Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.1Virgin polyethylene terephthalate feed
What ifWhat if virgin polyethylene terephthalate supplies the entire polyethylene terephthalate fraction of the blend?
Claim language“20-80 wt % of recycled polyethylene terephthalate”
Dry virgin polyethylene terephthalate pellets and copolyester pellets separately, then meter both feeds into the extruder. The polyethylene terephthalate supplies a crystallizable fraction that contributes stiffness to the molded wall.
1.4Solid state molecular weight increase
What ifWhat if solid state polycondensation raises the molecular weight of the recycled polyethylene terephthalate before blending, with no chain extending agent in the blend?
Claim language“a chain extending agent”
Crystallize the recycled polyethylene terephthalate pellets and hold them at about 210 °C under a dry nitrogen purge. The purge removes volatile condensation products as polyester end groups react, increasing molecular weight and melt viscosity before the pellets enter the blend extruder.
1.8Lower viscosity with rapid capture
What ifWhat if the blend has a melt viscosity of 8,000 to 9,000 poise at 1 rad/s and 260 °C and the mold captures a short parison immediately after extrusion?
Claim language“10,000 to 120,000 poise”
An accumulator head discharges the short parison rapidly, and the mold closes as soon as the parison reaches the pinch-off lands. The short hanging time and low suspended mass limit sag before inflation.
1.10Translucent wall with light scattering
What ifWhat if the wall has 40% to 60% haze and transmits enough light to show the liquid level?
Claim language“a haze value of 20% or less”
Meter a polyester masterbatch containing fine silica into the blend and disperse the particles during extrusion. Adjust silica loading using haze and total light transmission measured on molded wall samples, and check liquid-level visibility under side lighting.
1.11Thicker wall with extended cooling
What ifWhat if the article uses a 5 to 6 mm body wall to provide bending stiffness?
Claim language“a thickness of from 0.2-4 mm”
Program the annular die gap along the parison to feed additional material into sections that stretch farther during inflation. Circulate chilled water through the mold and extend the closed-mold cooling time until the wall holds its shape during ejection.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Transparent float for a sight gauge
Extrusion blow mold a closed cylindrical float from the recycled polyethylene terephthalate and copolyester blend using a split mold with pinch lands at both ends. Introduce inflation air through a sacrificial neck and heat seal the neck after withdrawing the blow pin. Fit the float with a colored indicator ring and size it to slide inside the bore of a vertical sight gauge. The float rises and falls with the liquid level while the ring provides a visible reference.
Component substitution
Oxazoline chain extension during compounding
Use 1,3-phenylene bis(2-oxazoline) as the chain extending agent in a blend of dried recycled polyethylene terephthalate and dried copolyester. Meter the bisoxazoline into a twin-screw extruder after the two polymers melt. The oxazoline groups react with polyester carboxyl end groups and couple chains. Adjust the feed rate using the measured carboxyl end-group concentration and melt viscosity, then feed the compounded melt to the blow molding head.
Parameter or scale variation
Cooling by separate mold zones
Build a split mold with separate water circuits for the shoulder, sidewall and base of a hollow article. Target a 1.0 mm sidewall and a 2.5 mm base, and use a wider die gap during extrusion of the parison segment that forms the base. Start with water inlet temperatures of 20 °C at the shoulder and sidewall and 12 °C at the base. Adjust the base water flow using the surface temperature at demolding and the flatness of the cooled base.
Four cavity molding with matched heads
Feed four annular extrusion heads from a common melt manifold and align each head with one cavity of a four-cavity split mold. Set each head to deliver a 40 g parison per cycle and weigh the four parisons separately during setup. Adjust the restrictor in each manifold branch until the parison masses match within 2%. Fit each cavity with a dedicated blow pin and trigger the four inflation valves from the same mold-closed signal.
Combination with existing systems
Inline recovery of molding trim
Connect the blow molding trimmer to an enclosed conveyor that feeds a low-speed granulator. Screen the granulate, remove fines, and dry the retained material in a desiccant hopper before returning it to the extruder through a separate gravimetric feeder. Calculate the recycled polyethylene terephthalate and copolyester already present in the trim when setting the fresh polymer feed rates. Adjust the fresh chain extender feed using the melt viscosity measured after compounding.
