raises melt strength during extrusion and reduces inter-layer warping when the spooled filament is deposited through a 0.4-millimeter heated nozzle at 245 degrees Celsius.

Component substitution

Epoxy-functionalized terpolymer substituted for acrylic styrene copolymer

A masterbatch replaces the acrylic styrene copolymer with a random terpolymer of styrene, methyl methacrylate, and glycidyl methacrylate having a specific gravity of 1.14 and an epoxide group concentration of 3.2 millimoles per gram. The terpolymer is compounded at 25 weight percent into a polyolefin elastomer carrier resin using a co-rotating twin-screw extruder operating at 195 degrees Celsius to prevent premature crosslinking of epoxide groups inside the pellets. When metered at 1.5 weight percent into reclaimed polyethylene terephthalate during sheet extrusion at 275 degrees Celsius, the epoxide rings react with terminal carboxyl and hydroxyl groups on degraded polyester chains. This chain-extension reaction rebuilds molecular weight and raises intrinsic viscosity during a melt residence window of 90 to 150 seconds.

Parameter or scale variation

High-loading masterbatch pellets with elevated copolymer concentration

A concentrated masterbatch contains 40 weight percent acrylic styrene copolymer and 60 weight percent amorphous copolyester carrier resin, where the copolymer comprises 70 weight percent n-butyl acrylate and 30 weight percent styrene with a specific gravity of 1.04. Compounding takes place in a twin-screw extruder with a length-to-diameter ratio of 40 at a barrel temperature profile of 175 to 215 degrees Celsius and a screw speed of 280 revolutions per minute. An underwater pelletizer cuts the extruded strands into spherical micro-pellets measuring 1.5 millimeters in diameter with a bulk density of 0.78 grams per cubic centimeter. Downstream converters meter these micro-pellets at 0.5 to 0.8 weight percent into recycled polyester feed streams, lowering carrier resin dilution and cutting masterbatch storage volume by half.

Combination with existing systems

Masterbatch integration with vacuum solid-state polycondensation reactors

A recycled polyester pelletizing line pairs a gravimetric masterbatch feeder with a twin-screw degassing extruder and a downstream continuous solid-state polycondensation reactor. The masterbatch containing 15 weight percent acrylic styrene copolymer in a crystalline polyester carrier is dosed into dried post-consumer flake at the extruder throat while a two-stage vacuum pump maintains 5 millibars of absolute pressure on the melt devolatilization zones. Extruded strands are pelletized, crystallized at 165 degrees Celsius in a fluidized bed crystallizer, and fed into a vertical moving-bed reactor operating at 210 degrees Celsius under a countercurrent dry nitrogen purge for 8 hours. The copolymer reduces thermal chain scission and yellowing during extrusion, supplying uniform pre-polymer pellets with consistent carboxyl end-group concentrations to the solid-state reactor.

Automated or data-driven variant

Closed-loop masterbatch dosing controlled by inline melt rheometry

A recycled polyester extrusion line incorporates an inline slit-die capillary rheometer, a spectrophotometric color sensor mounted over the melt stream, and a loss-in-weight gravimetric feeder for the acrylic styrene copolymer masterbatch. The rheometer samples apparent melt viscosity every 15 seconds while the optical sensor records continuous yellowness index values through a sapphire melt window. A programmable logic controller running a multivariable model predictive control algorithm compares real-time viscosity and color readings against target setpoints and adjusts the masterbatch feeder screw speed between 0.8 and 3.5 weight percent dosing. The controller uses upstream hopper moisture and flake bulk-density readings to compensate for feedstock batch transitions before off-specification resin reaches the die.

Specific version of a part

Epoxy-functionalized styrene-acrylate random copolymer

Continuous bulk free-radical polymerization at 180 to 220 °C reacts 40 to 55 wt % styrene, 20 to 35 wt % butyl acrylate, and 15 to 30 wt % glycidyl methacrylate to produce a random copolymer with a weight-average molecular weight of 5,000 to 12,000 g/mol. The solid copolymer has a specific gravity of 1.12 to 1.18 and an epoxy group concentration of 2.8 to 4.0 mmol/g. During melt processing of recycled polyethylene terephthalate at 270 to 285 °C, the pendant glycidyl rings open to form covalent ester and ether linkages with degraded chain ends.

