Questions about how individual parts of claim 1 might be changed. A question may describe something different from what the claim language recites, or a version of it; no view is offered on which.
1.2Polyamide shell replacing polyurethane coating
What ifWhat if the outer composition uses a semicrystalline aliphatic polyamide rather than a thermoplastic polyurethane?
A soft thermoplastic polyurethane core granule passes through a co-extrusion die or fluidized-bed coater that applies a 20 to 80 micrometer layer of a semicrystalline aliphatic polyamide with a melting point between 170 and 190 degrees Celsius. Hydrogen bonding between amide groups in the shell and urethane groups at the core surface promotes interfacial adhesion without urethane linkages in the outer layer. The rigid polyamide shell blocks tackiness during storage and melts during injection molding to disperse into the matrix.
1.4Separate granules in a dry blend
What ifWhat if composition (A) and composition (B) are formed as separate uncoated granules combined in a dry blend?
Claim language“at least partly covered with the composition (B)”
Soft polyurethane pellets of composition (A) are tumbled with 0.2 to 0.8 weight percent precipitated silica powder to prevent agglomeration in storage bags and feed hoppers. Separate pellets of composition (B) are metered gravimetrically into the same extruder throat at the target mass ratio. High-shear mixing inside a twin-screw or barrier-screw barrel homogenizes both molten streams prior to molding.
1.5Cyclic carbonate and diamine synthesis
What ifWhat if the core polymer is synthesized from a bis-cyclic carbonate and a polyether diamine with no diisocyanate or diol?
Claim language“a diisocyanate (I-A), a diol (D-A)”
A five-membered bis-cyclic carbonate monomer reacts with an aliphatic polyether diamine having a number-average molecular weight of 1000 to 2000 grams per mole at 80 to 120 degrees Celsius. Ring-opening polyaddition forms urethane linkages with pendant primary and secondary hydroxyl groups along the backbone. The resulting polyhydroxyurethane exhibits elastomeric flexibility while providing pendant hydroxyl sites that promote adhesion to the outer layer.
1.7Completely distinct monomer sets with compatibilizer
What ifWhat if the two polyurethanes share no monomers and rely on a reactive tie polymer for interfacial bonding?
Claim language“are at least partly the same”
The core polyurethane is synthesized from an aliphatic diisocyanate, a polycarbonate diol, and 1,6-hexanediol, while the shell polyurethane is synthesized from an aromatic diisocyanate, a polyether diol, and 1,4-butanediol. A 1 to 3 weight percent maleic-anhydride-grafted styrene-ethylene-butylene-styrene compatibilizer is compounded into the shell melt prior to coating. During co-extrusion at 195 to 210 degrees Celsius, the anhydride groups react with terminal hydroxyl or urethane nitrogen sites across the boundary to lock the two dissimilar phases together.
1.8Higher-hardness core with chemical blowing agent
What ifWhat if composition (A) has a type A durometer hardness between 85 and 95 and includes a chemical blowing agent?
Claim language“is less than 80”
The core polyurethane is formulated with a higher hard-segment fraction to give a type A durometer hardness of 85 to 95 and compounded with 1 to 2 weight percent endothermic citric-acid and sodium-bicarbonate blowing agent. Because the core is firmer, the granules resist deformation under silo weight during storage. During injection molding at 190 to 205 degrees Celsius, gas release creates a closed-cell microcellular foam structure that lowers the effective compressive modulus of the finished part to match that of a softer solid elastomer.
Section 2 · machine-generated
Variations
Further arrangements of the same subject matter, described here as of the publication date at the foot of this page.
Other field of use
Acoustic damping granules for automotive interior cavities
Core-shell thermoplastic polyurethane particles are poured into hollow structural cavities of vehicle door panels and floor pillars to attenuate low-frequency vibration and airborne noise. Each particle contains a soft polyester-based polyurethane core with a type A durometer hardness of 45 to 65 encased in a harder thermoplastic polyurethane shell with a type D durometer hardness of 40 to 50 that shares an aromatic diisocyanate building block with the core. The rigid outer shell prevents individual granules from tacking together during pneumatic conveying into narrow cavity ports and maintains free-flowing bulk packing under elevated cabin temperatures up to 85 degrees Celsius. Once packed inside the sealed cavity, the soft cores deform under acoustic pressure waves and convert mechanical vibration energy into heat through viscoelastic hysteresis.
