United States Patent Application Publication

US 2026/0365849 A1

Published
Nov 19, 2026
Filed
Jul 18, 2023
Earliest date on the face
Jul 21, 2022
Classification
C08L 75/06
First published here
Nov 23, 2026

Generated automatically. Not reviewed by a person. Not legal advice or an opinion.

Section 1 · machine-generated

What if?

Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.

1.1Liquid casting and curing

What ifWhat if the rubber component forms in the seal mold from a pourable reactive mixture?
Claim language“a millable rubber material”

A liquid polyester polyol reacts with a multifunctional isocyanate in the mold to form a crosslinked polyurethane seal. Water splits ester bonds in the cured network, reducing its strength until the seal breaks apart.

1.1Water soluble segment joints

What ifWhat if water breaks the seal into pieces by dissolving joints between silicone rubber segments?
Claim language“hydrolyzable rubber molecules”

Compression holds interlocking silicone segments together against the sealing surface, and water soluble polyvinyl alcohol pins retain the segments in a ring. Water enters channels on the exposed face and dissolves the pins, releasing the individual segments when the sealing load is removed.

1.2Liquid acid in channels

What ifWhat if molded channels supply the hydrolysis accelerator as a liquid acid solution?
Claim language“a powder exhibiting acidic properties upon contact with water”

Channels behind the sealing face hold an aqueous acetic acid solution behind water soluble plugs. Incoming water dissolves the plugs and carries the acid along the channel walls, where it accelerates ester bond cleavage in the rubber.

1.2Carbonate driven ester hydrolysis

What ifWhat if a basic powder drives hydrolysis of the rubber molecules?
Claim language“an acidic hydrolysis accelerator”

Dispersed sodium carbonate dissolves as water enters the rubber and raises the pH of the absorbed water. Hydroxide ions cleave ester bonds in the polyester segments, reducing network connectivity and tear strength.

1.3Lower loading with short diffusion paths

What ifWhat if the rubber contains 25 parts by mass of citric acid powder per 100 parts by mass of the rubber component?
Claim language“40 parts by mass or more”

Blind channels on the wetted face leave thin rubber webs behind a continuous sealing lip. Water reaches each web from the adjoining channels and dissolves the acid within it, accelerating ester cleavage across the short distance through the web.

Section 2 · machine-generated

Variations

Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.

Other field of use

Temporary plug for irrigation laterals

A compression-molded plug consists of millable polyester rubber compounded with 50 parts by mass of powdered citric acid per 100 parts by mass of rubber. A shoulder in a drip irrigation lateral supports the plug while it closes a flush outlet during initial watering. Repeated wetting dissolves the acid and promotes hydrolysis of the rubber until fragments pass through the outlet during flushing.

Component substitution

Soluble acid fibers in millable rubber

A continuous, water-soluble polyacrylic acid fiber mat replaces the acidic powder. Two sheets of millable polyester rubber enclose the mat, with trimmed sheet edges exposing the fibers to water. Water dissolves the fibers along the exposed edges, leaving channels that carry the acidic solution into contact with the rubber and promote ester hydrolysis.

Acid delivery through molded seal channels

An aqueous citric acid solution replaces the acidic powder and resides in a separate refillable cartridge. A molded millable polyester rubber seal has blind channels on its wet face and a continuous sealing land around its perimeter. A metering pump fills the channels after the sealing interval, bringing acidic liquid into contact with the channel walls to promote ester hydrolysis.

Parameter or scale variation

Seal discs with graded thickness

Three seal discs share a 25 mm diameter and have thicknesses of 1, 2, and 4 mm. Each disc contains 60 parts by mass of powdered citric acid per 100 parts by mass of millable polyester rubber. A holder clamps each disc at its rim and exposes both faces to water at 40 °C. The different thicknesses set different distances from the wetted faces to the disc center.

Combination with existing systems

Washout seal in a filter housing

A removable basket strainer has an annular gasket molded from millable polyester rubber containing 50 parts by mass of powdered citric acid per 100 parts by mass of rubber. The housing cover compresses the gasket into a groove with a flush port and a drain. During service, the flush port circulates warm water through the groove to activate the acid and hydrolyze the rubber. A removable screen in the drain collects gasket fragments as the groove flushes.