Automated or data-driven variant
Wall thickness feedback for parison control
Mount opposing optical displacement sensors at an inspection station downstream of trimming and cooling to measure the outer and inner surfaces of the open article. Calculate wall thickness at selected heights and register each height to a segment of the parison die-gap program. Apply bounded corrections to the corresponding die-gap setpoints using thickness measurements averaged over several articles. The controller sends the updated program to the die actuator for the next production interval.
Specific version of a part
Neopentyl glycol modified terephthalate blend
Use 40 wt % copolyester in the blend. Use 100 mole % terephthalic acid residues in its acid component and 80 mole % ethylene glycol residues and 20 mole % neopentyl glycol residues in its glycol component.
Copolyester with intermediate inherent viscosity
Use copolyester with an inherent viscosity of 0.75 dL/g. Dissolve 0.50 g of the resin per 100 mL of 60/40 by weight phenol/tetrachloroethane and measure the solution and solvent flow times in a capillary viscometer at 25 °C.
Copolyester with an 85 °C transition
Select a terephthalate copolyester with ethylene glycol and 1,4-cyclohexanedimethanol residues and a glass transition midpoint of 85 °C. Measure the midpoint of the heat capacity step by differential scanning calorimetry on a second heating scan at 10 °C per minute after controlled cooling.
Melting peak at 247 °C
Use recycled polyethylene terephthalate as the crystallizable phase and select an amorphous copolyester for the other polymer fraction. Heat a cut section of the molded wall at 10 °C per minute in a differential scanning calorimeter and use the first heating peak at 247 °C as the melting temperature.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1(1) 20-80 wt % of recycled polyethylene terephthalate (rPET) and
Examples of polymers which are water non-dispersible that may be blended with the sulfopolyester include, but are not limited to, polyolefins, such as homo- and copolymers of polyethylene and polypropylene; poly(ethylene terephthalate); poly(butylene terephthalate); and polyamides, such as nylon-6; polylactides; caprolactone;
A · US 2011/0091513 A1 · ¶ 90
1.2(2) 20-80 wt % of at least one copolyester which comprises: (a) a dicarboxylic acid component comprising: i) 70 to 100 mole % of terephthalic acid residues; ii) 0 to 30 mole % of aromatic and/or aliphatic dicarboxylic acid residues having up to 20 carbon atoms; and iii) 0 to 5 mole % of a branching monomer; and (b) a glycol component comprising: i) 0 to 35 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; ii) 0 to 50 mole % of 1,4-cyclohexanedimethanol residues, iii) 0 to 50 mole % of neopentyl glycol residues; iv) 0 to 35 mole % of other modifying glycols residues; v) up to 98 mole % of ethylene glycol residues; and vi) 0 to 5 mole % of a branching monomer; and
More specifically, the dicarboxylic portion of the sulfopolyester comprises between about 60-80 mole % terephthalic acid, about 0-30 mole % isophthalic acid, and about 4-20 mole % 5-sodiosulfoisophthalic acid (5-SSIPA). The diol portion comprises from about 0-50 mole % diethylene glycol and from about 50-100 mole % ethylene glycol.
A · US 2011/0091513 A1 · ¶ 121
(A) at least one polyester which comprises: (a) a dicarboxylic acid component comprising: i) 70 to 100 mole % of terephthalic acid residues; ii) 0 to 30 mole % of aromatic dicarboxylic acid residues having up to 20 carbon atoms; and iii) 0 to 10 mole % of aliphatic dicarboxylic acid residues having up to 16 carbon atoms; and (b) a glycol component comprising: i) 1 to 99 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and ii) 1 to 99 mole % of 1,4-cyclohexanedimeth
B · US 2013/0072628 A1 · ¶ 255
1.3wherein the total mole % of the dicarboxylic acid component is 100 mole %, and the total mole % of the glycol component is 100 mole %; and
In a particularly preferred embodiment, the sulfopolyester comprises from about 80-96 mole % dicarboxylic acid residues, from about 4 to about 20 mole % sulfomonomer residues, and 100 mole % diol residues (there being a total mole % of 200%, i.e., 100 mole % diacid and 100 mole % diol).
A · US 2011/0091513 A1 · ¶ 121
wherein the total mole % of the dicarboxylic acid component is 100 mole %, and the total mole % of the glycol component is 100 mole %; and wherein the inherent viscosity of said polyester is from 0.10 to 1.2 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.25 g/50 ml at 25° C.
B · US 2013/0072628 A1 · ¶
1.4(3) 0.05 to 5 weight % of a chain extending agent based on the weight of the blend;
1.5wherein the blend has 1-15 wt % total comonomer content from glycols and acids other than ethylene glycol (EG), terephthalic acid (TPA), or dimethyl terephthalate (DMT);
1.6wherein the inherent viscosity of the copolyester is 0.50 to 1.2 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.5 g/100 ml at 25 °C;
The sulfopolyesters described herein have an inherent viscosity, abbreviated hereinafter as “Ih.V.”, of at least about 0.1 dL/g, preferably about 0.2 to 0.3 dL/g, and most preferably greater than about 0.3 dL/g, measured in a 60/40 parts by weight solution of phenol/tetrachloroethane solvent at 25° C. and at a concentration of about 0.5 g of sulfopolyester in 100 mL of solvent.
A · US 2011/0091513 A1 · ¶ 77
(b) a glycol component comprising: i) greater than 81 to 99 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and ii) 1 to less than 19 mole % of 1,4-cyclohexanedimethanol residues, wherein the total mole % of the dicarboxylic acid component is 100 mole %, and the total mole % of the glycol component is 100 mole %; and wherein the inherent viscosity of said polyester is from 0.35 to 1.2 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration
B · US 2013/0072628 A1 · ¶ 184
1.7wherein the copolyester has a Tg of 70 to 115 °C;
The sulfopolyester has a glass transition temperature of at least 57° C. which greatly reduces blocking and fusion of the fiber during winding and long term storage.
A · US 2011/0091513 A1 · ¶ 32
1.8wherein the rPET/copolyester blend has a melt viscosity at 1 rad/s and 260 °C of 10,000 to 120,000 poise;
In another aspect, the sulfopolyester exhibits a melt viscosity of between about 1000-12000 poise, more preferably between 2000-6000 poise, and most preferably between 2500-4000 poise measured at 240° C. and 1 rad/sec shear rate.
A · US 2011/0091513 A1 · ¶ 118
In one embodiment, the melt viscosity of the polyester(s) useful in the invention is less than 30,000 poise as measured a 1 radian/second on a rotary melt rheometer at 290° C.
B · US 2013/0072628 A1 · ¶ 472
1.9wherein the article has a melting temperature (Tm) of 225-255 °C;
1.10wherein the article has a haze value of 20% or less; and
1.11wherein the article has a thickness of from 0.2-4 mm;
1.12wherein the article has a crystallization half time of about 1 minute to about 20 minutes at 180 °C; and wherein the article is transparent; or wherein the article is recyclable in a PET recycle stream.
Initially, the sample was visually clear with high light transmission and became opaque as the sample crystallized. The crystallization half-time was recorded as the time at which the light transmission was halfway between the initial transmission and the final transmission.
B · US 2013/0072628 A1 · ¶ 516
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.11.7. Only Document B has a passage for 1.12. Both have a passage for 1.21.31.61.8.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
Also, it is desirable for the polyester resins to exhibit good heat resistance.
B · US 2013/0072628 A1 · ¶ 3
Related claim parts: 1.7
The fibers and fibrous articles have applications in flushable personal care products and medical products.
A · US 2011/0091513 A1 · ¶ 2
The desirability of flushable personal care products has resulted in a need for fibers, nonwovens, and other fibrous articles with various degrees of water-responsivity.
A · US 2011/0091513 A1 · ¶ 4
A need also exists in the art for a diol component that is not EG-based but is capable of providing good water dispersibility.
B · US 2013/0072628 A1 · ¶ 6
The advantage of such a solution is to either improve the water dispersibility of such a polymer compared to other non-EG-based glycol modified polyesters, or retain an equivalent level of water dispersibility with a lower amount of hydrophilic groups, thereby improving the water resistance of the coating.
B · US 2013/0072628 A1 · ¶ 6