Free-flowing hot-melt adhesive pellets for automated dispensing
Core-shell polyurethane particles serve as non-blocking hot-melt adhesive feedstock for automated bulk melters in textile lamination and bookbinding lines. The soft core consists of a low-melting, tackified polyester polyurethane with a type A durometer hardness of 40 and a melt initiation temperature of 95 degrees Celsius, while the outer shell consists of a crystalline polyurethane with a type D durometer hardness of 45 and a melt temperature of 130 degrees Celsius sharing the same aromatic diisocyanate. Because the hard shell remains solid and dry during storage and vacuum transfer through uncooled flexible hoses, the adhesive pellets do not bridge or fuse inside feed hoppers. When the pellets enter the heated manifold of the dispensing gun at 155 degrees Celsius, both phases melt and blend through a static mixer into a uniform structural adhesive bead.
Component substitution
Polycarbonate diol shell with bio-derived polyester core
The core polyurethane is synthesized from a bio-derived sebacic acid polyester diol, a cycloaliphatic diisocyanate, and a short-chain diamine chain extender to yield an elastomeric core with a type A durometer hardness near 60. The surrounding shell polyurethane replaces a conventional polyether or polyester soft segment with a polycarbonate diol of 2000 grams per mole molecular weight reacted with the same cycloaliphatic diisocyanate to reach a type D durometer hardness of 48. Sharing the cycloaliphatic diisocyanate across both phases promotes covalent and hydrogen-bond adhesion at the core-shell interface during co-extrusion without an intermediate tie layer. The polycarbonate diol shell provides hydrolytic stability and abrasion resistance during wet underwater pelletizing and long-term humid storage.
Parameter or scale variation
Sub-millimeter core-shell powders for laser sintering
The encapsulated polyurethane architecture is scaled down from multi-millimeter pellets to spherical microparticles having a median diameter between 60 and 120 micrometers for powder-bed fusion additive manufacturing. Each microparticle comprises a soft aliphatic polyurethane core with a type A durometer hardness of 55 surrounded by a continuous harder polyurethane shell of 5 to 15 micrometers thickness and a type D durometer hardness of 38, both incorporating hexamethylene diisocyanate. The microparticles are produced by cryogenic grinding of co-extruded strands followed by thermal spheroidization in a heated nitrogen column at 175 degrees Celsius, or by dual-nozzle spray drying from immiscible solvent streams. During powder-bed recoating, the harder outer shell lowers interparticle cohesion so a roller spreads uniform 100-micrometer layers without clumping before selective infrared laser melting fuses the core and shell into a monolithic elastomer part.
Combination with existing systems
Inline co-extrusion encapsulation coupled with underwater pelletizing
Two twin-screw extruders feed a concentric crosshead die mounted directly upstream of a pressurized underwater pelletizer with rotating cutting blades. The primary extruder melts the soft core polyurethane at 170 degrees Celsius and forces it through an inner circular orifice, while the secondary extruder meters the harder shell polyurethane at 205 degrees Celsius through an annular channel around the core melt stream. Both polymer streams share a diphenylmethane diisocyanate component so the concentric interface bonds rapidly inside the die land before exiting through a heated die plate into a 35 degrees Celsius water chamber. The rotating knives slice the concentric melt into 3-millimeter cylindrical granules and the circulating water quenches the hard outer shell immediately, allowing pneumatic drying and direct transfer into gravimetric injection-molding hoppers.
Automated or data-driven variant
Closed-loop shell thickness control using optical coherence tomography
An inline optical coherence tomography sensor positioned downstream of the co-extrusion die continuously measures the radial shell thickness and core concentricity of the encapsulated polyurethane strand at 200 scans per second. A refractive index contrast between the soft core and harder shell produces distinct subsurface reflection peaks that a real-time signal processor converts into wall-thickness profiles around the strand circumference. A model predictive controller compares the measured thickness distribution against a target setpoint of 150 micrometers and adjusts the shell extruder screw speed and melt gear pump pressure to correct drift within two seconds. Simultaneously, a heated thermal-die-bolt actuator array shifts local melt viscosity around the annular die gap to center the core whenever eccentricity exceeds 5 percent of the strand diameter.
Composition (A) consists of a polyester-based thermoplastic polyurethane synthesized from poly(butylene adipate) diol with a number-average molecular weight of 2000 grams per mole, 4,4'-methylene diphenyl diisocyanate, and 1,4-butanediol. The polymer is compounded with 15 to 25 weight percent phthalate-free benzoate ester plasticizer and 0.5 weight percent hindered phenolic antioxidant. This formulation yields an elastomeric core with a type A durometer hardness between 55 and 65 and a melt flow index of 20 to 35 grams per 10 minutes at 190 degrees Celsius under a 2.16 kilogram load.
Two single-screw extruders feed molten composition (A) and molten composition (B) into a concentric annular co-extrusion die at melt temperatures of 185 and 205 degrees Celsius, respectively. The die forms a continuous core-shell strand in which composition (B) envelops the radial perimeter of composition (A) at a shell thickness of 50 to 150 micrometers, leaving the cut end faces exposed after underwater rotary knife pelletizing. Rapid water quenching at 35 to 45 degrees Celsius solidifies the outer shell before the cylindrical granules contact one another in the centrifugal dryer.
The outer thermoplastic polyurethane (PU-B) is polymerized in a twin-screw reactive extruder from 4,4'-methylene diphenyl diisocyanate, polytetramethylene ether glycol having a molecular weight of 1000 grams per mole, and 1,4-butanediol as the chain extender at an isocyanate index of 1.01. Maintaining a hard-segment mass fraction of 55 to 65 percent produces a semicrystalline polyurethane with a type D durometer hardness of 50 to 60 and a melting endotherm peak between 175 and 195 degrees Celsius. The high hard-segment content provides rapid crystallization upon cooling and low surface tack.
Shared aromatic diisocyanate and short-chain diol
Both the core polyurethane (PU-A) and the shell polyurethane (PU-B) incorporate 4,4'-methylene diphenyl diisocyanate as the diisocyanate component and 1,4-butanediol as the chain extender, while varying the soft-segment macrodiol content and molar ratio. In the core polymer, the molar ratio of 1,4-butanediol to macrodiol is 1.5 to 1, whereas in the shell polymer the ratio is increased to 6.0 to 1. Matching the hard-segment chemical structure allows urethane domains to co-crystallize across the core-shell interface during co-extrusion and subsequent molding.
Section 3 · quoted from USPTO records
Other work
Passages reproduced word for word from two earlier-published U.S. patent documents, placed beside the language of claim 1. No characterization is offered. Each passage is marked A or B for the document it comes from; ¶ numbers are the paragraph numbers in the USPTO’s published full text of that document.
1.1a composition (A) comprising a thermoplastic polyurethane (PU-A); and
Unless indicated otherwise, the following information refers to the polyurethanes and the components used for forming them and also to the polyurethanes PU-E and to the thermoplastic polyurethanes PU-1 and PU-2.
A · US 2012/0088889 A1 · ¶ 30
The bottom substrate was a 0.30 mm (12 mil) thick sheet of thermoplastic polyurethane made from TECOFLEX CLA 93A-V.
B · US 8,551,285 B2 · ¶ 105
1.2a composition (B) comprising a thermoplastic polyurethane (PU-B);
A 2-part polyurethane composition was prepared by mixing 6 grams of DESMODUR N3300 with 7.6 grams K-FLEX 188 polyol and 2 drops of dibutyltin dilaurate.
B · US 8,551,285 B2 · ¶ 105
1.3wherein:
1.4the composition (A) is at least partly covered with the composition (B);
1.5the thermoplastic polyurethane (PU-A) is a reaction product of the following building components: a diisocyanate (I-A), a diol (D-A), and optionally a chain extender (CE-A);
The isocyanates (a), the compounds (b) which are reactive toward isocyanate and, if used, the chain extenders (c) are also referred to as formative components. a) As organic isocyanates (a), it is possible to use generally known isocyanates, preferably aromatic, aliphatic, cycloaliphatic and/or araliphatic isocyanates, more preferably diisocyanates, preferably diphenylmethane 2,2′-, 2,4′- and/or 4,4′-diisocyanate (MDI), naphthylene 1,5-diisocyanate (NDI), tolylene 2,4- and/or
A · US 2012/0088889 A1 · ¶ 32
Step (ii) comprises introducing components comprising a diisocyanate and a diol into an extruder to provide a molten thermoplastic polyurethane; extruding the molten thermoplastic polyurethane through a die onto a third substrate; passing at least the third substrate and the extruded molten thermoplastic polyurethane through a nip to provide a layer of thermoplastic polyurethane on a substrate; and solidifying the thermoplastic polyurethane.
B · US 8,551,285 B2 · ¶ 79
1.6the thermoplastic polyurethane (PU-B) is a reaction product of the following building components: a diisocyanate (I-B), a diol (D-B), and optionally a chain extender (CE-B),
In some embodiments, said at least partially crosslinked polyurethane is the reaction product of a polyol and at least a diisocyanate, and said polyol is a polyester polyol, a polycarbonate polyol or a combination of both.
B · US 8,551,285 B2 · ¶ 28
1.7at least one of the building components of the thermoplastic polyurethane (PU-A) and at least one of building components of the thermoplastic polyurethane (PU-B) are at least partly the same;
PU-1.1 is a mixture of a polyester polyurethane based on 10.1% of MDI monomer, 0.7% of 1,4-butanediol and 59.3% of a polyester diol (butanediol-ethylene glycol-adipic acid with a 1:1 mixing ratio of the components butanediol/ethylene glycol) having a molecular weight of 2 kg/mol and a further high molecular weight polyurethane based on MDI, 1,4-butanediol and a polyester diol (butanediol-adipic acid) having a molecular weight of 2.5 kg/mol and 1% of polymeric carbodiimides as
A · US 2012/0088889 A1 · ¶ 77
1.8a Shore A hardness of the composition (A) measured according to DINISO 7619-1 (2016) is less than 80; and
1.9a Shore D hardness of the composition (B) measured according to DINISO 7619-1 (2016) is more than 30.
An empty cell means only that no passage was reproduced there.
Why these two documents?
Only Document A has a passage for 1.7. Only Document B has a passage for 1.21.6. Both have a passage for 1.11.5.
Additional background
Sentences reproduced word for word from these documents that state a problem, a purpose or benefit, a field of use, or an application or improvement.
To improve the property profile of TPU, the literature discloses introducing crosslinks into the TPU which lead to an increase in the strengths, an improvement in the heat distortion resistance, a reduction in tensile set and compression set, and an improvement in resistance to media of all types, rebound resilience and creep behavior.
A · US 2012/0088889 A1 · ¶ 3
Related claim parts: 1.21.6
A disadvantage of the known thermoplastic polyurethanes for particular applications is their mechanical properties, particularly in respect of compression set and the bending angle.
A · US 2012/0088889 A1 · ¶ 5
It was an object of the invention to provide polyurethanes which have improved mechanical properties.
A · US 2012/0088889 A1 · ¶ 6
Cite aspatent.fyi, US 2026/0365850 A1, claim 1, first published 2026-11-23T17:22:55-05:00, https://patent.fyi/US20260365850/, SHA-256 8038c0bf0a8857e0943e69cce1984913d6a97301057d6969e5b1bb42a4657c09