Automated or data-driven variant

Automated immersion and leak testing

An immersion fixture holds molded seal coupons made from millable polyester rubber containing 50 parts by mass of powdered citric acid per 100 parts by mass of rubber. A controller maintains the bath at 40 °C and periodically applies a 50 kPa pressure difference across each coupon. Flow and pressure sensors record the first sustained leak, and a camera records the onset of fragmentation after the controller vents the fixture.

Specific version of a part

Millable adipate polyester rubber

A polyester polyurethane gum contains soft segments derived from adipic acid and 1,4-butanediol. A two-roll mill disperses the accelerator in the gum, and the compound is compression molded and cured. Water cleaves ester bonds in the adipate segments.

Millable caprolactone polyester rubber

A millable polyurethane gum incorporates polycaprolactone diol as its polyester soft segment. A two-roll mill disperses the accelerator before molding and curing. Water cleaves ester bonds along the caprolactone segments.

Dispersed citric acid powder

Dry citric acid particles with diameters of 25 to 75 micrometers are dispersed through the rubber during milling. The particles dissolve as water enters the member and release hydrogen ions that catalyze ester hydrolysis.

Fifty parts citric acid

The mill blends 50 grams of dry citric acid powder into each 100 grams of the degradable rubber component. Water entering the molded member dissolves the distributed powder and acidifies the absorbed water.

Section 3 · quoted from USPTO records

Other work

Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.

Document AUS 7,105,623 B2
Published
Sep 12, 2006
Filed
Jun 2, 2004
Document BUS 2021/0198494 A1
Published
Jul 1, 2021
Filed
Jul 11, 2019
Class
C09D 1/04
Claim 1
Document A
Document B
1.1a degradable rubber component including a millable rubber material composed of hydrolyzable rubber molecules; and
Such polyurethanes can have rubber elasticity and wear resistance and strength, and can be millable. Polyol telechelics of low crystallizability, such as those having linear or branched side chains and those formed by random copolymerization (e.g, polyol polyethers, polyol polyesters, polyol polyetheresters, and others as disclosed herein), can be used to form such polyurethanes.
A · US 7,105,623 B2 · ¶ 266
1.2an acidic hydrolysis accelerator that is a powder exhibiting acidic properties upon contact with water and that accelerates hydrolysis of the rubber molecules upon contact with water,
In one embodiment, the alkoxysilane compound can be hydrolyzed by contacting an alkoxysilane with a weak acid.
B · US 2021/0198494 A1 · ¶ 35
1.3wherein the acidic hydrolysis accelerator is contained at a content of 40 parts by mass or more with respect to 100 parts by mass of the degradable rubber component.

An empty cell means only that no passage was reproduced there.

Why these two documents?

Only Document A has a passage for 1.1. Only Document B has a passage for 1.2.

Additional background

Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.

The components of the compositions can be saturated, i.e., substantially free of double or triple carbon-carbon bonds or aromatic groups, to produce light stable compositions.
A · US 7,105,623 B2 · ¶ 2
Components that are unsaturated or partially saturated can also be used.
A · US 7,105,623 B2 · ¶ 2
In some embodiments, the surface can be treated to make it easier to be cleaned.
B · US 2021/0198494 A1 · ¶ 2
It can be desirable to have a thick layer of the coating, because with use and cleaning, the coating layer can be diminished in thickness, leaving the substrate surface no longer modified and/or protected.
B · US 2021/0198494 A1 · ¶ 2
Cite aspatent.fyi, US 2026/0365849 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365849/, SHA-256 12766879402af0b7d5c069bf27d7323a1d5728f81da880ebe30c9ac3466bc381
First published
Permanent addresshttps://patent.fyi/US20260365849/
Content fingerprint (SHA-256)12766879402af0b7d5c069bf27d7323a1d5728f81da880ebe30c9ac3466bc381
Methodv2026-11-18.2 · automated, not reviewed by a person
Correctionscorrections@patent.fyi