Anhydride-functionalized methyl methacrylate styrene copolymer

Solution free-radical polymerization combines styrene, methyl methacrylate, and maleic anhydride at a weight ratio of 50:35:15 to form a copolymer with a specific gravity of 1.15 and a glass transition temperature of 105 °C. The cyclic anhydride rings react with terminal hydroxyl groups on recycled polyester chains at 265 to 285 °C to create ester bonds and increase melt viscosity. The aliphatic-aromatic backbone withstands polyester extrusion temperatures without generating conjugated yellowing chromophores.

Amorphous glycol-modified polyethylene terephthalate carrier

An amorphous glycol-modified polyethylene terephthalate resin with an intrinsic viscosity of 0.58 to 0.65 dL/g and a glass transition temperature of 78 °C forms the carrier matrix. Its low melt viscosity at 220 to 240 °C allows melt compounding with the reactive copolymer below the onset temperature of rapid premature crosslinking. Because the carrier shares the polyester ester repeat structure, it disperses uniformly into recycled polyethylene terephthalate hosts without phase separation or optical haze.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 2008/0160436 A1
Published
Jul 3, 2008
Filed
Nov 13, 2007
Class
G03G 13/04
Document BUS 8,709,609 B2
Published
Apr 29, 2014
Filed
Dec 14, 2010
Class
B32B 23/08
Claim 1
Document A
Document B
1.1an acrylic styrene copolymer having a specific gravity of 0.9 to 1.4; and
In the polymerization step are performed a polycondensation step in which a polyvalent carboxylic acid and a polyvalent alcohol are polycondensated within the oil-droplets dispersed in the aqueous medium to form a polyester resin, and a radical copolymerization step in which a styrene compound and a (meta)acrylic acid ester compound are radical-copolymerized to form a styrene-acryl resin; and the polyester resin and the styrene-acryl resin are high-homogeneously mixed to obta
A · US 2008/0160436 A1 · ¶ 75
The resin (a) is a styrene acrylic resin obtainable as the polymerization product of a monomer mixture comprising: styrene in an amount of up to 40 wt. %, preferably of from 10 to 40 wt. % and more preferably of from 20 to 30 wt. %, based on total monomers; and, one or more acrylic monomers such as (meth)acrylic acid, (meth)acrylic monomers containing a hydroxyl group, (meth)acrylic acid esters and (meth)acrylonitrile.
B · US 8,709,609 B2 · ¶ 33
1.2a carrier resin.
Preferred carriers include resin-coated carrier in which the surface of magnetic particles is covered with resin and a resin dispersion type carrier in which magnetic particle are dispersed in resin. Resins constituting the resin coated carrier are not specifically limited but an olefin resin, a styrene resin, a styrene/acryl resin, a silicone resin, an ester resin, and a fluorine-containing polymer resin are usable.
A · US 2008/0160436 A1 · ¶ 126

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.2. Both have a passage for 1.1.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

As one of such particulate resins constituting a polymerization toner is cited particulate styrene-acryl resin.
A · US 2008/0160436 A1 · ¶ 4

Related claim parts: 1.1

A styrene-acryl resin, which exhibits a relatively low softening point due to its non-crystalline structure, is suitably used for a toner which is desired to be fixed at a relatively low temperature, a so-called low-temperature fixable toner.
A · US 2008/0160436 A1 · ¶ 5

Related claim parts: 1.1

However, a toner using a styrene-acryl resin exhibits superior low temperature fixability but is inferior in fixing strength, having problems that when a force such as bending or abrasion is applied onto a fixed toner image on a transfer material, this influence renders it difficult to maintain a stable toner image.
A · US 2008/0160436 A1 · ¶ 6
In view of the foregoing, there has been studied development of a toner having advantages of both of a styrene-acryl resin and a polyester resin.
A · US 2008/0160436 A1 · ¶ 8
Wood substrates, in particular, contain a number of water-soluble, chromophoric staining agents: of these, tannins and lignin can readily leach from the substrate into an aqueous coating, causing staining which appears as discolouration on the surface of the coating.
B · US 8,709,609 B2 · ¶ 5
As a consequence, it has become desirable to develop stain-blocking aqueous coating compositions which did not contain reactive pigments.
B · US 8,709,609 B2 · ¶ 8
Cite aspatent.fyi, US 2026/0365846 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365846/, SHA-256 bcc3c5cdde814f29432e9fffd47c8fcb15b4001bc2653963a1c1eb5ebdf72b27
First published
Permanent addresshttps://patent.fyi/US20260365846/
Content fingerprint (SHA-256)bcc3c5cdde814f29432e9fffd47c8fcb15b4001bc2653963a1c1eb5ebdf72b27
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi